C22F1/002
Copper alloy for electronic and electrical equipment, copper alloy plate strip for electronic and electrical equipment, component for electronic and electrical equipment, terminal, busbar, and movable piece for relay
Provided is a copper alloy for electronic and electrical equipment including: 0.15 mass % or greater and less than 0.35 mass % of Mg; 0.0005 mass % or greater and less than 0.01 mass % of P; and a remainder which is formed of Cu and unavoidable impurities, in which a conductivity is greater than 75% IACS, and an average number of compounds containing Mg and P with a particle diameter of 0.1 μm or greater is 0.5 pieces/μm.sup.2 or less in observation using a scanning electron microscope.
METHOD FOR FINISHING A WORKPIECE MADE BY ADDITIVE MANUFACTURING
According to the invention, a metal workpiece made by additive manufacturing is subjected, following the additive manufacturing process, to a cold treatment in which the workpiece is cooled to a lower target temperature of less than minus 30° C. in a cooling phase and is then heated up to an upper target temperature in a heating phase. The cold treatment significantly improves the properties of the workpiece in respect of the mechanical quality thereof.
STRIP OF A COBALT IRON ALLOY, LAMINATED CORE AND METHOD OF PRODUCING A STRIP OF A COBALT IRON ALLOY
A method of producing a strip from a CoFe alloy is provided. A slab consisting substantially of 35 wt %≤Co≤55 wt %, 0 wt %≤V≤3 wt %, 0 wt %≤Ni≤2 wt %, 0 wt %≤Nb≤0.50 wt %, 0 wt %≤Zr+Ta≤1.5 wt %, 0 wt %≤Cr≤3 wt %, 0 wt %≤Si≤3 wt %, 0 wt %≤Al≤1 wt %, 0 wt %≤Mn≤1 wt %, 0 wt %≤B≤0.25 wt %, 0 wt %≤C≤0.1 wt %, the remainder being Fe and up to 1 wt % of impurities, is hot rolled and then quenched from a temperature above 700° C. to less than 200° C. The hot rolled strip is cold rolled. The cold rolled strip is stationary annealed to produce an intermediate strip, and the intermediate strip is continuously annealed.
Alloys and methods of forming same
In one aspect of the invention, an alloy includes a first element comprising magnesium (Mg), titanium (Ti), zirconium (Zr), chromium (Cr), or nickelaluminum (NiAl), a second element comprising lithium (Li), calcium (Ca), manganese (Mn), aluminum (Al), or a combination thereof, and a third element comprising zinc (Zn). According to the invention, nanoscale precipitates is produced in the magnesium alloy by additions of zinc and specific heat-treatment. These precipitates lower the energy for dislocation movements and increase the number of available slip systems in the magnesium alloy at room temperature and hence improve ductility and formability of the magnesium alloy.
Steel sheet for hot press formed member having excellent coating adhesion and manufacturing method for the same
Provided is a steel sheet for a hot press formed member having excellent coating adhesion, and a method for manufacturing the same. A steel sheet for hot press forming is an aluminum alloy plated steel sheet, wherein an average Fe content in a plating layer may be 40 wt % or more, and a concentration gradient of a section having a Fe content of 45 wt % to 80 wt % in the plating layer may 7 wt %/μm or less of a concentration gradient at a section having an Fe content of 45% to 80% in the plating layer in a thickness direction from a surface of the plating layer according to a result of GDS analysis.
Thermal shock synthesis of multielement nanoparticles
A formation of multielement nanoparticles is disclosed that includes at least three elements. Each of the at least three elements is uniformly distributed within the multielement nanoparticles forming nanoparticles having a homogeneous mixing structure. At least five elements may form a high-entropy nanoparticle structure. A method for manufacturing a formation of multielement nanoparticles includes providing a precursor material composed of the at least three component elements in multielement nanoparticles; heating the precursor material to a temperature and a time; and quenching the precursor to a temperature at a cooling rate to result in a formation of multielement nanoparticles containing at least three elements and the heating and the quenching representing a multielement nanoparticle thermal shock formation process. A corresponding system for manufacturing the formation of multielement nanoparticles and a method of using the multielement nanoparticles are also disclosed.
Method for cooling a metallic item and cooling bar
The invention relates to a method for cooling a metallic item (1) by discharging a cooling medium from a cooling bar (2) onto the item (1), wherein the cooling medium is discharged through a slot (3) in the cooling bar (2). According to the invention, in order to achieve improved cooling, during the cooling process the width (B) of the slot (3) in the conveying direction (F) of the item (1) or of the cooling bar (2) is altered in order to bring the cooling power of the cooling medium to a desired or predefined level by open-loop or closed-loop control. In addition, the invention relates to a cooling bar.
ALUMINUM ALLOY, ALUMINUM ALLOY WIRE, AND METHOD FOR PRODUCING ALUMINUM ALLOY
An aluminum alloy having a composition including 0.1% by mass or more and 2.8% by mass or less of Fe; and 0.002% by mass or more and 2% by mass or less of Nd.
QUENCHING A COMPONENT
The invention relates to a component in the form of a wheel comprising: a hub portion, a rim portion with an outer rim flange and an inner rim flange, a plurality of circumferentially distributed spokes extending between the hub portion and the rim portion, wherein the spokes and the hub portion are arranged offset with respect to a wheel center plane towards the outer rim flange and have an inner side facing the wheel center plane and an outer side directed away from the wheel center plane, wherein the outer rim flange has greater tensile residual stresses at least in a partial region than at least a partial region of the inner rim flange.
Alloy article, method for manufacturing said alloy article, product formed of said alloy article, and fluid machine having said product
An object of the invention is to provide an alloy article that exhibits even better mechanical properties than conventional high entropy alloy articles without sacrificing high corrosion resistance thereof. An alloy article according to the invention comprises matrix phase crystal grains being equiaxed crystals with an average crystal grain size of 150 μm or less, the alloy article having a metallic composition including: Co, Cr, Fe, Ni and Ti, each within a range of 5 atomic % or more and 35 atomic % or less; Mo within a range of more than 0 atomic % and less than 8 atomic %; and a balance comprising inevitable impurities, wherein in the matrix phase crystal grains, ultrafine particles with an average particle size of 100 nm or less and oxide particles with an average particle size of 100 nm or less are dispersedly precipitated.