Method for Manufacturing Fibrous Paper-plastic Disc-shaped Product
20200094509 ยท 2020-03-26
Inventors
Cpc classification
B31B50/742
PERFORMING OPERATIONS; TRANSPORTING
B31B50/59
PERFORMING OPERATIONS; TRANSPORTING
International classification
B31B50/59
PERFORMING OPERATIONS; TRANSPORTING
Abstract
In a method for manufacturing a fibrous paper-plastic disc-shaped product, a pulp sheet is prepared, sent to a cutting machine, and cut into a primitive sheet. The primitive sheet is formed by at least one primitive material for manufacturing a desired fibrous product and has a surface coated with a solution containing an additive. The primitive sheet is set still to achieve an osmotic balance inside the primitive sheet, and passed through a hot-press machine for hot pressing to press and dry the primitive sheet into a dry molded plate. Each primitive material of the original primitive sheet is pressed into a shape of the desired fibrous product to form a dry molded product. Finally, the dry molded plate is sent to a trimming machine for trimming and cutting, so that each dry molded product on the dry molded plate is formed into the fibrous product.
Claims
1. A method for manufacturing a fibrous paper-plastic disc-shaped product, comprising the steps of: (1) conveying a flat flaky pulp sheet to a cutting machine to cut the pulp sheet into a primitive sheet, wherein the primitive sheet is formed by at least one primitive material for manufacturing a desired fibrous product; (2) coating a solution containing an additive onto a surface of the primitive sheet; (3) sending the primitive sheet processed with the coating to a hot-press machine, and heating and pressurizing the primitive sheet by the hot-press machine, so that the primitive sheet is pressed and dried into a dry molded plate, and each original primitive material is pressed into a shape of the desired fibrous product to form a dry molded product; and (4) sending the dry molded plate to a trimming machine for trimming and cutting the dry molded plate according to the size of the fibrous product, so as to form the fibrous product from the original dry molded product.
2. The method for manufacturing a fibrous paper-plastic disc-shaped product according to claim 1, wherein the primitive sheet processed with the coating is set still, so that the solution received by the primitive sheet is further mixed and permeated into the primitive sheet uniformly to achieve an osmotic balance effect, and then the primitive sheet processed with the static balance is sent to the hot-press machine.
3. The method for manufacturing a fibrous paper-plastic disc-shaped product according to claim 1, wherein the pulp sheet is conveyed by a first conveyor, so that the pulp sheets are entered into the cutting machine sequentially.
4. The method for manufacturing a fibrous paper-plastic disc-shaped product according to claim 1, wherein the primitive sheet processed with the coating is conveyed by a second conveyor.
Description
BRIEF DESCRIPTION OF THE DRAWINGS
[0031]
[0032]
[0033]
[0034]
[0035]
[0036]
[0037]
[0038]
[0039]
DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0040] The technical characteristics, contents, advantages and effects of the present invention will be apparent with the detailed description of a preferred embodiment accompanied with related drawings as follows.
[0041] The present invention discloses a method for manufacturing a fibrous paper-plastic disc-shaped product, particularly the manufacturing applicable for manufacturing a fibrous product with a relatively large side-skewed angle and a relatively small (or shallow) depth. The fibrous product with a relatively large side-skewed angle and a relatively small (or shallow) depth refers to something like a shallow plate which is a typical example for the large side-skewed angle and small (or shallow) depth, and the fibrous product refers to a finished product made of a raw material formed by mixing paper pulp fiber materials and/or plant fiber material and manufactured by the manufacturing method of the present invention, wherein such product is the fibrous paper-plastic disc-shaped product of the present invention. Since the manufacturing method of the present invention does not use the suction setting technology, therefore the product is also called a fibrous product or fibrous paper-plastic disc-shaped product to be distinguished from the plastic product and molded product. Before the manufacture, the present invention prepares a material by using a pulp sheet as an initial material. The pulp sheet refers to a raw material formed by mixing paper pulp fiber materials and/or plant fiber materials and going through the manufacturing and consolidation processes to form a flat pulp sheet with a specific area to facilitate the storage and transportation. When the pulp sheet is solidified, the dimensions (including the length, width, and height) of the pulp sheet may be selected. Since the pulp sheet is used as a further manufacturing material, therefore it is not completely dry when being solidified, but the pulp sheet is a material with a relatively low wetness.
[0042] With reference to
[0043] In
[0044] The primitive sheet 4 is sent to a second conveyor 5 and moved forward. During the process, a solution containing an additive is coated onto a surface of the primitive sheet 4 as shown in
[0045] The primitive sheet 4 processed with the coating operation may be sent to a standing stable 62 and set still, so that the solution received by each primitive sheet 4 can be further permeated into the interior uniformly to achieve an osmotic balance effect, wherein the standing time of the primitive sheet 4 depends on the size of the object, and the primitive sheets 4 may stand still in a scattered flat fashion (if the space allows) or a stacked manner (if the space is insufficient for the scattered flat fashion), and the step of such static balance may be carried out selectively, and the details will be described below.
[0046] In
[0047] The dry molded plate 8 is sent to a trimming machine 9, and the remaining material of each dry molded product 81 is trimmed and cut. In other words, the remaining material is removed according to the external periphery or length and width of the desired fibrous product, so that the original dry molded products 81 are formed into independent fibrous products 10 (such as the shallow plates) one by one as shown in
[0048] In the aforementioned manufacturing procedure of the present invention, if the final fibrous product is a thin object, the solution may reach the osmotic balance easily and quickly after the roll-pressing process, so that the static balance system as shown in
[0049] In the aforementioned procedure of the manufacturing method of the present invention, the automated delivery of the pulp sheets 1 to the cutting machine 3 may be completed by the first conveyor 2. In other words, the pulp sheets 1 are manually sent to the cutting machine 3 one by one to complete the same action. Similarly, the primitive sheets 4 processed by the automated delivery of coating (such as being sprayed by the spraying machine 6) may be completed by the second conveyor 5. In other words, the primitive sheets 4 are manually sent one by one to complete the same action. Of course, if it is necessary to move the primitive sheets 4 to the standing stable 62 after the primitive sheets 4 are coated, then the removal may be completed manually or automatically (by a machine). Finally, the action of sending the primitive sheets 4 processed by pressing or static balance to the hot-press machine 7 may be completed manually or automatically (by a machine).
[0050] In view of the description above, the present invention skips the preparation of the conventional pulping system and directly carries out the work of the molding system, the static balance system and the trimming system. In the working process of the molding system, the operation of suction plastic molding is no longer needed, and the materials are directly spread out, cut and coated, and then a hot-press operation is carried out after the static balance, and finally the trimming operation is carried out to produce the expected fibrous product of the present invention. The manufactured is definitely very convenient.
[0051] Compared with the conventional method for manufacturing a molded product, the present invention has the following advantages regardless of including or excluding the procedure of the static balance system.
[0052] Saving equipment costs: The whole process of the method for manufacturing a fibrous paper-plastic disc-shaped product in accordance with the present invention simply comprises the steps of conveying the pulp sheets, cutting the pulp sheets into primitive sheets, coating a solution containing an additive, directly hot-press molding, and trimming the edges, so that the invention omits the conveying pipeline, vacuum system and equipment, suction pipeline, pulp beater, pulper, pulp preparer, slurry tank, transfer pump and valve required by the conventional method for manufacturing a molded product and lowers the mold cost, so that both equipment and manufacturing costs can be reduced significantly.
[0053] Saving energy: The method for manufacturing a fibrous paper-plastic disc-shaped product of the present invention directly uses the pulp sheets as the manufacturing material, and directly enters into the hot-press process without requiring the preparation of a complicated pulping system or the operation of suction molding operation, so that as to save the operation costs for beating, refining, pulping, and different manufacturing operations from the slurry tank to the suction tank and fluid delivery. During the process of the hot-press machine of the present invention, the requirement for dry humidity is not too strict, and the main effect resides on heating and pressing the primitive sheets into the dry molded plates, so that the heating time is not too long (generally falling within a range of 515 seconds depending on the size of the product), so that the power consumption can be reduced significantly. In general, the power consumption of the present invention is approximately one-tenth of that of the conventional method for manufacturing a molded product.
[0054] Saving equipment installation space: The method for manufacturing a fibrous paper-plastic disc-shaped product of the present invention directly uses the procedure of cutting the material and the coating operation to replace the conventional complicated pulping and suction molding processes, so as to save a huge pulping system installation area (including the installation areas of a conveying pipeline, a vacuum system, a beater, a pulper, a pulping pool, a slurry tank, etc.). As a result, the installation space of the whole production line can be reduced significantly.
[0055] Having environmental advantages: The method for manufacturing a fibrous paper-plastic disc-shaped product of the present invention requires no pulping system, slurry conveying loop pipeline, etc. in the manufacturing process, so that there is no environmental issue of producing or processing wastewater at all. Shortening working hour and improving production capacity significantly: In the manufacturing process of the method for manufacturing a fibrous paper-plastic disc-shaped product of the present invention, the hot-press machine has the features of fast hot-press molding and short working hour, so that the production cycle is much less than that of the conventional method for manufacturing a molded product. Therefore, the present invention can produce more products within the same time. The production capacity is increased, the production cycle is shortened, the productivity is improved, and the production cost is lowered significantly.
[0056] Improving the quality and strength of the product: The method for manufacturing a fibrous paper-plastic disc-shaped product of the present invention directly uses the pulp sheets as the manufacturing material without adding other fillers, so that the finished product has a higher fiber density, a better quality, a greater strength per unit product where are more than twice of the conventional method for manufacturing the molded product.
[0057] In summation of the above description, the present invention herein enhances the performance than the conventional structure and further complies with the patent application requirements and is submitted for patent application. While the invention has been described by means of specific embodiments, numerous modifications and variations could be made thereto by those skilled in the art without departing from the scope and spirit of the invention set forth in the claims.