Patent classifications
C03C2218/31
Method of making a mirror substrate for a vehicular rearview mirror assembly
A method of making a mirror substrate for a vehicular rearview mirror assembly includes providing a glass substrate having a planar front surface, a planar rear surface and a circumferential perimeter edge. The glass substrate is positioned at a fixture and the front perimeter edge portion of the glass substrate is ground by moving a grinding wheel around the periphery of the glass substrate to establish a rounded surface about and around the periphery of the glass substrate and between the planar front surface and a rear portion of the perimeter edge of the glass substrate. The rounded surface has a radius of curvature of at least 2.5 mm. The rounded surface provides a curved transition between the planar front surface of the glass substrate and the rear portion of the perimeter edge of the glass substrate. The planar rear surface of the glass substrate is coated with a coating.
Glass Container Having an Inkjet Printed Image and a Method for the Manufacturing Thereof
The present invention is directed to a method of inkjet printing an image on a glass container comprising the steps of: a) manufacturing a glass container having a CEC layer; b) removing at least part of the CEC layer to a level wherein the remaining CEC layer has a thickness of less than 20 nm by washing the CEC from the glass container with an aqueous solution containing nonionic surfactant, rinsing with water and blowing the water from the container by means of a pressurized air stream, c) inkjet printing an image on the glass container.
Glass container having an inkjet printed image and a method for the manufacturing thereof
The present invention is directed to a method of inkjet printing an image on a glass container comprising the steps of: a) manufacturing a glass container having a CEC layer; b) removing at least part of the CEC layer to a level wherein the remaining CEC layer has a thickness of less than 20 nm by washing the CEC from the glass container with an aqueous solution containing non-ionic surfactant, rinsing with water and blowing the water from the container by means of a pressurized air stream, c) inkjet printing an image on the glass container.
VEHICULAR INTERIOR REARVIEW MIRROR ASSEMBLY
A vehicular interior rearview mirror assembly includes a mounting structure, a plastic mirror casing, and a mirror reflective element having a glass substrate. The glass substrate includes a periphery surface extending between a planar first surface and a planar second surface and spanning a thickness dimension of the glass substrate. The mirror casing includes a central mounting portion and spaced apart attachment portions. The mirror reflective element is adhesively attached the spaced apart attachment portions. The central mounting portion includes a first pivot element and the mounting structure includes a second pivot element, the first pivot element and the second pivot element forming a pivot joint. The periphery surface of the glass substrate includes a curved outer surface that provides a rounded transition between the planar first surface of the glass substrate and a less-curved outer surface of a side wall of the mirror casing.
COATED GLASS ARTICLES WITH ADHESION PROMOTING REGION
A coated glass article includes a glass article comprising a glass having a surface. The surface has an adhesion promoting region comprising a nanostructure formed at the surface of the glass. The adhesion promoting region is constructed of materials that are the same as one or more constituents of a glass composition of the glass. The coated glass article further includes a coating disposed on the adhesion promoting region formed at the surface of the glass. The coating incudes one or more polymer coating materials. The adhesion promoting region improves adhesion of the coating to the glass while also eliminating the use of titania or other adhesion promoting compounds that can adversely affect the optical properties of the coatings.
Antireflective member and method of manufacture therefor
Provided is an antireflective member that has a water- and oil-repellent layer on a multi-layered antireflective layer and is capable of exhibiting excellent surface lubricity, water- and oil-repellent properties, and durability. The surface of the multi-layered antireflective layer on a base material has a root-mean-square surface roughness of 0.8 nm to 2.0 nm. The water- and oil-repellent layer has a thickness of 1 to 30 nm and is a cured product of water- and oil-repellents having as principal components a fluorooxyalkylene group-containing polymer modified organosilicon compound with the numerical average molecular weight of 4,500 to 10,000 of a fluoropolymer part and/or partial hydrolysis condensate thereof.
GLASS SUBSTRATE WITH SILICA FILM
A glass substrate with a silica film according to the present invention includes a glass substrate and a silica film formed using a silica film-forming composition, in which the composition includes at least one kind selected from the group consisting of a hydrolyzable compound, a hydrolyzate thereof, and a hydrolysis condensation compound thereof, and at least one kind selected from the group consisting of a silica particle and a zirconia particle, the hydrolyzable compound consisting of a tetraalkoxysilane, a compound (compound I) represented by formula I: (R.sub.3-p(L).sub.pSi-Q-Si(L).sub.pR.sub.3-p), optionally a fluoroalkylsilane having a hydrolysable group, and optionally a zirconium compound having a hydrolyzable group, and the contents of the tetraalkoxysilane, the compound I, and the at least one kind selected from the group consisting of a silica particle and a zirconia particle in terms of SiO.sub.2/ZrO.sub.2 fall within specified ranges, respectively.
Methods and apparatus for manufacturing a glass-based article
A glass-based article includes a first major surface and a first compressive stress region extending to a first depth of compression from the first major surface. The glass-based article includes a second major surface including a first surface portion and one or more edge surface portions recessed from the first surface portion. The glass-based article includes a second compressive stress region extending to a second depth of compression from the first surface portion. Additionally, methods of manufacturing a glass-based article are disclosed.
High-refractive-index hydrogenated silicon film and methods for preparing the same
A preparation method for a high-refractive index hydrogenated silicon film, a high-refractive index hydrogenated silicon film, a light filtering lamination and a light filtering piece. The method includes: (a) by magnetic controlled Si target sputtering, Si deposits on a base body, forming a silicon film, which (b) forms an oxygenic hydrogenated silicon film in environment of active hydrogen and active oxygen, the amount of active oxygen accounts for 4%-99% of the total amount of active hydrogen and active oxygen, or, a nitric hydrogenated silicon film in environment of active hydrogen and active nitrogen, the amount of active nitrogen accounts for 5%-20% of the total amount of active hydrogen and active nitrogen. Sputtering and reactions are separately conducted, Si first deposits on the base body by magnetic controlled Si target sputtering, and then plasmas of active hydrogen and active oxygen/nitrogen react with silicon for oxygenic or nitric SiH.
WATER-REPELLENT-FILM-ATTACHED GLASS ARTICLE AND METHOD FOR MANUFACTURING SAME
The present disclosure provides a glass substrate to which water repellency that is not lost by a heat treatment is imparted. Provided is a water-repellent-film-attached glass article including a glass substrate and a water-repellent film on the glass substrate. The water-repellent film includes cerium oxide, a contact angle of water on a surface of the water-repellent film is 75° or greater, and the contact angle is 75° or greater after the glass article is exposed to a thermal treatment at 760° C. for 4 minutes.