Method for manufacturing or for repairing a component of a rotary machine as well as a component manufactured or repaired using such a method
11318568 · 2022-05-03
Assignee
Inventors
Cpc classification
B33Y10/00
PERFORMING OPERATIONS; TRANSPORTING
B23K9/044
PERFORMING OPERATIONS; TRANSPORTING
B23K2103/26
PERFORMING OPERATIONS; TRANSPORTING
B23K2103/42
PERFORMING OPERATIONS; TRANSPORTING
B23K10/027
PERFORMING OPERATIONS; TRANSPORTING
F05D2220/30
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
F05D2230/80
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
F05D2230/10
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
B23P2700/06
PERFORMING OPERATIONS; TRANSPORTING
F04D29/2222
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
B22F7/08
PERFORMING OPERATIONS; TRANSPORTING
B33Y80/00
PERFORMING OPERATIONS; TRANSPORTING
B23P15/04
PERFORMING OPERATIONS; TRANSPORTING
F05D2230/60
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
B23K2103/08
PERFORMING OPERATIONS; TRANSPORTING
B23K9/167
PERFORMING OPERATIONS; TRANSPORTING
F05D2230/31
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
B23P6/007
PERFORMING OPERATIONS; TRANSPORTING
B22F10/28
PERFORMING OPERATIONS; TRANSPORTING
B22F5/009
PERFORMING OPERATIONS; TRANSPORTING
F04D29/026
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
F01D5/048
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
F04D29/023
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
Y02P10/25
GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
International classification
B23P15/04
PERFORMING OPERATIONS; TRANSPORTING
B23P6/00
PERFORMING OPERATIONS; TRANSPORTING
F04D29/28
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
F04D29/22
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
B22F5/00
PERFORMING OPERATIONS; TRANSPORTING
B23K9/167
PERFORMING OPERATIONS; TRANSPORTING
B23K9/04
PERFORMING OPERATIONS; TRANSPORTING
B23P15/00
PERFORMING OPERATIONS; TRANSPORTING
F04D29/02
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
B33Y80/00
PERFORMING OPERATIONS; TRANSPORTING
Abstract
A method for manufacturing a component of a rotary machine, the component extends in an axial direction and a radial direction vertical thereto, and has an inner channel, extending from a first end in a center of the component to a second end at a radial limiting surface of the component and which is partially closed. A blank includes the center of the component and is limited by an outer surface in the radial direction. The maximum dimension of the outer surface in the radial direction is smaller than the dimension of the limiting surface in the radial direction, A first subtractive process step is performed such that a part of the channel is manufactured by a machining process, with the part extending from the first end of the channel to the outer surface of the blank. Afterwards the channel is finished by a build-up process on the blank.
Claims
1. A method for manufacturing a component of a rotary machine, the component extending in an axial direction and a radial direction vertical thereto, and having at least one inner channel extending from a first end in a center of the component to a second end at a radial limiting surface of the component and which is at least partially closed, that the method comprising: providing a blank comprising the center of the component, and the blank being limited by an outer surface in the radial direction, the maximum dimension of the outer surface in the radial direction being smaller than a dimension of the limiting surface in the radial direction; performing a first subtractive process step in which a part of the channel is manufactured by a machining process, with the part extending from the first end of the channel to the outer surface of the blank; and afterwards finishing the channel by a build-up process on the blank by application of at least part of a shapeless or a neutrally shaped material, the build-up process on the blank including building the channel axially adjacent and radially outside of the outer surface of the blank.
2. The method according to claim 1, wherein the at least one inner channel includes a plurality of inner channels, each of the plurality of inner channels extending from a first end in the center of the component to a second end at the radial limiting surface of the component, adjacent channels are respectively separated by a separating wall, and for each channel, one part of the channel is manufactured in the first subtractive process step, with the part extending from the respective first end of the channel into the outer surface of the blank, and each separating wall and each channel is only finished by the build-up process.
3. The method according to claim 1, wherein the blank has a central bore before the first subtractive process step, the bore being arranged radially inwardly such, that in the finished state of the component each first end of a channel arranged in the center is separated from the central bore by an annular body.
4. The method according to claim 1, wherein the first subtractive process step is performed in such a manner, that after finishing the outer surface of the blank, the blank comprises a contiguous annular area covering the confluence of the channel into the outer surface.
5. The method according to claim 1, wherein the build-up process is performed layer by layer.
6. The method according to claim 1, wherein the build-up process comprises several additive process steps to successively build up the component.
7. The method according to claim 6, wherein at least one further subtractive process step is performed between the additive process steps.
8. The method according to claim 6, wherein in each case one further subtractive process step is performed between two additive process steps.
9. The method according to claim 1, wherein the component is built up part by part after the first subtractive process step.
10. The method according to claim 1, wherein the build-up process is performed by a laser.
11. The method according to claim 1, wherein the component is an impeller, a guide wheel or a diffusor of a rotary machine.
12. The method according to claim 1, wherein the shapeless or neutrally shaped material is a powder, a band or a wire.
13. The method according to claim 9, wherein during the build up part all of each separating wall is completed first.
14. The method according to claim 11, wherein the component is part of a pump, a turbine, a compressor, a compactor or an expander.
Description
BRIEF DESCRIPTION OF THE DRAWINGS
(1) The invention will be explained in more detail hereinafter with reference to the drawings.
(2)
(3)
(4)
(5)
(6)
DETAILED DESCRIPTION OF THE EMBODIMENTS
(7) The method according to the invention is used for manufacturing a component of a rotary machine, the component having at least one inner channel, extending out of a center to a limiting surface of the component and which channel is at least partially closed. Here a closed channel is a channel, which is completely closed, except for an inlet or an outlet, so the channel has a tubular shape, that is to say, the channel is limited by one wall or by several walls anywhere, vertical to its main direction of flow. In contrast, an open channel means a channel, which is not limited by a wall in a direction vertical to its main direction of flow, thus in a direction vertical to its longitudinal extension, but it is open. So, for example, a channel with an U-shaped or a V-shaped wall is an open channel. If the open side of the U-profile or of the V-profile were covered with a plate, the channel would be a closed channel.
(8) A partially closed channel means a channel, which is partially designed as a closed channel and partially as an open channel.
(9) In the following description of the invention it is referred to an important example for practice with an exemplary nature, wherein the component is a closed or a covered rotor (impeller), respectively, of a turbo engine, e.g. of a pump. For a better understanding,
(10) The component 1 or the impeller 1, respectively, extends in an axial direction A as well as in a radial direction R vertical thereto. The axial direction A usually means that direction which is determined by the axis of rotation of the rotary machine when the component 1 is installed in the rotary machine. The axis of rotation is that axis around which the rotor of the rotary machine rotates in the operating state.
(11) The impeller 1 rotates around the axis of rotation in the operating state, which axis determines the axial direction A. A direction vertical to this axial direction A is described as radial direction R.
(12) The impeller 1 is a rotationally symmetric component with respect to the axial direction A and comprises a shroud 2 in a manner known per se, with which the impeller 1 usually is mounted or fixed on an axis or a shaft, not shown here, and also a number of vanes 3, which are arranged on the shroud 2, as well as a cover plate 4 covering the vanes 3 at least partially at the side or edge, respectively, facing away from the shroud 2. According to the description (
(13) As a result according to the description, an internal space 6 is formed above the vanes 3, the space being limited by the cover plate 4 with respect to the radial direction R. This internal space 6 presents the inlet in the operating state, through which the fluid flows to the impeller 1. An inner channel 7 exists in each case between two adjacent vanes 3, which channel is designed as an at least partially closed channel 7 and here as a closed channel 7.
(14) Each channel 7 extends from a first end 72 in a center of the impeller 1, which is formed by the internal space 6, to a respective second end 71 in a limiting surface 42 of the impeller 1. The limiting surface 42 presents the radially outer surface of the impeller 1, which surface extends parallel to the axial direction A, that is to say, the surface limiting the impeller 1 outwards in the radial direction R. “Parallel to the axial direction A” means, that each vector of the surface normal of the limiting surface 42 is vertical on the axial direction A. The limiting surface 42 comprises the radially outer surfaces of the cover plate 4 and of the shroud 2 as well as the radially outer closing edges of the vanes 3, which are called trailing edges 31.
(15) Thus adjacent channels 7 are each separated by a separating wall 3, each separating wall 3 forming in each case one vane 3 of the impeller 1.
(16) Depending on the design of the impeller 1 it is also possible, that the closing edges of the vanes 3 are displaced backward with respect to the radial direction, that means they are not in the limiting surface 42. Then, the cover plate 4 and/or the shroud 2 protrudes over the vanes 3 or the closing edges of the vanes 3, respectively, with respect to the radial direction R. Such a design particularly is also possible regarding a rotor of a turbine, where the outer closing edges of the vanes 3 usually are the leading edges.
(17) Hence, each of the closed channels 7 is enclosed by a limiting surface 8, in each case composing of the surfaces of two adjacent vanes 3 facing each other, as well as of the intermediate surface segments of the surfaces of the shroud 2 and of the cover plate 4 facing each other, which surface segments forming the bottom and the top of the respect channel 7. Thus, the vanes 3 each form a separating wall between two adjacent inner channels 7. The second end 71 of each channel 7 comprises the port, with which the respective channel 7 joins the limiting surface 42. Adjacent second ends 71 in a peripheral direction are separated from each other by a trailing edge 31.
(18) The impeller 1 also has a central through bore 9, which is used to receive a shaft or an axis, on which the impeller 1 is mounted.
(19) An embodiment of the method according to the invention is explained in more detail below with reference to
(20) According to the method of an embodiment of the invention a blank is first provided.
(21) The blank 10 is a particularly preferred designed in a rotationally symmetric way with respect to the axial direction A, as also illustrated in
(22) The blank 10 has the central through bore 9, which is used to receive the shaft or the axis, on which the impeller 1 can be mounted. The bore 9 is limited in the area of its upper end (illustrated in
(23) The blank 10 further comprises the center formed by the internal space 6, which center presents the inlet of the impeller 1 in the operating state, through which the fluid flows to the impeller 1. The internal space 6 is designed as a cavity in the blank 10, which cavity rotationally symmetric and coaxially extends about the annular body 21. This cavity is radially inside limited by the annular body 21. Regarding the radial direction R external, the cavity forming the internal space 6 is limited by a cylindrical area 41, as well as by a substantially cone-mantle-shaped wall 61 joining the cylindrical area 41 below (illustrated in
(24) The blank 10 is limited by an outer surface 11 in the radial direction R, which outer surface 11 is designed to be cylinder-mantle-shaped in this embodiment and which extends coaxially to the bore 9 about the axial direction A. Consequently, the dimension of the outer surface 11 in the radial direction R is the diameter D1 of the cylinder-mantle-shaped outer surface 11.
(25) Naturally, such designs are also possible, wherein the radially external outer surface 11 of the blank 10 is not a cylinder mantle surface, but has another geometrical design, for example having the shape of a cone mantle surface or of a truncated cone mantle surface. In such cases, D1 indicates the maximum dimension of the outer surface 11 in the radial direction R, thus the maximum diameter, for example, which is enclosed by the outer surface 11.
(26) The maximum dimension of the blank 10 in the axial direction A is described with the height H1. The height of the outer surface 11 of the blank 10 in the axial direction A may be smaller than or equal to this height H1.
(27) The blank 10 is designed in such a way, that the diameter D1 of its outer surface 11 is smaller than the corresponding dimension of the limiting surface 42 in the radial direction R. The dimension of the limiting surface 42 in the radial direction R is the outer diameter D2 of the impeller 1 (see
(28) The height H2 of the impeller 1 in the axial direction A (see
(29) In this embodiment, the height H1 of the blank 10 is measured such, that the height is equal to the height H2 of the finished impeller, thus it is H1=H2.
(30) Of course, it can also be advantageous to measure the height H1 of the blank 10 smaller than the height H2 of the finished impeller. For example, a suitable choice of H1 can be made on the basis of the criterion how much volume of the component 1 is to be manufactured by a build-up process and which parts of the component 1 are to be manufactured already in the first subtractive process step. Of course, this depends on the specific geometry of the component 1 to be manufactured and on economic factors.
(31) The outer surface 11 of the blank 10 is preferably designed as a coherent surface having no openings.
(32) Particularly preferred, the blank 10 is made of a forged material, which may be a metal or a metal alloy. Thus, for example, steel is suitable in its known embodiments or aluminum, titanium, nickel, a nickel or cobalt base alloy or a non-ferrous metal. Of course, other than forged materials are also possible, for example a cast material, a synthetic material or a composite or another machinable material.
(33) The blank 10 is preferably manufactured or processed in such a way, that parts of the shroud 2 as well as of the cover plate 4 are already designed in its desired final form or at least substantially in its final form. In that regard, “substantially” means that, of course, post-processings can be performed at a later stage, as for example milling, turning, grinding, polishing or something similar, but the substantial design is already completed in the blank 10. Preferably, at least the following parts of the blank 10 are designed that way, that they substantially have the final form of the completed impeller: the central axial bore 9, the annular body 21 as a part of the shroud 2, the cylindrical area 41 as a part of the cover plate 4, the internal space 6, which forms the center and which is realized by the cavity in the blank 10. Furthermore, in the embodiment described here, the height H1 of the blank 10 is already substantially identical to the height H2 of the impeller 1.
(34) Now a first subtractive process step is performed on this blank 10, which process step is explained below.
(35) A subtractive process step means, that material is cut or removed, respectively, from the workpiece—here from the blank 10—in such a process step. As it is generally usual, a machining process means a process wherein excessive material is removed from the blank 10 or the workpiece, respectively, in the form of chips in order to achieve a desired geometrical form. For example, machining processes are milling, turning, drilling, planing, filing, grinding, honing or lapping, to mention only a few examples.
(36) The first subtractive process step preferably comprises milling by a machining device, comprising, for example a computer-controlled milling tool. Particularly preferred, the machining device is designed at least as a five-axes-milling tool, with which the desired geometrical form is elaborated out of the blank 10. The milling tool is usually guided by a manipulator, the guide being computer-assisted.
(37) One part is manufactured from each channel 7 in the first subtractive process step, which part extends from the first end 72 of the respective channel into the outer surface 11 of the blank 10. The first end 72 of each channel 7 joins the wall 61, limiting the internal space 6.
(38) As it particularly is illustrated in
(39) After the ports of the channels 7 into the outer surface 11 of the blank 10 have been finished, the outer surface 11 has a coherent annular area 12 covering the port of each channel 7 into the outer surface 11. Thus, all channels 7 are closed by the annular area. That is, after finishing the first subtractive process step (see
(40) The parts of each channel 7 being manufactured in the first subtractive process step, that means in each case the channel section from the first end 72 of the channel in the wall 61 of the internal space 6 to the port of the respective channel into the outer surface 11 of the blank 10, are preferably manufactured in such a way, that they substantially have at least their final form.
(41) After finishing the first subtractive process step (see
(42) It is understood, that the first subtractive process step can comprise a milling from the wall 61 or from the internal space 6, respectively, as well as a milling from the outer surface 11. Of course, it is also possible, to mill or to process by machining, respectively, only from the internal space 6 or only from the outer surface 11 in the first subtractive process step depending on the component.
(43) It is an advantage of the purely machining process, that a blank 10 made of a forged material retains all positive properties of the forged material.
(44) It is understood, that the diameter D1 of the blank 10, which in principle is a freely selectable parameters within wide limits, preferably is chosen such in the respective application, that these parts of the channels 7 manufactured in the first subtractive process step can be elaborated out of the blank 10 by machining without any problem, for example by milling, in particular with respect to the geometry.
(45) After finishing the first subtractive process step (see
(46) A build-up process means a process, wherein a shapeless or a neutrally shaped material is applied. In doing so, the shapeless material, for example a powder, or the neutrally shaped material, for example a strap-shaped material, usually is melted in order to build up the still missing parts of the component 1 on the blank or on the already existing structure, respectively. Thus, a build-up process is a process out of a shapeless or a neutrally shaped material.
(47) The build-up manufacturing comprises one or several additive process step(s). An additive process step or an additive manufacturing, which is also referred to as generative manufacturing, respectively, means a process step, wherein material is added or applied on the workpiece, here the blank 10. The desired structures usually are generated, for example by a build-up process on a workpiece, in an additive manufacturing out of a shapeless material, for example liquids or powders, or out of a neutrally shaped material, for example strap-shaped or wire-shaped material, by chemical and/or physical processes. Additive manufacturing methods known per se for metallic workpieces are, for example build-up welding methods, in particular inert gas methods as tungsten inert gas welding (TIG) or laser build-up welding or plasma methods or selective laser melting (SLM selective laser melting) or selective laser sintering (SLS).
(48) After finishing the first subtractive process step the still missing areas of the component 1 are generated by a build-up process, in particular these are the radial exterior parts of the separating walls 3 and of the channels 7, parts of the cover plate 4 as well as parts of the shroud 2.
(49) In a preferred embodiment, the still missing parts are generated in the build-up process by laser build up welding. The method of laser build-up welding with its different variants is well known to the person skilled in the art and, thus, no further explanations are required.
(50) Hence, it is possible to perform the build-up process of the blank 10 layer by layer, in particular by using the rotationally symmetric design.
(51) Another preferred embodiment is to build up the component 1 part by part in the build-up process, i.e. the individual parts of the component 1 as e.g. the separating walls 3 or the covers of the channels 7 are successively built up in this sense, that first a part, e.g. the separating walls, is completely built up to its final state and then the next part is completely built up. This process is repeated until the component is finished.
(52) Furthermore, it is possible, that the individual parts of the component 1 are not completely built up, but only part by part, in other words first a part of the separating walls 3 is built up, then a part of the covers of the channels 7, then a part of the separating walls 3 again and so on. In doing so, a further subtractive process step can preferably be performed after a partial build up.
(53) As already mentioned, according to a preferred embodiment the build-up process can comprise several additive process steps to build up the component 1 in a successive manner. Regarding this, it is particularly preferred performing at least one further subtractive process step between the additive process steps.
(54) Deviations from the desired geometry can be compensated in such a further subtractive process step, for example by a machining process, which deviations have arised in the preceding additive process step. Thus, for example, milling or grinding works can be performed in this further subtractive process step, in order to remove such material which was applied too much in the additive process step or in order to equalize or to grind junctions between adjacent layers or the like.
(55) It is particularly preferred performing a further subtractive process step in each case between two additive process steps, i.e. the additive process steps and the further subtractive process steps are performed alternately or in turns, respectively. This ensures a particularly high quality and precision of the component 1.
(56) Nowadays modern processing machines are known, with which subtractive process steps as well as additive process steps can be performed in the same process chamber without need to re-clamp the blank 10 or the component 1, respectively, or to put them into another holder. The blank 10 is only once clamped into a holder and then, the blank can be processed selectively or alternately in a subtractive or additive manner. Such processing machines comprise several processing heads for this purpose, at least one of them being designed for a subtractive process, for example as a milling tool, and at least one of them being designed for the additive process, for example as a device for laser build up welding. After finishing an additive process step, for example, the processing machine automatically changes the processing head and then it can perform a subtractive process step and vice versa. In doing so, a particularly fast and very precise manufacturing of the component 1 is possible.
(57) Deviating from the embodiment described above, it is also possible, according to another also preferred variant, that parts of the annular body 21 and/or of the cylindrical area 41 are only manufactured in the additive process.
(58) Thus, it is possible, for example, to manufacture the upper zone according to the illustration (
(59) Alternatively or additionally, it is also possible, that a part of the annular body 21 is only manufactured in regard to the build-up process. This also makes it possible to ensure a better accessibility to the ports of the channels 7 in the first subtractive process step, which channels are elaborated out of the blank 10 in this first subtractive process step.
(60) The invention also proposes an analogously same method for repairing damaged or worn out components of a rotary machine. Regarding the method for repairing a components 1 of a rotary machine, for example the impeller 1 of a pump, it is proceeded in the analogously same manner as described above, but the blank 10 is generated out of a damaged or worn out, respectively, impeller 1. For example, this can be an impeller 1, whose trailing edges 31 of the vanes 3 or of the separating walls 3, respectively, or the radially outer areas of the channels 7 are damaged. The method according to the invention for repairing the component is particularly characterized in that damaged areas of the component 1 are identified at the limiting area 42 or at the channels 7 or at a separating wall, that further a blank 10 is manufactured by a machining or by a separating removal of the damaged areas, which blank comprising the center of the component 1, and that the removed damaged areas are replaced by a build-up process on the blank in order to manufacture the final form of the component 1.
(61) Regarding the method according to the invention for repairing a component the blank 10 is manufactured in an analogously same manner as in the method for manufacturing a component, on which blank the still missing parts or areas of the component 1 are subsequently manufactured by a build-up process.
(62) Regarding the method for repairing, here the blank 10 is generated by removing the damaged areas of the component. After manufacturing the blank 10 by removing the damaged areas, the blank corresponds in principle to the blank 10 manufactured by the method for manufacturing the component after performing the first subtractive process step (see
(63) Regarding the method for repairing, it is particularly not necessary, that the blank generated by removing the damaged areas is rotationally symmetric. For example, in the case of an impeller 1 being the component, it can be possible, that the individual closed channels 7 or the individual separating walls 3 between them are differently damaged or worn out, so that larger areas have to be removed from a first channel 7 than from another second channel 7. In this case, the blank 10 is no longer rotationally symmetric after removing all damaged areas.
(64) The removal of the damaged areas can be performed by a machining method, for example by milling. Alternatively or additionally, it is also possible to remove the damaged areas by a separating process, as for example punching, cutting, torch cutting or sawing.
(65) The illustrations regarding the method for manufacturing the component 1 including the advantageous measures and variants are also valid in a same or in an analogously same manner for the method for repairing the component 1.
(66) Regarding the method according to the invention for manufacturing a component as well as the method according to the invention for repairing a component, it is possible to use one ore several materials for the build-up process, the materials being different from the material of which the blank is consisting. Of course, it is also possible to change the material during the build-up process, thus using different materials for the build-up process, for example up to four different materials. Thus, for example, a first material can be used for a first additive process step, the material being equal or different from the material of the blank 10 and then using a second material for a further additive process step, the material being different from the first material.
(67) In this way, layers can be generated, for example wear protective coatings for protecting particularly such areas of the component where the highest loads arise in the operating state. Here such coatings can be generated directly on areas, which are manufactured in the subtractive process step, as well as on areas, which are generated in a preceding additive process step.
(68) In this way, areas of the component can be optimized specifically with respect to hardness, wear resistance, corrosion resistance and so on.
(69) Regarding the impeller of a pump it is possible, for example, the radially external areas of the separating walls (vanes) between the channels, hence the trailing edges of the vanes as well as the area of the radial limiting surface of the impeller. Then, these areas can be manufactured out of a particularly wear-resistant material in the build-up process.
(70) Of course, it is also possible to change the material during the build-up process, thus, for example, initially using a material during the build-up process, the material being the same as the material of the blank, for example, and then using a different material, for example for the radially exterior areas of the component.
(71) In this way, it is also possible to generate a layer on individual parts or areas of the component by a build-up process, for example a wear protection coating.
(72) Thus, due to this measure it is possible, for example, to realize a higher hardness of the component at wear surfaces of the component in a selective way. Hereby the service life of the component is increased. Regarding the impeller of a pump it is also in particular possible to do without a wear ring, which may be disposed on the impeller, and to replace the wear ring by a coating, generated by the build-up process.
(73) Although the invention has been explained with reference to manufacturing or repairing, respectively, an impeller 1, the invention is, of course, not limited to such components 1 or their manufacturing or their repairing, respectively, but the invention is suitable for a plurality of other components 1, in particular for such components 1 where at least one inner channel 7 is provided, which geometry does not allow to elaborate that channel by machining or subtractively out of a blank 10 with a reasonable expenditure.
(74) In particular, the component 1 can also be designed as an impeller or as a diffusor of a rotary machine, wherein the rotary machine can be in particular a pump or a turbine or a compressor or a compactor or an expander.