C10L9/06

Method for preparing biochar
11359153 · 2022-06-14 ·

A method for preparing biochar, including steps as follows: dosing: putting pre-crushed biomass into a reactor; charring conversion: heating the reactor to a certain temperature and pressure, and putting an active group-containing active agent containing 1% to 5% by mass of biomass and a catalyst containing 1% to 10% by mass of biomass (or putting the catalyst first and then putting the active agent) into the reactor to perform solid solution charring on the biomass; and cooling: after the charring conversion is completed, cooling the reactor to 40° C. or lower to obtain the biochar. Feedstocks are abundant and cheap, farmland biomass waste is reused, and the active group-containing active agent is added in biomass charring, which can effectively inhibit side reactions and coordinate with the catalyst to perform solid solution charring on the biomass, thereby improving a biochar conversion rate and making the charring process clean and environmentally friendly.

A Process for the Production of Oxidized Wood Products

The present invention relates to a process for the production of oxidized wood products, comprising step a) reacting chips of one or more wood products in a basic solution at a pH between 8 and 14 under an oxygen atmosphere at a pressure of at least 0.1 MPa, or at least 0.9 MPa. A copper catalyst may be used in the process.

A Process for the Production of Oxidized Wood Products

The present invention relates to a process for the production of oxidized wood products, comprising step a) reacting chips of one or more wood products in a basic solution at a pH between 8 and 14 under an oxygen atmosphere at a pressure of at least 0.1 MPa, or at least 0.9 MPa. A copper catalyst may be used in the process.

CARBONIZED UPGRADED COAL, GRAPHITE, AND METHODS OF MAKING THE SAME
20230278874 · 2023-09-07 ·

A method of forming graphite includes carbonizing an upgraded coal, to form a carbonized upgraded coal. The method also includes graphitizing the carbonized upgraded coal, to form the graphite.

CARBONIZED UPGRADED COAL, GRAPHITE, AND METHODS OF MAKING THE SAME
20230278874 · 2023-09-07 ·

A method of forming graphite includes carbonizing an upgraded coal, to form a carbonized upgraded coal. The method also includes graphitizing the carbonized upgraded coal, to form the graphite.

Process for the production of oxidized wood products

The present invention relates to a process for the production of oxidized wood products, comprising step a) reacting chips of one or more wood products in a basic solution at a pH between 8 and 14 under an oxygen atmosphere at a pressure of at least 0.1 MPa, or at least 0.9 MPa. A copper catalyst may be used in the process.

Process for the production of oxidized wood products

The present invention relates to a process for the production of oxidized wood products, comprising step a) reacting chips of one or more wood products in a basic solution at a pH between 8 and 14 under an oxygen atmosphere at a pressure of at least 0.1 MPa, or at least 0.9 MPa. A copper catalyst may be used in the process.

LOW-SULFUR COAL PRODUCTION METHOD

A low-sulfur coal production method having an excellent desulfurization effect includes bringing coal into contact with a chemical material that is a mixed solution of hydrogen peroxide and acetic anhydride to remove sulfur in the coal. It is preferred that the molar ratio of the acetic anhydride to the hydrogen peroxide is 0.5 to 12.0 inclusive. It is preferred that the acetic anhydride is mixed with the hydrogen peroxide before the chemical material is brought into contact with the coal and the chemical material is brought into contact with the coal after 10 minutes or more has elapsed since the mixing.

LOW-SULFUR COAL PRODUCTION METHOD

A low-sulfur coal production method having an excellent desulfurization effect includes bringing coal into contact with a chemical material that is a mixed solution of hydrogen peroxide and acetic anhydride to remove sulfur in the coal. It is preferred that the molar ratio of the acetic anhydride to the hydrogen peroxide is 0.5 to 12.0 inclusive. It is preferred that the acetic anhydride is mixed with the hydrogen peroxide before the chemical material is brought into contact with the coal and the chemical material is brought into contact with the coal after 10 minutes or more has elapsed since the mixing.

METHOD FOR PREPARING BIOCHAR
20210155867 · 2021-05-27 ·

A method for preparing biochar, including steps as follows: dosing: putting pre-crushed biomass into a reactor; charring conversion: heating the reactor to a certain temperature and pressure, and putting an active group-containing active agent containing 1% to 5% by mass of biomass and a catalyst containing 1% to 10% by mass of biomass (or putting the catalyst first and then putting the active agent) into the reactor to perform solid solution charring on the biomass; and cooling: after the charring conversion is completed, cooling the reactor to 40° C. or lower to obtain the biochar. Feedstocks are abundant and cheap, farmland biomass waste is reused, and the active group-containing active agent is added in biomass charring, which can effectively inhibit side reactions and coordinate with the catalyst to perform solid solution charring on the biomass, thereby improving a biochar conversion rate and making the charring process clean and environmentally friendly.