Window in thin polishing pad
11161218 · 2021-11-02
Assignee
Inventors
- Yongqi Hu (Fremont, CA, US)
- Kadthala Ramaya Narendrnath (San Jose, CA, US)
- Thomas Lawrence TERRY (Hollister, CA, US)
Cpc classification
B24B37/205
PERFORMING OPERATIONS; TRANSPORTING
B24B37/22
PERFORMING OPERATIONS; TRANSPORTING
International classification
B24B37/20
PERFORMING OPERATIONS; TRANSPORTING
B24B37/24
PERFORMING OPERATIONS; TRANSPORTING
Abstract
A polishing pad includes a polishing layer stack that has a polishing surface, a bottom surface, and an aperture from the polishing surface to the bottom surface. The polishing layer stack includes a polishing layer that has the polishing surface. A fluid-impermeable layer spans the aperture and the polishing pad. A first adhesive layer of a first adhesive material is in contact with and secures the bottom surface of the polishing layer to the fluid-impermeable layer. The first adhesive layer spans the aperture and the polishing pad. The light-transmitting body is positioned in the aperture and has a lower surface in contact with, is secured to the first adhesive layer, and is spaced apart from a side-wall of the aperture by a gap. An adhesive sealant of a different second material is disposed in and laterally fills the gap.
Claims
1. A polishing pad, comprising: a polishing layer stack having a polishing surface, a bottom surface, and an aperture from the polishing surface to the bottom surface, the polishing layer stack including a polishing layer having the polishing surface; a fluid-impermeable layer spanning the aperture and spanning the polishing pad; a first adhesive layer of a first adhesive material in contact with and securing the bottom surface of the polishing layer stack to the fluid-impermeable layer, the first adhesive layer spanning the aperture and the polishing pad; a light-transmitting body positioned in the aperture, the light-transmitting body having a lower surface in contact with and secured to the first adhesive layer and spaced apart from a side-wall of the aperture by a gap; and an adhesive sealant of a different second material disposed in and laterally filling the gap; wherein an air gap separates the adhesive sealant from the first adhesive layer.
2. The polishing pad of claim 1, wherein the light-transmitting body is softer than the polishing layer.
3. The polishing pad of claim 2, wherein the polishing layer has a hardness of about 58-65 Shore D and the light-transmitting body has a hardness of about 45-60 Shore D.
4. The polishing pad of claim 1, wherein the adhesive sealant has about the same hardness as the light-transmitting body.
5. The polishing pad of claim 4, wherein the light-transmitting body and the adhesive sealant have a hardness of about 45-60 Shore D.
6. The polishing pad of claim 1, wherein the gap completely laterally surrounds the light-transmitting body.
7. The polishing pad of claim 1, comprising a second adhesive layer positioned on a side of the fluid-impermeable layer opposite the first adhesive layer and in contact with the fluid-impermeable layer.
8. The polishing pad of claim 7, comprising a second aperture through the second adhesive layer aligned with the light-transmitting body.
9. The polishing pad of claim 7, further comprising a removable liner covering the second adhesive layer.
10. The polishing pad of claim 1, wherein the first adhesive material comprises a pressure sensitive adhesive and the second material comprises a cured epoxy or polyurethane.
11. The polishing pad of claim 1, wherein the polishing layer stack comprises the polishing layer and a backing layer, and wherein the polishing layer is a napped polyurethane and the backing layer is a different material than the polishing layer.
12. The polishing pad of claim 11, wherein each of the backing layer and the fluid-impermeable layer are a polyester.
13. The polishing pad of claim 1, wherein the polishing pad has a total thickness less than about 3 mm.
Description
DESCRIPTION OF DRAWINGS
(1)
(2)
(3)
(4)
(5)
(6) Like reference symbols in the various drawings indicate like elements.
DETAILED DESCRIPTION
(7) As shown in
(8) The substrate can be, for example, a product substrate (e.g., which includes multiple memory or processor dies), a test substrate, a bare substrate, and a gating substrate. The substrate can be at various stages of integrated circuit fabrication, e.g., the substrate can be a bare wafer, or it can include one or more deposited and/or patterned layers. The term substrate can include circular disks and rectangular sheets.
(9) The polishing pad 18 can include a polishing layer stack 20. The polishing layer stack 20 has a polishing surface 24 to contact the substrate and a bottom surface 22 secured to the platen 16 by an adhesive structure 28.
(10) Referring to
(11) The polishing layer 70 can be disposed over a backing layer 72. The polishing layer 70 and the backing layer 72 can be formed of the same or different materials. The backing layer 72 can be a solid sheet or woven fabric. The backing layer 72 can have a lower porosity and lower compressibility than the polishing layer 70. The backing layer 72 can be a polyester, e.g., polyethylene terephthalate (PET).
(12) A polishing pad having such a polishing layer stack is available, for example, under the trade name H7000HN from Fujibo in Tokyo, Japan.
(13) Alternatively, the polishing layer stack 20 can have just a single layer, i.e., the polishing layer 70. Thus, the polishing layer stack can be formed of a single layer of homogenous material.
(14) The adhesive structure 28 can be a double sided adhesive tape. For example, still referring to
(15) Referring to
(16) Returning to
(17) The polishing head 12 applies pressure to the substrate 14 against the polishing pad 18 as the platen rotates about its central axis. In addition, the polishing head 12 is usually rotated about its central axis, and translated across the surface of the platen 16 via a drive shaft or translation arm 36. The pressure and relative motion between the substrate and the polishing surface, in conjunction with the polishing solution, result in polishing of the substrate.
(18) An optical aperture 42 is formed in the top surface of the platen 16. An optical monitoring system 40, including a light source 44, such as a laser, and a detector 46, such as a photodetector, can be located below the top surface of the platen 16. For example, the optical monitoring system can be located in a chamber inside the platen 16 that is in optical communication with the optical aperture 42, and can rotate with the platen. The optical aperture 42 can be filled with a transparent solid piece, such as a quartz block, or it can be an empty hole. The light source 44 can employ a wavelength anywhere from the far infrared to ultraviolet, such as red light, although a broadband spectrum, e.g., white light, can also be used, and the detector can be a spectrometer. Light can be carried from the light source 44 to the optical aperture 42, and back from the optical aperture 42 to the detector 46 by optical fibers, e.g., a bifurcated optical fiber 48.
(19) In some implementations, the optical monitoring system 40 and optical aperture 42 are formed as part of a module that fits into a corresponding recess in the platen. Alternatively, the optical monitoring system could be a stationary system located below the platen, and the optical aperture could extend through the platen.
(20) A window 50 is formed in the overlying polishing pad 18 and aligned with the optical aperture 42 in the platen. The window 50 and aperture 42 can be positioned such that they have a view of the substrate 14 held by the polishing head 12 during at least a portion of the platen's rotation, regardless of the translational position of the head 12.
(21) In some implementations, the optical aperture 42 is simply a hole in the platen, and the optical fiber 48 extends through the hole with an end of the optical fiber 48 in close proximity to or contacting the window 50.
(22) The light source 44 projects a light beam through the aperture 42 and the window 50 to impinge the surface of the overlying substrate 14 at least during a time when the window 50 is adjacent the substrate 14. Light reflected from the substrate 14 forms a resultant beam that is detected by the detector 46. The light source 44 and the detector 46 are coupled to an unillustrated computer that receives the measured light intensity from the detector and uses it to determine the polishing endpoint and/or control polishing parameters to improve polishing uniformity.
(23) One problem with placement of a normal large rectangular window (e.g., a 2.25 by 0.75 inch window) into a very thin polishing layer is delamination during polishing. In particular, the lateral frictional force from the substrate during polishing can be greater than the adhesive force of the molding of the window to the sidewall of the pad.
(24) Returning to
(25) The window 50 can have an approximately rectangular shape with its longer dimension substantially parallel to the radius of the polishing pad that passes through the center of the window. In some implementations, the window 50 has a ragged perimeter 52, e.g., the perimeter can be longer than a perimeter of a similarly shaped rectangle. This increases the surface area for contact of the window to the sidewall of the polishing pad, and can thereby improve adhesion of the window to the polishing pad. However, in some implementations, the individual segments of the perimeter 52 of the rectangular window 45 are smooth.
(26) The window 50 includes a solid light-transmitting body 60 that fits in an aperture 54 in the polishing layer stack 20. The light-transmitting body 60 is sufficiently transparent for light from the light source to pass through so that an endpoint signal can be detected with the detector. In some implementations, the light-transmitting body is substantially transparent to visible light, e.g., at least 80% transmittance for wavelengths from 400-700 Angstroms.
(27) The light-transmitting body can be softer than the polishing layer 70. For example, the light-transmitting body 60 can have a hardness of 45-60 Shore D, e.g., about 50 Shore D. The light-transmitting body 60 can be formed of a substantially pure polyurethane. For example the light-transmitting body 60 can be formed of a “water clear” polyurethane.
(28) The light-transmitting body 60 sits on and is bonded to the upper adhesive layer 82. Although the upper adhesive layer 82 is depicted as a continuous layer below the body 60, there may be small areas in which the adhesive has been delaminated. But in general, the adhesive can cover at least a majority of the area in the aperture 54.
(29) The fluid-impermeable layer 80 completely spans the aperture 54. In some implementations, the fluid-impermeable layer 80 spans the entire polishing pad 18. Since the fluid-impermeable layer 80 spans the aperture 54, the risk of leakage of polishing liquid can be reduced.
(30) The light-transmitting body 60 is slightly less thick than the polishing layer stack 20. Thus, the top surface 64 of the light-transmitting body 60 is slightly recessed relative to the polishing surface 24, e.g., by 7.5 to 9.5 mil. By having the light-transmitting body 60 recessed from the polishing surface 24, the risk of the conditioning process scratching the window surface and reducing transparency can be reduced.
(31) The light-transmitting body 60 is slightly narrower than the aperture 54 in the polishing layer stack 20, leaving a small gap on all sides between the light-transmitting body 60 and the polishing layer 20. A sealant 64 is disposed in the gap on all sides of the light-transmitting body 60. The sealant 64 laterally fills (i.e., extends from the side wall of the light-transmitting body 60 to the side wall of the aperture 54) the gap. However, the adhesive sealant 64 does not extend under the light-transmitting body 60, i.e., between the light-transmitting body 60 and the fluid-impermeable layer 80. In addition, the adhesive sealant 64 should not extend over the light-transmitting body 60, i.e., on the top surface 62. However, if some adhesive sealant 62 is on the top surface 62 near the perimeter of the light-transmitting body 60 without covering the center section where the light beam from the light source will pass, this can be acceptable.
(32) In some implementations, the adhesive sealant 64 completely vertically fills the gap between the light-transmitting body 60 and the side wall of the aperture 54.
(33) However, in some implementations, the adhesive sealant 64 need not completely vertically fill the gap. For example, as shown in
(34) Returning to
(35) In some implementations, the lower adhesive layer 84 is removed in a region 86 below the light-transmitting body 60. If the lower adhesive layer 84 is present, there can be a risk that heat from the light beam generated by the light source 44 will cause the lower adhesive layer 84 to liquidize, which can increase opacity of the window assembly.
(36) Referring to
(37) The polishing pad 18 is very thin, e.g., less than 3 mm, e.g., less than 1 mm, thick. For example, the total thickness of the polishing layer stack 20, adhesive structure 28 and liner 90 can be about 0.9 mm. The polishing layer 20 can be about 0.8 mm thick, with the adhesive 28 and the liner 90 providing the remaining 0.1 mm. The grooves 26 can be about half the depth of the polishing pad, e.g., roughly 0.5 mm.
(38) Since the light-transmitting body 60 is held within the polishing pad 18 both by the upper adhesive layer 82 (bonding the body 60 to the fluid-impermeable layer 80) and the adhesive sealant 64 (bonding the body 60 to the side wall of the polishing layer 20), the body 60 can be securely attached. Thus, even though the polishing pad is thin, the risk of delamination of the window can be reduced and/or the size of the window can be increased without increasing the risk of delamination.
(39) To manufacture the polishing pad, initially the polishing layer stack 20 is formed and the bottom surface of the polishing layer 20 is covered with the adhesive structure 28 and the liner 90, as shown by
(40) An aperture 54 is formed through the entire polishing layer stack 20, but not into the fluid-impermeable layer 80. For example, after the multi-layer adhesive structure 28 is attached to the polishing layer stack 20, a precision cut can be made into the polishing layer stack 20 in the shape of the aperture 54. Then the cut-out portion of the polishing layer stack 20 can be peeled away from the fluid-impermeable layer 80, leaving the aperture 54 and exposing at least a portion of the upper adhesive layer 82. Ideally, when the cut-out portion is peeled away, the upper adhesive layer 82 remains attached to the fluid-impermeable layer 80 and does not peel away with the cut-out portion. So the aperture 54 does not extend into the upper adhesive layer 82. However, if some small patches of the upper adhesive layer 82 peel away, this can still be acceptable.
(41) Referring to
(42) After the light-transmitting body 60 is positioned, a roller can be pressed and rolled across the top surface 62 of the body 60, from one end to the other, the press the body 60 uniformly against the upper adhesive layer 82. This can also squeeze out any air bubbles between the light-transmitting body 60 and the upper adhesive layer 82.
(43) The light-transmitting body 60 is positioned in the aperture 54 such that it is separated by a gap 68 from the side-walls of the aperture 54. Referring to
(44) As shown in
(45) The combination of the light-transmitting body 60, and a portion of the light-transmitting adhesive structure 28 below the light-transmitting body 60, thus provide the window 50 through the polishing pad.
(46) If the grooves 24 intersect the aperture 54, then when the liquid sealant 64 is dispensed into the aperture 54, a portion of the liquid sealant can flow along the grooves 24. Thus, some of the sealant 64 can extend past the edge of the aperture 54 to form projections into the grooves. When cured, these projections can further increase the bonding of the light-transmitting body 60 to the polishing pad.
(47) As noted above, a portion 86 of the lower adhesive layer 84 can be removed in the region below the light-transmitting body 60, while leaving the lower adhesive layer 84 over a remainder of the bottom surface 22 of the polishing pad 18 (see
(48) The scoring to define the cut-out portion of the polishing layer stack 20 can be performed by a first manufacturer, and the pad shipped with such scoring, and then the cut-out portion of the polishing layer stack 20 removed and the light-transmitting body 60 installed by another manufacturer or the final user. Alternatively, the first manufacturer can remove the cut-out portion of the polishing layer stack 20 and install a disposable cover in the aperture, and then the disposable cover can removed and the light-transmitting body 60 installed by another manufacturer or the final user. An advantage of such approaches is that the upper adhesive layer 82 can be protected from contamination when the pad is being shipped from one manufacturer to another. The disposable cover can be a different material, e.g., a lower cost material, than the polishing layer.
(49) While certain embodiments have been described, it will be understood that various modifications may be made. For example, although a window with a rectangular perimeter is described, the window could be other shapes, such as an oval. Accordingly, other embodiments are within the scope of the following claims.