B23K11/0873

Electric resistance welded steel pipe

An electric resistance welded steel pipe which has sufficient strength and low-temperature toughness and a low yield ratio and which is suitable as a line pipe to be laid in depths of the sea, characterized in that: the composition of the base material contains, in mass %, 0.05 to 0.10% of C, 1.00 to 1.60% of Mn, and 0.005 to less than 0.035% of Nb, and has a Ceq value of 0.23 to 0.38; and the metal microstructure of the base material contains 3 to 13% of martensite in area fraction with the balance being ferrite.

Low-yield ratio high-strength electric resistance welded steel pipe, steel strip for electric resistance welded steel pipes, and methods of manufacturing them
09765417 · 2017-09-19 · ·

A low-yield ratio high-strength electric resistance welded steel pipe has a yield ratio of 80% or less and a TS of 655 MPa or more. A steel material has a composition containing 0.38% to 0.45% C, 0.1% to 0.3% Si, 1.0% to 1.8% Mn, 0.03% or less P, 0.03% or less S, 0.01% to 0.07% sol. Al, and 0.01% or less N on a mass basis.

ELECTRIC RESISTANCE-WELDED STEEL TUBE FOR HOLLOW STABILIZER, HOLLOW STABILIZER, AND MANUFACTURING METHODS OF SAME
20220186331 · 2022-06-16 ·

This electric resistance-welded steel tube for a hollow stabilizer is an electric resistance-welded steel tube for a hollow stabilizer including a base material portion and a weld, in which the base material portion has predetermined chemical components, a wall thickness of the base material portion is 2.0 to 6.0 mm, an outer diameter of the electric resistance-welded steel tube is 10 to 40 mm, in a C direction cross section of the electric resistance-welded steel tube, a recessed bead cut is present in a region including the weld on an inner surface side of the electric resistance-welded steel tube, when an imaginary line is drawn from one opening edge to the other opening edge of the bead cut in a shortest distance, a maximum depth from the imaginary line to a bottom of the bead cut is 300 μm or less, a maximum inclusion diameter that is included in the base material portion is 300 μm or less, in the base material portion of the electric resistance-welded steel tube, a surface roughness of the inner surface side is 300 μm or less in terms of a maximum profile valley depth Rv, and maximum hardness of the electric resistance-welded steel tube including the weld is 300 Hv or less.

Article comprising additively manufactured metal portions

An article comprising additively manufactured metal portions is described. The article comprises a first additively manufactured metal portion, and a second additively manufactured metal portion coupled to the first additively manufactured metal portion at a welded joint. The article further comprises a resistive heating material disposed within an interior of the welded joint, the resistive heating material comprising a different material than the first additively manufactured metal portion and the second additively manufactured metal portion.

High frequency power supply system with closely regulated output for heating a workpiece

A method of controlling highly regulated power and frequency from a high frequency power supply system to provide a highly regulated power and frequency to a workpiece load where the highly regulated power and frequency can be independent of the workpiece load characteristics by inverter switching control and an inverter output impedance adjusting and frequency control network that can include precision variable reactor pairs with a geometrically-shaped moveable insert core section and a stationary split-bus section with a complementary geometrically-shaped split bus section and a split electric terminal bus section where the insert core section can be moved relative to the stationary split-bus section to vary the inductance of the variable reactors.

Welding operation monitoring system and welding operation monitoring method

The welding operation monitoring system includes an image capturing device that is disposed on a side opposite to a side to which the plasma flow is supplied out of a pipe inside and a pipe outside of the strip-shaped steel sheet formed in a tubular shape, and is configured to capture a color image including a plasma flow over the V-shaped region; and a welding operation monitoring device that is configured to generate a specific color component image obtained by extracting a specific color component from the color image, and specifies a V-shaped display region, which is a region corresponding to the V-shaped region within the color image, on the basis of the V-shaped region shown in the specific color component image, thereby analyzing a state of the welding operation.

Method of forming a bearing cage segment including a joint edge in the region of a to-be-formed bridge

A method of forming a bearing cage segment includes punching a plurality of openings in a sheet metal band to form a plurality of pockets separated by a plurality of bridges, the bridges having a length direction transverse to a length direction of the band and having a width in the length direction of the band and having a thickness in a direction perpendicular the length direction and to the width, and laser cutting the sheet metal band along one of the plurality of bridges transversely to the length direction of the band to form a joint edge.

Al plated welded pipe for hardening use and Al plated hollow member and method for producing same

An Al plated electric resistance welded steel pipe for hardening use suppressing the formation of scale to the inside of the plating layer while performing hot forming and an Al plated hollow member using that Al plated electric resistance welded steel pipe, wherein the Al plated electric resistance welded steel pipe for hardening use is comprised of a base material made of a tubular steel plate and having a predetermined chemical composition and an electric resistance welded zone provided at a seam portion of the steel plate and extending in a longitudinal direction of the steel plate, the base material is further provided with an intermetallic compound layer positioned on the surface of the steel plate and including an Al—Fe—Si-based intermetallic compound and an Al plating layer positioned on the surface of the intermetallic compound layer and containing Al and Si, and 70×X/D≤Y/t≤30 is satisfied, wherein X (μm) is a thickness of the intermetallic compound layer, Y (μm) is a thickness of the Al plating layer, t (mm) is a pipe thickness of the steel pipe, and D (mm) is an outside diameter of the steel pipe.

Air conditioner
11421292 · 2022-08-23 · ·

The present invention relates to an air conditioner. The air conditioner according to the present embodiment has a refrigeration capacity of 11 kW to 16 kW, inclusive, and uses R32 as a refrigerant circulating therein, and since a refrigerant pipe therein is made of a ductile stainless steel material having 1% or less of a delta-ferrite matrix structure with respect to the grain size area thereof, the refrigerant pipe can maintain strength and hardness as good as or better than those of a copper pipe, while also maintaining good processability.

Air conditioner
11413713 · 2022-08-16 · ·

The present invention relates to an air conditioner. The air conditioner according to the present embodiment has a refrigeration capacity of 7 kW to 11 kW, inclusive, and uses, as a refrigerant, a mixed refrigerant containing 50% or more of R32, and since a refrigerant pipe therein is made of a ductile stainless steel material having 1% or less of a delta-ferrite matrix structure with respect to the grain size area thereof, and includes a suction pipe guiding the suction of the refrigerant into a compressor and having an outer diameter of 15.88 mm, the refrigerant pipe can maintain strength and hardness as good as or better than those of a copper pipe, while also maintaining good processability.