C30B23/002
Shielding member and single crystal growth device having the same
A shielding member, wherein the shielding member is formed of at least one of structure which has a non-flat plate shape having an inclined surface, and the inclined surface is located on a side of a substrate support part when the shielding member is disposed in a single crystal growth device, wherein the single crystal growth device comprising: a crystal growth container; a source storage part that is positioned at a lower inner part of the crystal growth container; the substrate support part, wherein the support part is disposed above the source storage part and supports a substrate to make the substrate face the source storage part; and a heating device that is disposed on an outer circumference of the crystal growth container, wherein the shielding member is disposed between the source storage part and the substrate support part, and wherein a single crystal of a source is grown on the substrate by sublimating the source from the source storage part.
METHOD FOR DEPOSITING HIGH QUALITY PVD FILMS
Embodiments described herein include a method for depositing a material layer on a substrate while controlling a bow of the substrate and a surface roughness of the material layer. A bias applied to the substrate while the material layer is deposited is adjusted to control the bow of the substrate. A bombardment process is performed on the material layer to improve the surface roughness of the material layer. The bias and bombardment process improve a uniformity of the material layer and reduce an occurrence of the material layer cracking due to the bow of the substrate.
CRYSTAL GROWTH APPARATUS AND CRYSTAL GROWTH METHOD
A crystal growth apparatus according to the present embodiment includes a crucible, a heater which is installed on an outward side of the crucible and surrounds the crucible, and a coil which is installed on an outward side of the heater and surrounds the heater, in which an inner surface of the heater on the crucible side includes a first region, and a second region which is further away from an outer side surface of the crucible than the first region is.
MBE Growth Method To Enable Temperature Stability
Methods and systems for growing thin films via molecular-beam epitaxy (MBE) on substrates are provided. The methods and systems utilize a thermally conductive backing plate including an infrared-absorbing coating (IAC) formed, for example, on one side of the thermally conductive backing plate to provide an asymmetric emissivity that absorbs infrared radiation (IR) on the side having the IRC and does not on the non-coated side of the thermally conductive backing plate (e.g., refractive metal or alloy). The asymmetric emissivity shields the thin film being deposited on a substrate from the IR during formation.
METHOD FOR PREPARING SILICON CARBIDE WAFER AND SILICON CARBIDE WAFER
A method for preparing a SiC ingot includes: disposing a raw material and a SiC seed crystal facing each other in a reactor having an internal space; subliming the raw material by controlling a temperature, a pressure, and an atmosphere of the internal space; growing the SiC ingot on the seed crystal; and collecting the SiC ingot after cooling the reactor. The wafer prepared from the ingot, which is prepared from the method, generates cracks when an impact is applied to a surface of the wafer, the impact is applied by an external impact source having mechanical energy, and a minimum value of the mechanical energy is 0.194 J to 0.475 J per unit area (cm.sup.2).
NITRIDE SEMICONDUCTOR ELEMENT AND NITRIDE SEMICONDUCTOR ELEMENT PRODUCTION METHOD
A nitride semiconductor light-emitting element 1 contains an AlN layer 22 having a crystalline quality within a predetermined range and an n-type AlGaN formed atop the AlN layer 22 and having a predetermined Al composition ratio formed atop the AlN layer 22. In addition, as the crystalline quality falling within the predetermined range, the AlN layer 22 has a crystalline quality corresponding to an X-ray rocking curve half-width of 350 to 520 (arcsec vis--vis a (10-12) surface. As the predetermined Al composition ratio, the n-type AlGaN has an Al composition ratio of 40% to 70%.
METHODS AND MATERIAL DEPOSITION SYSTEMS FOR FORMING SEMICONDUCTOR LAYERS
Systems and methods for forming semiconductor layers, including oxide-based layers, are disclosed in which a material deposition system has a rotation mechanism that rotates a substrate around a center axis of a substrate deposition plane of the substrate. A material source that supplies a material to the substrate has i) an exit aperture with an exit aperture plane and ii) a predetermined material ejection spatial distribution from the exit aperture plane. The exit aperture is positioned at an orthogonal distance, a lateral distance, and a tilt angle relative to the center axis of the substrate. The system can be configured for either i) minimum values for the orthogonal distance and the lateral distance to achieve a desired layer deposition uniformity using a set tilt angle, or ii) the tilt angle to achieve the desired layer deposition uniformity using a set orthogonal distance and a set lateral distance.
METHODS AND MATERIAL DEPOSITION SYSTEMS FOR FORMING SEMICONDUCTOR LAYERS
Systems and methods for forming semiconductor layers, including oxide-based layers, are disclosed in which a material deposition system has a rotation mechanism that rotates a substrate around a center axis of a substrate deposition plane of the substrate. A material source that supplies a material to the substrate has i) an exit aperture with an exit aperture plane and ii) a predetermined material ejection spatial distribution from the exit aperture plane. The exit aperture is positioned at an orthogonal distance, a lateral distance, and a tilt angle relative to the center axis of the substrate. The system can be configured for either i) minimum values for the orthogonal distance and the lateral distance to achieve a desired layer deposition uniformity using a set tilt angle, or ii) the tilt angle to achieve the desired layer deposition uniformity using a set orthogonal distance and a set lateral distance.
UV-transparent aluminum nitride single crystal having a diameter of 35 mm to 150 mm and a predefined UV transparency metric at a wavelength of 265 nm
In various embodiments, single-crystal aluminum nitride boules and substrates having high transparency to ultraviolet light and low defect density are formed. The single-crystal aluminum nitride may function as a platform for the fabrication of light-emitting devices such as light-emitting diodes and lasers.
Methods and material deposition systems for forming semiconductor layers
Systems and methods for forming semiconductor layers, including oxide-based layers, are disclosed in which a material deposition system has a rotation mechanism that rotates a substrate around a center axis of a substrate deposition plane of the substrate. A material source that supplies a material to the substrate has i) an exit aperture with an exit aperture plane and ii) a predetermined material ejection spatial distribution from the exit aperture plane. The exit aperture is positioned at an orthogonal distance, a lateral distance, and a tilt angle relative to the center axis of the substrate. The system can be configured for either i) minimum values for the orthogonal distance and the lateral distance to achieve a desired layer deposition uniformity using a set tilt angle, or ii) the tilt angle to achieve the desired layer deposition uniformity using a set orthogonal distance and a set lateral distance.