C04B35/547

Method for manufacturing thermoelectric materials

Disclosed is a method for manufacturing a thermoelectric material having high thermoelectric conversion performance in a broad temperature range. The method for manufacturing a thermoelectric material according to the present disclosure includes forming a mixture by weighing Cu and Se based on the following chemical formula 1 and mixing the Cu and the Se, and forming a compound by thermally treating the mixture: <Chemical Formula 1> Cu.sub.xSe where 2<x≦2.6.

Method for manufacturing thermoelectric materials

Disclosed is a method for manufacturing a thermoelectric material having high thermoelectric conversion performance in a broad temperature range. The method for manufacturing a thermoelectric material according to the present disclosure includes forming a mixture by weighing Cu and Se based on the following chemical formula 1 and mixing the Cu and the Se, and forming a compound by thermally treating the mixture: <Chemical Formula 1> Cu.sub.xSe where 2<x≦2.6.

THREE-DIMENSIONAL SHAPED ARTICLE PRODUCTION METHOD, THREE-DIMENSIONAL SHAPED ARTICLE PRODUCTION APPARATUS, AND THREE-DIMENSIONAL SHAPED ARTICLE
20170252977 · 2017-09-07 ·

A three-dimensional shaped article production method includes a layer formation step of forming a layer by ejecting a composition containing particles and a solvent in a predetermined pattern using a dispenser, a measurement step of determining the height of the layer, and a bonding step of subjecting a stacked body including a plurality of layers to a bonding treatment for bonding the particles, wherein when n represents an arbitrary integer of 1 or more, by selecting driving waveform data for the dispenser when ejecting the composition from a data group including a plurality of pieces of driving waveform data based on the information of the height of the layer in the n-th position (n-th layer) determined in the measurement step, the ejection amount of the composition per unit area onto the n-th layer in the layer formation step of forming the layer in the (n+1)th position ((n+1)th layer) is adjusted.

Density enhancement methods and compositions

The present invention relates to granular composite density enhancement, and related methods and compositions. The application where the properties are valuable include but are not limited to: 1) additive manufacturing (“3D printing”) involving metallic, ceramic, cermet, polymer, plastic, or other dry or solvent-suspended powders or gels, 2) concrete materials, 3) solid propellant materials, 4) cermet materials, 5) granular armors, 6) glass-metal and glass-plastic mixtures, and 7) ceramics comprising (or manufactured using) granular composites.

Density enhancement methods and compositions

The present invention relates to granular composite density enhancement, and related methods and compositions. The application where the properties are valuable include but are not limited to: 1) additive manufacturing (“3D printing”) involving metallic, ceramic, cermet, polymer, plastic, or other dry or solvent-suspended powders or gels, 2) concrete materials, 3) solid propellant materials, 4) cermet materials, 5) granular armors, 6) glass-metal and glass-plastic mixtures, and 7) ceramics comprising (or manufactured using) granular composites.

New process for manufacturing a chromium alloyed molybdenum silicide portion of a heating element
20210403386 · 2021-12-30 · ·

A process of manufacturing a chromium alloyed molybdenum silicide portion of a heating element comprising the steps of: forming a mixture of a chromium powder and a silicon powder; reacting the mixture to a reaction product in an inert atmosphere at a temperature of at least 1100° C. but not more than 1580° C.; converting the reaction product to a powder comprising CrSi.sub.2; forming a powder ceramic composition by mixing the powder comprising CrSi.sub.2 with a MoSi.sub.2 powder and optionally with an extrusion aid; forming the portion of the heating element; and sintering the portion of the heating element in a temperature of from about 1450° C. to about 1700° C.; characterized in that the chromium powder and the silicon powder are provided separately to the mixture.

Solid state catholyte or electrolyte for battery using Li.SUB.a.MP.SUB.b.S.SUB.c .(M=Si, Ge, and/or Sn)

The present invention provides an energy storage device comprising a cathode region or other element. The device has a major active region comprising a plurality of first active regions spatially disposed within the cathode region. The major active region expands or contracts from a first volume to a second volume during a period of a charge and discharge. The device has a catholyte material spatially confined within a spatial region of the cathode region and spatially disposed within spatial regions not occupied by the first active regions. In an example, the catholyte material comprises a lithium, germanium, phosphorous, and sulfur (“LGPS”) containing material configured in a polycrystalline state. The device has an oxygen species configured within the LGPS containing material, the oxygen species having a ratio to the sulfur species of 1:2 and less to form a LGPSO material. The device has a protective material formed overlying exposed regions of the cathode material to substantially maintain the sulfur species within the catholyte material. Also included is a novel dopant configuration of the Li.sub.aMP.sub.bS.sub.c (LMPS) [M=Si, Ge, and/or Sn] containing material.

Devices and methods for making polycrystalline alloys

A process for preparing alloy products is described using a self-sustaining or self-propagating SHS-type combustion process with point-source ignition, preferably a laser, in a pressurized vessel. Binary, ternary and quaternary alloys can be formed with control over polycrystalline structure and bandgap. Methods to tune the bandgap and the alloys formed are described. The alloy products may be doped. Preferably sulfides, tellurides or selenides are formed. Cooling during reaction takes place.

Devices and methods for making polycrystalline alloys

A process for preparing alloy products is described using a self-sustaining or self-propagating SHS-type combustion process with point-source ignition, preferably a laser, in a pressurized vessel. Binary, ternary and quaternary alloys can be formed with control over polycrystalline structure and bandgap. Methods to tune the bandgap and the alloys formed are described. The alloy products may be doped. Preferably sulfides, tellurides or selenides are formed. Cooling during reaction takes place.

CERAMIC RADIATION DETECTOR DEVICE AND METHOD
20210395152 · 2021-12-23 ·

A ceramic lithium indium diselenide or like radiation detector device formed as a pressed material that exhibits scintillation properties substantially identical to a corresponding single crystal growth radiation detector device, exhibiting the intrinsic property of the chemical compound, with an acceptable decrease in light output, but at a markedly lower cost due to the time savings associated with pressing versus single crystal growth.