Hot-dip galvanization system for large-scale hot-dip galvanization of automotive components
11525176 · 2022-12-13 · ·

The invention relates to a system and a method for the hot-dip galvanization of motor-vehicle components, preferably for mass-production hot-dip galvanization of a plurality of identical or similar motor-vehicle components, in particular in batches, preferably for batch galvanization, especially preferably for high-precision hot-dip galvanization.

Apparatus for dip-coating a metal strip using a movable overflow

An equipment for the continuous hot dip-coating of a metal strip including an annealing furnace, a tank containing a liquid metal bath, a snout connecting the annealing furnace and the tank, through which the metal strip runs in a protective atmosphere and the lower part of the snout, the snout tip, is at least partly immersed in the liquid metal bath in order to define with the surface of the bath, and inside this snout, a liquid seal and a separate overflow attached/hold to the snout through fixings, the overflow including at least one tray, placed in the vicinity of the strip when entering the liquid metal bath and encompassed by the liquid seal.

Method and flux for hot galvanization
11499216 · 2022-11-15 · ·

The invention relates to the technical field of galvanization of iron-based or iron-containing components, especially steel-based or steel-containing components (steel components), preferably for the automotive or motor vehicle industry, but also for other industrial fields of application (for example for the construction industry, the field of general mechanical engineering, the electrical engineering industry etc.), by means of hot galvanization (hot clip galvanization). More particularly, the invention relates to a method of hot galvanization (hot dip galvanization) and to a plant for this purpose, and additionally to a flux and flux bath usable in this connection and to the respective uses thereof, and additionally also to the products obtainable by the method and/or in the plant (i.e. hot galvanized iron or steel components).

METHOD FOR SELECTIVELY PRETINNING A GUIDEWIRE CORE

A method of pretinning a core wire for a guidewire having an elongate axis, comprising placing a ball of solder within a pocket in a soldering block; melting the ball of solder; holding a core wire over the ball of solder, with the elongate axis in a horizontal orientation; lowering a portion of the core wire into the ball of solder while maintaining the elongate axis in a horizontal orientation; removing the core wire from the ball of solder.

Crossbow correction device, molten metal plating facility, and crossbow correction method

A crossbow correction device 16 for correcting crossbow of a steel strip S by a magnetic force during conveyance includes a plurality of electromagnets 57a to 57d, 67a to 67d arranged in a strip width direction of the steel strip S and facing each other so as to sandwich the steel strip S in a strip thickness direction, a moving mechanism 51 to 54, 61 to 64 capable of moving the electromagnets 57a to 57d, 67a to 67d relative to the steel strip S, and a controller 17 configured to operate the moving mechanism 51 to 54, 61 to 64, based on a current value flowing through the electromagnets 57a to 57d, 67a to 67d.

Pass roll for hot-dip galvanized steel sheet manufacturing facility, hot-dip galvanized steel sheet manufacturing facility, and hot-dip galvanized steel sheet manufacturing method
11479840 · 2022-10-25 · ·

A pass roll for a hot-dip galvanized steel sheet manufacturing facility, the pass roll includes: a roll body; and a heat-resistant felt layer covering the roll body, wherein the heat-resistant felt layer has a thermal decomposition temperature of 420° C. or higher and has a surface hardness evaluation index at 400° C. of more than 0.11 μm/N.

Apparatus and methods for depositing molten metal onto a foil substrate

A web coating platform for depositing molten metal on flexible substrates is provided. The web coating platform can be used for manufacturing solid lithium anodes for use in energy storage devices, for example, rechargeable batteries. The coating platform can be designed for double-sided coating of a continuous flexible substrate (e.g., a copper foil) with molten lithium followed by double-sided lamination or passivation. The coating platform integrates novel coating elements unique to handling and processing molten metals. For example, some implementations of the present disclosure incorporate double-sided molten metal coating elements, which include at least one of a molten metal application assembly (e.g., kiss roller, slot-die, Meyer bar, and/or gravure roller), a primary melt pool assembly, a secondary melt pool assembly, and an engagement mechanism.

Hot dip coated steel strip having an improved surface appearance and method for production thereof

The present invention relates to a method of hot dip coating of flat steel products, comprising a step of stripping the coated steel strip by means of at least one nozzle that emits a stripping gas having a temperature T.sub.3 at an angle α in the direction of the coated steel strip, wherein the angle α, the distance h between the surface of the melt bath and the lower edge of the nozzle in mm, the temperature of the stripping gas in ° C. and the differential between the temperature T.sub.2 of the melt bath and the temperature T.sub.1 of the steel strip are in a particular relationship to one another, and to a correspondingly produced hot dip-coated flat steel product.

Continuous hot dip galvanizing apparatus

A continuous hot-dip galvanizing apparatus has a vertical annealing furnace, one or more hearth rolls, a hot-dip galvanizing apparatus, an alloying line, and humidified gas supply ports. When the steel sheet having a Si content of 0.2 mass % or more is conveyed inside the annealing furnace, the humidified gas supply ports positioned in a latter part of the soaking zone supply the humidified gas to the soaking zone and the at least one dry gas supply port supplies the dry gas to the soaking zone. When the steel sheet having a Si content of less than 0.2 mass % is conveyed inside the annealing furnace, the plurality of the humidified gas supply ports do not supply the humidified gas to the soaking zone and the at least one dry gas supply port supplies the dry gas to the soaking zone.

Gas wiping nozzle and method of manufacturing hot-dip metal coated metal strip

A gas wiping nozzle configured to blow wiping gas onto a metal strip includes a first nozzle member and a second nozzle member provided to face each other, in which a slit as a gas blowing port is formed to extend in a length direction between end portions of the first nozzle member and the second nozzle member on the metal strip side; and a shim member configured to adjust a gap of the slit in a width direction orthogonal to the length direction, wherein the shim member is made of a ceramic material or a carbon material, each of the first nozzle member and the second nozzle member has a groove portion, and the shim member is fitted into both of the groove portions of the first nozzle member and the second nozzle member and fixes the first nozzle member and the second nozzle member.