Patent classifications
C22C2200/04
Additively manufacturing of amorphous structures
An additive manufacturing system configured to additively build an article can include an energy applicator, a build platform, and a powder nozzle configured to eject powder toward the build platform to be acted on by the energy applicator. The system can include a control module configured to control the energy applicator to create an amorphous structure forming at least a portion of the article.
PLURALITY OF FLAKY MAGNETIC METAL PARTICLES, PRESSED POWDER MATERIAL, AND ROTATING ELECTRIC MACHINE
Flaky magnetic metal particles of embodiments each have a flat surface and a magnetic metal phase containing iron (Fe), cobalt (Co), and silicon (Si). An amount of Co is from 0.001 at% to 80 at% with respect to the total amount of Fe and Co. An amount of Si is from 0.001 at% to 30 at% with respect to the total amount of the magnetic metal phase. The flaky magnetic metal particles have an average thickness of from 10 nm to 100 .Math.m. An average value of the ratio of the average length in the flat surface with respect to a thickness in each of the flaky magnetic metal particles is from 5 to 10,000. The flaky magnetic metal particles have the difference in coercivity on the basis of direction within the flat surface.
DEVICE AND METHOD FOR THE PRODUCTION OF A METALLIC STRIP
A device for the production of a metallic strip using a rapid solidification technology is provided. The device includes a movable heat sink with an external surface onto which a melt is poured and on which the melt solidifies to produce the strip, and which device includes a rolling device which can be pressed against the external surface of the movable heat sink while the heat sink is in motion.
Soft magnetic powder, Fe-based nanocrystalline alloy powder, magnetic component and dust core
This soft magnetic powder is represented by composition formula Fe.sub.aSi.sub.bB.sub.cP.sub.dCu.sub.e with the exception of unavoidable impurities. In the composition formula, a, b, c, d and e satisfy 79≤a≤84.5 at %, 0≤b<6 at %, 4≤c≤10 at %, 4<d≤11 at %, 0.2≤e<0.4 at %, and a+b+c+d+e=100 at %.
HEAT TREATMENT METHOD FOR AMORPHOUS ALLOY RIBBON AND HEAT TREATMENT APPARATUS FOR AMORPHOUS ALLOY RIBBON
The present invention provides a heat treatment method and a heat treatment apparatus for an amorphous alloy ribbon, said method and apparatus being capable of uniformly heat treating an amorphous alloy ribbon, while suppressing the occurrence of anisotropy in the magnetic characteristics. A heat treatment method for an amorphous alloy ribbon, said method comprising a step wherein an amorphous alloy ribbon is transferred, while being in contact with a heated projected surface, and the amorphous alloy ribbon is transferred, while having the part that is in contact with the projected surface pressed against the projected surface from a surface which is on the reverse side of the surface that is in contact with the projected surface.
Soft magnetic alloy, magnetic core, magnetic component, and electronic device
The present invention provides a soft magnetic alloy having good soft magnetic properties. The soft magnetic alloy includes nanocrystals having an average Heywood diameter value of 5.0 nm or more and 25.0 nm or less, in which an average circularity of the nanocrystals is 0.50 or more and 0.90 or less.
Device and method for the production of a metallic strip
A device for the production of a metallic strip using a rapid solidification technology is provided. The device includes a movable heat sink with an external surface onto which a melt is poured and on which the melt solidifies to produce the strip, and which device includes a rolling device which can be pressed against the external surface of the movable heat sink while the heat sink is in motion.
Magnetic material and method for producing same
The purpose of the present invention is to provide: a new magnetic material which exhibits high magnetic stability and excellent oxidation resistance and which can achieve both significantly higher saturation magnetization and lower coercive force than a conventional ferrite-based magnetic material by using a magnetic material obtained by nanodispersing α-(Fe,M) phases and M component-enriched phases (here, the M component is at least one component selected from among Zr, Hf, V, Nb, Ta, Cr, Mo, W, Cu, Zn and Si); and a method for producing same. This magnetic material powder exhibits high moldability, and is such that α-(Fe, M) phases and M-enriched phases are nanodispersed by chemically reducing M-ferrite nanoparticles, which are obtained by means of wet synthesis, in hydrogen and utilizing phase separation by means of a disproportionation reaction while simultaneously carrying out grain growth. Furthermore, a solid magnetic material is obtained by sintering this powder.
Magnetic material and method for producing same
The purpose of the present invention is to provide: a new magnetic material which exhibits high magnetic stability and excellent oxidation resistance and which can achieve both significantly higher saturation magnetization and lower coercive force than a conventional ferrite-based magnetic material by using a magnetic material obtained by nanodispersing α-(Fe,M) phases and M component-enriched phases (here, the M component is at least one component selected from among Zr, Hf, V, Nb, Ta, Cr, Mo, W, Cu, Zn and Si); and a method for producing same. This magnetic material powder exhibits high moldability, and is such that α-(Fe, M) phases and M-enriched phases are nanodispersed by chemically reducing M-ferrite nanoparticles, which are obtained by means of wet synthesis, in hydrogen and utilizing phase separation by means of a disproportionation reaction while simultaneously carrying out grain growth. Furthermore, a solid magnetic material is obtained by sintering this powder.
SOFT MAGNETIC POWDER, POWDER MAGNETIC CORE, MAGNETIC ELEMENT, AND ELECTRONIC DEVICE
A soft magnetic powder including particles having a composition represented by Fe.sub.xCu.sub.aNb.sub.b(Si.sub.1-yB.sub.y).sub.100-x-a-b [provided that a, b, and x are each a number whose unit is at % and satisfy 0.3≤a≤2.0, 2.0≤b≤4.0, and 73.0≤x≤79.5, respectively, and y is a number satisfying f(x)≤y≤0.99, in which f(x)=(4×10.sup.−34)x.sup.17.56], wherein the particle contains a crystal grain having a grain diameter of 1.0 nm or more and 30.0 nm or less, and includes a Cu segregated portion in which Cu is segregated, the Cu segregated portion is present at a position deeper than 30 nm from a surface of the particle, and a maximum Cu concentration in the Cu segregated portion exceeds 6.0 at %.