C04B24/18
Foaming of set-delayed cement compositions comprising pumice and hydrated lime
A variety of methods and compositions are disclosed, including, in one embodiment a method a cementing in a subterranean formation comprising: providing a set-delayed cement composition comprising water, pumice, hydrated lime, and a set retarder; foaming the set-delayed cement composition; activating the set-delayed cement composition; introducing the set-delayed cement composition into a subterranean formation; and allowing the set-delayed cement composition to set in the subterranean formation. Additional methods, foamed set-delayed cement composition, and systems for cementing are also provided.
Foaming of set-delayed cement compositions comprising pumice and hydrated lime
A variety of methods and compositions are disclosed, including, in one embodiment a method a cementing in a subterranean formation comprising: providing a set-delayed cement composition comprising water, pumice, hydrated lime, and a set retarder; foaming the set-delayed cement composition; activating the set-delayed cement composition; introducing the set-delayed cement composition into a subterranean formation; and allowing the set-delayed cement composition to set in the subterranean formation. Additional methods, foamed set-delayed cement composition, and systems for cementing are also provided.
Magnesium phosphate cement
Magnesium phosphate cement binder systems and method for providing magnesium phosphate cements are described. In an embodiment, a magnesium phosphate cement binder system may include magnesium oxide that has been calcined at a temperature of between about 900° F. to about 1800° F. The magnesium phosphate cement binder system may also include a phosphate material. Other formulations, compositions, and methods are also described.
Magnesium phosphate cement
Magnesium phosphate cement binder systems and method for providing magnesium phosphate cements are described. In an embodiment, a magnesium phosphate cement binder system may include magnesium oxide that has been calcined at a temperature of between about 900° F. to about 1800° F. The magnesium phosphate cement binder system may also include a phosphate material. Other formulations, compositions, and methods are also described.
Combined Set-Delayed Cement Compositions
Methods of using the set-delayed cement slurries and compositions resulting from the combination of the set-delayed cement slurries are also described. A method may comprise providing a first set-delayed cement slurry comprising a pozzolanic cement and/or a Portland cement, water, and a first cement set retarder; providing a second set-delayed cement slurry comprising calcium-aluminate and a second cement set retarder; mixing the first slurry and the second slurry to form a cement composition; and allowing the cement composition to set.
Combined Set-Delayed Cement Compositions
Methods of using the set-delayed cement slurries and compositions resulting from the combination of the set-delayed cement slurries are also described. A method may comprise providing a first set-delayed cement slurry comprising a pozzolanic cement and/or a Portland cement, water, and a first cement set retarder; providing a second set-delayed cement slurry comprising calcium-aluminate and a second cement set retarder; mixing the first slurry and the second slurry to form a cement composition; and allowing the cement composition to set.
EXTENDED-LIFE CEMENT COMPOSITIONS COMPRISING RED MUD SOLIDS
Extended-life cement compositions are provided and, more particularly, extended-life cement compositions are provided that comprise a cementitious component comprising red mud solids and hydraulic cement. A method of cementing may comprise providing an extended-life cement composition comprising a cementitious component, water, and a cement set retarder, wherein the cementitious component comprises red mud solids and a hydraulic cement; activating the extended-life cement composition; introducing the extended-life cement composition into a subterranean formation; and allowing the extended-life cement composition to set in the subterranean formation.
EXTENDED-LIFE CEMENT COMPOSITIONS COMPRISING RED MUD SOLIDS
Extended-life cement compositions are provided and, more particularly, extended-life cement compositions are provided that comprise a cementitious component comprising red mud solids and hydraulic cement. A method of cementing may comprise providing an extended-life cement composition comprising a cementitious component, water, and a cement set retarder, wherein the cementitious component comprises red mud solids and a hydraulic cement; activating the extended-life cement composition; introducing the extended-life cement composition into a subterranean formation; and allowing the extended-life cement composition to set in the subterranean formation.
Development of high temperature low density cement
The invention provides a low density cement composition. The composition includes a cement component, a glass sphere component, a bentonite component, a fine calcium carbonate component, a medium calcium carbonate component, a silica sand component, and a silica flour component.
Development of high temperature low density cement
The invention provides a low density cement composition. The composition includes a cement component, a glass sphere component, a bentonite component, a fine calcium carbonate component, a medium calcium carbonate component, a silica sand component, and a silica flour component.