In situ tribometer and methods of use
10908069 ยท 2021-02-02
Assignee
Inventors
Cpc classification
G01Q60/24
PHYSICS
G01Q80/00
PHYSICS
G01N2203/0246
PHYSICS
International classification
Abstract
Techniques for determining a characteristic of a sample using an atomic force microscope including a cantilever having a probe attached thereto, including positioning the sample within a cell and sliding the probe over a sliding zone of the sample within the cell. Lateral and vertical deformations of the cantilever are detected using the atomic force microscope as the probe is slid over the sliding zone. One or more characteristics are determined based on the detected lateral deformations of the cantilever.
Claims
1. A tribometer for determining one or more characteristics of a surface of a sample, comprising: an atomic force microscope comprising a cantilever configured to detect lateral and vertical deformations of the cantilever; a probe attached to an end of the cantilever of the atomic force microscope, wherein the probe comprises a spherical structure; a cell for holding the sample with the surface comprising a sliding zone to be characterized; a control unit communicatively coupled with the atomic force microscope and configured to slide the probe over the sliding zone of the sample and determine the one or more characteristics based on a lateral deflection signal of the cantilever generated from the detected deformations of the cantilever, wherein the control unit is configured to simultaneously cause the probe to form an antiwear tribofilm within the sliding zone, image a topography of the sliding zone of the sample, and determine the one or more characteristics without removing the sample from the cell; and a heating element adapted to maintain the cell at a predetermined temperature.
2. The tribometer of claim 1, wherein the one or more characteristics include one or more of a friction force or a coefficient of friction, a characteristic corresponding to wear, a characteristic corresponding to adhesion, or a characteristic corresponding to elastic modulus.
3. The tribometer of claim 1, wherein the cell comprises a liquid cell and the sliding zone of the sample is immersed in a lubricant.
4. The tribometer of claim 1, wherein the probe is a spherical probe.
5. The tribometer of claim 4, wherein the probe has a diameter of between 1 m and 100 m.
6. The tribometer of claim 1, wherein the probe is formed from steel.
7. A method for determining one or more characteristics of a surface of a sample using an atomic force microscope including a cantilever having a probe attached thereto, comprising: positioning the sample within a cell; sliding the probe over a sliding zone of the surface of the sample within the cell, wherein the probe comprises a spherical structure; detecting lateral and vertical deformations of the cantilever using the atomic force microscope as the probe is slid over the sliding zone; determining one or more characteristics of the sliding zone based on the detected lateral deformations of the cantilever; maintaining the cell at a predetermined temperature using a heating element; and simultaneously forming an antiwear tribofilm within the sliding zone, imaging a topography of the sliding zone of the sample, and determining the one or more characteristics without removing the sample from the cell.
8. The method of claim 7, wherein the one or more characteristics of the sliding zone includes one or more of a coefficient of friction, a characteristic corresponding to wear, a characteristic corresponding to adhesion, or a characteristic corresponding to elastic modulus.
9. The method of claim 7, wherein the cell comprises a liquid cell, further comprising: immersing the sliding zone of the sample in a lubricant.
10. The method of claim 7, wherein the probe is a spherical probe.
11. The method of claim 10, wherein the probe has a diameter of between 1 m and 100 m.
12. The method of claim 7, wherein the probe is formed from steel.
Description
BRIEF DESCRIPTION OF THE DRAWINGS
(1) Further features, the nature, and various advantages of the disclosed subject matter will be more apparent from the following detailed description and the accompanying drawings in which:
(2)
(3)
(4)
(5)
(6)
(7)
(8)
(9)
(10)
(11) Throughout the drawings, the same reference numerals and characters, unless otherwise stated, are used to denote like features, elements, components or portions of the illustrated embodiments. Moreover, while the disclosed subject matter will now be described in detail with reference to the figures, it is done so in connection with the illustrative embodiments.
DETAILED DESCRIPTION
(12) The disclosed subject matter is generally directed to systems and methods for simultaneously measuring friction at the sliding interface between a probe and a substrate surface, and measuring the morphology and nanoscale tribo-mechanical properties of the substrate and any resulting tribofilm deposited on the substrate or worn or modified region of the substrate.
(13) In accordance with one aspect of the disclosed subject matter, a tribometer can include a cantilever 110 and a spherical probe 120 coupled to the cantilever 110. Various views of an exemplary steel probe 120 mounted to a cantilever 110 in accordance with the disclosed subject matter are shown in
(14) In accordance with another aspect, the disclosed subject matter can include a method for using a tribometer including a spherical probe for simultaneous coefficient of friction measurements and in situ imaging.
(15) The tribometer can be used to measure certain characteristics of contact between the probe 120 and a surface of a substrate 150. The substrate 150 can be, for example, a steel substrate. The substrate can be part of a fluid cell 130. The fluid cell 130 can also include, for example, a heater 180 for simulating relevant operating temperatures. In accordance with one embodiment of the disclosed subject matter, the heater 180 can simulate operating temperatures between about room temperature and about 250 C. The disclosed methods can also be used at pressures up to 1 GPa.
(16) The fluid cell 130 can further include a lubricant 135. The lubricant 135 can include, for example, engine oil. The lubricant can also include additives such as, for example, Zinc Dialkyldithiophosphate (ZDDP) or nanoparticles.
(17) As further shown in
(18)
(19)
(20) As embodied herein, the spherical probe can be coupled to the cantilever using any coupling technique known in the art including, for example, with epoxy glue. The term spherical, as used herein, is not limited to a mathematical sphere and is intended to cover any probe that is generally spherical in shape. For example, the spherical probe can be spheroid such as an oblate spheroid. In accordance with other embodiments of the disclosed subject matter, the spherical probe can be a cylinder or a hemisphere.
(21) In accordance with an exemplary embodiment, the disclosed subject matter also provides in situ methods for gathering data about contact between a spherical probe and a substrate surface. An example method can include providing a spherical probe. The spherical probe can be coupled to a cantilever. The spherical probe can be, for example, a steel spherical probe. The method can further include providing a substrate having a first surface. The substrate can be, for example, a steel substrate. However, a person skilled in the art will recognize that the disclosed subject matter is not limited to use for steel-on-steel contact and can be used for characterizing the interaction between any material pair. For example, one or both of the probe and the first surface can be silicon, coatings such as diamond or metallic coatings, alloys, ceramics, or polymers.
(22) The method can further include contacting the first surface of the substrate with the spherical probe. For example, the method can include sliding the spherical probe across a sliding zone of the first surface of the substrate. In accordance with embodiments of the disclosed subject matter, contacting the first surface of the substrate with the spherical probe can include contacting the first surface of the substrate with the spherical probe in the presence of a lubricant such as, for example, engine oil. The lubricant can include one or more additives such as, for example, Zinc Dialkyldithiophosphates (ZDDPs), or nanoparticles. A heater can also be provided to simulate various operating temperatures. Temperatures relevant to certain engineering applications can range from about room temperature to about 250 C.
(23) In accordance with the disclosed subject matter, measurements can be taken while the spherical probe is in contact with the first surface. These measurements can include, for purposes of explanation and not limitation, measurements of topography, adhesion, elastic modulus, and conductivity between the spherical probe and the first surface. In accordance with one embodiment, for example, the coefficient of friction can be measured. The measurements can be taken using an atomic force microscope cantilever which carries the spherical probe. The atomic force microscope can include a laser and a photodetector. Known techniques for taking tribological measurements can be used.
(24) In accordance with the disclosed subject matter, the point of contact between the spherical probe and the first surface can be imaged. Imaging can be performed using conventional AFM topographic imaging methods which allow direct observation of the sliding zone during friction measurements, or immediately before and after. Thus, the disclosed subject matter can provide a method for real time, in situ imaging of the contact region while the tribometer is in use. The lateral resolution can depend upon the diameter of the probe (which can vary, for example, between about 1 m and about 100 m) and the surface roughness of the probe. In accordance with embodiments of the disclosed subject matter, the lateral resolution can be, for example, on the range of a few tens of nanometers.
(25) In accordance with embodiments of the disclosed subject matter, the spherical probe can be removed and a sharp AFM probe can be used to perform high resolution imaging and characterization of the sliding zone.
(26) In one aspect of the disclosed subject matter, an in situ tribological technique is provided. The in situ technique can allow investigation of a large variety of materials surfaces in multi-asperity geometry. A method or in situ measurement of tribological properties can include simultaneous measurement of the coefficient of friction during sliding in multi-asperity geometry and topographic imagining of the sliding interface with nanometer resolution. The technique can be used for a variety of materials, including technologically important materials such as steel, silicon, and diamond-like carbon (DLC). The techniques can be used, for example, for design of automotive engine components which are typically made of steel or DLC-coated surfaces. The sliding zone can be accessible for further in situ characterization of the morphology or mechanical properties with high spatial resolution, e.g., by using known nanometer sharp AFM probes. Other material imaging and characterization methods can also be used for ex situ characterization of the sliding zone.
EXAMPLE
(27) An example of the disclosed subject matter is provided herein for purpose of illustration, and not limitation.
(28) Steel substrates (52100 steel), heat treated to achieve 60 Rockwell C scale hardness (Heckel Tools & Mfg. Corp., Eagle, Wis., USA) were mirror polished using silicon carbide polishing paper discs (180, 240, and 320 Grit), followed by polishing on a Rayon polishing cloth using micro diamond suspension (South Bay Technologies, San Clemente, Calif.). Commercial silicon cantilevers (PPP-NCH, Nanosensors, Neuchatel, Switzerland) used in these measurements were first calibrated for their normal and lateral spring constants using the Sader method. The steel probes were prepared by gluing steel microspheres (SHS 7574 HVOF, The NanoSteel Co., Rhode Island, USA) on calibrated cantilevers using an inverted optical microscope (Alessi REL-4100A, Redwood City, Calif., USA) by first applying a small quantity of a two-part epoxy (J-B Weld, Sulphur Springs, Tex., USA) using a sharp tungsten wire (TGW0325, World Precision Instruments, Sarasota, Fla., USA) and then placing the bead using a strand of hair. The cantilevers were stored overnight in a dry, N.sub.2 purged box to allow the epoxy to fully cure. The diameters of the microspheres attached to the cantilevers were estimated either from optical imaging (Olympus BX51) or using field emission scanning electron microscopy (SEM, JOEL 7500F) as shown in
(29) The normal and lateral spring constants were corrected after gluing the bead, which results in a variation in the effective length of the cantilever (distance between the base of the cantilever to the center of the glued bead) as well as the tip height. Testing was performed using a commercial atomic force microscope (Keysight 5500, Keysight Technologies, Santa Clara Calif., USA), equipped with a sample heating plate, liquid cell and a temperature controller (Model 321, Lake Shore Cryotronics Inc., Westerville, Ohio, USA) as shown in the schematic (
(30) Steel probes mounted on AFM cantilevers were used to measure the coefficient of friction for lubricated steel-on-steel contacts. The calibration of the lateral force sensitivity of the steel probe cantilever can be calibrated based on friction loops, obtained by measuring the lateral deflection signal of the cantilever during the forward and reverse sliding directions.
(31) Next, the steel probe was used to image the topography of the substrate surface as well as perform simultaneous friction measurements. The morphology of the steel substrate can be substantially equally well-resolved using a sharp AFM probe and using a steel probe, enabled by the nanometer roughness of the steel probe, i.e., the asperity which protrudes more compared to the others can contribute most to the topographic image. The nanoscale roughness of the steel probe can be directly imaged using a sharp AFM probe by optically aligning the AFM cantilever with sharp tip right above the steel probe surface. The ability to easily perform high resolution direct imaging of the steel probe surface can also enable measurement of any wear occurring on the steel probe, within the contact zone.
(32) Coefficient of friction measurements were performed under PAO containing 1 wt % ZDDP in four different regions and the morphology of the substrate surface was continuously monitored. The normal load of 12.32 N was used which corresponds to a mean Hertzian pressure of 0.2 GPa. Sliding speed of 100 m/s was used and the tests were performed at room temperature. Coefficient of friction is plotted for measurements performed at room temperature as well as at elevated temperatures (
(33) The presently disclosed subject matter is not to be limited in scope by the specific embodiments herein. Indeed, various modifications of the disclosed subject matter in addition to those described herein will become apparent to those skilled in the art from the foregoing description and the accompanying figures. Such modifications are intended to fall within the scope of the appended claims.