C22C45/02
FE-BASED NANOCRYSTALLINE ALLOY AND ELECTRONIC COMPONENT USING THE SAME
An Fe-based nanocrystalline alloy is represented by Composition Formula, (Fe.sub.(1-a)M.sup.1a).sub.100-b-c-d-e-gM.sup.2.sub.bB.sub.cP.sub.dCu.sub.eM.sup.3.sub.g, where M.sup.1 is at least one element selected from the group consisting of Co and Ni, M.sup.2 is at least one element selected from the group consisting of Nb, Mo, Zr, Ta, W, Hf, Ti, V, Cr, and Mn, M.sup.3 is at least two elements selected from the group consisting of C, Si, Al, Ga, and Ge but necessarily includes C, and 0≤a≤0.5, 1.5<b≤3, 10≤c≤13, 0<d≤4, 0<e≤1.5, and 8.5≤g≤12.
AMORPHOUS METAL FOAM AND METHOD FOR PRODUCING SAME
An aspect of the present disclosure provides an amorphous metal porous body that is a metal porous body including pores, the amorphous metal porous body including: powder particle connection bodies in which at least portions of amorphous alloy powder particles adjacent to each other are connected in a network structure; and a plurality of pores provided between the powder particle connection bodies.
AMORPHOUS METAL FOAM AND METHOD FOR PRODUCING SAME
An aspect of the present disclosure provides an amorphous metal porous body that is a metal porous body including pores, the amorphous metal porous body including: powder particle connection bodies in which at least portions of amorphous alloy powder particles adjacent to each other are connected in a network structure; and a plurality of pores provided between the powder particle connection bodies.
Amorphous metal foil and method for producing an amorphous metal foil using a rapid solidification technology
Amorphous metal foil and method for the production of an amorphous metal foil using a rapid solidification technology is provided. An amorphous metal foil having a width of 2 mm to 300 mm, a thickness of less than 20 μm and a maximum of 50 holes per square metre is also provided.
Amorphous metal foil and method for producing an amorphous metal foil using a rapid solidification technology
Amorphous metal foil and method for the production of an amorphous metal foil using a rapid solidification technology is provided. An amorphous metal foil having a width of 2 mm to 300 mm, a thickness of less than 20 μm and a maximum of 50 holes per square metre is also provided.
Fe-Ni Nanocomposite Alloys
A nanocomposite comprising crystalline grains in an amorphous matrix, the crystalline grains comprising an iron (Fe)-nickel (Ni) compound and being separated from one another by the amorphous matrix; and one or more barriers between the crystalline grains and the amorphous matrix, the barriers being configured to inhibit growth of the crystalline grains during forming of the crystalline grains, a barrier of the one or more barriers being between a crystalline grain and the amorphous matrix; wherein the amorphous matrix comprises an increased resistivity relative to a resistivity of the crystalline grains; and wherein the amorphous matrix is configured to reduce losses of the crystalline grains caused by a change in a magnetic field applied to the crystalline grains relative to losses of the crystalline grains that occur without the amorphous matrix.
Iron alloy particle and method for producing iron alloy particle
The iron alloy particle is a particle including an iron alloy. The particle includes multiple mixed-phase particles, each including nanocrystals of 10 nm or more and 100 nm or less (i.e., from 10 nm to 100 nm) in crystallite size and an amorphous phase; and a grain boundary layer between the mixed-phase particles. Also, the iron alloy has a composition containing Fe, Si, P, B, C, and Cu.
Iron alloy particle and method for producing iron alloy particle
The iron alloy particle is a particle including an iron alloy. The particle includes multiple mixed-phase particles, each including nanocrystals of 10 nm or more and 100 nm or less (i.e., from 10 nm to 100 nm) in crystallite size and an amorphous phase; and a grain boundary layer between the mixed-phase particles. Also, the iron alloy has a composition containing Fe, Si, P, B, C, and Cu.
Fe-based soft magnetic alloy and method for manufacturing the same
The present disclosure relates to an iron (Fe)-based amorphous soft magnetic alloy and a method for manufacturing the soft magnetic alloy. According to the present disclosure, there is provided an Fe-based soft magnetic alloy including C and S meeting 1≥a+b≥6, wherein a is an atomic % content of C and b is an atomic % content of S, B meeting 4.5≥x≥13.0, wherein x is an atomic % content of B, Cu meeting 0.2≥y≥1.5, wherein y is an atomic % content of Cu, Al meeting 0.5≥z≥2, wherein z is an atomic % content of Al, and a remaining atomic % content of Fe and other inevitable impurities, wherein the Fe-based soft magnetic alloy includes a micro-structure, and wherein the micro-structure includes a crystalline phase with a mean crystalline grain size ranging from 15 nm to 50 nm in an amorphous base.
Fe-based soft magnetic alloy and method for manufacturing the same
The present disclosure relates to an iron (Fe)-based amorphous soft magnetic alloy and a method for manufacturing the soft magnetic alloy. According to the present disclosure, there is provided an Fe-based soft magnetic alloy including C and S meeting 1≥a+b≥6, wherein a is an atomic % content of C and b is an atomic % content of S, B meeting 4.5≥x≥13.0, wherein x is an atomic % content of B, Cu meeting 0.2≥y≥1.5, wherein y is an atomic % content of Cu, Al meeting 0.5≥z≥2, wherein z is an atomic % content of Al, and a remaining atomic % content of Fe and other inevitable impurities, wherein the Fe-based soft magnetic alloy includes a micro-structure, and wherein the micro-structure includes a crystalline phase with a mean crystalline grain size ranging from 15 nm to 50 nm in an amorphous base.