C08L71/14

CURABLE COMPOSITION AND CURED PRODUCT THEREOF

A curable composition includes an olefin-aromatic vinyl compound-aromatic polyene copolymer satisfying conditions (1) to (4) and an additive resin, which is a polyphenylene ether. (1) The number average molecular weight of the copolymer is 5000 to 100000. (2) The aromatic vinyl compound monomer has 8 to 20 carbon atoms, and the content of the unit of the monomer is 0 to 70 mass %. (3) The aromatic polyene is selected from polyenes having 5 to 20 carbon atoms and a plurality of vinyl and/or vinylene groups in the molecule, and the content of the groups is 1.5 to 20 pieces per number average molecular weight. (4) The olefin is selected from olefins having 2 to 20 carbon atoms, and the total monomer units of the olefin, aromatic vinyl compound, and aromatic polyene is 100 mass %.

CURABLE COMPOSITION AND CURED PRODUCT THEREOF

A curable composition includes an olefin-aromatic vinyl compound-aromatic polyene copolymer satisfying conditions (1) to (4) and an additive resin, which is a polyphenylene ether. (1) The number average molecular weight of the copolymer is 5000 to 100000. (2) The aromatic vinyl compound monomer has 8 to 20 carbon atoms, and the content of the unit of the monomer is 0 to 70 mass %. (3) The aromatic polyene is selected from polyenes having 5 to 20 carbon atoms and a plurality of vinyl and/or vinylene groups in the molecule, and the content of the groups is 1.5 to 20 pieces per number average molecular weight. (4) The olefin is selected from olefins having 2 to 20 carbon atoms, and the total monomer units of the olefin, aromatic vinyl compound, and aromatic polyene is 100 mass %.

COPOLYMER AND LAMINATE CONTAINING SAME

A laminate has an olefin-aromatic vinyl compound-aromatic polyene copolymer and a metal foil. The number average molecular copolymer weight is between 5000 and 100000; the aromatic vinyl compound monomer is aromatic vinyl compound having between 8 and 20 carbon atoms, and the aromatic vinyl compound monomer unit content is between 10 and 60 mass %; the aromatic polyene is selected having between 5 and 20 carbon atoms and vinyl and/or vinylene groups in the molecule, the content derived from the aromatic polyene unit is between 1.5 and 20 pieces per number average molecular weight; and the olefin is selected having between 2 and 20 carbon atoms, being ethylene alone, or having a mass ratio of -olefin monomer components other than ethylene to an ethylene monomer component contained in the olefin, of 1/7 or less, and the total monomer units of the olefin, aromatic vinyl compound, and aromatic polyene is 100 mass %.

COPOLYMER AND LAMINATE CONTAINING SAME

A laminate has an olefin-aromatic vinyl compound-aromatic polyene copolymer and a metal foil. The number average molecular copolymer weight is between 5000 and 100000; the aromatic vinyl compound monomer is aromatic vinyl compound having between 8 and 20 carbon atoms, and the aromatic vinyl compound monomer unit content is between 10 and 60 mass %; the aromatic polyene is selected having between 5 and 20 carbon atoms and vinyl and/or vinylene groups in the molecule, the content derived from the aromatic polyene unit is between 1.5 and 20 pieces per number average molecular weight; and the olefin is selected having between 2 and 20 carbon atoms, being ethylene alone, or having a mass ratio of -olefin monomer components other than ethylene to an ethylene monomer component contained in the olefin, of 1/7 or less, and the total monomer units of the olefin, aromatic vinyl compound, and aromatic polyene is 100 mass %.

Binder composition for making foundry molds
09636742 · 2017-05-02 · ·

A binder composition for making foundry molds, comprising an acid-hardening resin, one or more 5-position-substituted-furfural compounds selected from the group consisting of 5-hydroxymethylfurfural and 5-acetoxymethylfurfural, and one or more compounds selected from the group consisting of urea and derivatives of urea, wherein the content of the 5-position-substituted-furfural compound(s) by percentage is from 1 to 60% by weight of the binder composition. The content of the compound(s) by percentage selected from the group consisting of urea and derivatives of urea is preferably from 0.3 to 10% by weight of the binder composition.

Binder composition for making foundry molds
09636742 · 2017-05-02 · ·

A binder composition for making foundry molds, comprising an acid-hardening resin, one or more 5-position-substituted-furfural compounds selected from the group consisting of 5-hydroxymethylfurfural and 5-acetoxymethylfurfural, and one or more compounds selected from the group consisting of urea and derivatives of urea, wherein the content of the 5-position-substituted-furfural compound(s) by percentage is from 1 to 60% by weight of the binder composition. The content of the compound(s) by percentage selected from the group consisting of urea and derivatives of urea is preferably from 0.3 to 10% by weight of the binder composition.

ONE-COMPONENT COMPOSITION, FURAN RESIN CURED PRODUCT, AND KIT

Provided is a one-component composition that can be cured in a short time and can provide a furan resin cured product having excellent heat resistance and electric property, the furan resin cured product, and a kit that can provide the furan resin cured product. One aspect of the embodiment is a one-component composition that comprises a furan resin, an acid scavenger, and an acid catalyst in which the acid scavenger comprises an epoxy resin.

ONE-COMPONENT COMPOSITION, FURAN RESIN CURED PRODUCT, AND KIT

Provided is a one-component composition that can be cured in a short time and can provide a furan resin cured product having excellent heat resistance and electric property, the furan resin cured product, and a kit that can provide the furan resin cured product. One aspect of the embodiment is a one-component composition that comprises a furan resin, an acid scavenger, and an acid catalyst in which the acid scavenger comprises an epoxy resin.

ONE-COMPONENT COMPOSITION, FURAN RESIN CURED PRODUCT, AND KIT

Provided is a one-component composition that can be cured in a short time and can provide a furan resin cured product having excellent heat resistance and electric property, the furan resin cured product, and a kit that can provide the furan resin cured product. One aspect of the embodiment is a one-component composition that comprises a furan resin, an acid scavenger, and an acid catalyst in which the acid scavenger comprises an epoxy resin.

COMPOSITE MATERIAL BASED ON CHARCOAL AND POLYMER BINDER

Subject of the invention is a composite material comprising charcoal powder which is dispersed in a polymer matrix, wherein the polymer comprises polyfurfuryl alcohol (PFA). The invention also relates to shaped objects comprising the composite material, uses thereof and methods for the production.