METHOD FOR CONCENTRATING AND PURIFYING ELUATE BRINE FOR THE PRODUCTION OF A PURIFIED LITHIUM COMPOUND
20220144655 · 2022-05-12
Assignee
Inventors
Cpc classification
C02F1/52
CHEMISTRY; METALLURGY
Y02P10/20
GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
B01D61/463
PERFORMING OPERATIONS; TRANSPORTING
B01D61/025
PERFORMING OPERATIONS; TRANSPORTING
B01D2311/25
PERFORMING OPERATIONS; TRANSPORTING
B01D61/026
PERFORMING OPERATIONS; TRANSPORTING
C02F9/00
CHEMISTRY; METALLURGY
Y02W10/37
GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
B01D2009/0086
PERFORMING OPERATIONS; TRANSPORTING
B01D2311/08
PERFORMING OPERATIONS; TRANSPORTING
B01D2311/2642
PERFORMING OPERATIONS; TRANSPORTING
B01J47/12
PERFORMING OPERATIONS; TRANSPORTING
B01D2311/06
PERFORMING OPERATIONS; TRANSPORTING
International classification
B01D15/36
PERFORMING OPERATIONS; TRANSPORTING
B01D61/02
PERFORMING OPERATIONS; TRANSPORTING
B01J47/12
PERFORMING OPERATIONS; TRANSPORTING
Abstract
A method is disclosed for concentrating and purifying an eluate brine and producing a purified lithium compound. An extraction eluate, rich in lithium, is directed to a nanofiltration unit or a softening process that removes sulfate and/or calcium and magnesium. Permeate from the nanofiltration unit or the effluent from the softening process is directed through an electrodialysis unit. As the lithium-rich solution moves through the electrodialysis unit, lithium, sodium and chloride ions pass from the solution through a cation-transfer membrane and an anion-transfer membrane to concentrate compartments. A dilute stream is directed through the concentrate compartments and collects the lithium, sodium and chloride ions. The electrodialysis unit also produces a product stream which contains non-ionized impurities, such as silica and/or boron. Concentrate from the electrodialysis unit is subject to a precipitation process that produces a lithium compound that is subsequently subjected to a purification process.
Claims
1. A method of recovering lithium carbonate from a brine rich in lithium, sodium and chloride and having impurities in the form of hardness, sulfate, and silica, the method comprising: directing the brine to a nanofiltration unit and subjecting the brine to nanofiltration and removing sulfate from the brine, along with hardness associated with the sulfate; wherein after nanofiltration, the brine still contains silica and residual hardness and remains rich in lithium, sodium and chloride; after nanofiltration, maintaining conditions in the brine that result in the silica being substantially non-ionized; further after nanofiltration, directing the brine through an electrodialysis unit and subjecting the brine to an electrodialysis process and producing a concentrate rich in lithium, sodium and chloride and a product stream depleted in lithium, sodium and chloride but including the substantially non-ionized silica; after subjecting the brine to the electrodialysis process, directing the concentrate to an ion-exchange unit and removing residual hardness from the concentrate; after removing residual hardness from the concentrate, directing the concentrate of lithium, sodium and chloride to a precipitating unit and mixing a selected reagent with the concentrate and precipitating lithium carbonate; and recovering the precipitated lithium carbonate.
2. The method of claim 1 further including: directing the product stream from the electrodialysis unit to a reverse osmosis unit and producing a permeate stream and a concentrate stream containing silica; and utilizing the permeate stream in a lithium extraction process that take places upstream of the nanofiltration unit.
3. The method of claim 1 further including: directing the concentrate from the electrodialysis unit to an evaporator or crystallizer and further concentrating the concentrate; and thereafter directing the further concentrated concentrate to the ion exchange unit.
4. The method of claim 1 including mixing sodium carbonate with the concentrate rich in lithium, sodium and chloride and precipitating lithium carbonate.
5. The method of claim 1 wherein the electrodialysis unit comprises a feed compartment that produces the product stream and two concentrate compartments that produce the concentrate and which are disposed on opposite sides of the feed compartment; and wherein the concentrate compartments are separated from the feed compartment by a cation-transfer membrane and an anion-transfer membrane.
6. A method of recovering lithium from a natural brine containing lithium, sodium, chloride, hardness and in addition silica or boron, the method comprises: extracting lithium from the natural brine and producing an extraction eluate rich in lithium, sodium and chloride; subjecting the extraction eluate to a nanofiltration process or a softening process and removing hardness from the extraction eluate and producing a brine rich in lithium, sodium and chloride; maintaining conditions in the brine that result in the silica or boron being maintained substantially non-ionized; directing the brine through an electrodialysis unit and subjecting the brine to an electrodialysis process and producing a concentrate rich in lithium, sodium and chloride and a product stream depleted in lithium, sodium and chloride but including the substantially non-ionized silica or boron; directing the concentrate containing lithium, sodium and chloride to a precipitating unit and mixing a selected reagent with the concentrate and precipitating a lithium compound; and recovering the precipitated lithium compound.
7. The method of claim 6 wherein, after the electrodialysis process, the method includes directing the concentrate to an ion exchange unit and removing residual hardness from the concentrate.
8. The method of claim 6 wherein, after the electrodialysis process, directing the concentrate rich in lithium, sodium and chloride to a thermal evaporation or crystallization unit and further concentrating the concentrate from the electrodialysis unit.
9. The method of claim 6 wherein the electrodialysis process produces a product stream that includes the substantially non-ionized silica or boron and the method includes directing the product stream to a reverse osmosis unit and producing a permeate stream and a concentrate stream containing the substantially non-ionized silica or boron; and utilizing the permeate stream in the lithium extraction process.
10. The method of claim 6 wherein the selected reagent mixed with the brine rich in lithium, sodium and chloride causes lithium carbonate to precipitate, and the method further includes recovering the precipitated lithium carbonate.
11. The method of claim 6 wherein the electrodialysis unit comprises a feed compartment that produces a product stream and two concentrate compartments that produce the concentrate containing lithium, sodium and chloride ions, and wherein the concentrate compartments are disposed on opposite side of the feed compartment; and wherein the concentrate compartments are separated from the feed compartment by a cation-transfer membrane and an anion-transfer membrane.
12. A method of recovering lithium carbonate from a brine rich in lithium, sodium and chloride and having impurities in the form of hardness and silica, the method comprising: maintaining conditions in the brine that result in a substantial portion of the silica being non-ionized; directing the brine to an electrodialysis unit that employs monovalent selective membranes; in the electrodialysis unit, transporting monovalent cations including lithium and sodium and monovalent anions, including chloride, to concentration compartments which are fed with demineralized water and producing: (1) a concentrated demineralized water containing lithium, sodium, chloride, and hardness in the demineralized water; and (2) a product stream depleted in lithium, sodium and chloride but including non-ionized silica; directing the concentrated demineralized water to an ion exchange unit and removing hardness from the concentrated demineralized water; and extracting a lithium compound from the concentrated demineralized water.
Description
BRIEF DESCRIPTION OF THE DRAWINGS
[0008]
[0009]
[0010]
DESCRIPTION OF EXEMPLARY EMBODIMENTS
[0011] The present invention relates to a process for recovering lithium. Lithium is a highly reactive alkali metal that offers excellent heat and electrical conductivity. These properties make lithium particularly useful for lithium ion batteries for electric cars and consumer electronics, as well as useful for pharmaceutical and chemical applications. Because of its high reactivity, pure elemental lithium is not found in nature but is instead present as a constituent of salts and other compounds. Most commercial lithium is available in the form of lithium carbonate which is a relatively stable compound that can easily be converted to other salts or chemicals.
[0012] Lithium salts are found in underground deposits of brine, mineral ore as well as sea water and geothermal brines. While lithium is fairly abundant, not all lithium sources are deemed economically viable at this time. Generally speaking, however, commercial lithium arises from two main sources: underground brine and mineral ore deposits. A large amount of today's lithium is recovered from liquid brine reservoirs located beneath salt flats, known as salars. Other lithium-rich brine resources include geothermal and oil field brines.
[0013] Lithium recovery in general is a relatively long process. In the case of salar brine deposits, for example, drilling is generally required to access the brine deposits. Once accessed, the brine containing lithium is pumped to the surface and placed in solar ponds where an evaporation process takes place. Brine remains in the solar ponds until most of the water content has been removed through solar evaporation. Salar brines, for example, are concentrated and in addition to lithium, typically contain sodium, chloride, as well as any number of impurities such as sulfate, silica and/or boron.
[0014]
[0015] Typically, after brine preparation and filtration, the brine is rich in lithium and, in the present example, includes sodium chloride and other impurities. As noted above, the impurities in the brine can vary based on the source of the brine. In this exemplary process, the impurities include sulfate, silica and/or boron, along with hardness in the form of calcium and magnesium. There may also be small trace amounts of transitional metals. In any event, after the preparation and filtration step referred to above, the brine is subjected to a lithium extraction process 14. Here lithium is extracted from the effluent from the natural brine preparation and filtration stage discussed above. Various lithium extraction processes can be employed and people skilled in the art appreciate various lithium extraction processes. In the exemplary process shown in
[0016] Constituents of the exemplary eluate will vary depending on the lithium source and the particular lithium extraction process employed. In this example, the lithium extraction process 14 produces a brine rich in lithium and sodium chloride and having a range of impurities, such as silica, sulfate, boron, calcium and magnesium. In one example, the total suspended solids in the brine can be approximately 11,000 mg/L and contain approximately 20 mg/L of silica, 100 mg/L of boron, 50 mg/L of sulfate and approximately 50 mg/L of calcium, as well as approximately 50 mg/L of magnesium. It is stressed that these are exemplary concentrations and that the particular concentrations of these constituents will vary from one lithium production process to another.
[0017] After the lithium extraction process 14, the process focuses on removing some impurities from the lithium-rich brine. In the exemplary process discussed here, the sulfate, calcium and magnesium is first addressed. Various approaches, such as nanofiltration, chemical softening or ion exchange softening, can be employed, In this exemplary process, the lithium-rich brine is subjected to a nanofiltration process which produces a reject stream containing sulfate and calcium and magnesium associated with the sulfate. Tests indicate that 95%-99% of the sulfate can typically be removed from the lithium-rich brine. Thus, the permeate from the nanofiltration process will continue to be a brine rich in lithium and sodium chloride and may include some residual hardness (calcium and magnesium), along with other impurities which, in this example, are principally silica and boron. It is contemplated that, in some cases, the permeate from the nanofiltration process will contain 90% wt. of lithium and sodium chloride.
[0018] The permeate from the nanofiltration unit, rich in lithium and sodium chloride, is directed to an electrodialysis unit 16. The principal function of the electrodialysis unit 16 is to separate the lithium, sodium and chloride ions from the brine and produce a concentrate rich in lithium, sodium and chloride ions.
[0019] The feed to the electrodialysis unit 16 is rich in lithium, sodium and chloride ions, but there are still impurities in the feed. To address some impurities, the process takes steps to maintain these impurities in a non-ionized state. If the impurity is non-ionized, it will not pass through the cation-transfer membrane 16A or the anion-transfer membrane 16D but will remain in the product compartment 16G and ultimately will be a constituent of the demineralized product that leaves the product compartment. See
[0020] Referring to
[0021] As shown in
[0022] In some cases, it is possible that the impurities in the concentrate produced by the electrodialysis unit 16 require removal through thermal evaporation or crystallization. This is, however, optional in many cases. Even if required, the amount of impurities in the concentrate may still be sufficiently low that only a relatively small thermal evaporation and crystallization is required.
[0023] It is possible that the electrodialysis concentrate might still contain residual hardness above a trace amount, as well as transition metals. Residual hardness can be removed by ion exchange softening.
[0024] After brine polishing with an ion exchange unit, the effluent is subjected to a precipitation process that precipitates lithium carbonate. Various types of reagents can be employed at this stage to precipitate substantially pure lithium compounds. In one example, sodium carbonate is mixed with the lithium, sodium and chloride-rich stream to cause the precipitation of lithium carbonate. Once the lithium carbonate has been precipitated, various processes can be employed for the purification of lithium carbonate. See
[0025]
[0026] As seen in
[0027] The product stream containing the impurities, such as silica and/or boron, is directed to a reverse osmosis system where the impurities are concentrated into an RO concentrate and then directed to a waste management unit. See
[0028] As an alternative to the process discussed above and shown in
[0029] The present invention may, of course, be carried out in other specific ways than those herein set forth without departing from the scope and the essential characteristics of the invention. The present embodiments are therefore to be construed in all aspects as illustrative and not restrictive and all changes coming within the meaning and equivalency range of the appended claims are intended to be embraced therein.