METHOD OF MAKING POLYESTER FABRIC TREATED WITH A CBD POWDER
20210348324 · 2021-11-11
Assignee
Inventors
Cpc classification
D06M13/152
TEXTILES; PAPER
D06M23/08
TEXTILES; PAPER
D10B2331/04
TEXTILES; PAPER
International classification
Abstract
This invention relates to a method for making polyester fabric treated with a CBD powder to provide a novel CBD finish on the polyester fabric. The polyester fabric is treated with a CBD powder to provide a novel finish. The treatment process includes a washing step, wherein the treating CBD water is added to a water channel before the finishing step. Then, the polyester fabric is passed through the water channel having the treating CBD water in the ratio of 1:1000, which is one gram of CBD powder to each 1000 grams of water. The flow rate of the treating CBD water has a ratio of 5:1000, which adds 5 grams of CBD powder to each 1000 grams of water in order to apply the correct treatment of CBD water. In addition, the polyester fabric moves at a speed of approximately 20 meters per minute through the water channel, and the bathing treatment has a normal temperature of 30-35° C. The maximum temperature of the drying machine is 220° C., but has a preferred range of 170-220° C. In addition, the polyester fabric passes through the drying machine at a speed of 20 meters per minute.
Claims
1) This invention relates to a method for making polyester fabric treated with a CBD powder: a) said polyester fabric is treated with said CBD powder to provide a CBD finish using a CBD treatment process; b) said polyester fabric is treated with said CBD powder at 160° C.; c) said treatment process includes a washing step, wherein the treating CBD water is added to a water channel before a finishing step; d) said polyester fabric is then passed through said water channel having the treating CBD water in the ratio of 1:1000, which is one gram of CBD powder to each 1000 grams of water; e) the flow rate of the treating CBD water through said water channel has a ratio of 5:1000, which adds 5 grams of CBD powder to each 1000 grams of water in order to apply the correct treatment of CBD water; f) said polyester fabric moves at a speed of approximately 20 meters per minute through said water channel; g) the bathing treatment has a normal temperature of 30-35° C.; h) the maximum temperature of the drying step is 220° C., and has a preferred range of 170-220° C.; and i) said polyester fabric passes through the drying step at a speed of 20 meters per minute, in order to complete said treatment process.
Description
DETAILED DESCRIPTION OF THE EMBODIMENTS
[0009] This invention relates to a method for making polyester fabric treated with a CBD powder. The present invention relates to making and treating a polyester fabric treated with a CBD powder to obtain a CBD finish on the polyester fabric using a novel CBD treatment process.
[0010] The treatment process includes the following steps for treating the polyester fabric. The first step includes singeing the fabric, desizing it, washing it, and bleaching it. Then the polyester fabric may have a white finish, or it is mercerized and then color dyed.
[0011] After that, the polyester fabric is then finished with CBD powder at 160° C. Then, the CBD treated polyester fabric is sanforized.
[0012] The CBD treatment process of the present invention is further described in the 3 embodiments set forth below.
First Embodiment
[0013] In this first embodiment, during the washing step, the treating CBD water is added to the water channel before the finishing step. The polyester fabric is passed through the water channel having the treating CBD water in the ratio of 1:1000, which is 1 gram of CBD powder to each 1000 grams of water. Also, the flow rate of the treating CBD water has a ratio of 5:1000, which adds 5 grams of CBD powder to each 1000 grams of water in order to apply the correct treatment of CBD water.
[0014] In addition, the polyester fabric moves at a speed of approximately 20 meters per minute through the water channel, and the bathing treatment has a normal temperature of 30-35° C.
Second Embodiment
[0015] When the polyester fabric passes through the roller, the temperature setting is 30-35° C.
Third Embodiment
[0016] The process starts with the machine temperature having a setting of 140° C. Also, the maximum temperature of the drying machine is 220° C., and has a preferred range of 170-220° C. The polyester fabric passes through the drying machine in approximately 2 minutes and the drying machine is running at a speed of 20 meters per minute.
[0017] In this manner, the CBD powder is added to the polyester fabric in the most efficient manner.
[0018] For all of the embodiments, it is noted that even though the CBD powder dissolves in the water, the treated polyester fabric can be washed only 10 times. After that, the CBD powder does not stay in the fabric.
Operation of the Invention
[0019] This invention relates to a polyester fabric having treated with CBD powder, and a method for making same. The invention includes treating a polyester fabric with a CBD powder to provide a CBD finish using a CBD treatment process. The polyester fabric is treated with a CBD powder at 160° C. The treatment process includes a washing step, wherein the treating CBD water is added to a water channel before the finishing step. Then, the polyester fabric is passed through the water channel having the treating CBD water in the ratio of 1:1000, which is one gram of CBD powder to each 1000 grams of water. The flow rate of the treating CBD water has a ratio of 5:1000, which adds 5 grams of CBD powder to each 1000 grams of water in order to apply the correct treatment of CBD water. In addition, the polyester fabric moves at a speed of approximately 20 meters per minute through the water channel, and the bathing treatment has a normal temperature of 30-35° C. The maximum temperature of the drying machine is 220° C., but has a preferred range of 170-220° C. In addition, the polyester fabric passes through the drying machine at a speed of 20 meters per minute.
ADVANTAGES OF THE PRESENT INVENTION
[0020] It is an advantage of the present invention to provide a novel method of treating polyester fabric with a CBD powder.
[0021] Another advantage of the present invention is to potentially provide a better rest.
[0022] Another advantage of the present invention is to potentially relieve anxiety.
[0023] A latitude of modification, change and substitution is intended in the foregoing disclosure, and in some instances, some features of the invention will be employed without a corresponding use of other features. Accordingly, it is appropriate that the appended claims be construed broadly and in a manner consistent with the spirit and scope of the invention herein.