Patent classifications
C04B2235/3272
REFRACTORY OBJECT AND METHOD OF FORMING
A refractory object may include a zircon body that is intentionally doped with a dopant including an alkaline earth element and aluminum. The refractory object can have an improved creep deformation rate. In an embodiment, the refractory object can have a creep deformation rate of not greater than about 1.8 E-5 h.sup.−1 at a temperature of 1350° C. and a stress of 2 MPa. In another embodiment, the zircon body may include an amorphous phase including an alkaline earth metal element.
PIEZOELECTRIC MATERIAL COMPOSITION, METHOD OF MANUFACTURING THE SAME, PIEZOELECTRIC DEVICE, AND APPARATUS INCLUDING THE PIEZOELECTRIC DEVICE
A piezoelectric material composition, a method of manufacturing the same, a piezoelectric device, and apparatus including the piezoelectric device. The piezoelectric device may include a piezoelectric device layer including a first material and a second material surrounded by the first material, a first electrode portion disposed at a first surface of the piezoelectric device layer, and a second electrode portion disposed at a second surface of the piezoelectric device layer opposite to the first surface, wherein the piezoelectric device layer comprises a piezoelectric material composition represented by Chemical Formula 1: 0.96(Na.sub.aK.sub.1-a)(Nb.sub.b(T.sub.1-b))O.sub.3-(0.04-x)MZrO.sub.3-x(Bi.sub.cAg.sub.1-c)ZrO.sub.3+d mol % NaNbO.sub.3, wherein T is Sb or Ta, M is Sr, Ba or Ca, a is 0.4≤a≤0.6, b is 0.90≤b≤0.98, c is 0.4≤c≤0.6, d is 0≤d≤5.0, and x is 0≤x≤0.04 and wherein T is Sb or Ta and M is Sr, Ba, or Ca.
Bonded abrasive articles
An abrasive article includes a body having a bond material extending throughout the body and abrasive particles contained in the bond material. The bond material can include aluminum oxide (Al.sub.2O.sub.3) and lithium oxide (Li.sub.2O). In an embodiment, the bond material can include a ratio (Al.sub.2O.sub.3/Li.sub.2O) of a content of aluminum oxide (Al.sub.2O.sub.3) relative to a content of lithium oxide (Li.sub.2O), based on weight percent, of greater than 11.5 and at most 20. In another embodiment, the abrasive article can have a versatility factor of greater than 1.90.
Z-type hexaferrite having a nanocrystalline structure
In an aspect, a Co.sub.2Z ferrite has the formula: (Ba.sub.1-xSr.sub.x).sub.3Co.sub.2+yM.sub.yFe.sub.24-2y-zO.sub.41. M is at least one of Mo, Ir, or Ru. The variable x can be 0 to 0.8, or 0.1 to 0.8. The variable y can be 0 to 0.8, or 0.01 to 0.8. The variable z can be −2 to 2. The Co.sub.2Z ferrite can have an average grain size of 5 to 100 nanometers, or 30 to 80, or 10 to 40 nanometers as measured using at least one of transmission electron microscopy, field emission scanning electron microscopy, or x-ray diffraction.
Zirconia layered body
There is provided at least any of a layered body which has a change in color tone and in which it is unnecessary to select a colorant and the content of the colorant in consideration of a difference in the sintering behavior between layers, a precursor thereof, or a method for producing these. Provided is a layered body which has a structure, in which two or more layers containing stabilizer-containing zirconia and a colorant are layered, and in which types and contents of the colorants contained in the layers are equal to each other, the layered body including at least: a first layer containing a colorant and zirconia which has a stabilizer content of higher than or equal to 3.3 mol %; and a second layer containing a colorant and zirconia which has a stabilizer content different from that of the zirconia contained in the first layer.
Dielectric composition and multilayered electronic component comprising the same
A dielectric composition includes a main ingredient having a perovskite structure represented by ABO.sub.3, where A is at least one of Ba, Sr, and Ca and B is at least one of Ti, Zr, and Hf, and a first accessory ingredient. The first accessory ingredient comprises 0.1 mole or more of a rare earth element, 0.02 mole or more of Nb, and 0.25 mole or more and 0.9 mole or less of Mg, a sum of contents of the rare earth element and Nb is 1.5 mole or less.
Black sintered body and method for producing the same
A sintered body includes a solid solution containing cobalt and iron, with the balance being zirconia. The total content of cobalt in terms of CoO and iron in terms of Fe.sub.2O.sub.3 is more than 0.1 wt % and less than 3.0 wt %, and the proportion of cobalt regions larger than 5.5 μm.sup.2 in an elemental map obtained using an electron probe microanalyzer is 25% or less.
Process for Treating a Porous Dental Zirconia Block with Coloring Solutions
Process for treating a porous dental zirconia block with a coloring solution, the process comprising the steps of providing a porous dental zirconia block having two opposing surfaces, surface U and surface L, treating the upper surface U of the porous dental zirconia block with a coloring solution A.sub.1, wherein the coloring solution is provided with a volume VA.sub.1, turning the porous dental zirconia block around, treating the lower surface L with a coloring solution A.sub.2 which is provided with a volume VA.sub.2. wherein the coloring solutions A.sub.1 and A.sub.2 comprise a solvent and coloring ions, wherein the volume of at least one of the coloring solutions A.sub.1 or A.sub.2 is applied in portions, wherein the following condition is met: Vo=ΣV.sub.AX, with x≥2, with Vo being the overall amount of coloring solution used to infiltrate the porous dental zirconia block.
MEMBER FOR POWER STORAGE DEVICE, ALL-SOLID-STATE BATTERY, AND METHOD FOR MANUFACTURING MEMBER FOR POWER STORAGE DEVICE
Provided is a member for a power storage device that, even when the amount of electrode active material supported is increased, enables charge and discharge and thus achieves a high capacity. A member 6 for a power storage device includes: a solid electrolyte layer 1; and an electrode layer 2 provided on the solid electrolyte layer 1 and made of a sintered body of an electrode material layer 2A containing an electrode active material precursor powder having an average particle diameter of not less than 0.01 μm and less than 0.7 μm.
Shaped abrasive particles, methods of making, and abrasive articles including the same
A method of making abrasive particles includes: providing a slurry comprising non-colloidal solid particles and a liquid vehicle; forming at least a portion of the slurry into shaped bodies contacting a substrate; at least partially drying the shaped bodies to provide shaped abrasive precursor particles; separating at least a portion of the shaped abrasive precursor particles from the substrate; and converting at least a portion of the shaped abrasive precursor particles into shaped abrasive particles. The shaped abrasive particles comprise alpha alumina having an average crystal grain size of 0.8 to 8 microns and an apparent density that is at least 92 percent of the true density. Each shaped abrasive particle has a respective surface comprising a plurality of smooth sides that form at least four vertexes. Shaped abrasive particles, abrasive articles including them, and methods of using are also disclosed.