Patent classifications
B29C2948/9259
PELLETIZING APPARATUS FOR THE PRODUCTION OF POLYMER PELLETS
A pelletizing apparatus includes a filter device connected with a melt feed, a granulator downstream of the filter device, particularly an underwater granulator, a water treatment device, and a control means for controlling the filter device, underwater granulator, and water treatment device and adapted to provide at least one control parameter. The apparatus includes at least one machine-readable and -writable identification means for storing and providing an item of component-specific information and being associated with a component in the flow path of the melt or the process water, and a reading device communicating with the control means to receive the component-specific information from the identification means, and a writing device to write the identification means with the component-specific information, the control means to adapt the control parameter based on the component-specific information to provide the component-specific information, and, based on the component-specific information, to execute a diagnostic process.
CHEMICAL MECHANICAL POLISHING PAD AND PREPARATION THEREOF
The present invention concerns a chemical mechanical polishing pad having a polishing layer. The polishing layer contains an extruded sheet. The extruded sheet is prepared by extruding a compounded photopolymerizable composition followed by exposure to UV light.
Extrusion device
An extrusion device comprises at least one supply station suitable for containing a material to be extruded; a plurality of propellers operatively connected to at least one supply station for receiving the material to be extruded and at least one extrusion head connected to at least one propeller. Each propeller can also be selectively activated to modulate an extrusion speed and/or a quantity of material to be extruded as an output from the extrusion head.
Method and apparatus for reducing non-normal incidence distortion in glazing films
A method of manufacturing a polymer film includes melting a resin, extruding the melted resin through a die to produce a polymer film, shaping the polymer film, cooling the polymer film, capturing an image of a test pattern through the polymer film, calculating a modulation transfer function value from the image, and adjusting a process parameter of the melting, the extruding, the shaping, or the cooling based on the calculated modulation transfer function value.
Extruder Systems and Processes Thereof
The present disclosure relates to extruder systems and processes thereof. In at least one embodiment, a method of forming a thermoplastic vulcanizate (TPV) composition includes introducing a thermoplastic polymer to an extruder through a feed throat. The elastomeric polymer is introduced to a melt feeder and an elastomeric polymer melt including the elastomeric polymer is formed. The melt feeder is coupled to the extruder. Elastomeric polymer melt from the melt feeder is introduced to the extruder. The thermoplastic polymer and the elastomeric polymer melt are fed separately to the extruder. The thermoplastic polymer and the elastomeric polymer melt in the extruder are mixed with a plurality of intermeshing screws having a plurality of mixing zones.
EXTRUSION METHOD AND APPARATUS
Improvements in the extrusion of thermohardenable materials are achieved by cooling the material in the initial zone of the extruder and reducing residence time by use of a prescribed length to diameter ratio and screw speed, particularly useful for intermittent application during robotically controlled mass production.
WHITE POLYESTER FILM AND METHOD FOR MANUFACTURING SAME, SOLAR CELL BACK SHEET, AND SOLAR CELL MODULE
Provided are a white polyester film including a polyester and white particles having an average primary particle diameter of 0.20 to 0.40 μm, in which a content of the white particles is 1.0% to 5.0% by mass with respect to the total mass of the film, a ratio of agglomerated particles having particle diameters of 0.40 to 0.80 μm in a direction parallel to a surface direction of the film on the cross-section of the film to the total number of primary particles and agglomerated particles of the white particles dispersed in the film is 10% to 20% by number, and a concentration of terminal carboxyl groups is 6 to 30 equivalents/ton, a method for manufacturing the same, a solar cell back sheet, and a solar cell module.
Low-gloss heat-resistant abs resin composition and its preparation method
The present invention relates to a low-gloss heat-resistant ABS resin composition and its preparation method. The low-gloss heat-resistant ABS resin composition includes following components by weight: 100 parts of acrylonitrile-butadiene-styrene (ABS) resin, 5-30 parts of heat-resistant agent, 1-5 parts of matte masterbatch D, 0.2-1.0 parts of light stabilizer, and 0.5-2.0 parts of other additives. The preparation method includes steps of: stirring and fully mixing the above-mentioned raw materials in a high-speed mixer, and then feeding the raw materials into a twin-screw extruder through a metering device; melting and compounding the materials under the conveying, shearing and mixing of the screws, and then extruding, pulling, cooling and granulating, and finally obtaining the low-gloss heat-resistant ABS resin composition. The resin composition provided by the present invention not only has excellent mechanical properties, but also has an ultra-low gloss; therefore, it is very suitable for use in the field of automotive interior parts.
Chemical mechanical polishing pad and preparation thereof
The present invention concerns a chemical mechanical polishing pad having a polishing layer. The polishing layer contains an extruded sheet. The extruded sheet is prepared by extruding a compounded photopolymerizable composition followed by exposure to UV light.
METHOD FOR PREPARING DIAPHRAGM OF LITHIUM-ION BATTERY BY THREE LAYER CO-EXTRUSION
Disclosed is a method for preparing a three-layer-co-extruded diaphragm of a lithium-ion battery, falling into lithium-ion battery diaphragm technical field. The annealing box used comprises: box body, motor and sealing over, with uniformly-arranged heating plates fixedly connected to inner surface of the box body, a driving shaft arranged horizontally within the box body in front-back direction, a first and second driven shafts arranged on the left and right sides of the driving shaft correspondingly within the box body, an interlayer film coiling connected between the driving shaft and the first driven shaft within the box body horizontally; a diaphragm coiling connected between the driving shaft and the second driven shaft within the box body slantwise. Controllable annealing temperature and insulation from external environment avoid influence of external environment on diaphragm and ensure uniform heating of diaphragm. It produces a diaphragm of stable quality and is convenient to be mass-produced.