Patent classifications
C04B24/129
Biologically mediated precipitation of carbonates for use in oilfield applications
A method of enhancing carbonate precipitation in a downhole environment comprises introducing into the downhole environment a treatment composition comprising: a carbonate producing agent comprising a microbe, an enzyme, or a combination comprising at least one of the foregoing, and a substrate comprising N-oxyurea, semicarbazide, N,N-dioxyurea, or a combination comprising at least one of the foregoing. An organic feedstock and a geobacter can also be used to treating a wellbore or a subterranean formation. Encapsulated carbonate producing agent such as encapsulated bacterial spores are used to form self-healing cemented structure in a downhole environment.
Biologically mediated precipitation of carbonates for use in oilfield applications
A method of enhancing carbonate precipitation in a downhole environment comprises introducing into the downhole environment a treatment composition comprising: a carbonate producing agent comprising a microbe, an enzyme, or a combination comprising at least one of the foregoing, and a substrate comprising N-oxyurea, semicarbazide, N,N-dioxyurea, or a combination comprising at least one of the foregoing. An organic feedstock and a geobacter can also be used to treating a wellbore or a subterranean formation. Encapsulated carbonate producing agent such as encapsulated bacterial spores are used to form self-healing cemented structure in a downhole environment.
FOAMABLE RESIN COMPOSITION FOR CONTROLLING LOSS CIRCULATION
This disclosure relates to a foamable resin composition containing a nitrogen gas-generating compound and methods of using the composition for loss circulation control.
FOAMABLE RESIN COMPOSITION FOR CONTROLLING LOSS CIRCULATION
This disclosure relates to a foamable resin composition containing a nitrogen gas-generating compound and methods of using the composition for loss circulation control.
HIGH-CARBON RECOVERED PAPER AND PLASTIC MATERIALS WITH REDUCED ENDOTOXIN LEVELS
Provided herein are composite materials comprising at least 70 wt. % thermally consolidated recovered paper and plastic fragments and less than 5,000 ng water-soluble endotoxin per gram of composite materials, as well as methods of preparing said composite materials and methods of sanitizing recovered waste materials.
HIGH-CARBON RECOVERED PAPER AND PLASTIC MATERIALS WITH REDUCED ENDOTOXIN LEVELS
Provided herein are composite materials comprising at least 70 wt. % thermally consolidated recovered paper and plastic fragments and less than 5,000 ng water-soluble endotoxin per gram of composite materials, as well as methods of preparing said composite materials and methods of sanitizing recovered waste materials.
High-carbon recovered paper and plastic materials with reduced endotoxin levels
Provided herein are composite materials comprising at least 70 wt. % thermally consolidated recovered paper and plastic fragments and less than 5,000 ng water-soluble endotoxin per gram of composite materials, as well as methods of preparing said composite materials and methods of sanitizing recovered waste materials.
High-carbon recovered paper and plastic materials with reduced endotoxin levels
Provided herein are composite materials comprising at least 70 wt. % thermally consolidated recovered paper and plastic fragments and less than 5,000 ng water-soluble endotoxin per gram of composite materials, as well as methods of preparing said composite materials and methods of sanitizing recovered waste materials.
HIGH-CARBON RECOVERED PAPER AND PLASTIC MATERIALS WITH REDUCED ENDOTOXIN LEVELS
Provided herein are composite materials comprising at least 70 wt. % thermally consolidated recovered paper and plastic fragments and less than 5,000 ng water-soluble endotoxin per gram of composite materials, as well as methods of preparing said composite materials and methods of sanitizing recovered waste materials.
HIGH-CARBON RECOVERED PAPER AND PLASTIC MATERIALS WITH REDUCED ENDOTOXIN LEVELS
Provided herein are composite materials comprising at least 70 wt. % thermally consolidated recovered paper and plastic fragments and less than 5,000 ng water-soluble endotoxin per gram of composite materials, as well as methods of preparing said composite materials and methods of sanitizing recovered waste materials.