Method for laser carving of paint on an outer surface of a vehicle wheel
11738406 ยท 2023-08-29
Assignee
Inventors
- Ching Jui Chang (Douliu, TW)
- Jui Lung Kao (Chiayi County, TW)
- Yung Sheng Wang (Yunlin County, TW)
- Viktor Robertsson (Gothenburg, SE)
- Andreas Andreen (Gothenburg, SE)
- Juan Zhao (Shanghai, CN)
Cpc classification
B05D3/068
PERFORMING OPERATIONS; TRANSPORTING
B23K26/40
PERFORMING OPERATIONS; TRANSPORTING
B05D5/06
PERFORMING OPERATIONS; TRANSPORTING
International classification
B23K26/40
PERFORMING OPERATIONS; TRANSPORTING
B23K26/70
PERFORMING OPERATIONS; TRANSPORTING
Abstract
A method for laser carving of paint on an outer surface of a vehicle wheel includes a step of priming: priming an outer surface of the wheel to form a painted surface; a step of laser carving: carving the primer from a selected area of the wheel by laser to remove the painted surface from the selected area, the selected area having an exposed area with metallic luster, and a step of fine-polish: polishing the outer surface of the wheel to form a fine-polished area at the exposed area. The painted surface on the wheel can be quickly removed to disclose a selected area with metallic luster, while the wheel is prevented from corrosion so as to reduce manufacturing cost and increase precision.
Claims
1. A method for laser carving of paint on an outer surface of a vehicle wheel, comprising: a step of priming: applying a primer on an outer surface of the vehicle wheel to form a first layer or undercoat, and a color layer is applied on the primer and combined with the primer to obtain a colored painted surface; a step of applying a protective paint to the painted surface of the vehicle wheel to form a first protective layer on the color layer which is located between the primer and the first protective layer; a step of laser carving: carving a selected area of the primer from the vehicle wheel by laser to remove the painted surface from the selected area, the selected area having an exposed area with metallic luster, and being located on one of spokes of the vehicle wheel, the selected area of the painted surface being removed by way of carving to form patterns on the exposed area; a step of fine-polish: polishing the outer surface of the vehicle wheel to form a fine-polished area at the exposed area; and applying a protective paint to the outer surface of the vehicle wheel to form a second protective layer on the first protective layer, the fine polished face of the exposed area including the second protective layer formed thereon.
2. The method as claimed in claim 1, wherein a step of rough polish is added before the step of priming and comprises: cleaning and proceeding surface polish to the wheel to form a rough polished face on the outer surface of the vehicle wheel, the primer layer of the painted surface in the step of priming being applied to the rough polished face.
3. The method as claimed in claim 2, wherein in the step of fine-polish, the exposed area that is formed in the selected area by way of laser carving and the rough polished face are exposed, the rough polished face of the exposed area is polished to transfer the rough polished face into the fine polished face, a surface roughness of the fine polished face is less than that of the rough polished face.
Description
BRIEF DESCRIPTION OF THE DRAWINGS
(1)
(2)
(3)
(4)
(5)
(6)
(7)
(8)
DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENT
(9) The method of the present invention uses a laser carving machine to proceed the step of laser carving of the method, wherein the laser carving machine includes scanning speed of 100 mm/s to 4000 mm/s, laser frequency of 1 kHz to 6 kHz, power of 1 W to 500 W, wave length of 9000 nm (nanometers) to 11000 nm (nanometers), and light type of CO2/fiber.
(10) Referring to
(11) As shown in
(12) As shown in
(13) In the step of fine-polish S3, the outer surface of the wheel 1 is polished to form a fine-polished area 30 at the exposed area. The polished outer surface is smooth.
(14) As shown in
(15) The exposed area in the step of laser carving S2 is uneven and rough, and in the step of fine-polish S3, the fine-polished area 30 is formed on the exposed area, and the polished outer surface is smooth. The surface roughness of the fine polished face 30 is less than that of the rough polished face 40. It is noted that the rough-polish achieves that the treated surface becomes smooth to allow the first layer or undercoat 11 to be formed thereon, and the fine-polish makes the metallic luster appear.
(16) As shown in
(17) As shown in
(18) The advantages of the present invention are that the method uses laser to carve the outer surface of the wheel 1, and the painted surface 10 can be quickly removed to let the metallic luster appear, or to display the patterns carved to the wheel 1. The method includes ability for anti-corrosion and reduces cost.
(19) The outer surface of the wheel 1 treated by the method of the present invention is smooth so as to meet requirements of users.
(20) The second protective layer 60 protects the fine polished face 30 from being scratched, and enhances the protection to the painted surface 10.