C04B2111/00215

Composite mineralizers/fluxes for the production of alite/calcium sulfoaluminate clinkers

A cement clinker composition incorporates calcium fluoride and iron oxide to reduce firing temperatures and increase strength. High fly ash, aluminum dross, aluminum scrap, high aluminum clays and combinations thereof may also be substituted for bauxite in the cement clinker composition.

Lime-based cement extender compositions, and associated systems and methods

A composition configured to be mixed with cement, and associated systems and methods are disclosed herein. In some embodiments, the composition includes at least 10% by weight lime particles, and at least 35% by weight pozzolan particles. Properties of the composition can include a magnesium oxide concentration of at least 0.5%, and an iron oxide concentration of at least 0.5-2.0%, an aluminum oxide concentration of 2-8%, a silicon dioxide concentration of 20-40%, a potassium oxide concentration of 20,000-30,000 ppm, and a sodium oxide concentration of 10,000-20,000 ppm. In some embodiments, the lime-based cement extender composition, or product, is combined with cement to produce a cement blend for use in the mining industry as mine backfill.

HYDRATED SODIUM SILICATE ALUMINATE AS A BINDER AGENT FOR INORGANIC SUBSTRATES

Embodiments relate to the development of binder agents, and specifically to a hydrated silicate aluminate binder agents. The binder agents, whether combined or not with hardener agents, offer significant improvements in terms of mechanical strength and water resistance compared to soluble sodium-based silicates when used as agents for inorganic and organic substrates.

LIME-BASED CEMENT EXTENDER COMPOSITIONS, AND ASSOCIATED SYSTEMS AND METHODS

A composition configured to be mixed with cement, and associated systems and methods are disclosed herein. In some embodiments, the composition includes at least 10% by weight lime particles, and at least 35% by weight pozzolan particles. Properties of the composition can include a magnesium oxide concentration of at least 0.5%, and an iron oxide concentration of at least 0.5-2.0%, an aluminum oxide concentration of 2-8%, a silicon dioxide concentration of 20-40%, a potassium oxide concentration of 20,000-30,000 ppm, and a sodium oxide concentration of 10,000-20,000 ppm. In some embodiments, the lime-based cement extender composition, or product, is combined with cement to produce a cement blend for use in the mining industry as mine backfill.

Comprehensive utilization method for iron separation tailings from magnetizing-roasted red mud

A comprehensive utilization method for iron separation tailings from magnetizing-roasted red mud includes the following steps: performing a wet magnetic separation for tailing discarding on iron separation tailings from magnetizing-roasted red mud, to obtain a rough concentrate and non-magnetic minerals; performing a purification by gravity separation on the rough concentrate to obtain a wet iron concentrate and light minerals; dehydrating the wet iron concentrate to obtain an iron concentrate; combining, and then dehydrating, drying, and disintegrating the non-magnetic minerals and the light minerals, to obtain iron extraction tailings; uniformly mixing the iron extraction tailings, and crushed, ground, and dried limestone, clay, and quartz sand separation tailings according to a predetermined ratio to obtain a cement raw meal; pressing, and then calcining and quenching the cement raw meal to obtain a cement clinker; and mixing the cement clinker and a gypsum followed by a dry grinding to obtain a silicate cement.