Patent classifications
C04B24/026
Enhanced filtration control packages, wellbore servicing fluids utilizing the same, and methods of maintaining the structure of a wellbore
A wellbore servicing fluid comprises an aqueous base fluid, one or more alkali metal or alkali earth metal salts, at least one visocisifier, and a filtration control package. The filtration control package may comprise a carboxylic acid and an ethoxylated alcohol compound. Alternatively, the filtration control package may comprise a polyethylene glycol. The carboxylic acid may have from 8 to 20 carbon atoms. The ethoxylated alcohol compound may have a general formula R(OCH.sub.2CH.sub.2).sub.xOH, where R is a hydrocarbon having from 10 to 16 atoms and x is an integer from 6 to 9. The ethoxylated alcohol compound may have a hydrophilic-lipophilic balance of from 8.0 to 16.0. The polyethylene glycol may have a mass average molar mass (M.sub.w) of less than or equal to 1500 daltons.
Enhanced filtration control packages, wellbore servicing fluids utilizing the same, and methods of maintaining the structure of a wellbore
A wellbore servicing fluid comprises an aqueous base fluid, one or more alkali metal or alkali earth metal salts, at least one visocisifier, and a filtration control package. The filtration control package may comprise a carboxylic acid and an ethoxylated alcohol compound. Alternatively, the filtration control package may comprise a polyethylene glycol. The carboxylic acid may have from 8 to 20 carbon atoms. The ethoxylated alcohol compound may have a general formula R(OCH.sub.2CH.sub.2).sub.xOH, where R is a hydrocarbon having from 10 to 16 atoms and x is an integer from 6 to 9. The ethoxylated alcohol compound may have a hydrophilic-lipophilic balance of from 8.0 to 16.0. The polyethylene glycol may have a mass average molar mass (M.sub.w) of less than or equal to 1500 daltons.
Development of anti-bit balling fluids
Anti-bit balling drilling fluids and methods of making and using drilling fluids are provided. The anti-bit balling drilling fluid contains water, a clay-based component, and at least one of a surfactant having the formula: R(OC.sub.2H.sub.4).sub.xOH, where R is a hydrocarbyl group having from 10 to 20 carbon atoms and x is an integer from 1 and 10, or a polyethylene glycol having the formula: H(OCH.sub.2CH.sub.2).sub.nOH, where n is an integer from 1 to 50. Methods of making and using these drilling fluids are also provided.
Development of anti-bit balling fluids
Anti-bit balling drilling fluids and methods of making and using drilling fluids are provided. The anti-bit balling drilling fluid contains water, a clay-based component, and at least one of a surfactant having the formula: R(OC.sub.2H.sub.4).sub.xOH, where R is a hydrocarbyl group having from 10 to 20 carbon atoms and x is an integer from 1 and 10, or a polyethylene glycol having the formula: H(OCH.sub.2CH.sub.2).sub.nOH, where n is an integer from 1 to 50. Methods of making and using these drilling fluids are also provided.
Spacer fluids and cement slurries that include surfactants
According to at least one embodiment of the present disclosure, a well bore cementing system may comprise a spacer fluid and a cement slurry. The spacer fluid may be positioned within a well bore, and the spacer fluid may comprise a first surfactant package comprising one or more surfactants. The cement slurry may be positioned within the well bore, and the cement slurry may comprise a second surfactant package comprising one or more surfactants.
Spacer fluids and cement slurries that include surfactants
According to at least one embodiment of the present disclosure, a well bore cementing system may comprise a spacer fluid and a cement slurry. The spacer fluid may be positioned within a well bore, and the spacer fluid may comprise a first surfactant package comprising one or more surfactants. The cement slurry may be positioned within the well bore, and the cement slurry may comprise a second surfactant package comprising one or more surfactants.
STEROL BLENDS AS AN ADDITIVE IN ASPHALT BINDER
Disclosed are asphalt binder compositions and methods for making such compositions with pure sterol:crude sterol blends. The sterol blends improve various rheological properties.
STEROL BLENDS AS AN ADDITIVE IN ASPHALT BINDER
Disclosed are asphalt binder compositions and methods for making such compositions with pure sterol:crude sterol blends. The sterol blends improve various rheological properties.
COMPOSITION OF MATTER FOR INHIBITING WATER MIGRATION BETWEEN INSIDE AND OUTSIDE OF CONCRETE
A composition of matter, including a phlogopite powder or muscovite powder, clinoptilolite or mordenite, and kaolinite. The composition of matter is prepared as follows: 1) mixing the phlogopite powder or muscovite powder, the clinoptilolite or mordenite, and the kaolinite in a weight ratio of 50-70:0-30:0-50; adding a solution including isopropanol and n-butanol to a mixture of the phlogopite powder or muscovite powder, the clinoptilolite or mordenite, and the kaolinite, thereby yielding a mixed solution; 2) adding a silane coupling agent to the mixed solution, and continuously magnetically stirring the mixed solution for 30 min; adding distilled water to the mixed solution, and continuously magnetically stirring for 30 min; and adding methyl silicone oil to the mixed solution, and magnetically stirring for an hour, thereby yielding a slurry; and 3) drying the slurry at a temperature of 150-200 C.
COMPOSITION OF MATTER FOR INHIBITING WATER MIGRATION BETWEEN INSIDE AND OUTSIDE OF CONCRETE
A composition of matter, including a phlogopite powder or muscovite powder, clinoptilolite or mordenite, and kaolinite. The composition of matter is prepared as follows: 1) mixing the phlogopite powder or muscovite powder, the clinoptilolite or mordenite, and the kaolinite in a weight ratio of 50-70:0-30:0-50; adding a solution including isopropanol and n-butanol to a mixture of the phlogopite powder or muscovite powder, the clinoptilolite or mordenite, and the kaolinite, thereby yielding a mixed solution; 2) adding a silane coupling agent to the mixed solution, and continuously magnetically stirring the mixed solution for 30 min; adding distilled water to the mixed solution, and continuously magnetically stirring for 30 min; and adding methyl silicone oil to the mixed solution, and magnetically stirring for an hour, thereby yielding a slurry; and 3) drying the slurry at a temperature of 150-200 C.