C03C17/225

DISPLAY DEVICE AND METHOD OF FABRICATING THE SAME
20220059797 · 2022-02-24 ·

A display panel may include a first display substrate, a second display substrate disposed over the first display substrate, and a sealing member bonding the first display substrate and the second display substrate. The sealing member may include a frit sealing member including an outer region and an inner region, with the inner region disposed next to an inner side of the outer region and having a first crystallization temperature lower than a second crystallization temperature of the outer region, and an organic sealing member disposed next to an inner side of the frit sealing member.

ASYMMETRIC CHEMICAL STRENGTHENING

Asymmetrically strengthened glass articles, methods for producing the same, and use of the articles in portable electronic device is disclosed. Using a budgeted amount of compressive stress and tensile stress, asymmetric chemical strengthening is optimized for the utility of a glass article. In some aspects, the strengthened glass article can be designed for reduced damage, or damage propagation, when dropped.

ANTIREFLECTIVE NANOPARTICLE COATINGS AND METHODS OF FABRICATION

Antireflective nanoparticle coatings and methods of forming the coatings on substrates are disclosed. One method for forming an antireflective coating includes depositing a nanoparticle coating layer on a substrate, wherein the nanoparticle coating layer includes a colloidal solution of nanoparticles and a solidifying material. The solidifying material includes a silica precursor. The method further includes curing the solidifying material to form silica inter-particle connections between adjacent nanoparticles and between at least some of the nanoparticles and the substrate to bind the nanoparticles to each other and to the substrate to form the antireflective coating.

Methods and apparatus providing a substrate having a coating with an elastic modulus gradient

Methods and apparatus are provide for: a substrate having first and second opposing surfaces, and an elastic modulus; and layer(s) having a thickness between first and second opposing surfaces thereof, the first surface of the layer contacting the second surface of the substrate, forming an interface. The layer may exhibit one or more of: a first elastic modulus proximate to the first surface thereof and a second elastic modulus proximate to the second surface thereof, the second elastic modulus being substantially higher than the elastic modulus value, the first elastic modulus being lower than the elastic modulus of the substrate, the second elastic modulus being higher than the elastic modulus of the substrate, and the layer exhibiting an increasing elastic modulus gradient through the thickness thereof from the first elastic modulus to the second elastic modulus.

Coated articles with optical coatings having residual compressive stress

A coated article includes a substrate having a major surface, and an optical coating disposed on the major surface of the substrate. At least a portion of the optical coating includes a residual compressive stress of about 50 MPa or more. The coated article has strain-to-failure of about 0.5% or more as measured by a Ring-on-Ring Tensile Testing Procedure. The coated article has an average photopic transmission of about 80% or greater.

GLASS ARTICLES HAVING DAMAGE-RESISTANT COATINGS AND METHODS FOR COATING GLASS ARTICLES

A coated glass article and methods for producing the same are provided herein. The coated glass article includes a glass body having a first surface and a second surface opposite the first surface, wherein the first surface is an exterior surface of the glass body, and a damage-resistant coating formed by atomic layer deposition, the damage-resistant coating being disposed on at least a portion of the first surface of the glass body.

ANTIMICROBIAL GLASS COATING
20170231229 · 2017-08-17 ·

The invention relates to an object having a coating arranged on at least one surface of the object, which comprises at least one antimicrobially active layer having an antimicrobial agent, wherein the agent comprises a copper (I) compound and/or a copper (II) compound.

Coated article with low-E coating having absorbing layer over functional layer designed to increase outside reflectance
09772434 · 2017-09-26 · ·

A coated article includes a low-E coating having an absorbing layer located over a functional layer (IR reflecting layer) and designed to cause the coating to have an increased outside reflectance (e.g., in an IG window unit) and good selectivity. In certain embodiments, the absorbing layer is metallic, or substantially metallic, and is provided directly over and contacting a lower of two IR reflecting layers. In certain example embodiments, a nitride based layer (e.g., silicon nitride or the like) may be located directly over and contacting the absorbing layer in order to reduce or prevent oxidation thereof during heat treatment (e.g., thermal tempering, heat bending, and/or heat strengthening) thereby permitting predictable coloration, high outside reflectance values, and/or good selectivity to be achieved. Coated articles according to certain example embodiments of this invention may be used in the context of insulating glass (IG) window units, vehicle windows, other types of windows, or in any other suitable application.

Asymmetric chemical strengthening

Asymmetrically strengthened glass articles, methods for producing the same, and use of the articles in portable electronic device is disclosed. Using a budgeted amount of compressive stress and tensile stress, asymmetric chemical strengthening is optimized for the utility of a glass article. In some aspects, the strengthened glass article can be designed for reduced damage, or damage propagation, when dropped.

Scratch-resistant and optically transparent materials and articles
11203179 · 2021-12-21 · ·

Embodiments of a scratch-resistant and optically transparent material comprising silicon, aluminum, nitrogen, and optionally oxygen are disclosed. In one or more embodiments, the material exhibits an extinction coefficient (k) at a wavelength of 400 nm of less than about 1×10.sup.−3, and an average transmittance of about 80% or greater, over an optical wavelength regime in the range from about 380 nm to about 780 nm, as measured through the material having a thickness of about 0.4 micrometer. In one or more embodiments, the material comprises an intrinsic maximum hardness of about 12 GPa or greater as measured on a major surface of the material having a thickness of about 400 by a Berkovich Indenter Hardness Test along an indentation depth of about 100 nm or greater, low compressive stress and low roughness (Ra). Articles and devices incorporating the material are also disclosed.