Manufacturing method of display panel and display panel
10923687 ยท 2021-02-16
Assignee
Inventors
Cpc classification
H10K71/00
ELECTRICITY
H10K71/191
ELECTRICITY
International classification
Abstract
A manufacturing method of a display panel and a display panel are provided. The advantages thereof are that a shadow area of an edge of a pixel caused by an angle of evaporation can be avoided and reduced, a pixel position accuracy (PPA) shift caused by raising a temperature of a fine metal mask during a coating process can be prevented, and it is applicable to manufacture of high-resolution display panels.
Claims
1. A manufacturing method of a display panel, comprising steps of: providing a substrate having a first surface and a second surface, wherein the first surface is disposed opposite to the second surface, and forming a plurality of deposition regions and a plurality of non-deposition regions alternately arranged on the first surface; providing a mask comprising a plurality of blocking regions and a plurality of hollow regions spaced apart from each other, wherein the blocking regions are disposed corresponding to the deposition regions and the hollow regions are disposed corresponding to the non-deposition regions; providing a light source to irradiate the mask, wherein the light source in the hollow region irradiates the non-deposition regions after passing through the hollow regions, and the light source in the blocking region is blocked by the blocking region; and generating an organic material vapor by an evaporation source, wherein the organic material vapor contacts the first surface to form an organic material block on each of the deposition regions by the organic material vapor, and the organic material vapor does not form the organic material block on the non-deposition regions, wherein an edge of a side of the organic material block protrudes from a boundary between the deposition regions and the non-deposition regions; wherein the manufacturing method further comprises an aligning step to adjust positions of the substrate and the mask, so that the blocking regions are disposed corresponding to the deposition regions, and the hollow regions are disposed corresponding to the non-deposition regions.
2. The manufacturing method of a display panel according to claim 1, wherein each of the deposition regions is a sub-pixel region, each of the non-deposition regions is a non-sub-pixel region, and the organic material block which is disposed on each of the deposition regions is a sub-pixel.
3. The manufacturing method of a display panel according to claim 1, wherein a side of the organic material block protrudes from the boundary between the deposition regions and the non-deposition regions, and a thickness of the material organic block is gradually decreased in each of the non-deposition regions.
4. The manufacturing method of a display panel according to claim 1, wherein the light source is a laser light source.
5. A manufacturing method of a display panel, comprising steps of: providing a substrate having a first surface and a second surface, wherein the first surface is disposed opposite to the second surface, and forming a plurality of deposition regions and a plurality of non-deposition regions alternately arranged on the first surface; providing a light source and a mask, wherein the mask comprises a plurality of blocking regions and a plurality of hollow regions spaced apart from each other, the blocking regions are disposed corresponding to the deposition regions, the hollow regions are disposed corresponding to the non-deposition regions; irradiating the second surface and the non-deposition regions from the second surface by the light source, wherein the light source in the hollow regions irradiates the non-deposition regions after passing through the hollow regions, and the light source in the blocking regions is blocked by the blocking regions; and generating an organic material vapor by an evaporation source, wherein the organic material vapor contacts the first surface to form an organic material block on each of the deposition regions by the organic material vapor, and the organic material vapor does not form the organic material block on the non-deposition regions.
6. The manufacturing method of a display panel according to claim 5, wherein the manufacturing method further comprises an aligning step to adjust positions of the substrate and the mask, so that the blocking regions are disposed corresponding to the deposition regions, and the hollow regions are disposed corresponding to the non-deposition regions.
7. The manufacturing method of a display panel according to claim 5, wherein in the step of forming the organic material block, an edge of a side of the organic material block protrudes from a boundary between the deposition regions and the non-deposition regions.
8. The manufacturing method of a display panel according to claim 5, wherein each of the deposition regions is a sub-pixel region, each of the non-deposition regions is a non-sub-pixel region, and the organic material block which is disposed on each of the deposition regions is a sub-pixel.
9. The manufacturing method of a display panel according to claim 5, wherein a side of the organic material block protrudes from a boundary between the deposition regions and the non-deposition regions, and a thickness of the material organic block is gradually decreased in each of the non-deposition regions.
10. The manufacturing method of a display panel according to claim 5, wherein the light source is a laser light source.
11. A display panel formed by the manufacturing method of claim 5, comprising: a substrate having a plurality of deposition regions and a plurality of non-deposition regions alternately disposed thereon, wherein an organic material block is disposed on the deposition region, a side of the organic material block protrudes from a boundary between the deposition regions and the non-deposition regions, and a thickness of the material organic block is gradually decreased in each of the non-deposition regions.
12. The manufacturing method of a display panel according to claim 11, wherein the organic material block is a sub-pixel.
13. The manufacturing method of a display panel according to claim 11, wherein the side of the organic material block is arc-shaped.
Description
DESCRIPTION OF DRAWINGS
(1)
(2)
(3)
(4)
(5)
(6)
(7)
(8)
DETAILED DESCRIPTION OF PREFERRED EMBODIMENTS
(9) Exemplary embodiments of manufacturing methods of display panels and display panels provided by the present disclosure will be further described in detail with the accompanying drawings and the specific embodiments.
(10) The method for preparing the display panel and the concrete embodiments of the display panel provided by the present disclosure will be described in detail below with reference to the accompanying drawings.
(11)
(12) Please refer to step S20,
(13) Specifically, the substrate 300 is a conventional substrate used for manufacturing a display panel, for example, a glass substrate, a flexible substrate, etc. The arrangements of the deposition region B1 and the non-deposition region B2 may be set according to the concrete situations, for example, are set according to a function. Boundaries of the deposition region B1 and the non-deposition region B2 may be defined by an external structure or by height differences between the deposition region B1 and the non-deposition region B2.
(14) For example, in the present embodiment, the substrate 300 is a glass substrate, which is a transparent structure and allows light to pass through. Conventional structures, such as a thin film transistor layer (not shown in the drawing), are deposited on the substrate 300. In other embodiments of the present disclosure, the substrate can also be a flexible substrate. In the present embodiment, the deposition region B1 is a sub-pixel region, and the non-deposition region B2 is a non-sub-pixel region. The boundary between the deposition region B1 and the non-deposition region B2 is defined by edges of hollow regions of the mask (indicated in
(15) Please refer to step S21 and
(16) In the present embodiment, the light source 310 irradiate the substrate 300 through a mask 320, i.e., the mask 320 is disposed between the light source 310 and the substrate 300. The mask 320 is a conventional photo mask in the art. The mask 320 has a plurality of hollow regions 321 and a plurality of blocking regions 322. The hollow regions 321 are disposed corresponding to the non-deposition regions B2, and the blocking regions are disposed corresponding to the deposition regions B1. That is, the positions which correspond to the non-deposition regions B2 are not blocked by the mask 320, and the positions which correspond to the deposition region B1 is blocked by the mask 320. The light emitted by the light source 310 is shown as arrows in the figure. The light emitted by the light source 310 irradiates the mask 320. Then, the light emitted from the light source 310 directly irradiate the substrate 300 from the hollow regions 321 and pass through the substrate 300 to irradiate the non-deposition region B2, while the light generated by the light source 310 is blocked by the mask 320 in the blocking region 322. Thus, the light irradiated on the blocking region 322 does not irradiate the substrate 300, i.e., it does not irradiate the deposition region B1.
(17) Please refer to step S22 and
(18) The organic material vapor is blocked by the substrate 300 and then the organic material vapor is deposited on the first surface 301 of the substrate 300. Specifically, the organic material vapor in the deposition region B1 nucleates and undergoes film formation to form an organic material block 340. The organic material vapor in the non-deposition region B2 does not form an organic material block. It is because the non-deposition region B2 is irradiated by the light source 310. After the organic material vapor reaches the non-deposition region B2, it is irradiated and activated by the light source 310. Therefore, the organic material vapor cannot nucleate and undergo film formation, i.e., the organic material vapor cannot deposit at the non-deposition region B2 and form a block of organic material. In the present embodiment, the organic material block 340 is a sub-pixel.
(19) Using conventional mask technologies, the manufacturing method of a display panel of the present disclosure irradiates the mask 320 via a light source, such as a laser. The light of the light source 310 selectively irradiate the substrate 300 through the mask. The regions irradiated by the light source produces a thermal or a photochemical effect which activates particles of the vapor of the organic material and prevents the deposition of particles on those regions. The manufacturing method of the present disclosure avoids using a fine metal mask, which omits periodic mask-tensioning and cleaning processes, and reduces maintenance costs for mass production. Meanwhile, large shadow regions of edges of pixels caused by angles of evaporations can be avoided, and a pixel position accuracy (PPA) shift caused by raising temperature of the fine metal mask during the coating process can be prevented, and it is applicable to manufacture of high-resolution display panels.
(20) Further, in an embodiment, the manufacturing method further includes an aligning step to adjust positions of the substrate 300 and the mask 320, so that the blocking regions 322 are disposed corresponding to the deposition regions B1, and the hollow regions 321 are disposed corresponding to the non-deposited regions B2. The method for adjusting is a conventional method in the art. For example, the alignment system of each of the substrate 300 and the mask 320 can be employed to perform the adjustment, and details are not described herein.
(21) Further, please refer to
(22) The present disclosure also provides a display panel manufactured by the above method.
(23) The substrate 400 has a plurality of deposition regions B1 and a plurality of non-deposition regions B2 alternately disposed thereon. Organic material blocks 440 are disposed on the deposition regions B1. In the present embodiment, the organic material block 440 is a sub-pixel. A side of the organic material block 440 protrudes from a boundary E between the deposition region B1 and the non-deposition region B2. That is, the organic material block 440 covers a portion of the non-deposition region B2 in addition to the deposition region B1. The boundary between the deposition region B1 and the non-deposition region B2 is determined by processes thereof. In the present embodiment, the boundary between the deposition region B1 and the non-deposition region B2 is the edge of the hollow region of the mask used when manufacturing the display panel. At a portion of the organic material block 440 that protrudes from the boundary E, the thickness of the organic material block 440 is gradually decreased, and sides of the organic material block 440 are arc-shaped.
(24) The display device further comprises a structure, such as a cover 450, etc. Other structures of the display panel are not described herein, and people skilled in the art should be able to obtain other structures of the display panel from the prior art.
(25) The above descriptions are merely some exemplary embodiments of the present disclosure, and those skilled in the art may make various improvements and refinements without departing from the principle of the disclosure. All such modifications and refinements are covered by the present disclosure.
INDUSTRIAL APPLICABILITY
(26) The subject matters of the present application can be manufactured and used in the industry therefore, they possess industrial applicability.