Method for manufacture and structure of multiple electrochemistries and energy gathering components within a unified structure

11539070 · 2022-12-27

Assignee

Inventors

Cpc classification

International classification

Abstract

A method for using an integrated battery and device structure includes using two or more stacked electrochemical cells integrated with each other formed overlying a surface of a substrate. The two or more stacked electrochemical cells include related two or more different electrochemistries with one or more devices formed using one or more sequential deposition processes. The one or more devices are integrated with the two or more stacked electrochemical cells to form the integrated battery and device structure as a unified structure overlying the surface of the substrate. The one or more stacked electrochemical cells and the one or more devices are integrated as the unified structure using the one or more sequential deposition processes. The integrated battery and device structure is configured such that the two or more stacked electrochemical cells and one or more devices are in electrical, chemical, and thermal conduction with each other.

Claims

1. A thin film battery device comprising two or more electro-chemistries, the thin film battery device comprising: a first thin film battery cell having a first electrochemistry and comprising a first cathode layer, a first electrolyte layer, and a first anode layer, the first cathode layer having a thickness of 3-5 μm; a second thin film battery cell having a second electrochemistry and comprising a second cathode layer, a second electrolyte layer, and a second anode layer, the second cathode layer having a thickness of 3-5 μm; and a thermally conductive layer disposed between the first and second thin film batteries, wherein the second thin film battery cell overlays the first thin film battery cell, and the first electrochemistry of the first thin film battery cell is different than the second electrochemistry of the second thin film battery cell, and wherein the thermally conductive layer comprises aluminum nitride.

2. The thin film battery device of claim 1, comprising a separation layer deposited between the first thin film battery cell and the second thin film battery cell.

3. The thin film battery device of claim 1, wherein the first thin film battery cell comprises a first cathode current collector and a first anode current collector, and wherein the second thin film battery cell comprises a second cathode current collector and a second anode current collector.

4. The thin film battery device of claim 1, wherein the first thin film battery cell and the second thin film battery cell are deposited using a physical vapor deposition (PVD) process.

5. The thin film battery device of claim 1, wherein the first electrolyte layer comprises lithium and the second electrolyte layer comprises lithium.

6. The thin film battery device of claim 1, wherein the first electrolyte layer comprises lithium phosphorous oxynitride (LIPON).

7. The thin film battery device of claim 1, wherein the first electrolyte layer is 1-3 μm thick.

8. The thin film battery device of claim 1, wherein the second electrolyte layer comprises lithium phosphorous oxynitride (LIPON).

9. The thin film battery device of claim 1, wherein the second electrolyte layer is 1-3 μm thick.

10. The thin film battery device of claim 1, wherein the first cathode layer comprises lithium iron phosphate (LiFePO.sub.4).

11. The thin film battery device of claim 1, wherein the second cathode layer comprises a lithium manganese oxide (LiMn.sub.2O.sub.4).

12. The thin film battery device of claim 1, wherein the first anode layer and the second anode layer comprise lithium.

13. The thin film battery device of claim 1, wherein the first anode layer and the second anode layer are 3-5 μm thick.

14. A method of making the thin film battery device according to claim 1, the method comprising two or more electro-chemistries comprising: forming the first thin film battery cell having a first electrochemistry and comprising: depositing the first cathode layer having a thickness of 3-5 μm; depositing the first electrolyte layer on the first cathode layer; and depositing the first anode layer on the first electrolyte layer; and depositing the thermally conductive layer between the first thin film battery cell and the second thin film battery cell; and depositing the second thin film battery cell on the first thin film battery cell comprising: depositing the second cathode layer having a thickness of 3-5 μm on a first substrate comprising the first thin film battery cell; depositing the second electrolyte layer on the second cathode layer; and depositing the second anode layer on the second electrolyte layer, wherein the electrochemistry of the first thin film battery cell is different than the electrochemistry of the second thin film battery cell; and wherein the thermally conductive layer comprises aluminum nitride.

15. The method of making a thin film battery device of claim 14, wherein the first cathode layer, the first electrolyte layer, the first anode layer, the second cathode layer, the second electrolyte layer, and the second anode layer are deposited using physical vapor deposition processes.

16. The method of making a thin film battery device of claim 14, wherein the first thin film battery cell comprises a first cathode current collector and a first anode current collector, and wherein the second thin film battery cell comprises a second cathode current collector and a second anode current collector.

17. The method of making a thin film battery device of claim 14, wherein the first electrolyte layer comprises lithium and the second electrolyte layer comprises lithium.

18. The method of making a thin film battery device of claim 14, wherein the first electrolyte layer comprises lithium phosphorous oxynitride (LIPON).

19. The method of making a thin film battery device of claim 14, wherein the first electrolyte layer is 1-3 μm thick.

20. The method of making a thin film battery device of claim 14, wherein the second electrolyte layer comprises lithium phosphorous oxynitride (LIPON).

21. The method of making a thin film battery device of claim 14, wherein the second electrolyte layer is 1-3 μm thick.

22. The method of making a thin film battery device of claim 14, wherein the first cathode layer comprises lithium iron phosphate (LiFePO.sub.4).

23. The method of making a thin film battery device of claim 14, wherein the second cathode layer comprises a lithium manganese oxide (LiMn.sub.2O.sub.4).

24. The method of making a thin film battery device of claim 14, wherein the first anode layer and the second anode layer comprise lithium.

25. The method of making a thin film battery device of claim 14, wherein the first anode layer and the second anode layer are 3-5 μm thick.

Description

BRIEF DESCRIPTION OF THE DRAWINGS

(1) FIG. 1—Simplified cross-sectional view of a unified structure including an integrated silicon (Si) solar cell and a thin film battery.

(2) FIG. 2—Simplified cross-sectional view of a unified structure including two integrated thin film batteries having different chemistry.

(3) FIG. 3—Simplified cross-sectional view of a unified structure including an integrated hydrogen/oxygen fuel-cell and a thin film battery.

(4) FIG. 4—Simplified cross sectional view of a unified structure including an integrated ultra-capacitor and a thin film battery.

DETAILED DESCRIPTION OF THE INVENTION

Example 1

A Unified Structure Including a Silicon (Si) Solar Cell and a Thin Film Battery and Their Manufacturing Method

(5) Preparing a stacked cell on the back surface of a silicon (Si) solar cell as shown in FIG. 1 can be achieved by forming the cell components using physical vapor deposition. A solar cell exploiting p-type silicon is constructed using traditional Si wafers (Czochralski method). After forming a p-n junction by diffusing phosphorous (P) into the wafer, an aluminum (Al) back contact is created (metal back contact in FIG. 1), onto the p+ doped region (lower side) of the silicon wafer, using physical vapor deposition. The aluminum layer is grown to a thickness of 1-2 μm.

(6) After the back metal contact is created, a separation layer of electrically insulating and thermally conductive aluminum nitride (AlN), having a thickness of 3-5 μm, is fabricated onto the aluminum layer using PVD. This layer has the function of removing heat from the two elements and convey it to a heat sink.

(7) After the cooling element is completed, the battery components are deposited sequentially and conformally by a physical vapor deposition (PVD) process: an aluminum (Al) current collector layer (1-3 μm thick), a lithium manganese oxide (LiMn.sub.2O.sub.4) cathode layer (3-5 μm thick), a lithium phosphorous oxynitride (UPON) ceramic electrolyte layer (1-3 μm thick), a lithium (Li) metal anode layer (3-5 μm thick), and a copper (Cu) current collector layer (1-3 μm thick), respectively.

Example 2

A Unified Structure Including Two Thin Film Batteries Having Different Chemistry and Their Manufacturing Method

(8) Two stacked cells having different electrochemistries are fabricated onto each other by using physical vapor deposition as reported in FIG. 2.

(9) The first battery components are deposited using a PVD process onto an aluminum (Al) metal film used as cathode current collector: a lithium iron phosphate (LiFePO.sub.4) cathode layer (3-5 μm thick), a lithium phosphorous oxynitride (LIPON) ceramic electrolyte layer (1-3 μm thick), a lithium (Li) metal anode layer (3-5 μm thick) and a copper (Cu) current collector layer (1-3 μm thick), respectively.

(10) After the copper (Cu) metal current collector is created, a separation layer of electrically insulating and thermally conductive aluminum nitride (AlN), having a thickness of 3-5 μm, is fabricated onto the copper layer using PVD. This layer has the function of removing heat from the two elements and convey it to a heat sink.

(11) After the cooling element is completed, the second battery components are deposited sequentially and conformally by a PVD process: an aluminum (Al) current collector layer (1-3 μm thick), a lithium manganese oxide (LiMn.sub.2O.sub.4) cathode layer (3-5 μm thick), a lithium phosphorous oxynitride (LIPON) ceramic electrolyte layer (1-3 μm thick), a lithium (Li) metal anode layer (3-5 μm thick) and a copper (Cu) current collector layer (1-3 μm thick), respectively.

Example 3

A Unified Structure Including a Fuel-Cell and a Thin Film Battery and Their Manufacturing Method

(12) Preparing a stacked cell on the back surface of a proton-exchange membrane (PEM) fuel-cell as shown in FIG. 3 can be achieved by forming the cell components using physical vapor deposition (PVD). A PEM fuel-cell exploiting proton exchange membranes with high proton conductivity, employing perfluorosulfonate ionomers electrolytes such as Nation®, is constructed using traditional sol-gel methods for fabricating the membrane and wet slurry for the electrodes.

(13) After assembly of the fuel-cell a separation layer of electrically insulating and thermally conductive aluminum nitride (AlN), having a thickness of 3-5 μm, is fabricated onto the fuel-cell current collector using PVD. This layer has the function of removing heat from the two elements and conveying it to a heat sink.

(14) After the cooling element is completed, the battery components are deposited sequentially and conformally by a PVD process. Respectively an aluminum (Al) current collector layer (1-3 μm thick), a lithium manganese oxide (LiMn.sub.2O.sub.4) cathode layer (3-5 μm thick), a lithium phosphorous oxynitride (UPON) ceramic electrolyte layer (1-3 μm thick), a lithium (Li) metal anode layer (3-5 μm thick) and a copper (Cu) current collector layer (1-3 μm thick).

Example 4

A Unified Structure Including an Ultra-Capacitor and a Thin Film Battery and Their Manufacturing Method

(15) Preparing a stacked cell on the back surface of an electrochemical double layer capacitor (EDLC), which is also known as an ultra-capacitor) as shown in FIG. 3 can be achieved by forming the cell components using PVD. In such a hybrid system, the battery provides high energy density while the EDLC enables high power capability in the system.

(16) EDLCs describe a class of energy-storage devices that incorporate active materials including high-surface-area carbons (activated carbons), electroactive polymers, transition metal oxides and nitrides. The separation materials include advanced dielectrics, conventional and advanced polymer electrolytes and ionic conducting materials. Electrodes arrangement can be symmetric or anti-symmetric. In FIG. 4 an anti-symmetric electrode arrangement is presented for the device electrodes. The electrodes of the capacitor can be formed by high-surface-area materials such as activated carbon of high capacitance redox-active materials such as metal oxides (e.g. hydrous ruthenium oxides, RuO.sub.2.0.5H.sub.2O) prepared by sol-gel methods with capacitance up to 700 F/g. Using anti-symmetric electrodes and different anode and cathode materials resulting in higher working voltages enhances the energy-storage capability of this element.

(17) After assembly of the ultra-capacitor a separation layer of electrically insulating and thermally conductive aluminum nitride (AlN), having a thickness of 3-5 μm, is fabricated onto the dielectric material layer using PVD. This layer has the function of removing heat from the two elements and conveying it to a heat sink.

(18) After the cooling element is completed, the battery components are deposited sequentially and conformally by a PVD process: an aluminum (Al) current collector layer (1-3 μm thick), a lithium manganese oxide (LiMn.sub.2O.sub.4) cathode layer (3-5 μm thick), a lithium phosphorous oxynitride (LIPON) ceramic electrolyte layer (1-3 μm thick), a lithium (Li) metal anode layer (3-5 μm thick) and a copper (Cu) current collector layer (1-3 μm thick), respectively.

(19) It is also understood that the examples and embodiments described herein are for illustrative purposes only and that various modifications or changes in light thereof will be suggested to persons skilled in the art and are to be included within the spirit and purview of this application and scope of the appended claims.