Abstract
The present invention addresses the problem of improving both ion-selective electrode stability and adhesion between a sensitive film and a casing. This ion-selective electrode is characterized by being provided with: a sensitive membrane containing an ion-selective substance, a substrate, and a plasticizer; and a casing that holds the sensitive membrane, and by the casing material containing a substance having a solubility parameter (SP value) of 19.5 to 21.5.
Claims
1.-12. (canceled)
13. An ion-selective electrode comprising: a sensitive membrane containing an ion-selective substance, a base material, and a plasticizer; and a casing holding the sensitive membrane, wherein a material of the casing contains a substance having a solubility parameter (SP value) of 20.6 to 21.1.
14. The ion-selective electrode according to claim 13, wherein the substance is a methyl methacrylate acrylonitrile butadiene styrene resin.
15. The ion-selective electrode according to claim 13, wherein the casing and the sensitive membrane are adhered to each other inside the casing.
16. The ion-selective electrode according to claim 13, wherein the base material is polyvinyl chloride.
17. The ion-selective electrode according to claim 13, wherein the plasticizer is an adipic acid ester.
18. An ion-selective electrode comprising: a sensitive membrane containing an ion-selective substance, a base material, and a plasticizer; and a casing holding the sensitive membrane, wherein a material of the casing is a methyl methacrylate acrylonitrile butadiene styrene resin.
19. The ion-selective electrode according to claim 18, wherein the casing and the sensitive membrane are adhered to each other inside the casing.
20. The ion-selective electrode according to claim 18, wherein the base material is polyvinyl chloride.
21. The ion-selective electrode according to claim 18, wherein the plasticizer is an adipic acid ester.
22. An electrolyte concentration determination device comprising the ion-selective electrode according to claim 13.
23. An electrolyte concentration determination device comprising the ion-selective electrode according to claim 18.
Description
BRIEF DESCRIPTION OF DRAWINGS
[0016]
[0017]
[0018]
[0019]
[0020]
DESCRIPTION OF EMBODIMENTS
[0021] An embodiment of the present disclosure will be described below with reference to the accompanying drawings. The accompanying drawings show a specific embodiment consistent with principles of the present disclosure for the understanding of the present disclosure, and are not intended to be construed in a limiting sense.
<Configuration of Electrolyte Concentration Determination Device>
[0022]
[0023] The determination unit 180 includes a plurality of ion-selective electrodes 101 (ion-selective electrodes 101a to 101c), a reference electrode 104, a pinch valve 105, a vacuum aspiration nozzle 106, a shipper nozzle 107, a diluent supply nozzle 108, an internal standard solution supply nozzle 109, a dilution tank 110, a waste liquid tank 111, a vacuum pump 112, a switching valve 121, an internal standard solution syringe 131, a diluent syringe 132, a shipper syringe 133, an internal standard solution bottle 141, a diluent bottle 151, a reference electrode solution bottle 161, and a potential determination unit 171. For example, the ion-selective electrode 101a can be a chlorine ion electrode, the ion-selective electrode 101b can be a potassium ion electrode, and the ion-selective electrode 101c can be a sodium ion electrode. The number of the ion-selective electrodes 101 can be changed according to the number of types of ions to be determined. In addition, the ion-selective electrodes 101 are applicable to all ion types.
[0024] The reference electrode solution bottle 161 holds a reference electrode solution, and the reference electrode solution is introduced into a flow path of the reference electrode 104 by the shipper syringe 133. As the reference electrode solution, for example, an aqueous potassium chloride solution can be used. The internal standard solution bottle 141 holds an internal standard solution, and the internal standard solution is dispensed into the dilution tank 110 by the internal standard solution syringe 131 and the internal standard solution supply nozzle 109, and is introduced into flow paths of the ion-selective electrodes 101.
[0025] The specimen is dispensed into the dilution tank 110 by a sampling mechanism (not shown). The diluent bottle 151 holds a diluent, and the diluent is dispensed into the dilution tank 110 by the diluent syringe 132 and the diluent supply nozzle 108 to be mixed with the specimen, and the specimen diluted with the diluent is introduced into the flow paths of the ion-selective electrodes 101 by the shipper nozzle 107.
[0026] The pinch valve 105 prevents the specimen introduced into the flow paths of the ion-selective electrodes 101 from flowing back to a dilution tank 110 side. After analysis in the ion-selective electrodes 101, a liquid in the dilution tank 110 is aspirated from the vacuum aspiration nozzle 6 and discarded in the waste liquid tank 111 by driving the vacuum pump 112.
[0027] The reference electrode solution introduced into the reference electrode 104 is discarded in the waste liquid tank 111 by operating the switching valve 121, the vacuum pump 112, and the shipper syringe 133.
[0028] A potential difference (electromotive force) between the reference electrode 104 and each ion-selective electrode 101 varies depending on concentrations of ions to be analyzed in the liquid introduced into the flow paths of the ion-selective electrodes 101. The potential determination unit 171 determines the electromotive force and outputs a determination result to the recording calculation unit 181. The recording calculation unit 181 calculates the ion concentration based on the determination result of the recording calculation unit 181. As a method of determining the ion concentration using the electrolyte concentration determination device 100, for example, a method described in PTL 1 can be used.
<Configuration of Ion-Selective Electrode>
[0029]
[0030] As shown in
[0031]
[0032] The sensitive membrane 205 contains a base material, an ion-selective substance, and a plasticizer. The sensitive membrane 205 may contain an ordinary additive to be added to the sensitive membrane 205, such as an anion removing agent or a cation removing agent.
[0033] As the base material, any material may be used as long as the material itself does not have ion exchangeability and can maintain the ion-selective substance, the plasticizer, and various additives in a membrane shape, and typically polyvinyl chloride is used. In addition to polyvinyl chloride, as the base material, for example, polyvinylidene chloride, polyaniline, cellulose triacetate, polymethacrylate, polyacrylate, silicone, polyester, polyurethane, polyvinyl alcohol, and epoxy resin may be used alone or in combination.
[0034] The ion-selective substance is a substance that binds to specific ions, and is selected according to types of ions to be detected. When the ions to be detected are the cations such as sodium, potassium, calcium, magnesium, and ammonium, for example, crown ether, valinomycin, calixarene, phosphate ester, and nonactin can be used. When the ions to be detected are the anions such as chlorine, carbonate, thiocyanate, nitric acid, hydrofluoric acid, phosphoric acid, sulfuric acid, and iodine, in addition to a membrane containing an ion-selective substance such as a quaternary ammonium salt, silver halide such as silver chloride or silver bromide or an ion exchange membrane can be used.
[0035] The plasticizer can be appropriately selected according to the base material and the ion-selective substance to be used, and examples thereof include adipic acid esters such as dioctyl adipate and diisononyl adipate, phthalic acid esters such as dioctyl phthalate, diisononyl phthalate, diisodecyl phthalate, and dibutyl phthalate, trimellitic acid esters such as trioctyl trimellitate, o-nitrophenyl alkyl ethers such as o-nitrophenyl octyl ether and o-nitrophenyl decyl ether, and tris-alkyl phosphates such as tris-octyl phosphate.
[0036] The casing 201 and the sensitive membrane 205 are adhered by solvent adhesion using a solvent such as tetrahydrofuran (THF).
[0037] The casing 201 is typically formed of a vinyl chloride resin containing polyvinyl chloride as a main component. As described above, the plasticizer is likely to transfer to the vinyl chloride resin, and an electrode performance may change over time. As a result of intensive studies, the inventors have found that the above problem can be solved by using a methyl methacrylate acrylonitrile butadiene styrene resin (MABS resin) as a material of the casing 201.
[0038] The methyl methacrylate acrylonitrile butadiene styrene resin is a mixture or a copolymer of methyl methacrylate (PMMA) and acrylonitrile butadiene styrene (ABS). The methyl methacrylate acrylonitrile butadiene styrene resin is excellent in impact resistance and surface hardness, and has high thermal stability and high moldability. In addition, since the methyl methacrylate acrylonitrile butadiene styrene resin has fairly low hygroscopicity, the resin can hold the internal liquid 204 that is the electrolyte solution without absorbing the internal liquid 204.
[0039] If necessary, various additives such as a heat stabilizer, a light stabilizer, and a colorant may be added to the methyl methacrylate acrylonitrile butadiene styrene resin.
(Transfer Test of Plasticizer)
[0040] To confirm a transfer degree of the plasticizer to the material of the casing 201, a test sheet of the MABS was prepared in accordance with JIS K7114: 2001 “testing method for obtaining immersion effect in plastic-liquid chemicals”, and an immersion test was performed. A size of the test sheet was 60 mm×60 mm×1 mm, immersion temperature was 60° C., immersion time was one month at the longest, and an adipic acid-based plasticizer was used as the plasticizer in which the test sheet was immersed. As the test sheet, four types (MABS-1 to MABS-4) having different manufacturers or different model numbers among widely distributed methyl methacrylate acrylonitrile butadiene styrene resins and the vinyl chloride resin (PVC) were used.
[0041]
[0042] The weight change itself depends on the size of the test sheet and the immersion time. Therefore, to generalize an index that does not depends on the size of the test sheet and the immersion time, a weight relative change rate of the MABS resin with reference to the vinyl chloride resin was calculated.
[0043]
(Adhesion Test of Sensitive Membrane)
[0044] Next, it was confirmed whether the sensitive membrane was adhered to the casing when tetrahydrofuran was used as an adhesion solvent. First, a sodium ion-selective electrode and a potassium ion-selective electrode were produced using the methyl methacrylate acrylonitrile butadiene styrene resin as the material of the casing. When an adhesion operation between the casing and the sensitive membrane was performed using tetrahydrofuran, the methyl methacrylate acrylonitrile butadiene styrene resin was appropriately dissolved in tetrahydrofuran and the casing and the sensitive membrane easily adhered, and there was no problem in workability.
[0045] When air pressure of 100 kPa was applied to flow paths of the prepared sodium ion-selective electrode and potassium ion-selective electrode, no air leakage was observed. Therefore, it was determined that the casing formed of the methyl methacrylate acrylonitrile butadiene styrene resin was capable of sensitive membrane adhesion with tetrahydrofuran. As described above, it can be seen that when the methyl methacrylate acrylonitrile butadiene styrene resin is used as the material of the casing 201, the adhesion of the sensitive membrane can be implemented similarly to a case where the vinyl chloride resin is used.
[0046] Furthermore, the inventors have found that a solubility parameter is useful as an index for determining whether the material of the casing 201 is suitable for the ion-selective electrode 101.
[0047] The solubility parameter (SP value) is a value serving as an indication of solubility of a two-component solution, and it is empirically known that the solubility increases as a difference between SP values of the two components decreases.
[0048] The SP value includes a solubility parameter of Fedors, a solubility parameter of Hildebrand, a solubility parameter of Hansen, and the like. As the SP value for determining the transfer property between the resin and the plasticizer and the adhesion of the sensitive membrane in the present disclosure, it is more preferable to use the SP value of the solubility parameter of Hildebrand from a viewpoint that the SP value can be comprehensively calculated based on three energy parameters of dispersion, polarization, and hydrogen bond, and the solubility can be determined more accurately. A unit of the solubility parameter (SP value) is (MPa)1/2.
[0049] Table 1 shows solubility parameters (SP values) of typical plasticizers. As shown in Table 1, the solubility parameters (SP values) of these plasticizers are 17.4 to 18.4.
TABLE-US-00001 TABLE 1 Solubility parameter Plasticizer (SP value) [MPa].sup.1/2 Dioctyl phthalate 18.2 Diisononyl phthalate 18.2 Diisodecyl phthalate 17.6 Dioctyl adipate 17.8 Diisononyl adipate 17.4 Trioctyl trimellitate 18.4
[0050] According to H. Burrel, J. Brandrup, E. H. Immergut, “Polymer Handbook”, Interscience, New York (1966), it is known that the solubility parameter (SP value) of the vinyl chloride resin is 19.19 to 19.34, and the solubility parameter (SP value) of tetrahydrofuran is 21.9.
[0051] Here, solubility parameters of the four types of MABS-1 to MABS-4 were measured by a Hansen sphere method. Specifically, first, a target sample was mixed with a solvent having a known solubility parameter, and it was determined whether the sample was dissolved. Next, results of the solubility test were plotted in a three-dimensional space of solubility parameters (δD, δP, δH). Next, a sphere (Hansen sphere) including coordinates of the dissolved solvent and not including coordinates of the undissolved solvent was obtained.
[0052] Determination conditions of the solubility parameter were as follows.
[0053] Test temperature: room temperature (22° C. to 25° C.)
[0054] Test time: 24 hours
[0055] The solubility parameters of the MABS-1 to the MABS-4 were 20.6 to 21.1 as shown in Table 2.
TABLE-US-00002 TABLE 2 Solubility parameter MABS resin (SP value) [MPa].sup.1/2 MABS-1 21.1 MABS-2 20.6 MABS-3 20.6 MABS-4 20.6
[0056]
Technical Effects
[0057] As described above, in the ion-selective electrode according to the present disclosure, the substance having the solubility parameter (SP value) of 19.5 to 21.5, particularly the MABS resin, is used as the material of the casing. Accordingly, the transfer of the plasticizer contained in the sensitive membrane can be prevented, and both stability and adhesion between the casing and the sensitive membrane can be achieved. Further, since mass production and mass stock are possible due to a long life, the ion-selective electrode can be produced with high efficiency. Further, for a user, it is possible to reduce a frequency of exchange and operation time due to a lifetime of the ion-selective electrode, and thus it is possible to reduce maintenance cost.
<Modification>
[0058] The present disclosure is not limited to the embodiment described above, and includes various modifications. For example, the embodiment described above has been described in detail in order to describe the present disclosure in an easy-to-understand manner, and it is not necessary to include all the configurations described above. A part of one embodiment can be replaced with a configuration of another embodiment. The configuration of another embodiment may be added to the configuration of one embodiment. Further, a part of the configuration of another embodiment may be added to, deleted from, or replaced with a part of the configuration of each embodiment.
REFERENCE SIGN LIST
[0059] 100 electrolyte concentration determination device [0060] 101 ion-selective electrode [0061] 104 reference electrode [0062] 105 pinch valve [0063] 106 vacuum aspiration nozzle [0064] 107 shipper nozzle [0065] 108 diluent supply nozzle [0066] 109 internal standard solution supply nozzle [0067] 110 dilution tank [0068] 111 waste liquid tank [0069] 112 vacuum pump [0070] 121 switching valve [0071] 131 internal standard solution syringe [0072] 132 diluent syringe [0073] 133 shipper syringe [0074] 141 internal standard solution bottle [0075] 151 diluent bottle [0076] 161 reference electrode solution bottle [0077] 171 potential determination unit [0078] 180 determination unit [0079] 181 recording calculation unit [0080] 182 output unit [0081] 183 control unit [0082] 184 input unit [0083] 201 casing [0084] 202 flow path [0085] 203 silver/silver chloride electrode [0086] 204 internal liquid [0087] 205 sensitive membrane