C03C2218/31

SUBSTRATE MADE OF GLASS AND METHOD FOR THE PRODUCTION THEREOF

A substrate made of glass includes an essentially dimensionally stable portion, one or more flexible portions, and one or more recesses on one side or which do not penetrate the substrate, and which is/are disposed in an outer surface of the substrate, so as to reduce a material thickness of the substrate in the flexible portion relative to an adjacent portion. The recess is formed in each case by a plurality of concave depressions that are defined by microstructures, a course of which determines a remaining material thickness of the substrate in the flexible portion. The depressions extend at least in portions into an area having a thickness parallel to the outer surface which on bending the substrate encloses a plane of a neutral axis between an extension zone and a compression zone of the substrate.

Fire Rated Glass Unit
20230348325 · 2023-11-02 · ·

An article of fire rated glass and method of producing the same prepared by selecting a sheet of clear float annealed glass of at least 19 millimeters in thickness and providing the edge of the sheet substantially free of imperfections. The glass sheet is then specially tempered at a temperature of at least 575 degrees Celsius for a period of at least 750 seconds, followed by a cooling step.

Method for manufacturing glass article and method for heating thin sheet glass
11814729 · 2023-11-14 · ·

A method for manufacturing a glass article includes a heating step that heats a heating object made of glass. The heating step includes heating the heating object by converting, by a converter arranged between the heating object and a radiant heat source that radiates infrared light, a spectrum of the infrared light radiated from the radiant heat source and causing the heating object to absorb the infrared light radiated from the converter. The converter includes: an infrared light absorber that generates heat by absorbing the infrared light radiated from the radiant heat source; and an infrared light radiator made of a silicon-containing material. The infrared light radiator is heated through thermal conduction from the infrared light absorber. At least part of a surface of the converter facing the heating object includes at least part of a surface of the infrared light radiator.

SURFACE TREATMENT FILM, MANUFACTURING METHOD THEREFOR, AND ARTICLE

The present invention provides a surface treatment film that is capable of imparting durability such as wear resistance, friction resistance, chemical resistance, heat resistance, and solvent resistance to the surfaces of various substrates, and that exhibits excellent adhesion to the surfaces of the substrates. The surface treatment film is provided on the surface of a substrate. The surface treatment film has a laminated structure that includes a polymer layer (i) disposed on the surface side of the substrate and a polymer layer (ii) disposed on the polymer layer (i). The polymer layer (i) contains a first polymer derived from a polymerization initiation group-containing polymer, such as a polyester having, in a side chain, a functional group represented by formula (1) wherein R.sub.1 represents a hydrogen atom, a methyl group, or the like, R.sub.2 represents a methyl group or the like, X represents a chlorine atom or the like, Y represents O or NH, and * shows a bonding position. The polymer layer (ii) contains a second polymer which contains a constituent unit derived from a monomer such as an aromatic vinyl-based monomer and which extends using the functional group represented by formula (i) as a polymerization initiation point.

HIGH PRECISION TRACKPAD AND METHODS OF MANUFACTURE
20230018563 · 2023-01-19 ·

The present invention relates to a mouse pad comprising a flat metal alloy sheet having a surface that has been treated with a ceramic and polymer coating to provide the surface with a desired friction co-efficient. A method of manufacture of the mousepad is also provided.

Fire-rated glass unit
11479504 · 2022-10-25 · ·

An article of fire rated glass and method of producing the same prepared by selecting a sheet of clear float annealed glass of at least 19 millimeters in thickness and providing the edge of the sheet substantially free of imperfections. The glass sheet is then specially tempered at a temperature of at least 575 degrees Celsius for a period of at least 750 seconds, followed by fluid quenching.

Fixed and portable coating apparatuses and methods

A system and method for depositing a coating may comprise a coating chemical reactor, surface activation component, and a deposition component. A target surface may be prepared for deposition with the surface activation component. The coating chemical reactor may comprise a coating chemical dispenser and a coating chemical verifier that prepares the coating chemical for deposition. The coating chemical verifier may utilize an optical excitation source and at least one optical detector, wherein chemical substances are identified by unique signatures composed of binary code. The coating chemical may be received by the deposition component to depositing the coating chemical on the target surface.

Coupled Transmission Line Resonate RF Filter
20220278435 · 2022-09-01 ·

The present invention includes a method of creating electrical air gap low loss low cost RF mechanically and thermally stabilized interdigitated resonate filter in photo definable glass ceramic substrate. Where a ground plane may be used to adjacent to or below the RF filter in order to prevent parasitic electronic signals, RF signals, differential voltage build up and floating grounds from disrupting and degrading the performance of isolated electronic devices by the fabrication of electrical isolation and ground plane structures on a photo-definable glass substrate.

Fire Rated Glass Unit
20220250976 · 2022-08-11 · ·

An article of fire rated glass and method of producing the same prepared by selecting a sheet of clear float annealed glass of at least 19 millimeters in thickness and providing the edge of the sheet substantially free of imperfections. The glass sheet is then specially tempered at a temperature of at least 575 degrees Celsius for a period of at least 750 seconds, followed by a cooling step.

COATING FILM-ATTACHED GLASS, PRODUCTION METHOD THEREFOR, AND MODIFIED GLASS SUBSTRATE
20220250970 · 2022-08-11 ·

A coating film-attached glass comprising a glass substrate, and a coating film provided on at least a part of a surface of the glass substrate, in which a region from the surface of the glass substrate on the coating film side to a predetermined depth is a modified layer, and the modified layer has a microcrystalline structure at least in part.