C08L23/04

AQUEOUS DISPERSION AND LAMINATE
20220411675 · 2022-12-29 ·

An object of the present invention is to provide an aqueous dispersion with which a coating film having small dynamic frictional resistance can be formed immediately after coating. The present invention includes an aqueous dispersion containing a polyolefin (A), as unsaturated carboxylic acid polymer (B), an amide-based wax (C), and water.

AQUEOUS DISPERSION AND LAMINATE
20220411675 · 2022-12-29 ·

An object of the present invention is to provide an aqueous dispersion with which a coating film having small dynamic frictional resistance can be formed immediately after coating. The present invention includes an aqueous dispersion containing a polyolefin (A), as unsaturated carboxylic acid polymer (B), an amide-based wax (C), and water.

High strength heat resistant rubber composition and process for producing high strength heat resistant rubber product
11535730 · 2022-12-27 · ·

According to the invention, a high strength heat resistant rubber composition having both excellent strength and heat resistance, comprising: 80 to 85 parts by mass of a rubber base material; 5 to 11 parts by mass of attapulgite; 40 to 50 parts by mass of a linear low-density polyethylene; 4 to 6 parts by mass of a ceramic powder; 2 to 6 parts by mass of a cross-linking agent; 5 to 9 parts by mass of a filler; 5 to 9 parts by mass of a cross-linking aid; 8 to 13 parts by mass of rosin; 12 to 16 parts by mass of bismaleimide; and 7 to 12 parts by mass of yttrium oxide and a process for producing a high strength heat resistant rubber product using the composition are provided.

High strength heat resistant rubber composition and process for producing high strength heat resistant rubber product
11535730 · 2022-12-27 · ·

According to the invention, a high strength heat resistant rubber composition having both excellent strength and heat resistance, comprising: 80 to 85 parts by mass of a rubber base material; 5 to 11 parts by mass of attapulgite; 40 to 50 parts by mass of a linear low-density polyethylene; 4 to 6 parts by mass of a ceramic powder; 2 to 6 parts by mass of a cross-linking agent; 5 to 9 parts by mass of a filler; 5 to 9 parts by mass of a cross-linking aid; 8 to 13 parts by mass of rosin; 12 to 16 parts by mass of bismaleimide; and 7 to 12 parts by mass of yttrium oxide and a process for producing a high strength heat resistant rubber product using the composition are provided.

Peroxide containing polyolefin formulation
11535731 · 2022-12-27 · ·

A process of melt compounding a polyolefin formulation comprising a ethylenic-based (co)polymer, an antioxidant, and from 0.15 to 1.00 weight percent of an organic peroxide having a 1-hour half-life temperature of less than or equal to 155 degrees Celsius (° C.) and/or a 10-hour half-life temperature of less than or equal to 135° C. Also, intermediate compositions having a modified rheology and crosslinked polyolefin products made therefrom; methods of making and using same; and articles containing same.

Peroxide containing polyolefin formulation
11535731 · 2022-12-27 · ·

A process of melt compounding a polyolefin formulation comprising a ethylenic-based (co)polymer, an antioxidant, and from 0.15 to 1.00 weight percent of an organic peroxide having a 1-hour half-life temperature of less than or equal to 155 degrees Celsius (° C.) and/or a 10-hour half-life temperature of less than or equal to 135° C. Also, intermediate compositions having a modified rheology and crosslinked polyolefin products made therefrom; methods of making and using same; and articles containing same.

Weather-resistant flame-retardant resin composition, optical fiber cable, and electric wire

A weather-resistant flame-retardant resin composition includes: a polyolefin resin; a mixture of (poly) phosphate compounds, a total content of which is from 10 to 50 parts by mass with respect to 100 parts by mass of the polyolefin resin; 0.1 to 10 parts by mass a non-crosslinked silicone raw rubber having a number-average molecular weight of 10,000 to 1,000,000; and 0.1 to 20 parts by mass of an inorganic UV light shielding agent, and an electric wire and an optical fiber cable whose jacket is formed by the weather-resistant flame-retardant resin.

Weather-resistant flame-retardant resin composition, optical fiber cable, and electric wire

A weather-resistant flame-retardant resin composition includes: a polyolefin resin; a mixture of (poly) phosphate compounds, a total content of which is from 10 to 50 parts by mass with respect to 100 parts by mass of the polyolefin resin; 0.1 to 10 parts by mass a non-crosslinked silicone raw rubber having a number-average molecular weight of 10,000 to 1,000,000; and 0.1 to 20 parts by mass of an inorganic UV light shielding agent, and an electric wire and an optical fiber cable whose jacket is formed by the weather-resistant flame-retardant resin.

Polyethylene with polycarbonate-siloxane for increased environmental stress crack resistance

A polyethylene composition having increased environmental stress crack resistance (ESCR) is comprised of a polymer blend of a high density polyethylene (HDPE) and a polycarbonate-siloxane copolymer. The polycarbonate-siloxane copolymer is present in the polymer blend in an amount of from 0.5 wt. % to 15 wt. % by total weight of the polymer blend. In a method of forming a polyethylene composition having increased ESCR, a HDPE is modified by combining the HDPE with a polycarbonate-siloxane copolymer in a polymer blend, the polycarbonate-siloxane copolymer being present in an amount of from 0.5 wt. % to 15 wt. % by total weight of the polymer blend. The polymer blend can be formed into an article of manufacture, such as a bottle cap.

Polyethylene with polycarbonate-siloxane for increased environmental stress crack resistance

A polyethylene composition having increased environmental stress crack resistance (ESCR) is comprised of a polymer blend of a high density polyethylene (HDPE) and a polycarbonate-siloxane copolymer. The polycarbonate-siloxane copolymer is present in the polymer blend in an amount of from 0.5 wt. % to 15 wt. % by total weight of the polymer blend. In a method of forming a polyethylene composition having increased ESCR, a HDPE is modified by combining the HDPE with a polycarbonate-siloxane copolymer in a polymer blend, the polycarbonate-siloxane copolymer being present in an amount of from 0.5 wt. % to 15 wt. % by total weight of the polymer blend. The polymer blend can be formed into an article of manufacture, such as a bottle cap.