METHOD PREPARING SILVER-NANOCURCUMIN MATERIAL FOR INHIBITING NEW CORONAVIRUS

20220160673 · 2022-05-26

    Inventors

    Cpc classification

    International classification

    Abstract

    The present disclosure provides a method preparing Silver-nanocurcumin material for inhibiting new coronavirus. The turmeric powder is heated and stirred and then mixed with silver nitrate solution. After multiple steps of cooling, stirring for reaction and centrifuging and other steps, crude extract of Silver-nanocurcumin is obtained. Then, after further processes such as the multiple washing and centrifuging, a purified composition of Silver-nanocurcumin is obtained. The composition of Silver-nanocurcumin can be used to inhibit the new coronavirus and its similar viruses, and as a source of drugs for the prevention and treatment of diseases derived from the new coronavirus COVID-19 in the future.

    Claims

    1. A method of preparing Silver-nanocurcumin material for inhibiting new coronavirus is characterized in that it comprises the following steps in sequence: step1: mixing turmeric powder with deionized water; step2: heating to boiling; step3: cooling and stirring; step4: mixing the silver nitrate solution; step5: cooling and stirring for reaction; step6: centrifuging; step7: taking out the supernatant; step8: centrifuging the supernatant; step9: collecting the precipitate to obtain crude extract of Silver-nanocurcumin; step10: adding deionized water to mix and wash by shaking at high speed; step11: centrifuging; step12: collecting the precipitate; step13: repeating washing and centrifuging; and step14: obtaining a purified composition of the Silver-nanocurcumin.

    2. The method for preparing Silver-nanocurcumin material for inhibiting new coronavirus according to claim 1, characterized in that, in the step 1, 5 grams of the turmeric powder are weighed out and poured into 500 ml of the deionized water.

    3. The method for preparing Silver-nanocurcumin material for inhibiting new coronavirus according to claim 2, characterized in that, in the step 2, the deionized water is mixed with the turmeric powder in the step 1 is heated to boiling, and keeping boiling for 5 minutes.

    4. The method for preparing Silver-nanocurcumin material for inhibiting new coronavirus according to claim 3, characterized in that, in the step 3, the liquid in the step 2 is cooled and then stirred under the temperature ranging 75-85° C.

    5. The method for preparing Silver-nanocurcumin material for inhibiting new coronavirus according to claim 4, characterized in that, in the step 4, 5 ml of 1 mmol silver nitrate solution is added and stirred while carrying out the step 3.

    6. The method for preparing Silver-nanocurcumin material for inhibiting new coronavirus according to claim 5, characterized in that, in the step 5, the liquid temperature in the step 4 is lowered to 45˜55° C. and stirred for 24 hours then ending the reaction.

    7. The method for preparing Silver-nanocurcumin material for inhibiting new coronavirus according to claim 6, characterized in that, in the step 6, centrifuging is carried out at 3000 rpm under 4° C. for 10 minutes to remove the precipitate.

    8. The method for preparing Silver-nanocurcumin material for inhibiting new coronavirus according to claim 7, characterized in that, in the step 7, the supernatant is taken out of the liquid centrifugated in the step 6 from which the precipitate have been removed; in the step 8, the supernatant of the step 7 is centrifuged at 14000 rpm under 4° C. for 1 hour.

    9. The method for preparing Silver-nanocurcumin material for inhibiting new coronavirus according to claim 8, characterized in that, in the step 9, the precipitate is collected and the precipitate is crude extract of Silver-nanocurcumin; in the step 10, 50 ml of the deionized water is added to wash the crude extract of Silver-nanocurcumin with shaking.

    10. The method for preparing Silver-nanocurcumin material for inhibiting new coronavirus according to claim 9, characterized in that, in the step 11, the crude extract of Silver-nanocurcumin is centrifuged at 14000 rpm under 4° C. for 1 hour; in the step 12, the precipitate of the step 11 is collected; in the step 13, the precipitate of the step 12 is washed and centrifuged repeatedly at 14000 rpm under 4° C. to remove residual silver nitrate.

    Description

    BRIEF DESCRIPTION OF THE DRAWINGS

    [0033] The present disclosure will be further described in detail below with reference to the drawings and specific embodiments.

    [0034] FIG. 1 is a block diagram of the step flow of the present disclosure.

    DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

    [0035] The technical solutions in the embodiments of the present disclosure will be clearly and completely described below in conjunction with the drawings in the embodiments of the present disclosure. In the following description, many specific details are set forth in order to fully understand the present disclosure, but the present disclosure can also be implemented in other ways different from those described here, and those skilled in the art can do so without departing from the connotation of the present disclosure. Similar promotion, therefore, the present disclosure is not limited by the specific embodiments disclosed below.

    [0036] Please refer to FIG. 1, a method of preparing Silver-nanocurcumin material for inhibiting new coronavirus includes the following steps in sequence:

    [0037] step1: mixing turmeric powder with deionized water;

    [0038] step2: heating to boiling;

    [0039] step3: cooling and stirring;

    [0040] step4: mixing the silver nitrate solution;

    [0041] step5: cooling and stirring for reaction;

    [0042] step6: centrifuging;

    [0043] step7: taking out the supernatant;

    [0044] step8: centrifuging the supernatant;

    [0045] step9: collecting the precipitate to obtain the crude extract of Silver-nanocurcumin;

    [0046] step10: adding deionized water to mix and wash by shaking at high speed;

    [0047] step11: centrifuging;

    [0048] step12: collecting the precipitate;

    [0049] step13: repeating washing and centrifuging; and

    [0050] step14: obtaining a purified composition of Silver-nanocurcumin.

    [0051] Wherein, in the step 1, 5 grams of the turmeric powder are weighed out and poured into 500 ml of the deionized water; in the step 2, the deionized water is mixed with the turmeric powder in the step 1 is heated to boiling, and keeping boiling for preferably 5 minutes; in the step 3, the liquid in the step 2 is cooled and then stirred gently under the temperature ranging 75-85° C., and preferably 85° C.; in the step 4, 5 ml of 1 mmol silver nitrate solution is added and stirred while stirring; in the step 5, the liquid temperature in the step4 is lowered to 45-55° C., preferably 50° C., and stirred gently for 24 hours then ending the reaction; in the step 6, centrifuging is carried out at 3000 rpm under 4° C. for 10 minutes to remove the precipitate; in the step 7, the supernatant is taken out of the liquid centrifugated in the step 6 from which the precipitate have been removed; in the step 8, the supernatant of the step 7 is centrifuged at 14000 rpm under 4° C. for 1 hour; in the step 9, the precipitate is collected and the precipitate is crude extract of Silver-nanocurcumin; in the step 10, 50 ml of the deionized water is added to wash the crude extract of Silver-nanocurcumin with shaking; in the step 11, the crude extract of Silver-nanocurcumin is centrifuged at 14000 rpm under 4° C. for 1 hour; in the step 12, the precipitate of the step 11 is collected; in the step 13, the precipitate of the step 12 is washed and centrifuged repeatedly at 14000 rpm under 4° C. to remove residual silver nitrat; at last, in the step 14, a purified composition of Silver-nanocurcumin is obtained.

    [0052] The composition of Silver-nanocurcumin can be mixed with pure water to become a nasal spray during application, or mixed with various solids or liquids to form powder, liquid or gel-like anti-virus and anti-bacterial products.

    [0053] It should be further clarified that there is no safety concern about the normal use of nano-silver in the human body. Since the human body usually consumes silver from food and water daily, the human body has a normal mechanism for processing and metabolizing silver. The silver content in most foods is in the range of 10-100 μg/kg. The biological half-life of silver in the human liver ranges from several days to 50 days, and most of the absorbed silver will be excreted with the bile in the feces.

    [0054] After research, the inventors found that Silver-nanocurcumin of the present disclosure can be used to prevent the new coronavirus COVID-19 infection in healthy humans; Spraying Silver-nanocurcumin into the nasal cavity with a nasal spray can get the virus killed in the nasal cavity within a certain period of time. Spraying the appropriate amount multiple times in a day to make the nasal cavity partly with Silver-nanocurcumin within a few hours to kill the virus and block the cells to protect them from infection.

    [0055] The composition of Silver-nanocurcumin prepared by the present disclosure can not only be used to inhibit the new coronavirus and its similar viruses, but also be used as a drug source for the prevention and treatment of diseases derived from the new coronavirus COVID-19 in the future. In addition, it is a biological antiviral material, which is odorless, harmless, non-toxic and non-irritating to organisms. It can be used for cleaning, disinfection, sterilization, and anti-bacterial products such as desks, masks, door handles, mobile phones, elevator keys and other items, as well as medical disinfection and wound healing, influenza virus, enterovirus and other follow-up medical research and development applications, food processing and disinfection, fresh fruit and vegetable disinfection, frozen food disinfection, cosmetic hygiene operations; also can be used in confined spaces (For example, air disinfection in airplanes, vehicles, ships, skyscrapers, and any central air-conditioning facilities) is used to reduce the COVID-19 aerosol content in the air, thereby reducing the speed and capacity of COVID-19 transmission.

    [0056] Obviously, the described embodiments are only a part of the embodiments of the present disclosure, rather than all the embodiments. Based on the embodiments of the present disclosure, all other embodiments obtained by those of ordinary skill in the art without creative work shall fall within the protection scope of the present disclosure.