    Abstract

    A water-dissolvable and environmentally friendly pad for exfoliating the skin is obtained by mixing baking soda, powdered Foam Glass and PVA-co-VAC. Its simple manufacturing process, performed entirely at room temperature, includes mixing the powders, adding the glue, pouring the mixture into molds and letting it dry by evaporation. Due to its characteristics, the resulting pad is reusable and can be rinsed, not losing its abrasive properties as well as its ability to clean grease, remove dead skin and clean, alter use. It has a spongy, moist, elastic, flexible and resistant structure, not toxic to the skin, nor can it be absorbed by it.

    Claims

    1. A reusable water-dissolvable exfoliating pad for the skin comprising 5% to 65% in volume of baking soda, 5% to 65% in volume of powdered Foam Glass and 30% to 70% in volume of a water solvable polymer.

    2. The reusable water-dissolvable exfoliating pad for the skin of claim 1 wherein said water solvable polymer is PVA-co-VAC.

    3. The reusable water-dissolvable exfoliating pad for the skin of claim 1 wherein said water solvable polymer is a Transparent liquid adhesive poly (vinyl alcohol-co-vinyl acetate) school glue.

    4. A reusable water-dissolvable exfoliating pad for the skin comprising 30% in volume of baking soda, 30% in volume of powdered Foam Glass and 40% in volume of a water solvable polymer.

    5. The reusable water-dissolvable exfoliating pad for the skin of claim 4 wherein said water solvable polymer is PVA-co-VAC.

    6. The reusable water-dissolvable exfoliating pad for the skin of claim 4 wherein said water solvable polymer is a Transparent liquid adhesive poly (vinyl alcohol-co-vinyl acetate) school glue.

    7. A method for manufacturing a water-dissolvable exfoliating pad for the skin comprising the steps of (a) exhaustively mixing 5% to 65% in volume of Baking Soda and 5% to 65% in volume of powdered Foam Glass for about 15 minutes to obtain a powder mixture, (b) adding 30% to 70% in volume of Transparent liquid adhesive poly (vinyl alcohol-co-vinyl acetate) school glue to the powder mixture obtained in step a, at room temperature and mixing it together until obtaining a homogeneous final mixture, (c) introducing the final mixture obtained in step b into a mold having a thickness of between 1.5 millimeters and 2.5 millimeters, and (d) letting it dry in the mold by evaporation at room temperature for 24 to 48 hours.

    Description

    BRIEF DESCRIPTION OF THE DRAWINGS

    [0023] FIG. 1 is a schematic front view of the first step of a process to manufacture an embodiment of a reusable exfoliating pad in accordance with the present invention, consisting of preparing the powder mixture.

    [0024] FIG. 2 is a schematic front view of the second step of a process to manufacture an embodiment, of a reusable exfoliating pad in accordance with the present invention, consisting of mixing the powders.

    [0025] FIG. 3 is a schematic front view of the third step of a process to manufacture an embodiment of a reusable exfoliating pad in accordance with the present invention, consisting of adding the glue.

    [0026] FIG. 4 is a schematic front view of the fourth step of a process to manufacture an embodiment of a reusable exfoliating pad in accordance with the present invention, consisting of mixing the powders and the glue.

    [0027] FIG. 5 is a schematic front view of the fifth step of a process to manufacture an embodiment of a reusable exfoliating pad in accordance with the present invention, consisting of pouring the mixture into a mold.

    [0028] FIG. 6 is a schematic front view of the sixth step of a process to manufacture an embodiment of a reusable exfoliating pad in accordance with the present invention, consisting of letting the mixture dry.

    [0029] FIG. 7 is a perspective view of an embodiment of a reusable exfoliating pad in accordance with the present invention.

    DETAILED DESCRIPTION AND BEST MODE Of IMPLEMENTATION

    [0030] Disclosed is a reusable cosmetic article for exfoliating the skin, particularly useful for exfoliating the skin of the face. This article comes in the form of a reusable pad or sponge which is water-dissolvable and has a has a spongy, moist, flexible and resistant structure. This is attained in a cost-efficient manner thanks to a simple manufacturing process comprising the mixture of two powders and a glue, mixture which is then poured in molds and dried to obtain the final product. A method for manufacturing the pads is also disclosed.

    [0031] Some general aspects of the present invention have been summarized so far in this disclosure. Hereinafter, a detailed description of the invention as illustrated in the drawings will be provided. While some aspects of the invention will be described in connection with these drawings, it is to be understood that the disclosed embodiments are merely illustrative of the invention, which may be embodied in various forms. The specific, materials, methods, structures and functional details disclosed herein are not to be interpreted as limiting. Instead, the intended function of this disclosure is to exemplify some of the ways -including the presently preferred ways- in which the invention, as defined by the claims, can be enabled for a Person of Ordinary Skill in the Art. Therefore, the intent of the present disclosure is to cover all variations encompassed within the spirit and scope of the invention defined by the appended claims, and any reasonable equivalents thereof.

    [0032] Referring to the drawings in more detail, FIG. 1 schematically illustrates the first step of the process in which the powders are poured together into a container 4, in the adequate proportions to form the powder this example the powders used are Baking Soda 1, and Foam Glass 2. A funnel 3 is used to facilitate the mixture in accurate proportions, but in other embodiments the use of the funnel can be omitted. The baking soda 1 is added in proportion such that it will account for 25% of the total volume of the final mixture. In other embodiments, other percentage may be used as long as the general proportions established by this specification are respected. The Foam Glass 2 is added in a proportion such that it will account for 25% of the total volume of the final mixture. In other embodiments, other exfoliating particles may be used instead of or in addition to Foam Glass as long as the utility is conserved, In the preferred embodiment, powdered Foam Glass or cellular glass is used, such as commercially available Owens Corning's FOAMGLAS , Ningbo Yoyo Foam Glass Go Ltd. and others, which is sold in the form of Insulating rubble that, in order to be convened to the required powder form, can be placed in an industrial machine for brick dust or similar which produces a grain between 150 m and 250 m approximately. Alternatively, powdered Foam Glass can be manually obtained by rubbing block against block. The resulting mixture is called the powder mixture 5, which shall incorporate in this step any other powders in the embodiments that include additional granular elements and which in total amount, in the described embodiment, to 50% of the total volume of the final mixture. In other embodiments the powder mixture 5 may amount to other proportions ranging from 30% to 70% of the total volume of the final mixture. Different proportions yield different results. For example, 45% of baking soda and 5% Foam Glass powder, keeping the remaining 50% of glue, would form a solid but less abrasive product for the purpose of exfoliating more sensitive skin including the face. The glue may vary its percentage depending on its viscosity. Greater exfoliation power can be achieved by inverting the aforementioned percentages in 5% sodium bicarbonate and 45% Foam Glass powder and 50% glue. This will make a harder product, with more capacity for the exfoliation of very thick skin.

    [0033] FIG. 2 shows how the powder mixture 5 in the container 4 is exhaustively mixed at room temperature until acquiring a homogeneous state. This can be achieved by hand with the use of a spoon 6 stirring vigorously for at least 15 minutes, or with the use of industrial or laboratory V powder mixers, or other types of powder mixers to achieve homogeneity.

    [0034] In FIG. 3 the glue 7 is added to the container 4, so that together with the powder mixture 5 already in it, it forms the final mixture 9 completing the 100% of the final volume. This step can be implemented, in some embodiments, with the use of a separator funnel 8. As used in this specification and the appended claims, the term glue refers to a water-solvable polymer, preferably poly (vinyl alcohol-co-vinyl acetate) (PVA-co-VAC; chemical composition: CH2CHOH-co-(C4H6O2)n), but it may be replaced by other PVAc (PVAc or PVOH) variants or even other polymers as long as the utility is conserved. PVA-co-VAC is a colorless liquid with a distinctive aroma, it is a polyvinyl acetate, a polymer widely used in the industry. This glue dissolves in water at different temperatures depending on the brands. It is washable and does not stain.

    [0035] In the preferred embodiment, the type of glue used is Transparent liquid adhesive poly (vinyl alcohol-co-vinyl acetate) school glue, (Voligoma, Akapol SA, Argentina, with a with a molecular weight of 47,000 g/mol and 12% vinyl acetate). Due to its viscosity, it is one of those glues recommended to comply with drying times and product structure, (24 hours/30 hours between 22 C./25 C. with 40% to 50% ambient humidity, summer season or laboratory controlled). Other brands and varieties have also been tested, whose contents have different viscosity and water dispersion. The pads can still be manufactured with these products, but it is observed that an excessive water proportion, in comparison to the same quantity in grams in other brands such as Voligoma, have a negative impact in the product's drying time, resistance and elasticity. However, these and other brands may still be used, provided that the glue is based on polyvinyl alcohol, (PVOH) and the drying times and proportions are adjusted to achieve an acceptable final result. Therefore, the result is not limited to a specific brand.

    [0036] FIG. 4 shows how the final mixture 9 in the container 4 is exhaustively mixed at room temperature until acquiring a homogeneous state. This can be achieved by hand with the use of a spoon 6 stirring vigorously for at least 15 minutes, or with the use of industrial or laboratory mixers, or other types of mixers to achieve homogeneity. The resulting final mixture 9 shall incorporate in this step any other liquid or viscous ingredients such as perfumes and colorants in those embodiments that include them.

    [0037] In FIG. 5, the final mixture 9 is poured into molds 10, having a thickness of between 0.5 mm and 5 mm, being 2 mm the optimum thickness that allows an optimal mechanical strength and flexibility for handling and 2 mm to 3 mm the ideal range for an improved cost-benefit ratio. The molds can be rounded, squared, of have different shapes, including geometric shapes and decorative shapes such as leaves, hearts or stars. In FIG. 6 the final mixture 9 in the molds 10 are dried naturally by evaporation at room temperature for 24 to 48 hours. Once the mixture is dried, the pads 11 (FIG. 7) are extracted from the molds 10.

    [0038] The description as set forth is not intended to be exhaustive or to limit the invention to the precise form disclosed. Many modifications and variations are possible in light of the teachings above without departing from the spirit and scope of the forthcoming claims.