RECYCLABLE MATERIAL

20170246836 · 2017-08-31

    Inventors

    Cpc classification

    International classification

    Abstract

    A laminate composite material (1), suitable for the packaging of food products and having a multilayer structure comprising: a first outer layer (21) of paper or plastic film; an inner layer (22) of adhesive; and an intermediate layer (23) interposed between the first and the second layer and made of sodium silicate (Na.sub.2O×SiO.sub.2).

    Claims

    1. A laminate composite material suitable for the packaging of food products, which laminate composite material has a multilayer structure which includes: a first outer layer; a second inner layer, wherein said first outer layer and said second inner layer or a third intermediate layer interposed therebetween, comprise exclusively or in a predominant percentage a water-soluble material, so that two or more of said first outer layer, second inner layer and third intermediate layer are separable, after use, by means of a bath of water or with prevalence of water.

    2. The composite material according to claim 1, wherein said third intermediate layer, said first outer layer or said second inner layer comprises exclusively or in a predominant percentage an alkali metal silicate M with M.sub.2O×nSiO.sub.2 and n=1,5÷4.

    3. The laminate composite material according to claim 2, wherein M is selected from a group comprising sodium Na, potassium K and Lithium Li.

    4. The laminate composite material according to claim 1, wherein said water-soluble material is polyvinyl alcohol representing about 99% of the composition of its own layer or sodium silicate representing about 2% of the composition of its own layer.

    5. The laminate composite material according to claim 1, wherein said third intermediate layer, said first outer layer or said second inner layer comprises exclusively or in a predominant percentage one or more materials selected from a group comprising: sugars, starchs, gelatin, arabic gum, polyvinylpyrrolidone, carboxymethylcellulose, hydroxyethylcellulose, methylcellulose, polyvinyl alcohol.

    6. The laminate composite material according to claim 1, wherein said second inner layer is a layer of adhesive or a layer of hot-melt and/or heat-weldable and/or metallic film.

    7. The laminate composite material according to claim 1, wherein said first outer layer is breathable.

    8. The laminate composite material according to claim 1, wherein said first layer is of paper or of a paper-like, cellulosic or fibrous material.

    9. The laminate composite material according to claim 1, comprising a further layer adjacent to said second inner layer and selected from a group comprising an adhesive, a film material and a coating.

    10. The laminate composite material according to claim 9, wherein said second inner layer and/or said further layer is made of polyethylene PE.

    11. The laminate composite material according to claim 1, wherein said third intermediate layer, said first outer layer or said second inner layer comprises one or more additives selected in the following group: organic fillers, oils (such as glycerin, sorbitol, ethylene glycol), styrenic polymers, acrylics, mineral fillers (e.g. talc powder), polyvinyl alcohol PVA-PVOH, PLA Ethylene-Vinyl alcohol (EVOH), mica, vermiculite, feldspars, zeolites, sugar, starch or other.

    12. The laminate composite material according to claim 1, wherein said second inner layer is applied according to a discontinuous pattern, in such a way as to form channels for the water passage of the water bath.

    13. The laminate composite material according to claim 1, comprising a film and/or a coating coming from renewable sources PLA-Cellophane, PHB, PCL.

    14. The laminate composite material according to claim 1, which is in the form of a sheet or continuous tape.

    15. A packaging comprising a casing made of a laminate composite material according to claim 1 and a food, product received within said casing.

    16. A method for the manufacture of a composite material laminate suitable for the packaging of food products, which method comprises the steps of: providing an outer layer and an intermediate layer, the intermediate layer being made of a water-soluble material, said outer and intermediate layers being adhered one onto the other; providing a second inner layer of adhesive; drying said second inner layer, and joining said second inner layer to an assembly formed by said outer layer and intermediate layer, wherein two or more of said outer layer, intermediate layer and second inner layer are separable, after use, by means of a bath of water or with prevalence of water.

    17. The method according to claim 16, comprising a further step of providing a further layer of adhesive, a step of drying said further layer and a step of adhesion of said further layer on said second layer.

    18. The method according to claim 16, which is a method for making a laminate composite material.

    19. A method for recycling a laminate composite material according to claim 1, comprising a step of separating two or more components of said outer layer, intermediate layer and second inner layer by means of a bath of water or with prevalence of water.

    20. The laminate composite material according to claim 13, wherein said film and/or coating is selected from a group comprising: PLA-Cellophane, PHB, PCL.

    21. A method for packaging according to claim 16, comprising a step of separating two or more components of said outer layer, intermediate layer and second inner layer by means of a bath of water or with prevalence of water.

    Description

    BRIEF DESCRIPTION OF THE FIGURES

    [0031] Reference will be made to the figures of the enclosed drawings, wherein:

    [0032] FIG. 1 and FIG. 2, already introduced above, relate each one to a respective composite material of known art, showing a schematic exploded view thereof in cross section highlighting the component layers thereof;

    [0033] FIG. 3 shows a schematic view in cross section of a composite material according to a first embodiment of the invention, in an exploded configuration highlighting the component layers thereof;

    [0034] FIG. 4 shows a schematic view in cross section of a composite material of a second embodiment of the invention, in an exploded configuration highlighting the component layers thereof and the assembling modes;

    [0035] FIG. 5 shows a schematic view in cross section of a composite laminated material of a third embodiment of the invention, in an exploded configuration highlighting the component layers thereof;

    [0036] FIG. 6 shows a schematic perspective view of a cross portion of a composite material according to a fourth embodiment of the invention;

    [0037] FIG. 7 shows a schematic perspective view of a cross portion of a composite material according to a fifth embodiment of the invention; and

    [0038] FIGS. 8A, 8B and 8B relate to a sixth embodiment of the invention, showing respectively a schematic plan top view of a composite material during assembly, a schematic view in cross section of such material assembled to form a packaging and a schematic view in cross section of such packaging performed according to the line C-C of FIG. 8B.

    [0039] The thicknesses and the sizes represented in the figures mentioned above are to be meant by way of pure example, they are generally magnified and not necessarily shown proportionally.

    DETAILED DESCRIPTION OF PREFERRED EMBODIMENTS

    [0040] Different embodiments and variants of the invention will be described hereinafter and this by referring to the above-mentioned figures.

    [0041] Components analogous/common to the different embodiments will be designated with the same numeral reference.

    [0042] Furthermore, in the following detailed description, embodiments and variants in addition to embodiments and variants already discussed in the same description will be illustrated by limiting to the difference with respect to what already illustrated.

    [0043] The different embodiments and variants described hereinafter are subjected to be used in combination, where compatible.

    [0044] By firstly referring to FIG. 3, a laminate composite material according to a first preferred embodiment of the invention is designated as a whole with 1. The composite material 1 is in form of sheet or continuous tape.

    [0045] In the present example, the composite material 1 is suitable for the packaging of food products, in particular bread, biscuits, fresh or dry pasta or other.

    [0046] The composite material 1 of the present embodiment is formed by a multilayer structure.

    [0047] Such structure first of all comprises a first layer 21, which will be called outer layer thanks to its arrangement indeed outside the end packaging and which is made of paper material. In particular, the first layer 21 is made of paper or a cellulose material, with prevalence of cellulose or however fibre.

    [0048] The multilayer structure then comprises a second layer 22, which will be called inner layer thanks again to its arrangement indeed inside the end packaging. The second layer 22 of the present example is an adhesive.

    [0049] According to the invention, a third intermediate layer 23 is then provided interposed between the first and the second layer 21 and 22. The intermediate layer 23 is made of an alkali metal silicate M, with M.sub.2O×nSiO.sub.2, n=1,5÷4. Preferably, the third layer is sodium silicate or potassium silicate.

    [0050] In the present embodiment, the multilayer structure, at last, comprises a fourth layer 24, still more interior with respect to the second layer 22. In the present example, the third layer 24 is a film with barrier effect to the water vapour, for example a plastic film, in particular of polyethylene, polypropylene, metallised polypropylene, aluminium or the like. Additional subsequent layers of material can be inserted with the purpose of reaching the wished result in terms of mechanical resistance, machinability and barrier of the packaging.

    [0051] Based upon a method for implementing the composite material 1, the coupling between four or more layers mentioned above is obtained by hot or cold rolling.

    [0052] Based upon a preferred variant, the second layer of adhesive 22 is dried, that is desiccated, before being applied on, that is joined to, the set of the first and third layer 21 and 23.

    [0053] Preferably, in order to join the set of the layers 21 and 23 to the set of the layers 22 and 24, a rolling calender with controlled temperature and pressure (hot calender) is used. In such variant, the resulting composite material has an optimum seal between the layers.

    [0054] In an additional variant, the use of “solventless” adhesives for the second layer 22 or for the subsequent layers is provided, which, since they are without water, result to be able to implement an improved seal between the layers.

    [0055] FIG. 4 shows a second embodiment of the laminate composite material of the invention, in this case designated with 100. In such embodiment the application of an additional layer of adhesive 25, on the side of the film 24 faced towards the intermediate layer 23, is provided.

    [0056] Preferably, the method for implementing the composite material 100 provides, as exemplified in FIG. 4, a phase of drying, in case simultaneous and performed with the same means, the two adhesive layers 22 and 25 before adhering a set formed by adhesive 25 and film 24 on a set formed by paper 21, silicate 23 and adhesive 22.

    [0057] Even in this case, the two sets 21-23-22 and 24-25 the implementation method can provide a rolling calender with controlled temperature and pressure (hot calender). This technique provides optimum results of mechanical resistance and seal between the component materials.

    [0058] FIG. 5 relates to a third embodiment of laminate composite material, herein designated with 101. In this case, apart from the outer layer 21 and the intermediate layer 23, an inner layer 220 is provided implemented as covering (coating) or adhesive. Such layer can be constituted by thermo-temperable adhesive, or comprise a polyethylene (PE) melt.

    [0059] An additional embodiment can provide an outer layer of paper, a spreading of sodium silicate or other water-soluble material in the meaning of the invention and an additional spreading of film as inner layer, for example a coating or an adhesive. After spreading, the water-soluble material and the inner layer can result to be interpenetrated and suitable to implement substantially a same composite layer.

    [0060] Alternatively, the intermediate layer of water-soluble material and the inner layer can be integrated, actually, in a same layer, that is applied together in form of a single material.

    [0061] In all embodiments illustrated above, the different components of the laminate composite material can be separated therebetween by means of a simple bath of water or of a solution mainly constituted by water. In fact, the sodium silicate (or of another alkali metal), being hydrophilic and soluble in water, when the composite material is placed in a basin containing water, it melts, by implementing the detachment of the film glued thereon—or of the coating applied thereon—from the paper-like material of the first layer or from the film adhered thereto.

    [0062] The composite material described above, when associated to a second layer of adhesive, even exploits the flocculant capability of the silicate. In fact, the latter plays a function of “sequestrant” of adhesive particles in the water bath. In this way, one avoids the risk that such adhesive particles, by remaining under suspension in the water wherein the paper fibres are present, come again in contact with the latter, by generating subsequent problems during pulping and formation of the recycled sheet phase, with the creation of pellets and so-called “stikies” (agglomerations of paper and adhesive).

    [0063] In case of composite materials formed by a layer of paper and one of plastic film or coating as those considered so far, it is easy to bring the silicate in contact with the water by means of the capillarity of the cellulose carrier. In particular, there is a big contact surface between water and silicate, with consequent very short time for implementing the phase of detaching the two components film or coating—paper.

    [0064] In FIG. 6 another embodiment of laminate composite material is shown, herein designated with 102, similar to the embodiment of FIG. 3, but wherein the silicate layer is interposed between two layers of plastic film. In particular, in the composite material 102 a first outer layer 210 in form of plastic film, an intermediate layer 23 of silicate and a fourth layer 24 in form of film are provided. Furthermore, between the layers 23 and 24 a layer of adhesive 221 is interposed, applied according to a discontinuous pattern. In the represented example, it is an application with longitudinal strips.

    [0065] Such embodiment is particularly advantageous when it is indeed necessary to implement the separation of plastic films of different nature coupled therebetween in the composite material. In fact, in this case the contact surface of the silicate with the bath water is represented exclusively by the outer side section of the sheet, the layers adhered to the silicate not resulting permeable to water. The above-mentioned discontinuous pattern in the application of the adhesive implements passage channels, inside which the water infiltrates, generating swelling and solubilisation of the silicate and then facilitating the separation of the layers.

    [0066] In FIG. 7 an embodiment variant of the composite material with respect to FIG. 6 is shown, in this case designated with 103, providing a “step-like” deposit of silicate. In particular, it is provided that the layer of silicate 23 is interposed between two layers of adhesive, respectively 225 and 226, and that the adhesive involves even side portions of the material, joining directly the two layers of end film 210 and 24 by means of side depositions 201 and 202. In other words, the adhesive implements a frame wrapping the layer of silicate. In this way, there isn't the risk of accidental detachment of the layers during the useful life of the product due to humidity infiltration.

    [0067] Upon recycling, during separation in water bath, the material 103 can be sectioned in small fragments (for example wide 1 cm×1 cm), to ease the contact between silicate and water and then the detachment process.

    [0068] It is to be noted that the silicate, when dry, has high stiffness (and it is defined for this sometimes “liquid glass”). It is possible controlling, and in particular reducing, such stiffness by inserting into the silicate additives helping to make flexible the related layer (for example organic fillers, oils like glycerin, sorbitol, sucrose, variously modified starch, ethylene glycol, styrene polymers, acrylic, poly 2-Ethyl-2-Ossazoline, and so on).

    [0069] Furthermore, in order to ease setting of the adhesive layer(s) on the silicate layer, mineral fillers can be inserted such as for example calcium carbonate. In particular, by exploiting the natural features of some fillers, such as for example talcum, it is possible providing to the silicate layer features of barrier to the mineral oils. Such feature allows using in the structural stratification layers of recycled paper, without running into the risk of a migration of pollutants dangerous for the human health.

    [0070] The possibility of inserting more than one layer of silicate can be further considered, and this with the purpose of providing a specific function to each layer. In fact, the silicate of the intermediate layer, or of an additional intermediate layer of the herein considered composite material, can even be additivated—preferably in percentages variable between 0.5% and 99%—with additional components, for example polyvinyl alcohol PVA—PVOH, Ethylene Vinyl alcohol—EVOH, PLA, mica, vermiculite, metal oxides or other, to confer thereto specific properties, for example a barrier effect, in particular to the oxygen, to UV and so on, by avoiding the overlapping of additional layers of plastic film; that is to improve and/or modify, when requested, the solubility features of the used products with the purpose of reaching whole recyclability of the paper-like material.

    [0071] Furthermore, in case of particular applications wherein a higher resistance to humid environments is necessary, by exploiting the chemical features of the silicate, it is possible proceeding with a partial insolubilisation of the silicate layer, or of one of the most external layers by means of known techniques such as the acid reaction, the insertion of carbonates, the inertisation through CO.sub.2.

    [0072] In the applications wherein the packaging implemented with the composite material must be kept in the fridge, one can provide to protect the outer surface of the packaging itself with a coating barrier to water, so as to prevent the silicate from being influenced by the humidity of the environment. It is further possible to provide the spreading with a layer of variously combined silicate, of the outer face of the packaging especially if made of paper, in this way by constituting a surface able to implement an easy de-inking during the material recovery.

    [0073] By referring to FIGS. 8A-8C, the environmental advantage of the packagings made of the composite material of the invention can be increased even by means of reducing the thicknesses of the single layers composing the composite material. In fact, the higher stiffness of the structure implemented by means of the specific feature of the silicate allows obtaining optimum results with less use of raw materials.

    [0074] In particular, currently the packagings having the feature of sealing the inner air present on the market are formed by multilayer film wherein the inner layer generally is a hot-melt plastic film. The reason of this choice lies in the need for guaranteeing that the typical weldings performed by the standard packaging machines keep an hermetic sealing even in presence of material overlappings, for example due to the typical indentations of the so-called square-background packagings. In fact, usually the outer layer of the multilayer material used in such packagings is formed by a film which has no features of thermoweldability. The hot-melt film of the inner layer of the multilayer material usually has a thickness so as to cover the differences in thickness in the overlapping points of at least two bellows-like folds of the original material. Therefore, the known packagings characterize for an overall high thickness and, consequently, for the high economic incidence of raw materials and the high environmental impact consequent to the huge quantity of used material.

    [0075] In the material of FIGS. 8A-8C, the most external portion formed by the set paper 210 and silicate 23 is sufficiently stiff to guarantee that upon welding no uncontrolled folds generate (the use of silicate, as seen, helps in obtaining this characteristic stiffness, with low thickness of material). Such outer portion is not heat-weldable. The inner layer 28 of hot-melt film obviously is heat-weldable and can have, for example, a thickness comprised between 12 and 60 micron. The outer layer of paper 210 is punched at the cross points of the material upon implementing the packaging weldings, making that the weldings have a substantially flat contact surface, thus allowing to implement airtight packagings even by using film with low thickness, thanks to the stiffness given through the layer of silicate and, in case, heat-welding and not necessarily thermal fuses.

    [0076] In an additional variant, it is possible implementing a composite material comprising, in sequence, the following layers: [0077] an outer layer of Polyethylene or water-resistant paint; [0078] an ink layer; [0079] a silicate layer; [0080] a paper layer; [0081] a silicate layer; [0082] a layer of aluminium+silicate; [0083] a layer of so-called “solventless” material; and [0084] an inner layer of Polyethylene or a hot-melt plastic film in coupled film.

    [0085] Furthermore, among the coupling possibilities all categories of films and coatings coming from renewable sources can be used, such as for example PLA—Cellophane, PHB, PCL, that is, if it is the case, the precursors thereof in case in variable mixtures, such as sugars, vegetable oils, starchs and so on.

    [0086] At last, as replacement of the silicate of alkali metal mentioned above, it is possible using another water-soluble material, alone or in combination with the silicate and/or with one of the other additives mentioned above. In particular, the above-mentioned intermediate layer can be made in one or more materials selected from a group comprising: gelatin, arabic gum, polyvinylpyrrolidone, carboxymethylcellulose, hydroxyethylcellulose, methylcellulose, polyvinyl alcohol.

    [0087] The water-soluble material can be, as seen, portion of a layer including it in prevalent percentage, for example with a composition of 99% of polyvinyl alcohol and already mentioned additives/adjuvants, in particular sugar and/or starchs, or 2% of sodium silicate or other, and viceversa.

    [0088] The present invention has been sofar described by referring to preferred embodiments. It is to be meant that other embodiments belonging to the same inventive core can exist, as defined by the protective scope of the herebelow reported claims.