METHOD OF WAFER SCALE FABRICATION, ASSEMBLY AND ELECTRICAL CONNECTION OF A LIQUID CRYSTAL ELECTRO-OPTIC DEVICE

20170255047 · 2017-09-07

    Inventors

    Cpc classification

    International classification

    Abstract

    A method of wafer level manufacturing, separating and electrical connection of liquid crystal optical devices is disclosed. An electro-optic device having at least one liquid crystal cell for providing spatially variable control of light is also described. The electro-optic device includes: a pair of opposed substrates, each substrate having a lateral extent; a pair of electrodes for applying an electric field therebetween, each electrode having a pattern and being deposited on a corresponding substrate, each electrode having an electrical contact area extending to at least one side of the corresponding substrate; a pair of alignment layers sandwiching a liquid crystal layer therebetween, the alignment layers defining a predominant orientation direction for liquid crystal molecules of the liquid crystal layer; and a liquid crystal reservoir wall defining a lateral extent of the liquid crystal layer, the liquid crystal reservoir wall being spaced from at least one side of each substrate such that each electrode electrical contact area is exposed to air in an air gap between the substrates.

    Claims

    1. An electro-optic device having at least one liquid crystal cell for providing spatially variable control of light, the electro-optic device comprising: a pair of opposed substrates, each substrate having a lateral extent; a pair of electrodes for applying an electric field therebetween, each electrode being deposited on a corresponding substrate, each said electrode having an air-exposed electrical contact area extending to at least one side of said corresponding substrate; a pair of alignment layers sandwiching a liquid crystal layer therebetween, said alignment layers defining a predominant orientation direction for liquid crystal molecules of said liquid crystal layer; and a liquid crystal reservoir wall defining a lateral extent of said liquid crystal layer, said liquid crystal reservoir wall being spaced from said at least one side of each substrate such that each said electrical contact area of said electrodes is exposed in an air gap between said substrates.

    2. A device as claimed in claim 1, wherein each electrical contact area extends to the same side of said substrates.

    3. A device as claimed in claim 1, wherein said substrates have the same lateral extent.

    4. A device as claimed in claim 1, wherein said substrates have different lateral extent.

    5. A device as claimed in claim 1, wherein said reservoir wall comprises spacers defining a thickness of said liquid crystal reservoir.

    6. A method of wafer level manufacture of a plurality of polarization dependent electro-optic devices, the method comprising: depositing a corresponding top and bottom electrode layer of electrode material on a corresponding one of a top and bottom wafer substrates, each electrode layer defining electrical contact areas for each electro-optic device; depositing a corresponding top and bottom liquid crystal alignment layer on a corresponding one of said top and bottom electrode layers; imparting an orientation direction to each orientation layers; forming a closed liquid crystal reservoir wall for each device over said bottom alignment layer, each said liquid crystal reservoir wall having a perimeter configured to leave said electrical contact areas outside of said liquid crystal reservoir exposed to air; dispensing a liquid crystal material within each reservoir wall; and forming an array of liquid crystal cells by applying said top substrate with said alignment layer down on top of said bottom substrate such that said electrical contact areas remain exposed to air between said substrates outside said liquid crystal reservoir wall, said liquid crystal alignment layers having one of same and opposing alignment directions, said top and bottom liquid crystal alignment layers defining a liquid crystal alignment orientation.

    7. A method as claimed in claim 6, wherein in forming said liquid reservoir wall comprises spacers defining a thickness of each liquid crystal reservoir.

    8. A method as claimed in claim 6, comprising reservoir depressions formed in at least one of said wafer substrates.

    9. A method as claimed in claim 6, comprising scribing said top substrate of said wafer array of polarization dependent liquid crystal electro-optic devices in a pattern to define extents of each device thereon.

    10. A method as claimed in claim 9, wherein scribing said top substrate comprises one of a mechanically scribing said top substrate with a diamond tip and laser scribing at least said top substrate with a laser.

    11. A method of wafer level manufacture of a plurality of polarization independent electro-optical device, the method comprising: wafer level manufacturing a pair of wafers having corresponding pluralities of polarization dependent electro-optic devices in accordance with claim 6; rotating at least one of the wafers of polarization dependent electro-optic devices with respect to the other wafer of polarization dependent electro-optic devices such that liquid crystal alignment orientations between the wafers of polarization dependent electro-optic devices are orthogonal to each other; applying a thin layer of transparent adhesive to one of the wafers; bonding the wafers of polarization dependent electro-optic devices into a wafer of polarization independent electro optic devices; scribing a top-most substrate of said wafer of polarization independent electro optic devices to define extends of each device thereon; scribing a bottom-most substrate of said wafer of polarization independent electro optic devices to define extends of each device thereon; and singulating said polarization independent electro-optic devices from the wafer thereof.

    12. A method as claimed in claim 11, wherein scribing said top-most substrate and scribing said bottom-most substrate comprises employing the same scribe pattern as said scribe pattern scribed on said top substrate.

    13. A method as claimed in claim 11, wherein scribing said top-most substrate and scribing said bottom-most substrate comprises employing the a different scribe pattern from a scribe pattern scribed on said top substrate.

    14. A method as claimed in claim 13, further comprising covering said air exposed electrical contact areas with a metal layer for enabling direct soldering of external wiring to said electrode layers.

    15. In combination, the electro-optic device as defined in claim 1 and a lead frame comprising an insertion guide for receiving a side of the electro-optic device and at least one contact member inserted into said gap and making electrical contact with one of said pair of electrodes.

    16. The combination as defined in claim 15, wherein said contact member comprises one or more resilient metal strips with curled ends to be biased against said one of said pair of electrodes.

    17. The combination as defined in claim 15, wherein said lead frame forms part of a mounting for said electro-optic device.

    18. The combination as defined in claim 15, wherein said lead frame provides four electrode connections.

    19. The combination as defined in claim 15, comprising two said lead frames for receiving opposed sides of the electro-optic device.

    20. The combination as defined in claim 15, wherein said contact member comprises conductive adhesive.

    Description

    BRIEF DESCRIPTION OF THE DRAWINGS

    [0020] The invention can be better understood by way of the following detailed description of embodiments of the proposed solution with reference to the appended drawings, in which:

    [0021] FIG. 1 is a schematic diagram showing top view of a prior art wafer of liquid crystal optical devices during manufacture just prior to dicing;

    [0022] FIG. 2A is a schematic diagram showing a cross-sectional view through a diced prior art wafer level manufactured liquid crystal optical device having a liquid crystal filled reservoir;

    [0023] FIG. 2B is another schematic diagram showing a cross-sectional view through a diced prior art waver level manufactured liquid crystal optical device having overhanging substrates exposing electrode layers for external soldering;

    [0024] FIG. 2C is a perspective view illustrating a scanning electron microscope image showing a diamond scribed wafer as shown in FIG. 1;

    [0025] FIG. 2D is a perspective view illustrating a scanning electron microscope image showing spatially shifted cleaved substrates as shown in FIG. 2B;

    [0026] FIG. 3A is a schematic diagram showing general a prior art wafer of liquid crystal lens devices surrounded by backfill material;

    [0027] FIG. 3B is a schematic diagram illustrating a side view of a prior art wafer of liquid crystal lens devices surrounded by backfill material, each liquid crystal lens device having non-uniform electrodes extending to dicing lines;

    [0028] FIG. 3C is a schematic diagram illustrating a singulated liquid crystal lens device from a wafer illustrated in FIG. 3B;

    [0029] FIG. 3D is a schematic diagram illustrating external electrical edge connection to electrodes of the liquid crystal lens device illustrated in FIGS. 3B and 3C;

    [0030] FIG. 3E is a schematic diagram illustrating prior art use of conductive coatings for external electrical edge connection;

    [0031] FIG. 3F is a schematic diagram illustrating external electrical edge connection to electrodes of the liquid crystal lens device illustrated in FIG. 3E;

    [0032] FIG. 4 is another schematic diagram showing another prior art polarization independent liquid crystal lens using another electrical edge connectivity technique;

    [0033] FIG. 5A is a schematic diagram illustrating a wafer of polarization dependent LCL devices manufactured without back-fill material between individual LCL devices on the wafer, in accordance with an embodiment of the proposed solution;

    [0034] FIG. 5B is an illustration of a mechanical scribe tool employed in scribing a wafer of LCL devices;

    [0035] FIG. 5C is a schematic diagram illustrating an individual polarization dependent LCL device manufactured without back-fill material around the corresponding LC reservoir, in accordance with the proposed solution;

    [0036] FIG. 6 is a schematic diagram illustrating, in cross-section, providing electrical connectivity via soft leads inserted in side air gaps in contact with electrode layers in accordance with the proposed solution;

    [0037] FIGS. 7A and 7B are schematic diagrams illustrating patterned transparent electrode layers deposited on corresponding substrates in accordance with the proposed solution;

    [0038] FIG. 7C is a schematic diagram illustrating in cross-section transparent electrode layers extending to the same side of an LCL optical device die in accordance with the proposed solution;

    [0039] FIG. 8A is a schematic diagram illustrating a lead frame providing electrical connectivity for an individual LCL optical device illustrated in FIG. 7C in accordance with the proposed solution;

    [0040] FIG. 8B is a schematic diagram a housing providing electrical connectivity for an individual LCL optical device illustrated in FIG. 7C in accordance with another implementation of the proposed solution;

    [0041] FIG. 9A is a schematic diagram illustrating a side sectional view of a polarization independent LCL optical device in a wafer of such devices in accordance with the proposed solution;

    [0042] FIG. 9B is an illustration showing a side view of a cleaved polarization independent LCL optical device in accordance with the proposed solution;

    [0043] FIG. 9C is an illustration showing a perspective SEM view of a cleaved polarization independent LCL optical device in accordance with the proposed solution;

    [0044] FIG. 10A is a schematic diagram illustrating a side sectional view of a lead frame or housing providing electrical connectivity for a polarization independent LCL optical device in accordance with the proposed solution;

    [0045] FIG. 10B is a schematic diagram illustrating a top view of patterned electrodes on different substrates and a corresponding lead frame or housing providing electrical connectivity for a polarization independent LCL optical device in accordance with the proposed solution;

    [0046] FIGS. 11A and 11B are schematic diagrams illustrating scribe processes providing inner scribe lines on corresponding wafers of polarization dependent electro-optic devices according to the proposed solution;

    [0047] FIG. 11C is a schematic diagram illustrating a scribe process providing first external scribe lines on a wafer of polarization independent electro-optic devices according to the proposed solution;

    [0048] FIG. 11D is a schematic diagram illustrating a scribe process providing second external scribe lines on the wafer of polarization independent electro-optic devices of FIG. 11C according to the proposed solution;

    [0049] FIG. 12A is a schematic diagram illustrating a polarization independent electro-optic device layered structure having shifted scribe lines in accordance with the proposed solution;

    [0050] FIGS. 12B and 12C are illustrations showing singulated polarization independent electro-optic device layered structures respectively having outside and inside shifted scribe lines in accordance with the proposed solution;

    [0051] FIG. 13A is a schematic diagram illustrating a perspective view of a wafer laser cutting process in accordance with another embodiment of the proposed solution;

    [0052] FIG. 13B is a schematic diagram illustrating a perspective view of cleaved electro-optical dice in accordance with the proposed solution;

    [0053] FIG. 14A is a SEM micrograph showing top view of a laser scribed wafer array of electro-optic devices in accordance with the proposed solution;

    [0054] FIG. 14B is a SEM micrograph showing a front perspective view of a laser scribed wafer array of electro-optic devices in accordance with the proposed solution;

    [0055] FIG. 14C is a SEM micrograph showing a side perspective view of a laser scribed wafer array of electro-optic devices in accordance with the proposed solution; and

    [0056] FIGS. 15A and 15B are SEM micrographs showing corner regions of a laser cut electro-optic device die in accordance with the proposed solution,

    [0057] wherein similar features bear similar labels throughout the drawings. While the layer sequence described is of significance, reference to “top” and “bottom” qualifiers in the present specification is made solely with reference to the orientation of the drawings as presented in the application and do not imply any absolute spatial orientation.

    DETAILED DESCRIPTION

    [0058] The above mentioned electrical connectivity problems can be solved according to the proposed solution for example as described below.

    [0059] In accordance with a first embodiment schematically illustrated in FIG. 5A, a manufacturing process for polarization dependent LCL electro-optic device 11 arrays on a wafer 12 is followed; however the step of back-fill material injection is omitted (this is also referred to as “no-backfill material”). In this case, thousands of LCL electro-optic devices 11 are obtained on the same wafer 12, each having corresponding reservoir walls 3 (separating neighboring reservoirs 22) which are separated by air space instead of solid back-fill material. A mechanical scribe tool for example illustrated in FIG. 5B is employed to scribe (15) both sides of the wafer 12 illustrated in FIG. 5A along scribe lines 15 which form a 2D network of scribe lines, for example as illustrated in FIG. 2C. Individual polarization dependent LCL electro-optic devices 11 cleaved out of the wafer are schematically illustrated in FIG. 5C with separate electrode 5, 6 surfaces exposed inside air gaps between substrates 1, 2 alongside corresponding reservoir 22. For example, the air gap between two substrates can be 3 μm to 100 μm and the distance between the border of the substrates and the reservoir wall 3 can be 500 μm to 700 μm deep. FIG. 6 schematically illustrates, in cross-section, the use of soft solderable contacts or leads 16 inserted (and expanded) into the side air gaps to provide external electrical connectivity (8).

    [0060] For certainty, the invention is not limited to employing electrical contact leads 16 on multiple sides of a LCL electro-optic device die 11. FIG. 7A schematically illustrates a plan view of a patterned top transparent electrode 6 extending to the back right on the substrate 1, whereas FIG. 7B schematically illustrates a plan view of a patterned bottom transparent electrode 5 extending to the front right on the substrate 2. The electrode layers can be differently patterned while all electrode layers have electrically conductive area extensions which extend to one side of the die 11. As illustrated in cross-section in FIG. 7C, the assembled LCL electro-optic device die 11 includes top 6 and bottom 5 transparent electrodes extending to the right edge of the LCL electro-optic device die 11 without using back-fill material between substrates 1, 2. A lead frame 17 is illustrated in FIG. 8A having one sided leads 16. The LCL optical device die 11 of FIG. 7C can be inserted (slid) into the lead frame 17 employing insertion (sliding) guides 18. The invention is not limited to employing lead frames, an optical device housing having an aperture as illustrated in FIG. 8B can equally be employed to provide electrical connectivity in accordance with another implementation of the proposed solution. The same lead frame 17 or housing can also be employed to provide precise positioning of the electro-optic device within the overall apparatus (for example for positioning a LCL optical device within a camera).

    [0061] The invention is not limited to the above mentioned solution wherein electrical connectivity is provided for a polarization dependent LCL electro-optic device. FIG. 9 schematically illustrates a layered structure of a wafer level manufactured polarization independent LCL electro-optic device within an array thereof. Two wafers having arrays of polarization dependent LCL electro-optic devices 11 are assembled together in a stack for example by means of a thin layer of adhesive 19 using cross oriented liquid crystal layers LC.sub.∥ and LC.sub.⊥ to act on to perpendicular polarizations of incident light. In accordance with the embodiment of the proposed solution, prior to assembly, the inner bottom substrates 2, 2* of each polarization dependent LCL electro-optic device wafer 12 are scribed 15. The two external top substrates 1 can be scribed 20 after assembly. The entire assembled layered structure can be cleaved into individual polarization independent LCL electro-optic devices 11. FIG. 9B illustrates a cleaved polarization independent LCL electro-optic device showing stacked side air gaps corresponding to each liquid crystal layer 4. For example, the air gaps have a clearance of about 40 μm and are about 700 μm deep. FIG. 9C illustrates an SEM image showing a perspective view of a cleaved polarization independent LCL electro-optic device 11.

    [0062] Schematically illustrated in FIG. 10A is a side view of a mechanical housing or lead frame 17 including specific lead electrodes 16 at multiple levels which can be inserted into contact with air exposed electrode layer contact areas of the LCL electro-optic device 11 as described hereinabove. Multiple layers of electro-optic wafers can be assembled without employing back-fill material, at least some support substrates having thereon various patterned electrodes 5, 6 extending to one side of die. FIG. 10B illustrates a top view of an electrode layer configuration and of a housing having a corresponding lead 16 configuration.

    [0063] A manufacturing process in accordance with the proposed solution, includes holding, for example on a vacuum table, polarization dependent electro-optic device wafers for example having glass substrates, and using a mechanical scribe having a diamond tip for example as illustrated in FIG. 5B to scribe one of the substrates. The scribe process illustrated in FIGS. 11A and 11B scores (15) corresponding substrates 2 of each polarization dependent electro-optic device 11 while the mechanical integrity of each layered structure is maintained. The substrates 2 of each polarization dependent electro-optic device 11 can be scribed in similar fashion.

    [0064] Next, FIG. 11C illustrates an assembled polarization independent electro-optic device array (12) during fabrication, where the wafer 12 illustrated in FIG. 11A is assembled on top of the wafer 12 illustrated in FIG. 11B using a thin layer of transparent adhesive 19. Without limiting the invention, the previously made scribe lines 15 can be aligned and these scribe lines 15 are hereafter referred to internal scribe lines 15. Another scribe process (20) can be applied after this assembly process as illustrated in FIG. 11C to provide first external scribe lines 20. Without limiting the invention, the first external scribe lines 20 can be aligned with the internal scribe lines 15.

    [0065] Another final scribe process (20) can be applied to the opposed side of the polarization independent electro-optic device layered structure, as illustrated in FIG. 11D to provide second external scribe lines 20. For example, the layered wafer structure illustrated in FIG. 11C can be lifted using an adhesive tape and flipped. Without limiting the invention the second external scribe lines 20 can be aligned with the internal scribe lines 15 or with the first external scribe lines 20.

    [0066] The electrical connection of such a die 11 can be achieved if external electrodes or conductive (polymerizable) adhesive are inserted between the substrates 1&2 or 3&4.

    [0067] For certainty, the invention is not limited to vertically aligned scribe lines 15/20. In accordance with another implementation, the external scribe lines 20 can be laterally shifted 21 with respect to the internal scribe lines 15 as schematically illustrated in FIG. 12A. Depending upon the relative positions of external 20 and internal 15 scribe lines, the cleaved die 11 can have different electrode layer areas exposed to air. For example, laterally shifted scribed lines 15/20 can be employed independently in each x, y electro-optic device array direction. FIG. 12B illustrates a singulated polarization independent electro-optic device die 11 corresponding to FIG. 12A for example having a 150 μm lateral shift between the scribe lines 15/20. FIG. 12C illustrates a singulated polarization independent electro-optic device die 11 for example having a 150 μm lateral shift between the scribe lines 15/20 which would enable connection of stacked electrode 6 exposed areas with a common lead 16 expanded between the top and bottom substrates 1.

    [0068] While fast singulation of high quality electro-optic devices from a wafer is possible using the mechanical scribe and cleave process described above, the cleaved substrate edges are not equal. For example, with reference to FIGS. 9C and 9B the substrate edge offsets for aligned scribe lines can be in the range of ±40 μm.

    [0069] For certainty, the invention is not limited to employing grids of scribe lines, both internal 15 and external 20 scribes can also be circular, providing dies 11 of circular form.

    [0070] In accordance with another embodiment of the proposed solution, improved results can be obtained by employing laser cutting techniques. With reference to FIG. 13A a laser cut technique includes focusing a laser beam to score dicing lines on a wafer 12. FIG. 13A illustrates laser scoring of a wafer 12 of polarization dependent LCL electro-optic devices 11 for cutting the individual dies of LCL out of the wafer 12. FIG. 13B illustrates individual polarization dependent electro-optic device dies 11 obtained after cleaving along the laser scored lines. Without limiting the invention, cleaving can include exposing the laser scored wafer array to thermal or acoustic shock. The laser cut process can involve a bulk (glass) substrate damage (or scribe), followed by a cleave or a direct cut by local melting or evaporation or other type of damage of the substrate.

    [0071] FIGS. 14A, 14B and 14C respectively illustrate top, side and perspective scanning electron microscope micrographs of an example of a symmetric cut of an array of polarization independent electro-optic devices 11 providing horizontally exposed electrode areas enabling electrical connectivity by external electrodes' insertion as illustrated in FIGS. 10A and 10B.

    [0072] Dice edge comparison between mechanical dicing and laser dicing can be appreciated by observing FIGS. 9B and 15A, while dice edge comparisons can be appreciated by observing FIGS. 9C and 15B for the same layered geometry. No appreciable damage to the surface of the substrates nor to the thin layer of adhesive is observed. As it can be seen, it is clear that the laser cutting technique, allows obtaining air exposed electrode areas, which are still in the x-y plane while their cross section in the x-z or y-z planes is very small. The electrical connection of such a die 11 can be achieved if external electrodes or conductive (polymerizable) adhesive are inserted between the substrates 1&2 or 3&4, which have separations typically defined by the LC thickness (typically between 25 μm to 50 μm).

    [0073] While the above described laser cutting technique does not provide for vertical electrode surface exposure for example illustrated in FIGS. 12A, 12B and 12C, the laser cutting technique provides fast singulation with high quality kerf and low edge roughness in comparison with mechanical dicing techniques.

    [0074] With respect to LCL electro-optic devices, the layered geometries schematically illustrated in FIGS. 2B, 3A, 3B, 3C, 4, 5A, 5C, 9 and 12A are simplified by omitting additional layers. A person of skill in the art, would understand that the LC layer orientation of LC layers for example illustrated in FIGS. 9 and 12A is defined by corresponding alignment layers sandwiching each LC layer. An alignment orientation can imparted to each alignment layer during wafer level manufacture.

    [0075] While extensive reference has been made in the above description to LC lens optical device, the invention is not limited thereto, for example the above can equally be applied to electro-optical device providing spatially variable control of light including shutters, mirrors and beam steering devices.

    [0076] While the invention has been illustrated and described with referenced to preferred embodiments thereof, it will be recognized by those skilled in the art that various changes in form and detail may be made therein without departing from the spirit and scope of the invention as defined by the appended claims