C08L9/04

Method for producing rubber wet masterbatch and method for producing rubber composition
11459428 · 2022-10-04 · ·

A method for producing a rubber wet master batch is disclosed including: producing a carbon black-containing rubber latex solution by mixing carbon black, a dispersion solvent and a rubber latex solution; producing a carbon black-containing rubber coagulum by coagulating the thus-obtained carbon black-containing rubber latex solution; and producing a rubber wet master batch by dehydrating and drying the thus-obtained carbon black-containing rubber coagulum. With respect to this method for producing a rubber wet master batch, the carbon black satisfies conditions such that: the DBP oil absorption is 105-230 mL/100 g; STSA is 90-205 m.sup.2/g; and the value obtained by subtracting the value of STSA from the value of DBP oil absorption is 15 or more. This method for producing a rubber wet master batch enables the achievement of a vulcanized rubber that has wear resistance and low heat generation properties.

A LATEX DIPPED ARTICLE CONTAINING A NATURAL MINERAL COMPOSITE WITH A MAGNETICALLY DETECTABLE PROPERTY AND METHOD OF MAKING

A latex dipped article, specifically an unsupported glove having magnetically detectable property and its method of manufacturing is disclosed here. The glove contains at least one layer of elastomeric material that consist of a composition of evenly dispersed natural mineral composite containing; magnetite, illmenite, zircorn and quartz. The composition renders the article or small pieces of the latex dipped article magnetically detectable property.

A LATEX DIPPED ARTICLE CONTAINING A NATURAL MINERAL COMPOSITE WITH A MAGNETICALLY DETECTABLE PROPERTY AND METHOD OF MAKING

A latex dipped article, specifically an unsupported glove having magnetically detectable property and its method of manufacturing is disclosed here. The glove contains at least one layer of elastomeric material that consist of a composition of evenly dispersed natural mineral composite containing; magnetite, illmenite, zircorn and quartz. The composition renders the article or small pieces of the latex dipped article magnetically detectable property.

ELASTOMERIC GLOVE AND METHOD OF FABRICATION

An elastomeric glove includes a body-facing layer of a first elastomeric material, a middle layer of a second elastomeric material, and an outer layer of a third elastomeric material different than at least the second elastomeric material. The third elastomeric material has an acrylonitrile content greater than at least the second elastomeric material.

ELASTOMERIC GLOVE AND METHOD OF FABRICATION

An elastomeric glove includes a body-facing layer of a first elastomeric material, a middle layer of a second elastomeric material, and an outer layer of a third elastomeric material different than at least the second elastomeric material. The third elastomeric material has an acrylonitrile content greater than at least the second elastomeric material.

Elastomeric composition for an elastomeric article
11390743 · 2022-07-19 · ·

The present invention relates to an elastomeric composition, wherein the elastomeric composition comprises an additive selected from any one or a combination of fluorine and silicone compounds in the production of a hypoallergenic elastomeric article.

Latex composition
11414536 · 2022-08-16 · ·

A latex composition including a latex (A) of a diene rubber (a) having a weight average molecular weight of 50,000 or more and 1,000,000 or less and containing an ethylenically unsaturated acid monomer unit; and a latex (B) of a diene rubber (b) having a weight average molecular weight of 500 or more and less than 50,000 and containing an ethylenically unsaturated acid monomer unit.

Latex composition
11414536 · 2022-08-16 · ·

A latex composition including a latex (A) of a diene rubber (a) having a weight average molecular weight of 50,000 or more and 1,000,000 or less and containing an ethylenically unsaturated acid monomer unit; and a latex (B) of a diene rubber (b) having a weight average molecular weight of 500 or more and less than 50,000 and containing an ethylenically unsaturated acid monomer unit.

Latex composition
11414536 · 2022-08-16 · ·

A latex composition including a latex (A) of a diene rubber (a) having a weight average molecular weight of 50,000 or more and 1,000,000 or less and containing an ethylenically unsaturated acid monomer unit; and a latex (B) of a diene rubber (b) having a weight average molecular weight of 500 or more and less than 50,000 and containing an ethylenically unsaturated acid monomer unit.

Carboxylic Acid Modified-Nitrile Based Copolymer Latex
20220251346 · 2022-08-11 · ·

A carboxylic acid-modified nitrile-based copolymer latex includes a carboxylic acid-modified nitrile-based copolymer including: 65.5 wt % to 82.5 wt % of a conjugated diene-based monomer-derived unit, 15 wt % to 30 wt % of an ethylenic unsaturated nitrile-based monomer-derived unit, and 2.5 wt % to 4.5 wt % of an ethylenic unsaturated acid monomer-derived unit, wherein the carboxylic acid-modified nitrile-based copolymer latex satisfies General Formula 1:


1.0 mm.sup.2/s≤CV.sub.0≤3.0 mm.sup.2/s  [General Formula 1]

wherein CV.sub.0 represents a capillary viscosity of the carboxylic acid-modified nitrile-based copolymer latex which is measured in a swollen state in a methyl ethyl ketone solvent.