SECONDARY BATTERY AND BATTERY PACK INCLUDING THE SAME

20220416341 · 2022-12-29

Assignee

Inventors

Cpc classification

International classification

Abstract

A secondary battery includes an electrode assembly, a battery case surrounding the electrode assembly, and a sealing member located between the electrode assembly and the battery case. The sealing member includes polymer particles that are configured to expand in all directions.

Claims

1. A secondary battery comprising: an electrode assembly, a battery case surrounding the electrode assembly, and a sealing member located between the electrode assembly and the battery case, wherein the sealing member includes polymer particles that are expandable in all directions.

2. The secondary battery according to claim 1, wherein the sealing member includes an adhesive layer, and wherein the polymer particles are located on the adhesive layer.

3. The secondary battery according to claim 2, wherein the polymer particles are configured to absorb an electrolyte solution to expand in all directions.

4. The secondary battery according to claim 3, wherein the adhesive layer contacts the electrode assembly.

5. The secondary battery according to claim 3, wherein the polymer particles include a super absorbent polymer.

6. The secondary battery according to claim 2, wherein the polymer particles are mixed with a polyurethane material or a polyacrylate material to form a film layer.

7. The secondary battery according to claim 6, wherein the film layer is configured to expand in a surface direction of the adhesive layer and a direction perpendicular to the surface direction.

8. The secondary battery according to claim 1, wherein the sealing member is configured to fill a gap between the electrode assembly and the battery case.

9. The secondary battery according to claim 1, wherein the sealing member is provided as a plurality of sub-sealing members separated from each other.

10. The secondary battery according to claim 1, wherein the battery case is cylindrical.

11. A battery pack comprising the battery secondary battery according to claim 1.

Description

BRIEF DESCRIPTION OF THE DRAWINGS

[0022] FIG. 1 is a cross-sectional perspective view of a secondary battery according to one embodiment of the present disclosure.

[0023] FIG. 2 is a perspective view illustrating a wound state of the electrode assembly of the secondary battery of FIG. 1.

[0024] FIG. 3 is a cross-sectional view illustrating a sealing member attached to the electrode assembly of the secondary battery of FIG. 2.

[0025] FIG. 4 is a cross-sectional view illustrating a sealing member according to a comparative example.

[0026] FIG. 5 is a perspective view illustrating a wound state of the electrode assembly of a secondary battery according to another exemplary embodiment of the present disclosure.

DETAILED DESCRIPTION OF THE EMBODIMENTS

[0027] Hereinafter, various embodiments of the present disclosure will be described in detail with reference to the accompanying drawings so that those skilled in the art can easily implement them. The present disclosure may be modified in various different ways, and is not limited to the embodiments set forth herein.

[0028] Portions that are irrelevant to the description will be omitted to clearly describe the present disclosure, and like reference numerals designate like elements throughout the specification.

[0029] Further, in the figures, the size and thickness of each element are arbitrarily illustrated for convenience of description, and the present disclosure is not necessarily limited to those illustrated in the figures. In the figures, the thickness of layers, regions, etc. are exaggerated for clarity. In the figures, for convenience of description, the thicknesses of some layers and regions are shown to be exaggerated.

[0030] In addition, it will be understood that when an element such as a layer, film, region, or plate is referred to as being “on” or “above” another element, it can be directly on the other element or intervening elements may also be present. In contrast, when an element is referred to as being “directly on” another element, it means that other intervening elements are not present. Further, the word “on” or “above” means disposed on or below a reference portion, and does not necessarily mean being disposed on the upper end of the reference portion toward the opposite direction of gravity.

[0031] Further, throughout the specification, when a portion is referred to as “including” a certain component, it means that the portion can further include other components, without excluding the other components, unless otherwise stated.

[0032] Further, throughout the specification, when referred to as “planar”, it means when a target portion is viewed from the upper side, and when referred to as “cross-sectional”, it means when a target portion is viewed from the side of a cross section cut vertically.

[0033] FIG. 1 is a cross-sectional perspective view of a secondary battery 100 according to one embodiment of the present disclosure.

[0034] Referring to FIG. 1, the secondary battery 100 according to the present embodiment includes a jelly-roll type electrode assembly 120, a top insulator 160 located at the top of the electrode assembly 120 and a bottom insulator 170 located at the bottom of the electrode assembly 120.

[0035] The electrode assembly 120 has a jelly-roll type structure in which a cathode 121 and an anode 123 is wound with a separator 122 interposed therebetween, and a center pin 150 may be inserted in the central part thereof

[0036] The secondary battery 100 according to the embodiment of the present disclosure can be formed by housing the electrode assembly 120 in a battery case 130, injecting an electrolyte solution into the battery case 130, and then connecting a cap assembly 140 to the top of the battery case 130. In this embodiment, the battery case 130 may be cylindrical.

[0037] At this time, the battery case 130 may include a beading part 132 and a crimping part 133. The beading part 132 refers to a part in which a part of the battery case 130 is recessed in the central direction of the electrode assembly 120, which is for stable coupling of the cap assembly 140 and preventing the flow of the electrode assembly 120. The crimping part 133 is located above the beading part 132 and refers to a part surrounding the cap assembly 140, which is for stable coupling of the cap assembly 140.

[0038] The cap assembly 140 may include a top cap 141 forming a cathode terminal, a cap plate 142 to which the cathode tab 144 extending upward from the electrode assembly 120 is connected, and an airtight gasket 143.

[0039] The gasket 143 is mounted on the upper inner surfaces of the crimping part 133 and the beading part 132, thereby increasing a sealing force between the cap assembly 140 and the battery case 130.

[0040] As described above, the cathode tab 144 may be extended upward from the electrode assembly 120. Specifically, it may be extended from the cathode 121 of the electrode assembly 120.

[0041] The cathode tab 144 is connected to a cap plate 142, so that a top cap 141 can operate as a cathode terminal. An opening 161 is formed in a top insulator 160, and the cathode tab 144 can pass through the opening 161 to be connected to the cap plate 142.

[0042] The center pin 150 generally includes a metallic material to impart a predetermined strength, and is formed in a cylindrical structure in which a plate material is bent into a round shape. In addition to self-heating, the center pin 150 can function as a passage for fixing and supporting the electrode assembly 120 and releasing gas generated by an internal reaction during charging/discharging and operation.

[0043] On the other hand, the electrolyte solution injected into the battery case 130 may be a lithium salt-containing non-aqueous electrolyte solution, and the lithium salt-containing non-aqueous electrolyte solution is composed of a non-aqueous electrolyte solution and a lithium salt. The non-aqueous electrolyte used herein includes a non-aqueous organic solvent, an organic solid electrolyte, an inorganic solid electrolyte, or the like, but is not limited thereto.

[0044] As examples of the non-aqueous electrolyte, mention may be made of non-protic organic solvents, such as N-methyl-2-pyrollidinone, propylene carbonate, ethylene carbonate, butylene carbonate, dimethyl carbonate, diethyl carbonate, gamma-butyro lactone, 1,2-dimethoxy ethane, tetrahydroxyfuran, 2-methyl tetrahydrofuran, dimethylsulfoxide, 1,3-dioxolane, formamide, dimethylformamide, dioxolane, acetonitrile, nitromethane, methyl formate, methyl acetate, phosphoric acid triester, trimethoxy methane, dioxolane derivatives, sulfolane, methyl sulfolane, 1,3-dimethyl-2-imidazolidinone, propylene carbonate derivatives, tetrahydrofuran derivatives, ether, methyl propionate, and ethyl propionate.

[0045] Examples of the organic solid electrolyte include polyethylene derivatives, polyethylene oxide derivatives, polypropylene oxide derivatives, phosphoric acid ester polymers, polyalginate lysine, polyester sulfide, polyvinyl alcohols, polyvinylidene fluoride, and polymers containing ionic dissociation groups.

[0046] Examples of the inorganic solid electrolyte include nitrides, halides and sulfates of lithium (Li) such as Li.sub.3N, LiI, Li.sub.5NI.sub.2, Li.sub.3N—LiI—LiOH, LiSiO.sub.4, LiSiO.sub.4—LiI—LiOH, Li.sub.2SiS.sub.3, Li.sub.4SiO.sub.4, Li.sub.4SiO.sub.4—LiI—LiOH, Li.sub.3PO.sub.4—Li.sub.2S—SiS.sub.2.

[0047] The lithium salt is a material that is readily soluble in the above-mentioned non-aqueous electrolyte. The lithium salt may include, for example, LiCl, LiBr, LiI, LiC1O.sub.4, LiBF.sub.4, LiB.sub.10Cl.sub.10, LiPF.sub.6, LiCF.sub.3SO.sub.3, LiCF.sub.3CO.sub.2, LiAsF.sub.6, LiSbF.sub.6, LiAlCl.sub.4, CH.sub.3SO.sub.3Li, CF.sub.3SO.sub.3Li, (CF.sub.3SO.sub.2).sub.2NLi, chloroborane lithium, lower aliphatic carboxylic acid lithium, lithium tetraphenyl borate, and imide.

[0048] In addition, in order to improve charge/discharge characteristics and flame retardancy, the non-aqueous electrolyte may further include, for example, pyridine, triethylphosphite, triethanolamine, cyclic ether, ethylenediamine, n-glyme, hexaphosphoric triamide, nitrobenzene derivatives, sulfur, quinone imine dyes, N-substituted oxazolidinone, N,N-substituted imidazolidine, ethylene glycol dialkyl ether, ammonium salts, pyrrole, 2-methoxy ethanol, aluminum trichloride, or the like. In some cases, in order to impart incombustibility, the electrolyte may further include halogen-containing solvents, such as carbon tetrachloride and ethylene trifluoride. Furthermore, in order to improve high-temperature retention characteristics, the electrolyte may further include carbon dioxide gas. In addition, it may further include fluoro-ethylene carbonate (FEC), propene sultone (PRS), and the like.

[0049] In one specific example, lithium salts such as LiPF.sub.6, LiClO.sub.4, LiBF.sub.4 and LiN(SO.sub.2CF.sub.3).sub.2 are added to a mixed solvent of a cyclic carbonate of EC or PC as a highly dielectric solvent and a linear carbonate of DEC, DMC or EMC as a low-viscosity solvent to prepare a lithium salt-containing non-aqueous electrolyte.

[0050] FIG. 2 is a perspective view illustrating a wound state of the electrode assembly of the secondary battery of FIG. 1.

[0051] Referring to FIG. 2, the secondary battery according to one embodiment of the present disclosure includes a sealing member 230 that is located on an outer peripheral surface of an electrode assembly 120 including a cathode 121, an anode 123, and a separator 122. The sealing member 230 is located between the electrode assembly 120 and the battery case 130. The sealing member 230 according to the present embodiment includes swollen polymer particles that expand in all directions.

[0052] The sealing member 230 in FIG. 2 is illustrated in a form that is located separately from the top and bottom of the outer peripheral surface of the electrode assembly 120, but this is for convenience of description, and may be located so as to surround the entire outer peripheral surface of the electrode assembly 120.

[0053] The electrode assembly 120 may have electrode tabs 144 and 164 that are located between at least a part of the sealing member 230 and an outer peripheral surface of the electrode assembly 120.

[0054] The electrode tabs 144 and 164 include an anode tab 164 attached to an anode 123 and a cathode tab 144 attached to a cathode 121. In FIG. 2, the anode tab 164 is attached to the outer peripheral surface of the electrode assembly 120 so that the anode tab 164 is located between at least a part of the sealing member 230 and the outer peripheral surface of the electrode assembly 120, and the cathode tab 144 is shown to be located at the central part of the electrode assembly 120. However, it goes without saying that the cathode tab 144 may be attached to the outer peripheral surface of the electrode assembly 120 and the anode tab 164 may be located at the central part of the electrode assembly 120. In addition, although not illustrated, one or more cathode tabs and anode tabs may be additionally attached for a high-power model.

[0055] At least a part of the sealing member 230 may be adhered to a finishing part 155 of the outer peripheral surface of the electrode assembly 120, and the finishing part 155 may be located at the outermost end of the separator 122. Since at least a part of the sealing member 230 is pressed against the electrode assembly 120 while covering the finishing part 155, the wound state of the electrode assembly 120 can be maintained, and a phenomenon in which the electrode assembly 120 is unwound due to internal stress can be prevented.

[0056] FIG. 3 is a cross-sectional view illustrating a sealing member attached to the electrode assembly of the secondary battery of FIG. 2.

[0057] Referring to FIGS. 2 and 3, the sealing member 230 according to the present embodiment may form a structure in which swollen polymer particles 230b are applied onto an adhesive layer 230a to form a film layer. The lower surface of the adhesive layer 230a may come into contact with the electrode assembly 120. At this time, the swollen polymer particles 230b may expand in multiple directions when the electrolyte solution is absorbed. Specifically, the swollen polymer particles 230b not only expand in the horizontal and vertical directions on the basis of a surface parallel to the adhesive layer 230a, but also can expand in a direction perpendicular to the adhesive layer 230a. Accordingly, as shown on the right side of FIG. 3, it is possible to show a state in which the swollen polymer particles 230b′ are relatively expanded.

[0058] As described above, since the sealing member 230 according to the present embodiment absorbs the electrolyte solution and expands in multiple directions, the gap between the electrode assembly 120 and the battery case 130 of FIG. 1 can be evenly filled, so that the secondary battery can improving the stability against vibration.

[0059] The sealing member 230 according to the present embodiment may be formed by applying swollen polymer particles 230b onto the adhesive layer 230a. The swollen polymer particles 230b may be a super absorbent polymer (SAP).

[0060] In a modified embodiment, the sealing member 230 may be formed through the following steps.

[0061] First, the polymer resin monomer and the swollen polymer particles are mixed and polymerized, and then a polymer resin film containing the swollen polymer particles is formed. The polymer resin may be composed of an aromatic isocyanate compound, a polyol compound, an acrylic-based compound, or a fluorine-based compound that are not reactive with the electrolyte solution. The polymerization of the resin may be the same as a polyurethane, acrylate polymerization, polyvinylidene-fluoride (PVDF) polymerization method, or the like. Thereafter, an acrylic-based adhesive is applied onto a polymer film containing swollen polymer particles to prepare a swelling tape.

[0062] As such, the swollen polymer particles 230b can be applied onto the adhesive layer 230a in a state of being mixed with other polymer materials such as polyurethane and polyacrylate, thereby forming a film layer. When the swollen polymer particles 230b are mixed with other polymer materials such as polyurethane to form a film layer in this way, the miscibility between the swollen polymer particles and the polymer material matrix is excellent, so that a film can be stably formed. Since the matrix swells in the surface direction and the swollen polymer particles are swellable in all directions, the swelling effect can be maximized. Further, according to a modified embodiment, by simply applying the swollen polymer particles onto the adhesive layer, it is possible to prevent the swollen polymer particles from being separated from the sealing member due to the electrolyte solution after the battery cell is assembled.

[0063] FIG. 4 is a cross-sectional view illustrating a sealing member according to a comparative example.

[0064] Referring to FIG. 4, when the sealing member 230 is formed with a structure in which a polymer film 23b is attached on the adhesive layer 23a, it expands only in the direction of one side, which is a surface parallel to the adhesive layer 230a, so that an adhesive layer 23a′ having wrinkles and a polymer film 23b′ are formed. Since the gap between the electrode assembly and the battery case is filled by the winkled structure, it is difficult to securely fix the electrode assembly. For example, the polymer film 23b according to the comparative example may be formed of any one of a polymer material containing an ester group or a carboxyl group, polyvinyldifluoride, polybutadiene, and polyisoprene.

[0065] FIG. 5 is a perspective view illustrating a wound state of the electrode assembly of a secondary battery according to another exemplary embodiment of the present disclosure. Since the embodiment of FIG. 5 is almost the same as the embodiment described with reference to FIG. 2, only the parts having differences will be described below.

[0066] Referring to FIG. 5, the sealing members 330 according to the present embodiment are separated from each other at regular intervals and are attached to the outer peripheral surface of the electrode assembly 120. Specifically, the sealing member 330 is made of a plurality of sub-sealing members separated from each other, and the sub-sealing member may be attached to a certain area of the electrode assembly 120 to cover the closing part 155. The front surface of the sub-sealing member can be formed into a square shape. Preferably, it may be formed in a vertically long rectangular shape to achieve a uniform shape.

[0067] Except for the differences described above, the contents described in FIG. 2 are applicable to all of the present embodiment.

[0068] The secondary battery according to the present exemplary embodiment described above may be mounted on one or more frames to form a battery pack. The secondary battery or battery pack described above can be applied to various devices. These devices may be applied to transportation means such as an electric bicycle, an electric vehicle, a hybrid vehicle, but the present disclosure is not limited thereto and can be applied to various devices that can use the battery module or the battery pack including the same.

[0069] Although the preferred embodiments of the present disclosure have been described in detail above, the scope of the present disclosure is not limited thereto, and various modifications and improvements of those skilled in the art using the basic concepts of the present disclosure defined in the following claims also belong to the scope of rights.

DESCRIPTION OF REFERENCE NUMERALS

[0070] 100: secondary battery

[0071] 120: electrode assembly

[0072] 230: sealing member

[0073] 144: cathode

[0074] 164: anode

[0075] 230a: adhesive layer