Patent classifications
C08G59/20
THERMALLY REWORKABLE ADHESIVES FOR ELECTRONIC DEVICES
A thermally reworkable adhesive includes at least one di-epoxide, at least one diamine that is reactive with the at least one di-epoxide, at least one additive that is miscible, but not reactive, with the at least one di-epoxide and/or the at least one diamine. Reaction of the at least one di-epoxide and the at least one diamine forms a crosslinked polymer network and the at least one additive offsets the stoichiometry of the crosslinked polymer network by 5-50%. The offset crosslinked polymer network forms the thermally reworkable adhesive that once cured, at a temperature in the range of 20-200° C., can be de-bonded from a device to which it is attached at a temperature in the range of 50-200° C.
ADDITIVES FOR WINTERIZATION OF PARAFFIN INHIBITORS
A winterized paraffin inhibitor, which is capable of being used for preventing the deposition of paraffins in hydrocarbon streams and capable of withstanding freezing or crystallization at freezing or sub-freezing temperatures, may be formed by adding an oxyalkylated branched aliphatic compound having 12 or more carbons to a high molecular weight aliphatic polymer paraffin inhibitor, the oxyalkylated branched aliphatic compound having 12 or more carbons being produced by the oxyalkylation of the branched aliphatic compound having 12 or more carbon atoms in which the branched aliphatic compound having 12 or more carbon atoms is grafted with a polyether via a ring-opening reaction, wherein the polyether is a polymer of ethylene oxide, propylene oxide, butylene oxide, and combinations thereof.
ADDITIVES FOR WINTERIZATION OF PARAFFIN INHIBITORS
A winterized paraffin inhibitor, which is capable of being used for preventing the deposition of paraffins in hydrocarbon streams and capable of withstanding freezing or crystallization at freezing or sub-freezing temperatures, may be formed by adding an oxyalkylated branched aliphatic compound having 12 or more carbons to a high molecular weight aliphatic polymer paraffin inhibitor, the oxyalkylated branched aliphatic compound having 12 or more carbons being produced by the oxyalkylation of the branched aliphatic compound having 12 or more carbon atoms in which the branched aliphatic compound having 12 or more carbon atoms is grafted with a polyether via a ring-opening reaction, wherein the polyether is a polymer of ethylene oxide, propylene oxide, butylene oxide, and combinations thereof.
ROOM TEMPERATURE STABLE ONE-PART VOID FILLER
A curable void filler composition comprising at least one epoxy resin; at least one epoxy curing agent comprising at least one bicyclic carboxylic acid anhydride; and at least one epoxysilane compound according to formula (1), where formula (1) is Glycidoxy-R1Si(OR2)(OR3)(OR4), and R1 is selected from linear or branched alkyl comprising from 1 and 15 carbon atoms; and R2, R4 and R4 may be different or the same, and are independently selected from linear or branched alkyl comprising from 2 to 15 carbon atoms.
ROOM TEMPERATURE STABLE ONE-PART VOID FILLER
A curable void filler composition comprising at least one epoxy resin; at least one epoxy curing agent comprising at least one bicyclic carboxylic acid anhydride; and at least one epoxysilane compound according to formula (1), where formula (1) is Glycidoxy-R1Si(OR2)(OR3)(OR4), and R1 is selected from linear or branched alkyl comprising from 1 and 15 carbon atoms; and R2, R4 and R4 may be different or the same, and are independently selected from linear or branched alkyl comprising from 2 to 15 carbon atoms.
Sizing agent for carbon fibers, aqueous dispersion of sizing agent for carbon fibers, and sizing agent-adhered carbon fiber bundle
A sizing agent for carbon fiber includes component (A), component (B), and component (C), in which the component (A) is at least one selected from the group consisting of component (A-1), component (A-2), and component (A-3); the component (A-1) is a urethane compound having a structure of Formula (1-1) in the molecule, the component (A-2) is an ester compound having a structure represented by Formula (1-2) in the molecule, the component (A-3) is an amide compound having a structure of Formula (1-3) in the molecule; the component (B) is an epoxy compound selected from the group consisting of an epoxy compound represented by Formula (2), an epoxy compound represented by Formula (3), and an epoxy compound represented by Formula (4); and the component (C) is a bisphenol type epoxy compound.
Sizing agent for carbon fibers, aqueous dispersion of sizing agent for carbon fibers, and sizing agent-adhered carbon fiber bundle
A sizing agent for carbon fiber includes component (A), component (B), and component (C), in which the component (A) is at least one selected from the group consisting of component (A-1), component (A-2), and component (A-3); the component (A-1) is a urethane compound having a structure of Formula (1-1) in the molecule, the component (A-2) is an ester compound having a structure represented by Formula (1-2) in the molecule, the component (A-3) is an amide compound having a structure of Formula (1-3) in the molecule; the component (B) is an epoxy compound selected from the group consisting of an epoxy compound represented by Formula (2), an epoxy compound represented by Formula (3), and an epoxy compound represented by Formula (4); and the component (C) is a bisphenol type epoxy compound.
Additives for winterization of paraffin inhibitors
A winterized paraffin inhibitor, which is capable of being used for preventing the deposition of paraffins in hydrocarbon streams and capable of withstanding freezing or crystallization at freezing or sub-freezing temperatures, may be formed by adding an oxyalkylated branched aliphatic compound having 12 or more carbons to a high molecular weight aliphatic polymer paraffin inhibitor, the oxyalkylated branched aliphatic compound having 12 or more carbons being produced by the oxyalkylation of the branched aliphatic compound having 12 or more carbon atoms in which the branched aliphatic compound having 12 or more carbon atoms is grafted with a polyether via a ring-opening reaction, wherein the polyether is a polymer of ethylene oxide, propylene oxide, butylene oxide, and combinations thereof.
Additives for winterization of paraffin inhibitors
A winterized paraffin inhibitor, which is capable of being used for preventing the deposition of paraffins in hydrocarbon streams and capable of withstanding freezing or crystallization at freezing or sub-freezing temperatures, may be formed by adding an oxyalkylated branched aliphatic compound having 12 or more carbons to a high molecular weight aliphatic polymer paraffin inhibitor, the oxyalkylated branched aliphatic compound having 12 or more carbons being produced by the oxyalkylation of the branched aliphatic compound having 12 or more carbon atoms in which the branched aliphatic compound having 12 or more carbon atoms is grafted with a polyether via a ring-opening reaction, wherein the polyether is a polymer of ethylene oxide, propylene oxide, butylene oxide, and combinations thereof.
Additives for winterization of paraffin inhibitors
A winterized paraffin inhibitor, which is capable of being used for preventing the deposition of paraffins in hydrocarbon streams and capable of withstanding freezing or crystallization at freezing or sub-freezing temperatures, may be formed by adding an oxyalkylated branched aliphatic compound having 12 or more carbons to a high molecular weight aliphatic polymer paraffin inhibitor, the oxyalkylated branched aliphatic compound having 12 or more carbons being produced by the oxyalkylation of the branched aliphatic compound having 12 or more carbon atoms in which the branched aliphatic compound having 12 or more carbon atoms is grafted with a polyether via a ring-opening reaction, wherein the polyether is a polymer of ethylene oxide, propylene oxide, butylene oxide, and combinations thereof.