C04B2103/0017

COATING STRUCTURE, TURBINE PART HAVING SAME, AND METHOD FOR MANUFACTURING COATING STRUCTURE

Provided are a coating structure, a turbine part having the same, and a method for manufacturing the coating structure. The coating structure is provided on a surface of a base portion including a ceramic matrix composite. The coating structure is layered on the surface of the base portion, and includes a bond coat layer formed of a rare-earth silicate and a top coat layer layered on the bond coat layer. The residual stress present in the bond coat layer is compressive residual stress. The oxygen permeability coefficient of the bond coat layer is no greater than 10.sup.9 kg.Math.m.sup.1.Math.s.sup.1 at a temperature of not lower than 1200 C. and a higher oxygen partial pressure of not less than 0.02 MPa. The bond coat layer may contain carbonitride particles or carbonitride whiskers.

COATING STRUCTURE, TURBINE PART HAVING SAME, AND METHOD FOR MANUFACTURING COATING STRUCTURE

Provided are a coating structure, a turbine part having the same, and a method for manufacturing the coating structure. The coating structure is provided on a surface of a base portion including a ceramic matrix composite. The coating structure is layered on the surface of the base portion, and includes a bond coat layer formed of a rare-earth silicate and a top coat layer layered on the bond coat layer. The residual stress present in the bond coat layer is compressive residual stress. The oxygen permeability coefficient of the bond coat layer is no greater than 10.sup.9 kg.Math.m.sup.1.Math.s.sup.1 at a temperature of not lower than 1200 C. and a higher oxygen partial pressure of not less than 0.02 MPa. The bond coat layer may contain carbonitride particles or carbonitride whiskers.

Environmental barrier coating

An environmental barrier coating includes a barrier layer which includes a matrix, diffusive particles, and gettering particles; and a calcium-magnesia alumina-silicate (CMAS)-resistant component. The CMAS-resistant component includes hafnium silicate and a rare earth hafnate. An article and a method of fabricating an article are also disclosed.

Environmental barrier coating

An environmental barrier coating includes a barrier layer which includes a matrix, diffusive particles, and gettering particles; and a calcium-magnesia alumina-silicate (CMAS)-resistant component. The CMAS-resistant component includes hafnium silicate and a rare earth hafnate. An article and a method of fabricating an article are also disclosed.

Compositions for cores used in investment casting

The present disclosure generally relates to a ceramic core comprising predominantly mullite, which is derived from a precursor comprising alumina particles and siloxane binders. Free silica is present in the ceramic body, but is largely unavailable for reaction with metal alloys used in investment casting. Methods of making cast metal articles are also disclosed.

Compositions for cores used in investment casting

The present disclosure generally relates to a ceramic core comprising predominantly mullite, which is derived from a precursor comprising alumina particles and siloxane binders. Free silica is present in the ceramic body, but is largely unavailable for reaction with metal alloys used in investment casting. Methods of making cast metal articles are also disclosed.

COMPOSITIONS FOR CORES USED IN INVESTMENT CASTING

The present disclosure generally relates to a ceramic core comprising predominantly mullite, which is derived from a precursor comprising alumina particles and siloxane binders. Free silica is present in the ceramic body, but is largely unavailable for reaction with metal alloys used in investment casting. Methods of making cast metal articles are also disclosed.

COMPOSITIONS FOR CORES USED IN INVESTMENT CASTING

The present disclosure generally relates to a ceramic core comprising predominantly mullite, which is derived from a precursor comprising alumina particles and siloxane binders. Free silica is present in the ceramic body, but is largely unavailable for reaction with metal alloys used in investment casting. Methods of making cast metal articles are also disclosed.

Protective coating for ceramic matrix composites
12351531 · 2025-07-08 · ·

An article has a substrate and a layer atop the substrate. The layer has: a matrix comprising at least one of hafnium silicate (HfSiO.sub.4) and ytterbium disilicate (Yb.sub.2Si.sub.2O.sub.7); and barium magnesium alumino silicate (BMAS).

Protective coating for ceramic matrix composites
12351531 · 2025-07-08 · ·

An article has a substrate and a layer atop the substrate. The layer has: a matrix comprising at least one of hafnium silicate (HfSiO.sub.4) and ytterbium disilicate (Yb.sub.2Si.sub.2O.sub.7); and barium magnesium alumino silicate (BMAS).