C04B40/0658

Sorel cement composition and method to cure loss of circulation
11148977 · 2021-10-19 · ·

A system and method for applying a cement composition, including storing a slurry, adding magnesium oxide to the slurry to give a magnesium-oxychloride cement slurry, pumping the magnesium-oxychloride cement slurry into a wellbore, and sealing a loss circulation zone in the wellbore.

GEOPOLYMER CEMENT FOR USE IN SUBTERRANEAN OPERATIONS

Methods and compositions for using geopolymers to create storable cementitious slurries used for oil and gas well cementing are provided. The methods of the present disclosure include providing a set-delayed geopolymer cement composition including a geopolymer; activating the set-delayed geopolymer cement composition; introducing the set-delayed geopolymer cement composition into at least a portion of a subterranean formation; and allowing the set-delayed geopolymer cement composition to set in the subterranean formation.

GEOPOLYMER CEMENT FOR USE IN SUBTERRANEAN OPERATIONS

Methods and compositions for using geopolymers to create storable cementitious slurries used for oil and gas well cementing are provided. The methods of the present disclosure include providing a set-delayed geopolymer cement composition including a geopolymer; activating the set-delayed geopolymer cement composition; introducing the set-delayed geopolymer cement composition into at least a portion of a subterranean formation; and allowing the set-delayed geopolymer cement composition to set in the subterranean formation.

Phosphorylated amino polycarboxylic acid cement retarder

A variety of systems, methods and compositions are disclosed, including, in one method, a method of cementing may comprise: providing a cement composition comprising: a hydraulic cement comprising Portland cement in an amount of about 50% by weight of hydraulic cement or less, water, and a phosphorylated amino polycarboxylic acid cement retarder; placing the cement composition in a wellbore; and allowing the cement composition to set. A cement composition, the composition comprising: a hydraulic cement comprising Portland cement in an amount of about 50% by weight of hydraulic cement or less; water; and a phosphorylated amino polycarboxylic acid cement retarder.

Phosphorylated amino polycarboxylic acid cement retarder

A variety of systems, methods and compositions are disclosed, including, in one method, a method of cementing may comprise: providing a cement composition comprising: a hydraulic cement comprising Portland cement in an amount of about 50% by weight of hydraulic cement or less, water, and a phosphorylated amino polycarboxylic acid cement retarder; placing the cement composition in a wellbore; and allowing the cement composition to set. A cement composition, the composition comprising: a hydraulic cement comprising Portland cement in an amount of about 50% by weight of hydraulic cement or less; water; and a phosphorylated amino polycarboxylic acid cement retarder.

Cement Activator Composition for Treatment of Subterranean Formations

Various embodiments disclosed relate to cement activator compositions for treatment of subterranean formations. In various embodiments, the present invention provides a method of treating a subterranean formation including placing in the subterranean formation a liquid cement activator composition including water, an alkali sulfate salt, a polyphosphate salt, and a stabilizer polymer.

Sorel Cement Composition and Method to Cure Loss of Circulation
20210101833 · 2021-04-08 ·

A system and method for applying a cement composition, including storing a slurry, adding magnesium oxide to the slurry to give a magnesium-oxychloride cement slurry, pumping the magnesium-oxychloride cement slurry into a wellbore, and sealing a loss circulation zone in the wellbore.

Sorel Cement Composition and Method to Cure Loss of Circulation
20210101833 · 2021-04-08 ·

A system and method for applying a cement composition, including storing a slurry, adding magnesium oxide to the slurry to give a magnesium-oxychloride cement slurry, pumping the magnesium-oxychloride cement slurry into a wellbore, and sealing a loss circulation zone in the wellbore.

Extended-life calcium aluminophosphate cement compositions

Methods, compositions, and systems for cementing are included. The method comprises providing an extended-life calcium aluminophosphate cement composition comprising calcium aluminate cement, a polyphosphate, water, and a cement set retarder. The method further comprises mixing the extended-life calcium aluminophosphate cement composition with a cement set activator to activate the extended-life calcium aluminophosphate cement composition, introducing the activated extended-life calcium aluminophosphate cement composition into a subterranean formation, and allowing the activated extended-life calcium aluminophosphate cement composition to set in the subterranean formation.

Extended-life calcium aluminophosphate cement compositions

Methods, compositions, and systems for cementing are included. The method comprises providing an extended-life calcium aluminophosphate cement composition comprising calcium aluminate cement, a polyphosphate, water, and a cement set retarder. The method further comprises mixing the extended-life calcium aluminophosphate cement composition with a cement set activator to activate the extended-life calcium aluminophosphate cement composition, introducing the activated extended-life calcium aluminophosphate cement composition into a subterranean formation, and allowing the activated extended-life calcium aluminophosphate cement composition to set in the subterranean formation.