ALUMINOTHERMIC WELDING OF PIPES
20200368844 ยท 2020-11-26
Inventors
Cpc classification
B23K2103/20
PERFORMING OPERATIONS; TRANSPORTING
International classification
Abstract
An aluminothermic welding device for and a method of welding together of first and second pipe members (10, 12) are described. A sleeve (30) is configured to cover both pipe members (10, 12) and to form a cavity (33) surrounding said pipe members (10, 12) when it is in a welding position. A crucible (50) is also provided, wherein a drain channel (44) is connected to a second opening in a wall of said sleeve (30), in an upper part of said sleeve (30) when said sleeve is in said welding position. Said second opening is configured to drain gases and dross from said cavity (33). There is further an input channel (54) between said crucible (50) and said cavity (33), wherein said input channel (54) enters into said cavity (33) through a first opening in a wall of said sleeve (30) in a lower part of said sleeve (30), when said sleeve (30) is in said welding position.
Claims
1. A method for aluminothermic welding together of first and second pipe members, comprising the steps of; arranging a sleeve (30) in a welding position where it covers both said pipe members (10, 12) and forms a cavity surrounding said pipe members, arranging an input channel between a crucible and said cavity, wherein said input channel enters into said cavity through a first opening in a wall of said sleeve in a lower part of said sleeve when said sleeve is in said welding position, providing an exothermic mixture in said crucible, igniting said exothermic mixture to create a melt of said exothermic material, allowing said melt to flow down said input channel, through said first opening before it continues to flow up through said cavity on both sides of said pipe members, until said cavity is filled up with said melt, draining gases through a second opening in a wall of said sleeve in an upper part of said sleeve, when said sleeve is in said welding position.
2. The method of claim 1, comprising the step of arranging said crucible above said cavity when said sleeve is in said welding position.
3. The method of claim 1, comprising the step of pre-heating said first and second pipe members before igniting said exothermic mixture.
4. The method of claim 1, comprising the step of; cooling said melt to establish a solid weld joint.
5. The method of claim 4 comprising the step of; controlling a temperature of said melt to allow oxidation products being separated from the melt to flow upwards through said second opening ( ).
6. The method of claim 5, comprising the step of; circulating cooling fluid inside a cooling mantle surrounding said sleeve.
7. The method according to claim 1, comprising the step of; extracting said oxidation products through a drain channel.
8. The method according to claim 1, comprising the step of; creating said melt comprised of iron and alumina by creating an exothermic reaction from a transformation of said exothermic mixture comprising iron oxide and aluminum.
9. The method according to claim 1, wherein said exothermic mixture comprises iron powder or iron particles.
10. An aluminothermic welding device for welding together of first and second pipe members comprising; a sleeve configured to cover both pipe members and to form a cavity surrounding said pipe members when it is in a welding position, a crucible, a drain channel connected to a second opening in a wall of said sleeve (30), in an upper part of said sleeve when said sleeve is in said welding position, wherein said second opening is configured to drain gases from said cavity, and an input channel between said crucible and said cavity, wherein said input channel enters into said cavity through a first opening in a wall of said sleeve in a lower part of said sleeve when said sleeve is in said welding position.
11. The welding device of claim 10, wherein said crucible is arranged above said cavity when said sleeve is in said welding position.
12. The welding device of claim 10 above, wherein at least a portion of said input channel is arranged inside said wall of said sleeve between an upper part of said sleeve and said first opening.
13. The welding device of claim 10, wherein an inner surface of said sleeve has a groove forming an outer wall of said cavity.
14. The welding device of claim 10, wherein said pipe members have tapered ends, configured towards and adjacent each other forming an inner wall of said cavity.
15. The welding device of claim 10, wherein said sleeve has a circular inner cross section and said cavity is annular.
16. The welding device of claim 10, comprising a support ring configured to be arranged inside said first pipe member before welding.
17. The welding device of claim 10, comprising and forming a cooling cavity between said cooling mantle and said sleeve and forming a cooling cavity between said cooling mantle and said sleeve.
Description
BRIEF DESCRIPTION OF THE DRAWINGS
[0028]
[0029]
[0030]
[0031]
EMBODIMENTS OF THE INVENTION
[0032] In the following description, various examples and embodiments of the invention are set forth in order to provide the skilled person with a more thorough understanding of the invention. The specific details described in the context of the various embodiments and with reference to the attached drawings are not intended to be construed as limitations. Rather, the scope of the invention is defined in the appended claims.
[0033] The invention is in the following described in relation to joining two pipes or pipe members, such as a pipe and a pipe flange. The invention may be applied to metal parts in general which are to be joined.
[0034] An embodiment of an aluminothermic welding device according to the invention is illustrated in
[0035] When the welding device is used for welding, it should be aligned properly to ensure the best result. For the remainder of the document, the device is defined to be in a welding position when it is aligned for welding.
[0036] One such welding position can be the one illustrated in
[0037] One of the main components of the welding device is the sleeve (30), which is configured to cover both pipe members (10, 12) and to form a cavity (33) surrounding the pipe members (10, 12) when it is in a welding position. The inside of the sleeve (30) fits tightly to pipe surfaces (11, 13), which can be provided by known means with different tightening means. The sleeve (30) can e.g. be in two parts and rotate about a hinge, where the free ends are moved towards each other and joined and tightened by means of screw connections or similarly such that the inside of the sleeve (30) is tightly fitted to the pipe surfaces (11, 13).
[0038] The welding device also comprises a crucible (50), where the exothermic reaction can be carried out. The crucible is adapted to melting substances of high temperatures according to prior art as described previously.
[0039] Further, the welding device comprises an input channel (54) connected to the crucible (54) where melt can flow into the cavity (33) and a drain channel (44) where resulting gases and dross can be drained or extracted from the cavity (33).
[0040] The drain channel (44) is connected to a second opening (45) in a wall of the sleeve (30), in an upper part of the sleeve (30), and the input channel (54) is arranged between the crucible (50) and the cavity (33), wherein the input channel (54) enters into the cavity (33) through a first opening (35) in a wall of the sleeve (30) in a lower part of the sleeve (30) when the sleeve is in the welding position.
[0041] In an embodiment the first opening (35) is arranged at the top of said cavity (33). In an embodiment the second opening (45) is arranged in at the bottom of said cavity (33).
[0042] In an embodiment the first and/or second opening (35, 45) are arranged along a vertical line through a center of said sleeve (35).
[0043] In an embodiment, the crucible (50) is arranged above the cavity (33) when the sleeve (30) is in the welding position.
[0044] In an embodiment, at least a portion of the input channel (54) runs inside the wall of the sleeve (30) between an upper part of the sleeve and the first opening ( ). The sleeve (30) may be seen as a mold for the welding where the first opening (35) and the input channel (54) constitute a single channel running inside the mold.
[0045] In an embodiment, an inner surface of the sleeve (30) has a groove (32) forming an outer wall of the cavity (33).
[0046] In an embodiment, the pipe members (10, 12) have tapered ends, configured towards and adjacent each other forming an inner wall of the cavity (33).
[0047] The groove (32) in the sleeve (30) can in an embodiment be combined with the tapered ends of the pipe member s (10, 12). The groove (32) together with the slot defined by the tapered ends forms a surrounding drop shaped volume, i.e. the cavity (33), which is to be filled with melted welding material.
[0048] In an embodiment, the sleeve (30) has a circular inner cross section and the cavity (33) is annular.
[0049] In an embodiment, the welding device comprises a support ring (38) configured to be arranged inside the first pipe member (10) before welding. The support ring prevents melt to enter into the inner diameter between the two adjacent pipe members (10, 12).
[0050] In an embodiment, the welding device comprises a cooling mantle as illustrated in
[0051] The cooling mantle (60) is arranged about the sleeve (30) and forms a cooling cavity (66) between the cooling mantle (60) and the sleeve (30). In a further detailed embodiment the end portions of the mantle (60) is closely fitted to the surface (11, 13) of the pipes (10, 12) by means of suitable packings marked as (63) and (65).
[0052] The cooling mantle can be made of different tyoes of materials. In an embodiment, the cooling mantle (60) is made of steel.
[0053] An inlet is illustrated as pipe socket (61), and a corresponding outlet is shown as pipe socket (62). The roof or wall portions of the cooling mantle (60) comprise openings for the crucible (50) and the drain channel (44).
[0054] An annealing fluid such as a gas or a liquid can, in ways known in the art, be supplied to the cooling cavity (66) through pipe socket (61), flow through the cooling cavity (66) and further be exhausted through outlet (62).
[0055] Although the previous embodiments have been illustrated with pipes, one or both of the pipe members (10, 12) may also be pipe flanges (70) as illustrated in
[0056] Depending on the specific pipe flange, the cooling mantel may have to be adapted, as will be understood by a person skilled in the art.
[0057] Embodiments of the welding method according to the invention will be described with reference to
[0058] As previously noted the invention is also a method for aluminothermic welding together of first and second pipe members (10, 12).
[0059] One step to be performed, is to arrange the input channel (54) between a crucible (50) and the cavity (33), such that the input channel (54) enters into the cavity (33) through a first opening (35) in a wall of the sleeve (30) in a lower part of the sleeve (30) when the sleeve is in the welding position. Please see above for definition of welding position. The first opening (35) is allows melt from the crucible (50) to be in fluid communication with the cavity (33) via the input channel (54).
[0060] The crucible (50) is filled with an exothermic mixture, such as a thermite mixture. The exothermic mixture is ignited, or inflamed to create a melt (36), which can now flow freely down the input channel (54), through the first opening (35) before it continues to flow up through the cavity on both sides of the pipe members (10, 12), until the cavity (33) is filled up with the melt (36).
[0061] At the same time the oxidation product is secreted as a solid dross floating upwards to the top of the cavity (33). This is due to iron in a liquid state has a higher density than the oxides and will sink, while the oxide phase and dross phase will float. This dross phase will float to the top and be diverted together with the gas which also could be released by the exothermic conversion draining gases and dross, out of a second opening (45) in a wall of the sleeve (30) in an upper part of the sleeve (30).
[0062] The purpose of the second opening (45) is that a need for ventilation of gases/dross immediately arises when the exothermic reaction takes place, and melt flows up in the cavity (33). As gases released from the melt leads to a certain pressure increase, it is important that such gas can freely escape through the second opening (45). The removal of gases and dross has been optimized in the device and method according to the invention, where the melt enters the lower part of the cavity (33). Gases and dross will therefore escape easily upwards inside the cavity (33) and through the second opening (45). The result is a welding joint with less volumetric failures than prior art.
[0063] As part of the process the sleeve (30) should be arranged in the welding position. This should be done before igniting the exothermic mixture, such that the melt flows properly through the channels and a high-quality weld can be achieved.
[0064] Pre-heating can be used to further improve the quality of the weld. In an embodiment the method comprises pre-heating the first and second pipe members (10, 12) before igniting said exothermic mixture.
[0065] In an embodiment the pipe members (10, 12) are heated to about 700 degree Celsius.
[0066] This can be achieved by various means. In its simplest form the pipe members (10, 12) may be pre-heated directly before arranging them in the sleeve (30) by heat from e.g. a gas burner, electric heater or chemical heater.
[0067] It can also be achieved by heating the pipe members (10, 12) after they have been arranged in the sleeve by e.g. blowing a gas flame from a gas burner into the sleeve (30), or using an electric or chemical heat element to pre-heat the form.
[0068] In an embodiment, the method comprises the step of arranging the crucible (50) above the cavity (33) when the sleeve (30) is in the welding position.
[0069] In this part of the process, it is important to control that the temperature does not drop too fast, such that the dross phase and gases is allowed to float completely to allow upwards through the second opening (45). These substances can be removed before the viscosity of the melt is too high, and the melt solidifies. Voids in the weld joint, generated due to impurities such as oxides/dross and/or gases, should be avoided as far as possible.
[0070] In an embodiment the method comprises the step of cooling the melt (36) to establish a solid weld joint.
[0071] Temperature control could in an embodiment be carried out by adding hot fluid, e.g. hot gases in circulation through cooling cavity (66), and then controlling the temperature drop in the melt joint via the temperature in the mantle gas. As a coolant for circulation in the cooling cavity (66), water or other liquid/gas could be utilized, if the temperature at the inlet is adapted to the temperature in the joining area.
[0072] Before the cooling mantle (60) has mounted to the pipes (10, 12), alternatively before the melting process has been initialized, the pipe ends are in an embodiment pre-heated up to the temperature at which the melt flows from the crucible (50), and then the temperature is brought to drop in a controlled manner.
[0073] In an embodiment, the method comprises the steps of extracting the oxidation products through a drain channel (44). An external drain pump connected to the drain channel (44) may be used to improve extraction.
[0074] In an embodiment, the method comprises the step of creating the melt comprised of iron and alumina by creating an exothermic reaction from a transformation of the exothermic mixture comprising iron oxide and aluminum.
[0075] In an embodiment, the exothermic mixture comprises iron powder or iron particles. However, other metals or mixture of metals may also be used in other embodiments to weld alloys, such as e.g. Chromium, Nickel and Molybdenum.
[0076] When the welding joint has cooled down, the cooling mantle (60) and sleeve (30) are removed, upon which the joint can be treated by grinding, polishing or other suitable processing in order to form an even and smooth joint. Alternatively, the sleeve (30) could form part of the pipe joint and be left welded in place.
[0077] In the exemplary embodiments, various features and details are shown in combination. The fact that several features are described with respect to a particular example should not be construed as implying that those features by necessity have to be included together in all embodiments of the invention. Conversely, features that are described with reference to different embodiments should not be construed as mutually exclusive. As those with skill in the art will readily understand, embodiments that incorporate any subset of features described herein and that are not expressly interdependent have been contemplated by the inventor and are part of the intended disclosure. However, explicit description of all such embodiments would not contribute to the understanding of the principles of the invention, and consequently some permutations of features have been omitted for the sake of simplicity or brevity.