C04B28/344

ANTICORROSIVE COMPOSITION

A mineral wool or other fibrous product which comprises in at least a surface layer thereof an anticorrosive composition comprising one or more alkali metal silicate components of the formula Me.sub.2O.Math.xSiO.sub.2, wherein x has a value of from 0.5 to 4.0, one or more alkali metal phosphate components of the formula Me.sub.2O:nP.sub.2O.sub.5, wherein n has a value of from 0.33 to 1 and/or hydrates thereof, and one or more carboxylic acids having 6-22 carbon atoms and/or salts thereof.

ANTICORROSIVE COMPOSITION

A mineral wool or other fibrous product which comprises in at least a surface layer thereof an anticorrosive composition comprising one or more alkali metal silicate components of the formula Me.sub.2O.Math.xSiO.sub.2, wherein x has a value of from 0.5 to 4.0, one or more alkali metal phosphate components of the formula Me.sub.2O:nP.sub.2O.sub.5, wherein n has a value of from 0.33 to 1 and/or hydrates thereof, and one or more carboxylic acids having 6-22 carbon atoms and/or salts thereof.

Anticorrosive composition

An anticorrosive composition comprising (a) one or more alkali metal silicate components of the formula Me.sub.2O.Math.xSiO.sub.2, wherein x has a value of from 0.5 to 4.0, (b) one or more alkali metal phosphate components of the formula Me.sub.2O:nP.sub.2O.sub.5, wherein n has a value of from 0.33 to 1 and/or hydrates thereof, (c) one or more carboxylic acids having 6-22 carbon atoms and/or salts thereof: and the use of the composition for imparting anticorrosive properties to a material such as a mineral wool product.

Anticorrosive composition

An anticorrosive composition comprising (a) one or more alkali metal silicate components of the formula Me.sub.2O.Math.xSiO.sub.2, wherein x has a value of from 0.5 to 4.0, (b) one or more alkali metal phosphate components of the formula Me.sub.2O:nP.sub.2O.sub.5, wherein n has a value of from 0.33 to 1 and/or hydrates thereof, (c) one or more carboxylic acids having 6-22 carbon atoms and/or salts thereof: and the use of the composition for imparting anticorrosive properties to a material such as a mineral wool product.

Anticorrosive composition

An anticorrosive composition comprising (a) one or more alkali metal silicate components of the formula Me.sub.2O.Math.xSiO.sub.2, wherein x has a value of from 0.5 to 4.0, (b) one or more alkali metal phosphate components of the formula Me.sub.2O:nP.sub.2O.sub.5, wherein n has a value of from 0.33 to 1 and/or hydrates thereof, (c) one or more carboxylic acids having 6-22 carbon atoms and/or salts thereof: and the use of the composition for imparting anticorrosive properties to a material such as a mineral wool product.

ANTICORROSIVE COMPOSITION

The present invention relates to an anticorrosive composition and the use of such a composition for imparting anticorrosive properties to a material, and a material comprising such a composition.

Preparation and fully compounded stock for use in medical or dental applications, medical or dental product and use and preparation thereof

According to the invention, a preparation is described which contains at least one calcium compound selected from the group consisting of calcium phosphates, calcium fluorides and calcium fluorophosphates and hydroxyl derivatives and carbonate derivatives of these calcium salts, calcium hydroxides and calcium oxides precipitated using at least one protein component selected from proteins and protein hydrolysates, and at least one crosslinking agent for the protein component and/or non-set cement.

ACTIVE AND PASSIVE INTEGRATED FIREPROOF HEAT-INSULATING BOARD AND PREPARATION METHOD THEREOF

Provided are an active and passive integrated fireproof heat-insulating board and a preparation method thereof, including: n passive fireproof layers and n or n+1 active fireproof layers, the passive fireproof layers and the active fireproof layers are overlapped with each other into a whole. Each passive fireproof layer includes an inorganic fiber felt and an aerogel; the aerogel is obtained by curing an aerogel stock solution having adhesiveness, and the aerogel stock solution includes, in parts by mass, 1000 to 4000 parts of silica sol, 50 to 150 parts of soluble silicate, 10 to 50 parts of a phosphate adhesive, 5 to 20 parts of quicklime, 5 to 50 parts of titanium dioxide, 10 to 50 parts of calcium stearate, 5 to 50 parts of a hydrophobic modifier, 5 to 50 parts of an acid-base regulator, and 1000 to 4000 parts of a solvent.