METHOD FOR SEALING A SEAM REGION, AND PLASTIC SKIN

20210187869 · 2021-06-24

Assignee

Inventors

Cpc classification

International classification

Abstract

The invention relates to a method by which stitch openings in the area of a seam in a plastic skin (10), in particular a PVC or TPU skin, are sealed, said PVC or TPU skin being provided for a foamed part. Foamed parts of this type are used especially as interior fitting parts, e.g. as a dashboard, in the field of automobile manufacturing. The invention further relates to a PVC or TPU skin comprising a seam of said type.

Claims

1. Method for sealing a seam region of a plastic skin, in particular a PVC or TPU slush skin, with stitch openings being present in the plastic skin in the seam region owing to the incorporation of a yarn in the plastic skin, providing a plastic skin having a visible side and provided with at least one yarn such that the rear side of the plastic skin is accessible, heating the rear side of the plastic skin in the seam region such that the plastic skin contacts the yarn in the region of the stitch openings.

2. Method according to claim 1, characterised in that the heating of the plastic skin is carried out by means of a heating device with a relative movement being provided between the heating device and the skin.

3. Method according to claim 2, characterised in that the heating device is a gas burner, a hot air source, an infrared source, a heating element, a soldering iron, a pressure roller with a heat source or pressure pad with a heat source, or a laser.

4. Method according to claim 1, characterised in that the at least one yarn is a fire-resistant yarn.

5. Method according to claim 1, characterised in that in the step of preparing the plastic skin, the skin is placed visible side facing down on a support, in particular a machine table, or in one half of a foaming tool.

6. Method according to claim 1, characterised in that when heating the rear side of the plastic skin in the seam region, the plastic skin is at least partially melted.

7. Method according to claim 1, characterised in that the plastic skin is provided with two yarns spaced apart from one another which define a common seam region, with the heating of the rear side of the plastic skin in the common seam region being carried out in a single pass.

8. Method according to claim 1, characterised in that the stitch openings extend substantially perpendicular to and through the rear side of the plastic skin.

9. Method according to claim 1, characterised in that the skin in the seam region is heated at least in parts to a temperature of at least 80° C., preferably at least 100° C., further preferred at least 110° C.

10. Method according to claim 1, characterised in that when heating the rear side of the plastic skin in the seam region, or subsequent thereto, a mechanical influence is exerted in the seam region, in particular by means of a pressure roller or a pressure pad.

11. Method for producing a panel component, in particular an interior panel component, using a plastic skin processed according to claim 1, comprising the steps of: placing the plastic skin and a dimensionally stable carrier in a moulding tool, inserting a filling material, in particular a polyurethane foam or a thermoplastic elastomer, in a region between the rear side of the plastic skin and the dimensionally stable carrier.

12. Plastic skin, preferably a PVC or TPU skin, comprising a visible side as well as a rear side, the visible side having a preferably grained surface, wherein the plastic skin comprises a seam region having a yarn, which yarn penetrates through the plastic skin in sections, with heated, or melted, and resolidified sections of the plastic skin being present in the seam region such that the plastic skin contacts the yarn in the region of the stitch openings.

Description

BRIEF DESCRIPTION OF THE DRAWINGS

[0034] FIG. 1 is a schematic cross-section view of a region of a PVC skin, in which a yarn has been incorporated.

[0035] FIG. 2 is a perspective top view of an under side of a skin with an incorporated yarn.

DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0036] A preferred embodiment of the present invention is described in detail below by means of the enclosed figures. Further modifications of certain features cited in this context can each be individually combined to form new embodiments.

[0037] The cross-section shown in FIG. 1 schematically shows a seam region of a PVC or TPU slush skin 10 (also referred to as “skin” in the following within the scope of the present embodiment). The skin 10 comprises a visible side 10a, which is normally provided with a grain pattern, for example so as to imitate a leather surface, as well as a rear side 10b. The rear side 10b forms the non-visible inner side in a foamed component provided with a skin 10.

[0038] In the described embodiment, yarns 20 are sewn into the skin 10 at a certain distance to one another, which penetrate the skin 10 along its progression through stitch openings alternately from the visible side 10a to the rear side 10b and vice versa. The yarns 20 are thereby formed from a fire-resistant material or a material with low flammability. A groove 11 is furthermore provided on the visible side 10a of the skin 10 (at the bottom of FIG. 1), in the region of which the skin 10 has a depression in order to imitate a connecting region between two pieces of skin.

[0039] During the method according to the invention, the skin 10 is placed on a support 30 with its visible side 10a facing down such that the rear side 10b of the skin 10, which comes into contact with the foamed material (preferably polyurethane) or a thermoplastic elastomer during a later foaming process, is accessible.

[0040] In order to seal the stitch openings of the seams, a local thermal influence is now exerted by means of a heating device 50. In the present embodiment, this thermal influence is exerted by means of a flame, a soldering iron or by means of hot air. The heating device 50 is accordingly configured as a gas burner, a soldering iron or a hot air blower.

[0041] For this purpose, a heating device 50 is guided along the seam region of the skin 10, thereby heating the skin 10 in this region. Owing to the heating, a temporary softening of the skin 10 in the seam region occurs, such that the skin 10 contacts the yarn 20 and thus seals the stitch openings.

[0042] It is also possible according to a further modification to use a combined pressure and heating device, for example a pressure roller/pressure pad with a heat source.

[0043] It is also possible to first of all heat the seam region and then, whilst the skin 10 in the seam region is at least partially still in the heated state, to apply pressure.

[0044] The skin 10 can thereby be heated to at least 80° C., preferably at least 100° C., further preferred at least 120° C. A maximum temperature range is, for example, 2000° C.

[0045] Once the skin has cooled, it remains in this state so that during a subsequent foaming process, during which the skin 10 is connected to a dimensionally stable carrier by means in particular of polyurethane, no foam material can penetrate to the visible side.

[0046] Even though it is preferred according to the described preferred embodiment that the skin 10 is placed on a support arranged so as to be stationary and that the heating device 50 is moved, it is possible according to another alternative to place the skin 10 on a moveable support (moveable table) and to bring about a relative movement between the skin 10 and the heating device in this manner. Furthermore, according to another alternative, both the support with the skin and the heating device can be moved.