Patent classifications
C23C24/02
POWDER SHERARDIZING AGENT, ANTI-CORROSION METAL PART, AND SHERARDIZING METHOD
The disclosure provides a powder sherardizing agent, anti-corrosion metal part and sherardizing method. The powder sherardizing agent in parts by mass includes 20-100 parts of a metal powder, 40-80 parts of a dispersing agent, 0.2-5 parts of decomposing agent. The metal powder includes 60-97 parts of zinc powder and 3-40 parts of magnesium powder. The powder sherardizing agent provided by this disclosure can realize the infiltration of magnesium during the sherardizing process. Zinc and magnesium can form a zinc-magnesium alloy phase with high corrosion resistance, thereby greatly improving the corrosion resistance of the infiltration layer. The sherardizing method provided by this disclosure has the advantages of simple operation, convenient use, low cost, high economic benefit, and wide application range.
Sliding member with carbon transfer layer
A sliding member includes a carbon transfer layer and can superiorly effectively decrease friction and reduce wear. A method produces the sliding member. The sliding member includes a substrate and a carbon transfer layer. The carbon transfer layer is disposed on the surface of the substrate and includes both sp.sup.2 bonded carbon and sp.sup.3 bonded carbon. The carbon transfer layer preferably has a ratio sp.sup.3/(sp.sup.2+sp.sup.3) of the sp.sup.3 bonded carbon to the totality of the sp.sup.2 bonded carbon and the sp.sup.3 bonded carbon of 0.1 or more.
Sliding member with carbon transfer layer
A sliding member includes a carbon transfer layer and can superiorly effectively decrease friction and reduce wear. A method produces the sliding member. The sliding member includes a substrate and a carbon transfer layer. The carbon transfer layer is disposed on the surface of the substrate and includes both sp.sup.2 bonded carbon and sp.sup.3 bonded carbon. The carbon transfer layer preferably has a ratio sp.sup.3/(sp.sup.2+sp.sup.3) of the sp.sup.3 bonded carbon to the totality of the sp.sup.2 bonded carbon and the sp.sup.3 bonded carbon of 0.1 or more.
Method of depositing titania on a substrate and composite article
A method comprises rubbing a powder comprising titanium dioxide particles against a surface of an aluminum substrate to form a layer bonded to the surface of the aluminum substrate. The powder comprises titanium dioxide and is essentially free of organic particles. Composite articles preparable by the method are also disclosed.
Method of depositing titania on a substrate and composite article
A method comprises rubbing a powder comprising titanium dioxide particles against a surface of an aluminum substrate to form a layer bonded to the surface of the aluminum substrate. The powder comprises titanium dioxide and is essentially free of organic particles. Composite articles preparable by the method are also disclosed.
LIGHT WEIGHT COMPONENT WITH INTERNAL REINFORCEMENT AND METHOD OF MAKING
A method of making a light weight component is provided. The method including the steps of: forming a metallic foam core into a desired configuration; applying an external metallic shell to an exterior surface of the metallic foam core after it has been formed into the desired configuration; forming an inlet opening and an outlet opening in the external metallic shell in order to provide a fluid path through the metallic foam core; and injecting a thermoplastic material into the metallic foam core via the inlet opening.
LIGHT WEIGHT COMPONENT WITH INTERNAL REINFORCEMENT AND METHOD OF MAKING
A method of making a light weight component is provided. The method including the steps of: forming a metallic foam core into a desired configuration; applying an external metallic shell to an exterior surface of the metallic foam core after it has been formed into the desired configuration; forming an inlet opening and an outlet opening in the external metallic shell in order to provide a fluid path through the metallic foam core; and injecting a thermoplastic material into the metallic foam core via the inlet opening.
Process of fabricating a shield and process of preparing a component
A process of fabricating a shield, a process of preparing a component, and an erosion shield are disclosed. The process of fabricating the shield includes forming a near-net shape shield. The near-net shape shield includes a nickel-based layer and an erosion-resistant alloy layer. The nickel-based layer is configured to facilitate secure attachment of the near-net shaped to a component. The process of preparing the component includes securing a near-net shape shield to a substrate of a component.
Process of fabricating a shield and process of preparing a component
A process of fabricating a shield, a process of preparing a component, and an erosion shield are disclosed. The process of fabricating the shield includes forming a near-net shape shield. The near-net shape shield includes a nickel-based layer and an erosion-resistant alloy layer. The nickel-based layer is configured to facilitate secure attachment of the near-net shaped to a component. The process of preparing the component includes securing a near-net shape shield to a substrate of a component.
METHOD FOR SOLID STATE ADDITIVE MANUFACTURING
A method for forming an impact weld used in an additive manufacturing process. The method includes providing a wire having a powder filler metal core located within a sheath. The wire is then inserted within a conduit having an opening. Further, the method includes providing at least one energy pulse that interacts with the sheath to pinch off at least one segment of the wire, wherein the energy pulse causes propulsion of the segment toward a substrate with sufficient velocity to form an impact weld for welding the metal core to the substrate. In particular, the energy pulse is an electromagnetic pulse, a laser energy pulse or a high electric current pulse.