CLT PANEL REINFORCING STRUCTURE
20220275644 ยท 2022-09-01
Inventors
Cpc classification
E04C2/521
FIXED CONSTRUCTIONS
International classification
Abstract
To provide a means for efficiently reinforcing strength around a through hole of a CLT panel. A CLT panel reinforcing structure includes a CLT panel having a through hole; hole; a first reinforcing member having a first plate and a first pipe, the first plate having a first opening; and a second reinforcing member having a second plate and a second pipe, the second plate having a second opening. In the first reinforcing member, the first pipe is inserted into the through hole in a state where an outer peripheral surface of the first pipe abuts on an inner peripheral surface of the through hole, and a largest surface of the first plate abuts on a first surface of the CLT panel. In the second reinforcing member, the second pipe is inserted into the through hole in a state where an outer peripheral surface of the second pipe abuts on an inner peripheral surface of the first pipe, and a largest surface of the second plate abuts on a second surface located opposite to the first surface of the CLT panel.
Claims
1. A CLT panel reinforcing structure comprising: a CLT panel having a through hole; a first reinforcing member having a first plate and a first pipe, the first plate having a first opening; and a second reinforcing member having a second plate and a second pipe, the second plate having a second opening, wherein the first pipe extends from a first region including the first opening of the first plate in a direction crossing a largest surface of the first plate, the second pipe extends from a second region including the second opening of the second plate in a direction crossing a largest surface of the second plate, in the first reinforcing member, the first pipe is inserted into the through hole in a state where an outer peripheral surface of the first pipe abuts on an inner peripheral surface of the through hole, and the largest surface of the first plate abuts on a first surface of the CLT panel, and in the second reinforcing member, the second pipe is inserted into the through hole in a state where an outer peripheral surface of the second pipe abuts on an inner peripheral surface of the first pipe, and the largest surface of the second plate abuts on a second surface located opposite to the first surface of the CLT panel.
2. The CLT panel reinforcing structure according to claim 1, wherein the first pipe extends to the second plate, and the second pipe extends to the first plate.
3. The CLT panel reinforcing structure according to claim claim 1, wherein the first region is a peripheral edge of the first opening, and the second region is a peripheral edge of the second opening.
4. The CLT panel reinforcing structure according to claim 1, wherein the first plate and the second plate are adhered to the CLT panel by an adhesive.
5. The CLT panel reinforcing structure according to claim 1, wherein the first plate, the first pipe, the second plate, and the second pipe are each formed of metal.
6. The CLT panel reinforcing structure according to claim 1, wherein the CLT panel forms a wall of a building.
Description
BRIEF DESCRIPTION OF DRAWINGS
[0018]
[0019]
[0020]
[0021]
[0022]
[0023]
DESCRIPTION OF EMBODIMENTS
[0024] Hereinafter, an embodiment of the present invention is described. It is a matter of course that the embodiment described below is merely an example of the present invention and the embodiment of the present invention can be altered as appropriate insofar as the gist of the present invention is not altered. In the following description, a vertical direction 7 is defined with a state where a CLT panel reinforcing structure 10 is installed for use (state of
[0025] The CLT panel reinforcing structure 10 of this embodiment is illustrated in
[0026] The CLT panel reinforcing structure 10 includes the CLT panel 20, a first reinforcing member 30, a second reinforcing member 40, and screws 50.
[0027] [CLT Panel 20]
[0028] The CLT panel 20 forms a wall of a building, such as a house or a condominium. The CLT panel 20 is a flat board obtained by laminating and adhering wooden boards, such as sawn boards, such that fiber directions are orthogonal to each other in each layer. The size of the CLT panel 20 is not particularly limited, and for example, the CLT panel 20 has a flat plate shape with a vertical length of 3000 mm, a horizontal length of 2000 mm, and a thickness of 90 mm. As illustrated in
[0029] As illustrated in
[0030] [First Reinforcing Member 30]
[0031] As illustrated in
[0032] The first plate 31 is a rectangular metal flat plate and has the first opening 31A formed substantially in the center. The first plate 31 has largest surfaces 31B, 31C which are in a front-and-rear relationship. The largest surface 31B abuts on the first surface 22 of the CLT panel 20. The largest surface 31C faces in the same direction as that of the first surface 22 of the CLT panel 20. The largest surface 31B and the first surface 22 are adhered to each other by an adhesive. The size of the first plate 31 is not particularly limited, and for example, when the diameter of the through hole 21 is about 110 mm, the vertical length and the horizontal length are each about 300 mm and the thickness is about 3 mm. For example, the diameter of the first opening 31A is about 110 mm, which is substantially the same as the diameter of the through hole 21.
[0033] The first pipe 32 extends from a part of a peripheral edge 34 of the first opening 31A of the first plate 31 in a direction orthogonal to the largest surface 31B of the first plate 31 (example of a crossing direction). As illustrated in
[0034] The first pipe 32 is a metal circular pipe. The first pipe 32 is joined to the first plate 31 by welding an outer peripheral surface 32A to the first opening 31A. In the connection place 33, a weld metal is charged or laminated between the outer peripheral surface 32A and the largest surface 31B. The outer diameter of the first pipe 32 is substantially the same as the diameter of the through hole 21. The dimension where the first pipe 32 projects from the largest surface 31B of the first plate 31 is equal to the thickness of the CLT panel 20 and is 90 mm in this embodiment. When the weld metal is present in a connection place 43 in the outer periphery of a second pipe 42 of a second plate 41 as in this embodiment, the first pipe 32 only needs to extend to the connection place 43 and may not necessarily project in a length equal to the thickness of the CLT panel 20.
[0035] [Second Reinforcing Member 40]
[0036] As illustrated in
[0037] The second plate 41 is a rectangular metal flat plate and has the second opening 41A formed substantially in the center. The second plate 41 has largest surfaces 41B, 41C which are in a front-and-rear relationship. The largest surface 41B abuts on the second surface 23 of the CLT panel 20. The largest surface 41C faces in the same direction as that of the second surface 23 of the CLT panel 20. The largest surface 41B and the second surface 23 are adhered to each other by an adhesive. The size of the second plate 41 is not particularly limited and is the same as the size of the first plate 31, for example.
[0038] The second pipe 42 extends from a part of a peripheral edge 44 of the second opening 41A of the second plate 41 in a direction orthogonal to the largest surface 41B of the second plate 41 (example of a crossing direction). As illustrated in
[0039] The second pipe 42 is a metal circular pipe. The second pipe 42 is joined to the second plate 41 by welding an outer peripheral surface 42A to the second opening 41A. In the connection place 43, a weld metal is charged or laminated between the outer peripheral surface 32A and the largest surface 41B. The second pipe 42 extends to the first plate 31. The outer diameter of the second pipe 42 is substantially the same as the inner diameter of the first pipe 32. The outer peripheral surface 42A of the second pipe 42 inserted into the through hole 21 abuts on an inner peripheral surface 32B of the first pipe 32.
[0040] [Screws 50]
[0041] As illustrated in
[0042] [CLT Panel Reinforcing Structure 10]
[0043] As illustrated in
[0044] As illustrated in
Operational Effects of Embodiment
[0045] As illustrated in
[0046] As illustrated in
[0047] The first pipe 32 and the second pipe 42 overlap with each other in the entire region in the width direction 12 of the through hole 21 of the CLT panel 20, and therefore the bearing strength in the vicinity of the through hole 21 of the CLT panel 20 is more efficiently reinforced.
[0048] The diameter of the first opening 31A and the diameter of the through hole 21 are designed to be substantially the same and the diameter of the second opening 41A and the inner diameter of the first pipe 32 are designed to be substantially the same. Therefore, the first plate 31 does not project from an opening end of the first pipe 32 into the opening, and the second plate 41 does not project from an opening end of the second pipe 42 into the opening.
[0049] The first plate 31 and the second plate 41 are fixed to the CLT panel 20 by the adhesive. Reinforcement in the vicinity of the through hole 21 of the CLT panel 20 by the first reinforcing member 30 and the second reinforcing member 40 is not realized by fixing the first plate 31 and the second plate 41 to the CLT panel 20 by the screws 50, but is realized by increasing bearing strength caused by increasing the cross-sectional areas of the first reinforcing member 30 and the second reinforcing member 40 in the connection places 33, 43 and the place 51, as described above. Hence, the number of the screws 50 used for fixing the first plate 31 and the second plate 41 to the CLT panel 20 can be reduced as small as possible, which prevents cutting wooden fibers of the CLT panel 20 by the screws 50.
MODIFICATION EXAMPLES
[0050] In the above-described embodiment, the first pipe 32 extends to the second plate 41 and a tip 32C is located in the vicinity of the second opening 41A as illustrated in
[0051] In the connection place 43, a weld metal may be laminated on the largest surface 41C and the tip 32C may abut on the largest surface 41B. Thus, the first pipe 32 and the second pipe 42 overlap with each other without any gap in the entire region in the width direction 12 of the through hole 21 of the CLT panel 20, and therefore the bearing strength in the vicinity of the through hole 21 of the CLT panel 20 is more efficiently reinforced. In the first pipe 32, the tip 32C abutting on the second plate 41 may be adhered to the largest surface 41B of the second plate 41 by an adhesive.
[0052] The diameter of the first opening 31A may not necessarily be substantially the same as the diameter of the through hole 21. For example, as illustrated in
[0053] The first pipe 32 extends from a part of a peripheral edge 134 of the first opening 131A of the first plate 131. When the diameter of the first opening 131A is 50% of the inner diameter of the first pipe 32, the peripheral edge 134 refers to a region of a largest surface 131B from a boundary with the first opening 131A to a boundary represented by a circle having the same center as the center of the first opening 131A and having a diameter about twice the diameter of the first opening 131A, for example. At this time, the first plate 131 is joined to the first pipe 32 by welding the largest surface 131B to an end surface of the first pipe 32. Even such a configuration prevents the first plate 131 from projecting from the opening end of the first pipe 32 into the opening. The peripheral edge 134 and the first opening 131A are examples of the first region.
[0054] The diameter of the second opening 41A may not necessarily be substantially the same as the inner diameter of the first pipe 32. For example, as illustrated in
[0055] The second pipe 42 extends from a part of a peripheral edge 144 of the second opening 141A of the second plate 141. When the diameter of the second opening 141A is 50% of the inner diameter of the second pipe 42, the peripheral edge 144 refers to a region of a largest surface 141B from a boundary with the second opening 141A to a boundary represented by a circle having the same center as the center of the second opening 141A and having a diameter about twice the diameter of the second opening 141A, for example. At this time, the second plate 141 is joined to the second pipe 42 by welding the largest surface 141B to an end surface of the second pipe 42. Even such a configuration prevents the second plate 141 from projecting from the opening end of the second pipe 42 into the opening. The peripheral edge 144 and the second opening 141A are examples of the second region.
[0056] The screws 50 may be unnecessary for fixing the first plate 31 and the second plate 41 to the CLT panel 20. Thus, the wooden fibers of the CLT panel 20 are not cut by the screws 50.
[0057] In the above-described embodiment, one through hole 21 is provided, and therefore one pipe is provided for each of the plates 31, 41. When the CLT panel 20 has a plurality of through holes 21, each plate may be provided with a plurality of pipes.
[0058] In the connection place 33, a weld metal may be laminated on the largest surface 31C. At this time, in the through hole 21, the opening end on the first surface 22 side may not necessarily be chamfered.
[0059] The position where the first plate 31 is welded to the outer peripheral surface 32A may not necessarily be an end along the width direction 12 of the first pipe 32.
[0060] The position where the second plate 41 is welded to the outer peripheral surface 42A may not necessarily be an end along the width direction 12 of the second pipe 42.
[0061] The second pipe 42 extends from the peripheral edge of the second opening 41A of the second plate 41 and extends to the first plate 31 along the width direction 12, but may extend beyond the first plate 31. In the second pipe 42, a place located in the first opening 31A may be joined to the first reinforcing member by welding. In the second pipe 42, the outer peripheral surface 42A may be adhered to the inner peripheral surface 32B of the first pipe 32 by an adhesive.
[0062] The first pipe 32 may extend from a region outside the peripheral edge 34 surrounding the first opening 31A. The second pipe 42 may extend from a region outside the peripheral edge 44 surrounding the second opening 41A.
DESCRIPTION OF REFERENCE NUMERALS
[0063] 10 CLT panel reinforcing structure
[0064] 20 CLT panel
[0065] 21 through hole
[0066] 21A inner peripheral surface
[0067] 22 first surface
[0068] 23 second surface
[0069] 30 first reinforcing member
[0070] 31 first plate
[0071] 31A first opening
[0072] 31B largest surface
[0073] 32 first pipe
[0074] 32A outer peripheral surface
[0075] 32B inner peripheral surface
[0076] 34 peripheral edge (example of first region)
[0077] 40 second reinforcing member
[0078] 41 second plate
[0079] 41A second opening
[0080] 41B largest surface
[0081] 42 second pipe
[0082] 42A outer peripheral surface
[0083] 44 peripheral edge (example of second region)
[0084] 100 CLT panel reinforcing structure
[0085] 131 first plate
[0086] 131A first opening
[0087] 131B largest surface
[0088] 134 peripheral edge (example of first region)
[0089] 141 second plate
[0090] 141A second opening
[0091] 141B largest surface
[0092] 144 peripheral edge (example of second region)