C04B28/32

Composite Fireproof Board and Method of Processing and Preparing the Same
20220025644 · 2022-01-27 ·

A composite fireproof board has structure that includes, from top to bottom, a bottom layer, a lower reinforcement mesh layer, a middle layer, an upper reinforcement mesh layer, and a surface layer. The middle layer includes an organic frame and an inorganic fireproof material filled within the frame. The frame is provided with fixed grooves on edges adjacent to the fireproof material, and is further provided with through holes.

COMPOSITE MATERIAL FOR SLURRY YIELD ENHANCEMENT

Cement compositions and associated methods for cementing. An example method includes introducing a cement composition into a wellbore penetrating a subterranean formation, the cement composition comprising a composite material, a cement, and an aqueous fluid. The composite material comprises a monophase amorphous hydraulic binder material and a particulate core. The monophase amorphous hydraulic binder material coats the particulate core. The method further comprises allowing the cement composition to set in the wellbore.

COMPOSITE MATERIAL FOR SLURRY YIELD ENHANCEMENT

Cement compositions and associated methods for cementing. An example method includes introducing a cement composition into a wellbore penetrating a subterranean formation, the cement composition comprising a composite material, a cement, and an aqueous fluid. The composite material comprises a monophase amorphous hydraulic binder material and a particulate core. The monophase amorphous hydraulic binder material coats the particulate core. The method further comprises allowing the cement composition to set in the wellbore.

ENGINEERED FLOORING PRODUCT AND METHOD OF MANUFACTURING THEREOF
20220010564 · 2022-01-13 ·

The present disclosure relates to a method of manufacturing an engineered flooring product comprising a core layer. The method provides the steps of: (a) mixing a hydrate compound, one or more stabilizing agents, and water in a mixer, forming a raw material slurry; (b) spreading a first layer of the raw material slurry onto a cull plate; (c) curing the first layer of raw material slurry; (d) after step (c), releasing the cured first layer of raw material slurry from the cull plate; (e) after step (d), trimming the cured first layer of raw material slurry released from the cull plate; and, (f) after step (e), cooling the cured first layer of raw material slurry released from the cull plate for at least about 24 hours at a temperature ranging from about 10° C.-30° C. thereby forming the engineered flooring product.

ENGINEERED FLOORING PRODUCT AND METHOD OF MANUFACTURING THEREOF
20220010564 · 2022-01-13 ·

The present disclosure relates to a method of manufacturing an engineered flooring product comprising a core layer. The method provides the steps of: (a) mixing a hydrate compound, one or more stabilizing agents, and water in a mixer, forming a raw material slurry; (b) spreading a first layer of the raw material slurry onto a cull plate; (c) curing the first layer of raw material slurry; (d) after step (c), releasing the cured first layer of raw material slurry from the cull plate; (e) after step (d), trimming the cured first layer of raw material slurry released from the cull plate; and, (f) after step (e), cooling the cured first layer of raw material slurry released from the cull plate for at least about 24 hours at a temperature ranging from about 10° C.-30° C. thereby forming the engineered flooring product.

CURABLE FORMULATIONS FOR STRUCTURAL AND NON-STRUCTURAL APPLICATIONS

According to some embodiments, a curable mixture configured to set in the presence of water, wherein the mixture comprises magnesium oxide, a primary cementitious component and at least one accelerant. A proportion by weight of the primary cementitious component is 80% to 120% of a proportion of magnesium oxide by weight.

CURABLE FORMULATIONS FOR STRUCTURAL AND NON-STRUCTURAL APPLICATIONS

According to some embodiments, a curable mixture configured to set in the presence of water, wherein the mixture comprises magnesium oxide, a primary cementitious component and at least one accelerant. A proportion by weight of the primary cementitious component is 80% to 120% of a proportion of magnesium oxide by weight.

Composite fireproof board and method of processing and preparing the same
11162258 · 2021-11-02 · ·

A composite fireproof board has a structure that includes, from top to bottom, a bottom layer, a lower reinforcement mesh layer, a middle layer, an upper reinforcement mesh layer, and a surface layer. The middle layer includes an organic frame and an inorganic fireproof material filled within the frame. The frame is provided with fixed grooves on edges adjacent to the fireproof material, and is further provided with through holes.

Ultra stable cementitious material formulation, process for its making, and ultra stable tile backer board formulation and processes for its making
11777440 · 2023-10-03 · ·

An ultrastable cementitious material with nano-molecular veneer makes a cementitious material by blending 29 wt % to 40 wt % of a magnesium oxide dry powder containing 80 wt % to 98 wt % of magnesium oxide based on a final total weight of the cementitious material, with 14 wt % to 18 wt % of a magnesium chloride dissolved in water and reacting to form a liquid suspension, mixing from 2 to 10 minutes, adding a phosphorus-containing material, and allowing the liquid suspension to react into an amorphous phase cementitious material, wherein a portion of the amorphous phase cementitious material grows a plurality of crystals. The plurality of crystals are encapsulated by the amorphous phase cementitious material forming a nano-molecular veneer. A process to make the ultrastable cementitious material. A tile backer board incorporating the ultrastable cementitious material and a process for making the tile backer board.

Ultra stable cementitious material formulation, process for its making, and ultra stable tile backer board formulation and processes for its making
11777440 · 2023-10-03 · ·

An ultrastable cementitious material with nano-molecular veneer makes a cementitious material by blending 29 wt % to 40 wt % of a magnesium oxide dry powder containing 80 wt % to 98 wt % of magnesium oxide based on a final total weight of the cementitious material, with 14 wt % to 18 wt % of a magnesium chloride dissolved in water and reacting to form a liquid suspension, mixing from 2 to 10 minutes, adding a phosphorus-containing material, and allowing the liquid suspension to react into an amorphous phase cementitious material, wherein a portion of the amorphous phase cementitious material grows a plurality of crystals. The plurality of crystals are encapsulated by the amorphous phase cementitious material forming a nano-molecular veneer. A process to make the ultrastable cementitious material. A tile backer board incorporating the ultrastable cementitious material and a process for making the tile backer board.