C03C1/008

Glass composite particles and uses thereof
11299670 · 2022-04-12 · ·

A composite particle including a core and a shell, wherein the core has at least one inorganic nanoparticle and the shell is made of vitrified glass, methods for obtaining thereof and uses thereof. The uses include a film having a host material and at least one composite particle and an optoelectronic devise including at least one composite particle or the film.

ORGANIC-INORGANIC METAL HALIDE GLASS
20220115593 · 2022-04-14 ·

The present disclosure describes an organic-inorganic metal-halide-based semiconducting material that melts at lower temperatures compared to conventional inorganic semiconductors. The hybrid material is structurally engineered to easily access both crystalline and amorphous glassy states, with each state offering distinct physical properties.

GRADIENT GLASS-LIKE CERAMIC STRUCTURES AND BOTTOM-UP FABRICATION METHOD THEREOF

Thin glass-like ceramic films which possess organic or physically functional structures with thicknesses in the 15 to 500 nm range and bottom-up methods for their fabrication are described. SiO.sub.2-rich structures having gradient properties are formed from a silsesquioxane having an electronegative β substituent and at least one organofunctional silane or at least one metal alkoxide.

Coating Liquid Used For Forming Ultraviolet Absorption Coating And Ultraviolet Absorption Glass
20210261798 · 2021-08-26 ·

Provided is an ultraviolet absorption glass comprising: a glass substrate, and an ultraviolet absorption coating arranged on at least one surface of the glass substrate, wherein the ultraviolet absorption coating comprises silicon dioxide, an ultraviolet absorber, and MOz used for storing and releasing electrons excited by ultraviolet light in the ultraviolet absorber. The ultraviolet absorption glass is low cost and has good resistance to discoloration and devitrification.

HIGH TEMPERATURE OXIDATION PROTECTION FOR COMPOSITES
20210276924 · 2021-09-09 · ·

An oxidation protection system disposed on a substrate is provided, which may comprise a base layer comprising a first pre-slurry composition comprising a first phosphate glass composition, and/or a sealing layer comprising a second pre-slurry composition comprising a second phosphate glass composition and a strengthening compound comprising boron nitride, a metal oxide, and/or silicon carbide.

High temperature oxidation protection for composites
11046619 · 2021-06-29 · ·

An oxidation protection system disposed on a substrate is provided, which may comprise a base layer comprising a first pre-slurry composition comprising a first phosphate glass composition, and/or a sealing layer comprising a second pre-slurry composition comprising a second phosphate glass composition and a strengthening compound comprising boron nitride, a metal oxide, and/or silicon carbide.

Coating liquid used for forming ultraviolet absorption coating and ultraviolet absorption glass

Coating liquid used for forming an ultraviolet absorption coating on a surface of an object such as glass and the like, ultraviolet absorption glass arranged with the ultraviolet absorption coating formed by the coating liquid, and a method for preparing the ultraviolet absorption glass. The coating liquid used for forming the ultraviolet absorption coating, the ultraviolet absorption glass and the method for forming the ultraviolet absorption glass, by storing and releasing electrons excited by ultraviolet lights in an ultraviolet absorber, reduce the excited electrons that are gradually accumulated during a process in which the ultraviolet absorber absorbs the ultraviolet lights, thus protecting the ultraviolet absorber and a silicon dioxide matrix, preventing the ultraviolet absorption glass from discoloring or devitrifying, ensuring weather resistance of the ultraviolet absorption coating and ensuring color consistency of the ultraviolet absorption glass.

INSULATING COATING-ATTACHED ELECTRICAL STEEL SHEET AND MANUFACTURING METHOD THEREFOR

An insulating coating-attached electrical steel sheet has, on at least one surface, an insulating coating including an insulating tensile coating layer A. A tension applied to the steel sheet by an insulating tensile coating layer having a coating weight of M/2 from a surface of the insulating tensile coating layer A is 0.80.sub.A or more, where M is a weight of the insulating tensile coating layer A, and .sub.A is the tension applied to the steel sheet by the insulating tensile coating layer A. The insulating coating-attached electrical steel sheet has excellent adhesion of the insulating coating. A method for manufacturing the insulating coating-attached electrical steel sheet is also provided.

METHOD FOR PRODUCING MEMBER FOR MOLTEN METAL BATH
20210010124 · 2021-01-14 ·

It is an object to provide a method for producing a member for a molten metal bath which is less likely to form minute cracks and pores in a pores-sealing coating film, and to provide a method for producing a member for a molten metal bath which can restrain adhesion of an alloy such as dross. The method for producing a member for a molten metal bath is characterized by applying or spraying, to a cermet thermal spray coating film formed on a base material or an oxide-based ceramic thermal spray coating film formed on a base material, a mixed solution obtained by adding aluminum dihydrogen phosphate and inorganic particles having a layered hexagonal crystal structure to a silica sol solution as a solution for sealing pores of the thermal spray coating film, and firing the mixed solution which is applied or sprayed to the thermal spray coating film.

COATED GLASS SHEET AND METHOD FOR PRODUCING SAME
20200399170 · 2020-12-24 ·

The coated glass sheet of the present invention includes: a glass sheet; and a coating film provided on at least one principal surface of the glass sheet and having a smooth surface. The coating film includes: isolated closed pores present within the coating film; and a matrix. The coating film is substantially free of open pores open at the surface of the coating film. For the coated glass sheet of the present invention, a transmittance gain is 2.5% or more, the transmittance gain being calculated by subtracting an average transmittance of the glass sheet as determined by applying light having wavelengths of 380 to 1100 nm to the glass sheet in the absence of the coating film on the surface of the glass sheet from an average transmittance of the coated glass sheet as determined by applying light having the wavelengths to the coated glass sheet from a side on which the coating film lies.