Metal diaphragm damper and manufacturing method for the same
11181220 ยท 2021-11-23
Assignee
Inventors
Cpc classification
F16J3/02
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
F02M59/44
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
F16J3/04
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
F16L55/053
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
F02M2200/315
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
F02M2200/8084
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
F02M55/04
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
International classification
F16L55/053
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
F16J15/52
MECHANICAL ENGINEERING; LIGHTING; HEATING; WEAPONS; BLASTING
Abstract
A metal diaphragm damper includes disc-shaped damper main body having two diaphragms between which a gas is sealed and each of which is provided with a deformable portion at the center thereof and two regulation members that are disposed outside of the deformable portions of the two diaphragms. The metal diaphragm damper includes a first welding part provided with a first welding layer WD1 that seals an annular periphery portion of the regulation member and an outer edge portion of the diaphragm, and a second welding layer WD1 that seals an annular periphery portion of the other regulation member and an outer edge portion of the other diaphragm. The metal diaphragm damper further includes a second welding part provided with a welding layer WD2 that seals the annular periphery portions of the two regulation members.
Claims
1. A metal diaphragm damper comprising: a damper main body formed in a disc shape and including a first diaphragm and a second diaphragm between which a gas is sealed and each of which is provided with a deformable portion at a center thereof; a first regulation member disposed outside the deformable portion of the first diaphragm; a second regulation member disposed outside the deformable portion of the second diaphragm; a first welding part provided with a first welding layer that is formed by welding to seal an annular periphery portion of the first regulation member and an outer edge portion of the first diaphragm, and a second welding layer that is formed by welding to seal an annular periphery portion of the second regulation member and an outer edge portion of the second diaphragm; and a second welding part provided with a welding layer that is formed by welding to seal the annular periphery portions of the first and second regulation members, wherein each of the annular periphery portions of the first and second regulation members has a recess formed in each of inner surfaces of the annular periphery portions facing to each other on radially inner sides of the annular periphery portions, respectively, the outer edge portions of the first and second diaphragms are disposed in the recesses of the first and second regulation members, respectively, and depths of the recesses of the first and second regulation members in an axial direction are substantially equal to thicknesses of the outer edge portions of the first and second diaphragms, respectively.
2. The metal diaphragm damper according to claim 1, wherein an outer diameter of the annular periphery portion of the first regulation member is formed larger than an outer diameter of the first diaphragm, an outer diameter of the annular periphery portion of the second the regulation member is formed larger than an outer diameter of the second diaphragm, and the second welding part is located radially outward with respect to the outer edge portions of the first and second diaphragms.
3. The metal diaphragm damper according to claim 2, wherein the first diaphragm includes a curved portion formed between the deformable portion and the outer edge portion of the first diaphragm and protruding from the annular periphery portion of the first regulation member in a direction opposite to a protruding direction of the deformable portion of the first diaphragm in a natural state of the first diaphragm, and the second diaphragm includes a curved portion formed between the deformable portion and the outer edge portion of the second diaphragm and protruding from the annular periphery portion of the second regulation member in a direction opposite to a protruding direction of the deformable portion of the second diaphragm in a natural state of the second diaphragm.
4. The metal diaphragm damper according to claim 1, wherein the first diaphragm includes a curved portion formed between the deformable portion and the outer edge portion of the first diaphragm and protruding from the annular periphery portion of the first regulation member in a direction opposite to a protruding direction of the deformable portion of the first diaphragm in a natural state of the first diaphragm, and the second diaphragm includes a curved portion formed between the deformable portion and the outer edge portion of the second diaphragm and protruding from the annular periphery portion of the second regulation member in a direction opposite to a protruding direction of the deformable portion of the second diaphragm in a natural state of the second diaphragm.
5. A metal diaphragm damper comprising: a damper main body formed in a disc shape and including a first diaphragm and a second diaphragm between which a gas is sealed and each of which is provided with a deformable portion at a center thereof; a first regulation member disposed outside the deformable portion of the first diaphragm; a second regulation member disposed outside the deformable portion of the second diaphragm; a first welding part provided with a first welding layer that is formed by welding to seal an annular periphery portion of the first regulation member and an outer edge portion of the first diaphragm, and a second welding layer that is formed by welding to seal an annular periphery portion of the second regulation member and an outer edge portion of the second diaphragm; and a second welding part provided with a welding layer that is formed by welding to seal the annular periphery portions of the first and second regulation members, wherein the first diaphragm includes a curved portion formed between the deformable portion and the outer edge portion of the first diaphragm and protruding from the annular periphery portion of the first regulation member in a direction opposite to a protruding direction of the deformable portion of the first diaphragm in a natural state of the first diaphragm, and the second diaphragm includes a curved portion formed between the deformable portion and the outer edge portion of the second diaphragm and protruding from the annular periphery portion of the second regulation member in a direction opposite to a protruding direction of the deformable portion of the second diaphragm in a natural state of the second diaphragm.
6. A method of manufacturing a metal diaphragm damper comprising a damper main body with a disk shape including a first diaphragm and a second diaphragm between which a gas is sealed and each of which is provided with a deformable portion at a center thereof; a first regulation member disposed outside the deformable portion of the first diaphragm; and a second regulation member disposed outside the deformable portion of the second diaphragm, the method comprising: a first welding step of fixing an annular periphery portion of the first regulation member to an outer edge portion of the first diaphragm by welding; a second welding step of fixing an annular part of the second regulation member to an outer edge portion of the second diaphragm by welding; and a third welding step of fixing the annular parts of the first and second regulation members by welding after the first and second steps, wherein the first welding step and the second welding step are performed in an atmosphere made of air, and the third welding step is performed in an atmosphere made of the gas to be sealed between the first and second diaphragms.
Description
BRIEF DESCRIPTION OF DRAWINGS
(1)
(2)
(3)
(4)
(5)
(6)
(7)
(8)
(9)
(10)
(11)
(12)
(13)
(14)
(15)
DESCRIPTION OF EMBODIMENTS
(16) In the following, modes that carry out a metal diaphragm damper and a manufacturing method for the same according to the present invention will be described based on embodiments.
First Embodiment
(17) Referring to
(18) As shown in
(19) As a mechanism of the pressurization and discharge of the fuel in the high-pressure fuel pump 10, first, a suction process is performed in which when the plunger 12 descends, a suction valve 13 is opened and fuel is sucked from a fuel chamber 11 that is formed on the fuel inlet side to a pressurizing chamber 14. Subsequently, a volume adjustment process is performed in which when the plunger 12 ascends, a part of the fuel in the pressurizing chamber 14 is returned to the fuel chamber 11, and after the suction valve 13 is closed, a pressurizing process is performed in which when the plunger 12 further ascends, the fuel is pressurized.
(20) As described above, the high-pressure fuel pump 10 repeats a cycle of the suction process, the volume adjustment process, and the pressurizing process, and the high-pressure fuel pump 10 pressurizes fuel, opens a discharge valve 15, and discharges the fuel to the injector side. At this time, pulsation that repeats a high pressure and a low pressure is produced in the fuel chamber 11. The metal diaphragm damper 1 is used for reducing pulsation produced in the fuel chamber 11 of the high-pressure fuel pump 10 described above.
(21) As shown in
(22) The diaphragms 4 and 5 are formed in a dish shape with a uniform thickness overall in almost the same shape by press working of a metallic plate of the same metal. On the center sides in the radial direction, i.e., at the centers of the diaphragms 4 and 5, deformable portions 19 are formed, respectively. On the radially outward side of the deformable portions 19, outer edge portions 20 with a flat annular shape are formed extending from the deformable portions 19 in an outer radial direction, respectively.
(23) Next, the diaphragm 4 and the diaphragm 5 will be described. Note that since the diaphragm 4 and the diaphragm 5 are in the same shape, here, the one diaphragm 4 will be described, and the description of the other diaphragm 5 is omitted.
(24) The deformable portion 19 of the diaphragm 4 is mainly composed of a third curved portion 24 that is continuously connected to the radially inner side part of the outer edge portion 20, a first curved portion 22 on the center side (i.e., on the radially inner side), and a second curved portion 23 that is located between the third curved portion 24 and the first curved portion 22.
(25) The first curved portion 22, the second curved portion 23, and the third curved portion 24 are each formed at a certain curvature. The first curved portion 22 is formed protruding to the outside of the diaphragm 4 (i.e., to the side of the regulation member 6 in
(26) Next, the regulation member 6 and the regulation member 7 will be described. Note that since the regulation member 6 and the regulation member 7 are in the same shape, here, one regulation member 6 will be described, and the description of the other regulation member 7 is omitted.
(27) As shown in
(28) The annular periphery portion 25 of the regulation member 6 has a flat annular shape opposite in parallel with an annular periphery portion 25 of the regulation member 7. The annular periphery portion 25 has an inner surface 25a facing to the annular part 25 of the regulation member 7 and is provided with a recess 29 formed in the inner surface 25a so as to continuously run in the circumferential direction. The recess 29 is formed such that the recess 29 is recessed in the thickness direction of the annular periphery portion 25 and opened at the radially inner side of the annular periphery portion 25.
(29) On the bottom portion 28 of a cover member 3 constituted by the regulation members 6 and 7, a plurality of holes 30 is formed, and the outer side of the cover member 3 communicates with the inner side through these holes 30.
(30) As shown in
(31) Next, the manufacturing process of the metal diaphragm damper 1 will be described. As shown in
(32) In the present embodiment, laser welding is used for the first welding step. In detail, a laser beam is applied from the inside of the outer edge portion 20 to an inner surface 20b of the outer edge portion 20 of the diaphragm 4, the boundary part of the bottom surface 29a in the recess 29 of the regulation member 6 and the bottom surface 20a at the outer edge portion 20 of the diaphragm 4 is melted so that a welding layer (i.e., first half the first welding part) WD1 is formed to penetrate the outer edge portion 20 of the diaphragm 4 and sink into the annular periphery portion 25 of the regulation member 6 (see
(33) As shown in
(34) Similarly, in the atmosphere made of air, in the state in which the bottom surface 29a of the recess 29 of the annular periphery portion 25 of the other regulation member 7 and the outer surface 20a of the outer edge portion 20 of the other diaphragm 5 are brought inti surface contact with each other, these components are fixed by welding throughout the circumference, and another welding layer WD1 is formed at the boundary portions between the annular periphery portion 25 of the regulation member 7 and the outer edge portion 20 of the diaphragm 5 (referred to as a second welding step).
(35) Next, in the atmosphere made of a gas at a predetermined pressure that is sealed between the diaphragms 4 and 5, the regulation member 6 and the regulation member 7 that have been fixed to the diaphragms 4 and 5 are laid on each other in symmetry, specifically in a state in which the opposite surface 25a of the annular part 25 of the regulation member 6 and the opposite surface 25a of the annular part 25 of the regulation member 7 are in surface contact, the components are fixed and welded throughout the circumference (referred to as a third welding step), and a welding layer (i.e., a second welding part) WD2 is formed at the outermost circumferential boundary portions between the inner surface 25a of the regulation member 6 and the inner surface 25a of the regulation member 7 (see
(36) By welding the annular periphery portion 25 of the regulation member 6 to the annular periphery portion 25 of the regulation member 7, the assembly of the cover member 3 is completed as well as the assembly of the damper main body 2 is completed.
(37) The outer edge portion 20 of the diaphragm 4 and the annular periphery portion 25 of the one regulation member 6 are fixed to each other throughout the circumference with the first welding layer WD1 and hermetically sealed in the first welding step, similarly, the outer edge portion 20 of the other diaphragm 5 and the annular periphery portion 25 of the other regulation member 7 are fixed to each other throughout the circumference with the second welding layer WD1 and hermetically sealed in the second welding step, the annular periphery portion 25 of the regulation member 6 and the annular periphery portion 25 of the regulation member 7 are fixed to each other in the third welding step. As a result, the fixing of the diaphragm 4 to the diaphragm 5 are completed throughout the circumference with the welding layer WD2 and hermetically sealed, and thus the hermeticity of the damper main body 2 is secured.
(38) In the enclosed space inside the damper main body 2, a gas made up of, e.g., argon or helium at a predetermined pressure is sealed. Note that the damper main body 2 adjusts the amount of volumetric change by the internal pressure of the gas sealed in the inside and thus a desired pulsation absorption performance can be obtained.
(39) In the cover member 3, since the plurality of holes 30 is formed on the bottom part 28 of the regulation member 6 and the bottom part 28 of the regulation member 7, the outer side of the cover member 3, i.e., the internal space of the fuel chamber 11 are communicated with the inner side of the cover member 3, i.e., the space around the damper main body 2 through the plurality of holes 30. Thus, the fuel pressure associated with pulsation that is introduced into the fuel chamber 11 and repeats a high pressure and a low pressure directly acts on the damper main body 2.
(40) Next, the pulsation absorption of the metal diaphragm damper 1 when receiving the fuel pressure associated with pulsation that repeats a high pressure and a low pressure will be described with reference to
(41) As shown in
(42) In detail, the first curved portion 22 is deformed in the direction to the inside of the diaphragm 4 due to the fuel pressure that is an external pressure and deformed so as to expand in the outer radial direction, and stress is applied to the parts on the outer diameter side from the first curved portion 22 of the diaphragm 4 in the outer radial direction.
(43) The stress in the outer radial direction applied to the outer diameter side of the diaphragm 4 is transmitted along the surface of the diaphragm 4. Since the second curved portion 23 is a curved surface recessed in the inward direction, on the radially inner side from a bottom point T2 of the second curved portion 23 in the axial direction, the stress follows the shape of the second curved portion 23, and also acts in the direction to the inside of the diaphragm 4. Thus, as shown in
(44) As described above, the second curved portion 23 is deformed such that its bottom point T2 moves in the direction to the inside of the diaphragm 4 and in the outer radial direction, and on the third curved portion 24 that runs to the second curved portion 23, force that pulls the third curved portion 24 in the direction to the inside of the diaphragm 4 also acts on the third curved portion 24 on the radially inner side from its top point T3, in addition to the stress in the outer radial direction. Thus, the third curved portion 24 is deformed such that the curvature radius is smaller than at a low pressure, and the third curved portion 24 is deformed so as to protrude on the outer diameter side.
(45) Accordingly, the stress in the outer radial direction that acts on the first curved portion 22 is converted into the force that reduces the curvature radius of the third curved portion 24, a part of the stress in the outer radial direction is absorbed by the deformation of the third curved portion 24, and thus the stress applied to the diaphragm 4 is dispersed, and thus the diaphragm 4 is prevented from being fractured. The third curved portion 24 of the diaphragm 4 is apart from the side wall portion 27 of the regulation member 6, and the side wall portion 27 of the regulation member 6 does not hamper the deformation of the third curved portion 24 in the outer radial direction due to a fuel pressure.
(46) As described above, since the diaphragm 4 is configured in which a part of the stress in the outer radial direction can be absorbed by the deformation of the third curved portion 24, the annular part 25 of the regulation member 6 is located the outer side of the outer edge portion 20 of the diaphragm 4, and the stress applied to the diaphragm 4 can be dispersed in the outer radial direction while the deformation of the outer edge portion 20 in the outer radial direction is regulated.
(47) As described above, for securing the hermeticity of the damper main body 2, in the metal diaphragm damper 1 according to the present embodiment, since the annular periphery portions 25 of the regulation member 6 and the regulation member 7 which have been fixed to the outer edge portions 20 of the diaphragms 4 and 5, respectively, have only to be welded to each other, the region in which the welding layer WD2 formed by welding is formed is relatively small, and welding work is easy. In addition to this, since variation hardly occurs in the depth of penetration in welding, hermeticity can be reliably secured.
(48) Since the outer diameter of the annular periphery portions 25 of the regulation members 6 and 7 is formed larger than the outer diameter W2 of the diaphragms 4 and 5, in sealing the damper main body 2, the two annular periphery portions 25 of the regulation members 6 and 7 have only to be welded to each other. Since the outer edge portions 20 of the two diaphragms 4 and 5 do not interfere, the annular periphery portions 25 of the regulation members 6 and 7 can be highly accurately welded to each other, and the region in which welding is performed can be reduced.
(49) As shown in
(50) Since the outer diameter W1 of the recess 29 defined by the inner side surface 29b, on the radially outward side, of the recess 29 of the annular periphery portion 25 of the regulation member 6 has a diameter almost the same as the outer diameter W2 of the outer edge portion 20 of the diaphragm 4 (i.e., W1=W2), force that is to deform the diaphragm 4 such that the diaphragm 4 expands in the outer radial direction due to a fuel pressure can be received on the inner side surface 29b, on the radially outward side, of the recess 29 of the annular part 25 of the regulation member 6. Accordingly, the concentration of stress on the welding layer WD1 that is a welding place of the regulation member 6 to the diaphragm 4 can be prevented, and the welding strength of the first welding layer WD1 can be maintained.
(51) Additionally, as shown in
(52) In order to inject the gas into the inside of the damper main body 2, the third welding step in which the annular periphery portion 25 of the regulation member 6 is welded to the annular periphery portion 25 of the regulation member 7 is performed in the atmosphere made of the gas. In detail, in a small room (or chamber) for welding work filled with a gas a predetermined pressure, the third welding step is performed. At this time, a conventional metal diaphragm damper 1 has a problem that since four plate bodies, which are the outer edge portions of two diaphragms, the annular periphery portion of an upper support member, and the annular periphery portion of a lower support member, are simultaneously fixed and welded, the amount of molten metal necessary for welding is increased, and welding fumes produced in welding are increased. An increase in the welding fumes has a problem that in the case in which laser welding is used, welding fumes hamper a beam and welding accuracy is degraded, and in addition to this, there is a risk that arises problems, such as degradation in productivity due to the necessity of frequent cleaning of the inside of a room for welding work.
(53) In comparison with such a conventional metal diaphragm damper, the metal diaphragm damper 1 according to the present embodiment can provide advantages that the occurrence of welding fumes can be suppressed, that the impediment to a beam can be suppressed in laser welding, and that the number of cleaning of the inside of a small room for welding work can be reduced. The advantages result from the fact that in the atmosphere of a gas that is sealed in the damper main body 2, two parts, which are the annular periphery portion 25 of the regulation member 6 and the annular periphery portion 25 of the regulation member 7, have only to be fixed by welding (i.e., the third welding step), Additionally, since the fixing of the regulation member 6 to the diaphragm 4 by welding (i.e., the first welding step) and the fixing of the regulation member 7 to the diaphragm 5 by welding (i.e., the second welding step) are completed in the atmosphere made of air in advance, the advantages described above are more noticeable.
(54) Since the annular periphery portion 25 of the regulation member 6 and the annular periphery portion 25 of the regulation member 7 have distal ends on the outer diameter side formed in a thin thickness, the region in which welding is performed is small, and the welding layer WD2 of excellent accuracy can be easily formed. Moreover, since the outer edge portion of the cover member 3 formed by the annular periphery portion 25 of the regulation member 6 and the annular periphery portion 25 of the regulation member 7 has a tapered shape so as to become thinner toward the tip thereof, the boundary part of the annular periphery portion 25 of the regulation member 6 and the annular periphery portion 25 of the regulation member 7, i.e., portions at which the welding layer WD2 is formed is easily distinguished, and working efficiency in the third welding step is excellent.
Second Embodiment
(55) Next, a metal diaphragm damper according to a second embodiment of the present invention will be described with reference to
(56) As shown in
(57) Thus, in the state in which the annular periphery portion 44 of the regulation member 42A is fixed by welding to an annular periphery portion 44 of the regulation member 42B, an inner surface 48a of the outer edge portion 48 of the diaphragm 46A and an inner surface 48a of an outer edge portion 48 of a diaphragm 46B are bought into surface contact with each other throughout the circumference. According to this, since the inner surfaces 48a of the outer edge portions 48 of the two diaphragms 46A and 46B contacts each other and regulate each other's motions in the opposite directions, the durability of first and second welding layers WD1 (see
(58) Note that since welding deformation in the opposite surfaces 48a of the outer edge portions 48 of the diaphragms 46A and 46B can be suppressed using laser welding for the first welding step, the opposite surface 48a of the outer edge portion 48 of the diaphragm 46A and the opposite surface 48a of the outer edge portion 48 of the diaphragm 46B can be in surface contact throughout the circumference only through surface treatment, such as simple polishing.
Third Embodiment
(59) Next, a metal diaphragm damper according to a third embodiment of the present invention will be described with reference to
(60) As shown in
(61) A recess 55 formed on the annular periphery portion 54 of the regulation member 52A has a depth H5 in the axial direction smaller than a distance H6 from the outer edge portion 58 of the diaphragm 56A to the bottom point, i.e., lowermost point, of the curved portion 57 in the axial direction (i.e., H5<H6). Thus, as shown in
(62) According to this, the curved portions 57 of the diaphragms 56A and 56B are pressed against each other, and the reaction force of the pressing force brings a state in which on the outer edge portion 58 of the diaphragms 56A and an outer edge portion 58 of the diaphragm 56B, stress to a bottom surface 55a of the recess 55 of the annular periphery portion 54 of the regulation member 52A and stress to the bottom surface 55a side of a recess 55 of the annular periphery portion 54 of the regulation member 52B act. The durability of first and second welding layers WD1 (see
Fourth Embodiment
(63) Next, a metal diaphragm damper according to a fourth embodiment of the present invention will be described with reference to
(64) As shown in
(65) According to the aforesaid configuration, as shown in
(66) As described above, the embodiments according to the present invention are described with reference to the drawings. The specific configurations are not limited to these embodiments, and even though modifications and additions are made within the scope of the present invention, these modifications and additions are included in the present invention.
(67) For example, in the embodiments, the first and second welding layers WD1 are formed by laser welding such that parts of the outer edge portions 20 of the diaphragms 4 and 5 and parts of the annular periphery portions 25 of the regulation members 6 and 7 are melted and mixed, respectively. Similarly, the welding layer WD2 is formed by laser welding such that parts of the annular periphery portions 25 of the regulation members 6 and 7 are melted and mixed. However, not limited to these, the first and second welding layers WD1 and the welding layer WD2 may be formed such that a filler metal and part of the diaphragm, part of the regulation member or another filler metal.
(68) The diaphragms 4 and 5 are not necessarily in the same shape. Similarly, the regulation members 6 and 7 are not necessarily in the same shape.
(69) Like a first example modification shown in
(70) In the foregoing embodiments, the metal diaphragm damper 1 is described in the configuration in which the annular periphery portions 25 of the regulation members 6 and 7 with the outer edge portions 20 of the diaphragms 4 and 5 fixed to each other by welding are further fixed by welding and thus the fuel pressure in the fuel chamber 11 is absorbed on both sides of the diaphragm 4 and the diaphragm 5. However, the configuration is not limited to this. For example, like a second example modification shown in
(71) In the embodiments, the metal diaphragm damper 1 is described in the form in which the metal diaphragm damper 1 is provided in the fuel chamber 11 of the high-pressure fuel pump 10 to reduce pulsation in the fuel chamber 11. However, not limited to this, the metal diaphragm damper 1 may reduce pulsation by being provided in a fuel pipe, for example, that is connected to the high-pressure fuel pump 10.
(72) A configuration may be provided in which contact of the diaphragm 4 with the diaphragm 5 at a high pressure is prevented by disposing a core material made of an elastically deformable synthetic resin, for example, in the enclosed space (i.e., in the inside of the metal diaphragm damper 1) formed between the connected diaphragm 4 and the diaphragm 5.
(73) In the embodiments, a form is described in which the first and second welding steps are performed in the atmosphere made of air and the third welding step is performed in the atmosphere made of a gas to be sealed in the damper main body 2. However, the first and second welding steps may be performed in the atmosphere of the gas to be sealed in the damper main body 2 as well.
REFERENCE SIGNS LIST
(74) 1 Metal diaphragm damper
(75) 2 Damper main body
(76) 3 Cover member
(77) 4, 5 Diaphragm
(78) 6, 7 Regulation member
(79) 10 High-pressure fuel pump
(80) 11 Fuel chamber
(81) 12 Plunger
(82) 13 Suction valve
(83) 14 Pressurizing chamber
(84) 15 Discharge valve
(85) 19 Deformable portion
(86) 20 Outer edge portion
(87) 20a Outer surface
(88) 20b Inner surface
(89) 25 Annular periphery portion
(90) 25a inner surface
(91) 27 Side wall portion part
(92) 28 Bottom part
(93) 29 Recess
(94) 29a Recess bottom surface
(95) 29b Recess inner surface
(96) 30 Hole
(97) 31 Support member
(98) 31a Opening
(99) WD1 First and second welding layers (first welding part)
(100) WD2 Welding layer (second welding part)