SPRING LEAF AND METHOD FOR PRODUCING A SPRING LEAF

20210054895 ยท 2021-02-25

    Inventors

    Cpc classification

    International classification

    Abstract

    In a method for producing a spring leaf (2) for a leaf spring, in particular a parabolic spring or suspension spring, wherein the spring leaf (2) comprises two end regions, a central region, a top side which is subjected to tensile stress in the operative state, and a bottom side (1) which is subjected to pressure in the operative state, at least one hole (3) is introduced into the bottom side (1). The bottom side (1) is peened locally in the region around the hole (3).

    Claims

    1. A method for producing a spring leaf for a leaf spring, in particular a parabolic spring or a suspension spring, wherein the spring has two end regions, a central region, a top side which is subjected to tension in the operative state, and a bottom side which is subjected to pressure in the operative state, and wherein at least one hole is introduced into the bottom side, wherein that the bottom side is peened in the region around the hole.

    2. A method according to claim 1, wherein the bottom side is peened locally in the region around the hole.

    3. A method according to claim 1, wherein the bottom side is shot-peened in the region around the hole.

    4. A method according to one of the claim 1, wherein a peening medium is applied via a jet nozzle, wherein the jet nozzle and the region of the hole are aligned with one another.

    5. A method according to claim 4, wherein the jet nozzle is moved towards the spring leaf and/or the spring leaf is moved towards the jet nozzle.

    6. A method according to claim 1, wherein a region around the hole is peened, so that the distance from the hole to the transition between the peened and non-peened surface of the bottom side lies in the range of approximately 5 cm or 4 cm or 3 cm or 2 cm or 1 cm.

    7. A method according to claim 1, wherein a through-hole or a blind hole is introduced as a hole.

    8. A method according to claim 7, wherein a clamping region with a continuous central hole is formed in the central region, and that the region is peened around the central hole.

    9. A method according to claim 1, wherein the spring is produced from flat bar steel, in particular spring steel.

    10. A method according to claim 1, wherein the spring leaf is hot-deformed, in particular rolled, and thereafter hardened and tempered, in that the top side of the spring leaf, especially under pretensioning of the spring leaf, is peened, and that the bottom side of the spring leaf is peened in the region around the hole after the peening of the top side of the spring leaf.

    11. A spring leaf for a leaf spring, a parabolic spring or a suspension spring, wherein the spring leaf comprises two end regions, a central region, a top side which is subjected to tension in the operative state, and a bottom side which is subjected to pressure in the operative state, and wherein the bottom side has at least one hole, is peened locally in the region around the hole.

    12. A spring leaf according to claim 11, wherein the bottom side is shot-peened in the region around the hole.

    13. A spring leaf according to claim 11, wherein the distance from the hole to the transition between the peened and non-peened surface of the bottom side lies in the range of approximately 5 cm or 4 cm or 3 cm or 2 cm or 1 cm.

    14. A spring leaf according to claim 11, wherein the hole is a through-hole or a blind hole.

    15. A spring leaf according to claim 14, wherein a clamping region with a continuous central hole is provided in the central region, and that the region is peened around the central hole.

    16. A spring leaf according to claim 11 made of flat bar steel, said flat bar steel being spring steel.

    Description

    [0035] The drawings show as follows:

    [0036] FIG. 1 shows a region of a bottom side of a spring leaf in the region of a hole, and

    [0037] FIG. 2 shows a block diagram with an embodiment of a method sequence according to the invention.

    [0038] In FIG. 1 a region of a bottom side 1 of a spring leaf 2 for a leaf spring is shown in which a hole 3 is introduced. The leaf spring may, for example, be a parabolic spring or a suspension spring. The hole 3 can be a through-hole or a blind hole. The hole 3 can be a central hole provided in a clamping area or in another area of the spring 2 leaf, for example in an end area.

    [0039] The bottom side 1 of the spring leaf 2 is subjected to pressure in the operative state of the leaf spring.

    [0040] The spring leaf 2 is preferably made of flat bar steel, in particular spring steel. The bottom side 1 of the spring leaf 2 is peened locally in the region around the hole 3, in particular shot-peened. The distance from the hole 3 to the transition 4 between the peened and non-peened surface of the bottom side 1 is in the range of a few centimetres. During peening, a first region 5, which is uniformly peened, is formed around the hole, as well as a second region 6 adjacent thereto, in which the transition from the non-peened and peened region takes place gradually in a certain scattering region.

    [0041] The peening can take place via a jet nozzle 7 which applies a peening agent 8 to the bottom side 1, wherein the jet nozzle 7 and the region of the hole 3 are aligned with one another.

    [0042] FIG. 2 shows an exemplary process sequence for producing a spring leaf 2 according to the invention in a block diagram, wherein individual blocks provided with reference numerals can consist of single or multiple process steps.

    [0043] In block 9, for example, a profile bar can be cut to a desired length and heated.

    [0044] In block 10, heat processing and heat-forming processes can be carried out. In particular, the heated profile bar can be rolled and, if necessary, further cut to size, wherein at least one hole 3 is introduced into the bottom side 1 of the spring leaf 2 to be produced. In block 10, in particular, a central hole can be introduced into the clamping area. Alternatively or additionally, at least one longitudinal end of the spring leaf 2 can be machined in that at least one end section is formed into a means for connecting the spring leaf to a vehicle chassis or to connecting parts of a wheel suspension, in particular into a spring eye. Likewise, an embodiment is conceivable in which at least one end section is converted into a securing means, such as a safety wraparound.

    [0045] In block 11 further mechanical machining can take place. Processes for bending, tempering, hardening and annealing the spring leaf 2 may take place. Likewise, the top side of the spring leaf 2 can be peened, in particular peened under the pretensioning of the spring leaf 2.

    [0046] Blocks 9 to 11 comprise method steps known from the prior art.

    [0047] In block 12, the method step proposed according to the invention takes place, in which the bottom side 1 is peened in the region around the hole 3, in particular locally peened, preferably shot-peened.

    [0048] After the block 12, further processes can take place up to the completion of a leaf spring, wherein the leaf spring can have one spring leaf 2 or two or more spring leaves 2.

    [0049] If a spring eye has been rolled, an eye bearing can be pressed in, for example. For example, the spring 2 can be painted. The leaf spring can be set, tested and packaged.

    [0050] The peening of the bottom side of the spring leaf 2 described in block 12 can take place immediately after the stress peening of the top side of the spring leaf 2 or further processes can take place between the peening of the top side and the peening of the bottom side, for example setting.