C04B28/184
Curable formulations for structural and non-structural applications
[A] curable mixture configured to set in the presence of water, wherein the mixture comprises magnesium oxide, a primary cementitious component and at least one accelerant and at least one second accelerant, the at least one second accelerant is different than the at least one first accelerant, wherein a proportion by weight of the at least one second accelerant is equal to or less than 2% of a proportion of magnesium oxide by weight of the mixture. A proportion by weight of the primary cementitious component is 80% to 120% of a proportion of magnesium oxide by weight.
Lime-based cement extender compositions, and associated systems and methods
A composition configured to be mixed with cement, and associated systems and methods are disclosed herein. In some embodiments, the composition includes at least 10% by weight lime particles, and at least 35% by weight pozzolan particles. Properties of the composition can include a magnesium oxide concentration of at least 0.5%, and an iron oxide concentration of at least 0.5-2.0%, an aluminum oxide concentration of 2-8%, a silicon dioxide concentration of 20-40%, a potassium oxide concentration of 20,000-30,000 ppm, and a sodium oxide concentration of 10,000-20,000 ppm. In some embodiments, the lime-based cement extender composition, or product, is combined with cement to produce a cement blend for use in the mining industry as mine backfill.
Lime-based cement extender compositions, and associated systems and methods
A composition configured to be mixed with cement, and associated systems and methods are disclosed herein. In some embodiments, the composition includes at least 10% by weight lime particles, and at least 35% by weight pozzolan particles. Properties of the composition can include a magnesium oxide concentration of at least 0.5%, and an iron oxide concentration of at least 0.5-2.0%, an aluminum oxide concentration of 2-8%, a silicon dioxide concentration of 20-40%, a potassium oxide concentration of 20,000-30,000 ppm, and a sodium oxide concentration of 10,000-20,000 ppm. In some embodiments, the lime-based cement extender composition, or product, is combined with cement to produce a cement blend for use in the mining industry as mine backfill.
LIME-BASED CEMENT EXTENDER COMPOSITIONS, AND ASSOCIATED SYSTEMS AND METHODS
A composition configured to be mixed with cement, and associated systems and methods are disclosed herein. In some embodiments, the composition includes at least 10% by weight lime particles, and at least 35% by weight pozzolan particles. Properties of the composition can include a magnesium oxide concentration of at least 0.5%, and an iron oxide concentration of at least 0.5-2.0%, an aluminum oxide concentration of 2-8%, a silicon dioxide concentration of 20-40%, a potassium oxide concentration of 20,000-30,000 ppm, and a sodium oxide concentration of 10,000-20,000 ppm. In some embodiments, the lime-based cement extender composition, or product, is combined with cement to produce a cement blend for use in the mining industry as mine backfill.