    Abstract

    A wooden wick comprising a strip of wood. Such wick further includes a wood booster member connected to the strip of wood. At least the strip of wood or the booster member comprises a grain, wherein the grain is figured.

    Claims

    1-20. (canceled)

    21. A wick, comprising: a planar strip of wood having each of a first predetermined length, a first predetermined width, and a first predetermined thickness; and a secondary planar member having each of a second predetermined length, a second predetermined width, and a second predetermined thickness; wherein at least one of the planar strip of wood and the secondary planar member comprises a wood having a figured grain.

    22. The wick according to claim 21, wherein the planar strip of wood has a length of up to 8 inches.

    23. The wick according to claim 21, wherein the planar strip of wood has a width of less than 1 inch.

    24. The wick according to claim 21, wherein the figured grain is curly.

    25. The wick according to claim 21, the planar strip of wood comprises at least one wood selected from the group consisting of koa, walnut, ash, and ebony.

    26. The wick according to claim 21 wherein the planar strip of wood has a moisture content of less than 6 percent.

    27. The wick according to claim 21, wherein the secondary planar member is joined to the planar strip of wood with an adhesive.

    28. The wick according to claim 21, wherein the secondary planar member is joined to the planar strip of wood by at least one of fastening, clipping, banding, and riveting.

    29. The wick according to claim 21, wherein the wick is obtained by a method comprising treating with a coloring agent.

    30. The wick according to claim 29, wherein the coloring agent is a vegetable coloring agent.

    31. A method of manufacturing a wick, the comprising: cutting wood into a strip having each of a first predetermined length, a first predetermined width, and a first predetermined thickness; forming a secondary planar member having each of a second predetermined length, a second predetermined width, and a second predetermined thickness; and joining the secondary planar member to the strip of wood; wherein at least one of the strip of wood and the secondary planar member comprises a wood having a figured grain.

    32. The method according to claim 31, further comprising treating the planar strip of wood and the secondary planar member with an oil.

    33. The method according to claim 31, further comprising heating the strip of wood and the secondary planar member.

    34. The method according to claim 31, further comprising pressing the strip of wood and the secondary planar member.

    35. The method according to claim 31, further comprising subjecting the strip of wood and the secondary planar member to a vacuum.

    36. The method according to claim 31, wherein the strip of wood and the secondary planar member are joined by at least one of fastening, clipping, banding, riveting, and application of an adhesive.

    Description

    BRIEF DESCRIPTION OF THE DRAWINGS

    [0025] FIG. 1 is a plan view of a wooden wick according to an embodiment of the invention;

    [0026] FIG. 2 is a perspective view of a wooden wick according to an embodiment of the invention;

    [0027] FIG. 3 is a profile view of a wooden wick according to an embodiment of the invention;

    [0028] FIG. 4 is a plan view of a wooden wick according to another embodiment of the invention;

    [0029] FIG. 5 is a perspective view of a wooden wick according to another embodiment of the invention;

    [0030] FIG. 6 is a profile view of a wooden wick according to another embodiment of the invention;

    [0031] FIG. 7 is a plan view of a wooden wick according to another embodiment of the invention with adhesive applied in an S pattern;

    [0032] FIG. 8 is a plan view of a wooden wick according to another embodiment of the invention with adhesive applied in an S pattern and a booster member ready to receive the wooden wick;

    [0033] FIG. 9 is a perspective view of a candle comprising a wooden wick with a booster member; and

    [0034] FIG. 10 is a close-up profile view of a portion of the wooden wick with a booster member showing airflow while burning the wick.

    BRIEF DESCRIPTION OF THE INVENTION

    [0035] Prior to proceeding to the more detailed description of the present invention it should be noted that, for the sake of clarity and understanding, identical components which have identical functions have been identified with identical reference numerals throughout the several views illustrated in the drawing figures.

    [0036] The object of the invention is to provide a wood wick with a figured grain.

    [0037] In one embodiment, the invention is a wooden wick comprising a strip of wood and a wooden booster member. Either the wooden wick and/or the wooden booster member comprise a grain that is figured.

    [0038] In one embodiment of the invention, the strip of wood has a first predetermined length that will generally be between about 4.375 and about 5.125 inches, up to 10 inches, up to 8 inches or up to 6 inches. In this embodiment, the booster member comprises a second predetermined length that will generally be between about 4.375 and about 5.125 inches, up to 10 inches, up to 8 inches or up to 6 inches. The strip of wood and booster member may be wood or wood-like boards. The board may be cut to a predetermined width at any time within the method to form the wood wick.

    [0039] In one embodiment, the strip of wood has a first predetermined width, and the wooden booster has a second predetermined width. In one embodiment, the first predetermined width may be greater than the second predetermined width. In another embodiment, the first predetermined width and the second predetermined width are approximately the same. The first predetermined width and/or the second predetermined width may be between about 0.7 inch and about 0.8 inch, up to 1 inch, greater than 0.06 inches or between 0.6 inches and 1 inch.

    [0040] Figured grain is due to the grain of the wood and to the way that the wood is cut. Straight grain is grain that runs along the longitudinal surface of the wood. Figured grain is grain that is not straight. Types of figured grain include burl, cluster burl, burr, pippy, birdseye, curly, tiger stripe, ropey/flame, quilted, pomelle, beeswing, bear claw, waterfall, crotch, spalting and fiddleback.

    [0041] In one embodiment, the strip of wood or the booster member is infused with oil. This is done by soaking the strip of wood or the booster member in oil. The oil may be applied by spraying the oil onto the strip of wood or the booster member. While any oil may be used, in one embodiment, the oil is a vegetable oil. In another embodiment, the oil is soy oil. The oil aids in a consistent burn of the wick.

    [0042] In another embodiment, the strip of wood or booster member is infused with a solution. The strip of wood or booster member may be soaked in the solution. The solution may be sprayed onto the strip of wood or booster member. The solution may comprise salt water, vinegar, or a combination of salt water and vinegar.

    [0043] The salt water has a water to salt ratio (in terms of pounds) of 10 to 60 lbs of water to 1 lb of salt; 20 to 50 lbs of water to 1 lb of salt; 25 to 45 lbs of water to 1 lb of salt; 28 to 40 lbs of water to 1 lb of salt; 30 to 35 lbs of water to 1 lb of salt; 32 to 34 lbs of water to 1 lb of salt; or 33 to 34 lbs of water to 1 lb of salt. The salt may be any salt, including any edible salt. For example, the salt may be Anglesey sea salt, alacea salt, black lava salt, brine, butter salt, celery salt, curing salt, dairy salt, flake salt, fleur de sel, garlic salt, halite, Himalayan salt, jukyeorn, Kala namak, kosher salt, LoSalt, pickling salt, sal de tavira, sale marino di Trapani, sea salt, sel gris, sel de guérande, smoked salt, or truffle salt. Alternatively, the salt may comprise calcium chloride, calcium nitrate, lithium chloride, lithium nitrate, potassium chloride, potassium nitrate, magnesium chloride, magnesium nitrate, sodium chloride or sodium nitrate.

    [0044] The vinegar may be 5 to 20 percent acetic acid; 7 to 15 percent acetic acid; 8 to 12 percent acetic acid or 10 percent acetic acid. In the embodiment wherein the planar body is infused with a combination of salt water and vinegar, the solution comprises the following ratio of salt water to vinegar 1 to 10 gallons of salt water to 1 gallon of vinegar; 2.5 to 7.5 gallons of salt water to 1 gallon of vinegar; 4 to 6 gallons of salt water to 1 gallon of vinegar; 4.5 to 5.5 gallons of salt water to 1 gallon of vinegar; or 5 gallons of salt water to one gallon of vinegar.

    [0045] In one embodiment, the invention is a wooden wick comprising a strip of wood and a booster member wherein the booster member is joined to or adhered to the strip of wood. This may be done by using an adhesive, a fastener, a clip, a band, a rivet, an epoxy, a cement, or the like. In one preferred embodiment, an adhesive is used to adhere the strip to the booster member. The adhesive may be any adhesive useful in adhering materials to wood or wood-like material. The adhesive may be a natural adhesive, such as a vegetable based adhesive. The adhesive is preferably applied in an S pattern.

    [0046] The wooden wick described above may further comprise a sustainer. A sustainer provides support to a wick that is in a candle. The wick can be inserted into the sustainer. The sustainer holding the wick may be positioned in the bottom of a container. The sustainer may be secured in place with an adhesive to hold the sustainer and wick in place at the bottom of the container. The sustainer may be self-extinguishing or heat resistant before the wick and sustainer or placed into the container that would hold the meltable fuel. Alternatively, the sustainer may be non-heat resistant or not be self-extinguishing. Examples of sustainers previously used can be found in U.S. Pat. Nos. 1,226,850; 1,267,968; 1,309,545; 1,320,109; 1,344,446; 1,505,092; 2,291,067; 2,324,753; 3,462,235; 3,998,922; and 4,381,914.

    [0047] In one embodiment, the invention is a wooden wick comprising a strip of wood, a first booster member and a second booster member. The first booster member is joined to or adhered to the strip of wood. The second booster member is joined to or adhered to the strip of wood. In this embodiment, at least the strip of wood, the first booster member, or the second booster member comprises the grain described above.

    [0048] In one embodiment, the invention is a candle comprising the wooden wick described above.

    [0049] In another embodiment, the invention is a method of manufacturing a wooden wick. The method comprises providing a strip of wood. A booster member is adhered to the strip of wood. Optionally, a second booster member is adhered to the strip of wood. In this embodiment, at least the strip of wood, the first booster member, or the optional second booster member comprises the grain described above.

    [0050] In further embodiment of the method of manufacturing the wooden wick, the method further comprises cutting the strip of wood, the booster member or the optional second booster member to a predetermined length, a predetermined width and a predetermined length. The width may vary between the strip of wood and booster member and/or second booster member. Thus, the first booster member may have a width that is similar to or smaller than the width for the strip of wood. Similarly, the second booster member may have a width that is similar to or smaller than the width of the strip of wood. The first and second booster member do not need to have the same width. In a preferred embodiment, the first and second booster member have similar widths.

    [0051] The method of manufacturing the wooden wick may further comprise pressing the wood wick. The wood wick is pressed for a period of time in a wood press. The period of time may be at least 1 hour, at least 2 hours, at least 4 hours or at least 8 hours. The heating step may occur before or after the strip of wood and first booster and optional second booster member are joined to or adhered to one another.

    [0052] The method may further comprise heating the wood wick after the strip of wood and first booster and optional second booster member are joined to or adhered to one another. The heating step may comprise baking the wood wick. The baking step may comprise placing the wood wick in an oven set to a temperature between 100° F. and 250° F., between 125° F. and 200 ° F., or between 130 ° F. and 180 ° F. The heating step may occur over about 1-12 hours, about 2-10 hours, 4-8 hours or about 8 hours.

    [0053] In a further embodiment of the method of manufacturing the wooden wick, the wooden wick is treated with the solution described above. This treatment step may occur after the pressing step described above, or before the strip of wood and booster member(s) are joined to or adhered together. In one embodiment, the strip of wood and the booster member are treated separately before they are adhered to or joined together. The solution may be sprayed onto the wood wick, or the wood wick may be soaked in the solution. Alternatively, the wood wick may be treated before the pressing step described above. In the event that the wood wick is treated before the pressing step, the adhesive should be cured before proceeding to the treating step. Alternatively, the wood wick may be treated before the shavings or adhesive are applied, or after the shavings and adhesive are applied.

    [0054] The method may further comprise treating the wooden wick with the oil described above. The oil may be sprayed onto the wooden wick, or the wooden wick may be soaked in the oil. The wooden wick may be treated with the oil after the wooden wick is treated with the solution, or before the wooden wick is treated with the solution. The oil may be applied onto the wooden wick before the wood wick is pressed, or after the wood wick is pressed. In one embodiment, the strip of wood and the booster member are treated separately before they are adhered to or joined together.

    [0055] The method may further comprise treating the wooden wick with a vacuum. To do so, the wooden wick is placed into a bag, and the bag is connected to a hose that is connected to a vacuum. This step may be done after the wooden wick is treated with the oil, or before the wood wick is treated with the oil. The step may be done after the wooden wick is treated with the solution, or before the wooden wick is treated with the solution. This step may be done after the wooden wick is pressed or before the wood wick is pressed. In one embodiment, the strip of wood and the booster member are treated separately before they are adhered to or joined together.

    [0056] In another embodiment of the method of manufacturing a wood wick, comprising providing a board that is wood or wood-like material. The board may comprise a first board, a second board and an optional third board, wherein the second board and optional third board are adhered to or joined to the first board. At least one of the boards comprises a grain that is figured. The board may be treated with the oil. The board may be treated with the solution. The board may be treated with the vacuum. The board may be heated. In this particular embodiment, the method may further comprise cutting the board to form wood wicks have a predetermined length, predetermined width and predetermined thickness.

    [0057] The wooden wick has a moisture content. Since wicks can absorb moisture after processing, the moisture content for the purposes of this discussion means the moisture content at the final stage of processing. The final stage of processing can be after the last one of these steps is completed: a after the treating with the solution step; after the treating with the oil step; or after the treating with the vacuum step. The moisture content may be less than 10 percent, less than 8 percent, less than 6 percent, less than 4 percent, less than 3 percent or less than 2 percent.

    [0058] Another embodiment of the invention is a method of manufacturing a candle. The candle comprises the wooden wick described above, and a meltable fuel. For example, the wicks of the present invention may be placed in a container. The container may be filled with the meltable fuel. The meltable fuel may be a vegetable wax, such as soy wax, jojoba wax, bayberry wax, candelilla wax, carnauba wax, castor wax or a combination thereof. Alternatively, the wooden wick may comprise a sustainer, described above, and the sustainer is first secured to the bottom of the container, and then the meltable fuel is poured into the container.

    [0059] The wick of the present invention is made from all natural materials, and burns natural wax completely at a safe temperature. The planar body, the first planar booster, the second planar booster the adhesive, and/or the shavings are all natural materials. By using all natural materials, better performance is achieved.

    [0060] Reference is now made, more particularly, to FIGS. 1-3 which show an embodiment of the wick of the present invention. Illustrated therein is a wooden wick, generally designated 10, for use in a wax candle (not shown). The wooden wick 10 includes a strip of a predetermined wood 12 having each of a first predetermined length, a first predetermined width and a first predetermined thickness. Further, the wooden wick, according to the present invention, includes a booster member 14 having each of a second predetermined length, a second predetermined width and a second predetermined thickness. The strip 12 and/or the booster member 14 have a specific grain. The grain 18 is figured.)

    [0061] One example of figured grain is curly grain. Curly grain is grain that is compressed perpendicularly crossing the face of the wood that produces alternate stripes of fiber. Curly grain may be present in many species of wood, including koa, maple, walnut, ash, oaks, and ebony.

    [0062] Reference is now made, more particularly, to FIGS. 4-6 which show an embodiment of the wick of the present invention. Illustrated therein is a wooden wick, generally designated 10, for use in a wax candle (not shown). The wooden wick 10 includes a strip of a predetermined wood 12 having each of a first predetermined length, a first predetermined width and a first predetermined thickness. Further, the wooden wick, according to the present invention, includes a booster member 14 having each of a second predetermined length, a second predetermined width and a second predetermined thickness. In one embodiment, the strip has a grain 18 wherein the grain is figured. In a preferred embodiment, the grain is curly. In another embodiment, the booster member 14 has a grain 18, wherein the grain 18 is figured, or preferably curly.

    [0063] In one embodiment of the invention, the first predetermined length of such strip of wood 12 will generally be between about up to 8 inches. In this embodiment, the first predetermined width of the strip of wood 12 will generally be between about 0.06 inches and about 1 inch. In one embodiment of the invention, the second predetermined length of such booster member 14 will generally be between about 3.45 and about 3.55 inches, and the second predetermined width of the booster member 14 will generally be between about 0.06 inches and about 1 inch. Further, in this embodiment such first and second predetermined thickness will be substantially identical.

    [0064] Reference is now made, more particularly, to FIGS. 7 and 8 which show an embodiment of the wick of the present invention in the assembly process. The strip of wood 12 comprises a means for adhering the booster member 14 to such strip of wood 12. Such means is preferably an adhesive 20. Adhesive 20 is preferably applied in an S pattern as shown in FIGS. 7 and 8. The strip of wood 12 is then mated with booster member 14 as directed by directional arrow 22. This configuration has been shown to keep the strip of wood 12 and booster member 14 closely bound to each other while still allowing gases, steam and air to move between the strip of wood 12 and booster member 14. Other means for adhering the booster member to a strip of wood 12 could comprise at least one fastener, clip, band, rivet, epoxy, cement, or the like. In one embodiment, the strip of wood 12 has a grain 18, wherein the grain is figured, or preferably curly. In another embodiment, the booster member 14 has a grain 18, wherein the grain 18 is figured or preferably curly.

    [0065] Reference is now made to FIG. 9 which shows the wick 10 embedded in wax 24 to create candle 26.

    [0066] Reference is now made to FIG. 10 which shows the wick 10 with directional arrows 28 which indicate the general direction of air and gas movement while the wick 10 is burning. The chimney effect of the wick 10 has a significant effect on the efficient burning of the wick 10 and the candle 26 as a whole. The extent of the peeling away between the wood strip 12 and booster member 14 is exaggerated in this drawing for illustrative purposes.

    [0067] While presently preferred and various alternative embodiments of the present invention have been described in sufficient detail above to enable a person skilled in the relevant art to make and use the same, it should be obvious that various other adaptations and modifications can be envisioned by those persons skilled in such art without departing from either the spirit of the invention or the scope of the appended claims.