Optical film, method for manufacturing optical film, and liquid crystal display

10317582 ยท 2019-06-11

Assignee

Inventors

Cpc classification

International classification

Abstract

Provided are an optical film, a method for manufacturing an optical film, and a liquid crystal display. An optical film includes: a polarizer, a diffusion sheet adhered to a bottom surface of the polarizer, the diffusion sheet including a plurality of first beads, and an adhesive layer between the polarizer and the diffusion sheet, the adhesive layer attaching the polarizer to the diffusion sheet, the adhesive layer including a plurality of second beads.

Claims

1. An optical film, comprising: a polarizer comprising: a core layer; and a lower protection layer under the core layer; a diffusion sheet adhered to a bottom surface of the polarizer, the diffusion sheet comprising a plurality of first beads, the diffusion sheet having an uneven surface comprising a plurality of convex parts corresponding to the first beads; an adhesive layer between the polarizer and the diffusion sheet, the adhesive layer attaching the polarizer to the diffusion sheet, the adhesive layer comprising a plurality of second beads, the adhesive layer having an uneven surface comprising a plurality of convex parts corresponding to the second beads; and an air layer between the polarizer and the diffusion sheet, wherein the uneven surface of the diffusion sheet directly contacts the uneven surface of the adhesive layer only at respective pairs of convex parts of the diffusion sheet and convex parts of the adhesive layer, and wherein a part of a lower surface of the lower protection layer is exposed between the plurality of convex parts of the adhesive layer, the part of the lower surface of the lower protection layer contacting the air layer.

2. The optical film of claim 1, wherein the air layer is in a remaining space other than in the adhesive layer between the polarizer and the diffusion sheet.

3. The optical film of claim 1, wherein the diffusion sheet and the adhesive layer are partially spaced apart from each other.

4. The optical film of claim 1, wherein the diffusion sheet and the adhesive layer contact each other only at separated portions at pairs of directly contacting convex parts of the diffusion sheet and the adhesive layer.

5. The optical film of claim 1, wherein the adhesive layer has a dot shape.

6. The optical film of claim 1, wherein the plurality of second beads is grouped to form a plurality of groups.

7. The optical film of claim 1, wherein an area density of the plurality of second beads is 50 to 200 per mm.sup.2.

8. The optical film of claim 1, further comprising a prism sheet adhered to a bottom surface of the diffusion sheet.

9. A method for manufacturing an optical film, the method comprising: forming a diffusion sheet by coating a resin comprising a plurality of first beads on a support film, the diffusion sheet having an uneven surface comprising a plurality of convex parts corresponding to the first beads; providing adhesives comprising a plurality of second beads in a spray device; forming an adhesive layer by spraying the adhesives on a polarizer, the polarizer comprising a core layer and a lower protection layer under the core layer, the adhesive layer having an uneven surface comprising a plurality of convex parts corresponding to the second beads; laminating the diffusion sheet and the polarizer using the adhesive layer therebetween, such that the uneven surface of the diffusion sheet directly contacts the uneven surface of the adhesive layer only at respective pairs of convex parts of the diffusion sheet and convex parts of the adhesive layer; and providing an air layer between the polarizer and the diffusion sheet, wherein a part of a lower surface of the lower protection layer is exposed between the plurality of convex parts of the adhesive layer, the part of the lower surface of the lower protection layer contacting the air layer.

10. The method of claim 9, wherein the spray device comprises a sprayer.

11. A liquid crystal display, comprising: a display panel; and an optical film adhered under the display panel, the optical film comprising: a polarizer comprising: a core layer, and a lower protection layer under the core layer; a diffusion sheet adhered to a bottom surface of the polarizer, the diffusion sheet comprising a plurality of first beads, the diffusion sheet having an uneven surface comprising a plurality of convex parts corresponding to the first beads; an adhesive layer between the polarizer and the diffusion sheet, the adhesive layer attaching the polarizer to the diffusion sheet, the adhesive layer comprising a plurality of second beads, the adhesive layer having an uneven surface comprising a plurality of convex parts corresponding to the second beads; and an air layer is between the polarizer and the diffusion sheet, wherein the uneven surface of the diffusion sheet directly contacts the uneven surface of the adhesive layer only at respective pairs of convex parts of the diffusion sheet and convex parts of the adhesive layer, and wherein a part of a lower surface of the lower protection layer is exposed between the plurality of convex parts of the adhesive layer, the part of the lower surface of the lower protection layer contacting the air layer.

12. The optical film of claim 1, wherein a part of the plurality of second beads contacts the convex parts of the diffusion sheet.

Description

BRIEF DESCRIPTION OF THE DRAWINGS

(1) The accompanying drawings, which are included to provide a further understanding of the invention and are incorporated in and constitute a part of this specification, illustrate implementations of the invention and together with the description serve to explain the principles of the disclosure.

(2) FIG. 1 is an exploded perspective view showing the structure of a liquid crystal display that includes an edge-type backlight unit according to a related art.

(3) FIG. 2 is a cross-sectional view showing the structure of the liquid crystal display that includes an edge-type backlight unit according to the related art, taken along line I-I of FIG. 1.

(4) FIG. 3 is a cross-sectional view showing the structure of optical films including a diffusion film in a liquid crystal display according to a related art.

(5) FIG. 4 is a cross-sectional view showing the structure of optical films, including a high brightness diffusion film, in a liquid crystal display according to a related art.

(6) FIG. 5 is a cross-sectional view showing the structure of a liquid crystal display according to an embodiment of the present disclosure.

(7) FIG. 6 is a cross-sectional view showing a portion of the liquid crystal display according to an embodiment of the present disclosure.

(8) FIGS. 7 to 9 are plan views showing an adhesive layer according to an embodiment of the present disclosure.

(9) FIGS. 10 to 12 are cross-sectional views showing a process for manufacturing an optical film according to an embodiment of the present disclosure.

(10) FIG. 13 is a table showing a light profile and brightness according to the density of beads included in a first adhesive layer in the liquid crystal display of FIG. 5 according to an embodiment of the present disclosure.

(11) FIG. 14 is a cross-sectional view showing a liquid crystal display according to a comparative example 1.

(12) FIG. 15 is a cross-sectional view showing a liquid crystal display according to a comparative example 2.

(13) FIG. 16 shows a light profile image of the liquid crystal display according to the comparative example 1.

(14) FIG. 17 shows a light profile image of the liquid crystal display according to the comparative example 2.

(15) FIG. 18 shows a light profile image of the liquid crystal display according to an embodiment of the present disclosure.

(16) Throughout the drawings and the detailed description, unless otherwise described, the same drawing reference numerals should be understood to refer to the same elements, features, and structures. The relative size and depiction of these elements may be exaggerated for clarity, illustration, and convenience.

DETAILED DESCRIPTION

(17) Reference will now be made in detail to embodiments of the present disclosure, examples of which are illustrated in the accompanying drawings. In the following description, when a detailed description of well-known functions or configurations related to this document is determined to unnecessarily cloud a gist of the invention, the detailed description thereof will be omitted. The progression of processing steps and/or operations described is an example; however, the sequence of steps and/or operations is not limited to that set forth herein and may be changed as is known in the art, with the exception of steps and/or operations necessarily occurring in a certain order. Like reference numerals designate like elements throughout. Names of the respective elements used in the following explanations are selected only for convenience of writing the specification and may be thus different from those used in actual products.

(18) In the description of embodiments, when a structure is described as being positioned on or above or under or below another structure, this description should be construed as including a case in which the structures contact each other as well as a case in which a third structure is disposed therebetween.

(19) FIG. 5 is a cross-sectional view showing the structure of a liquid crystal display according to an embodiment of the present disclosure. FIG. 6 is a cross-sectional view showing a portion of the liquid crystal display according to an embodiment of the present disclosure. FIGS. 7 to 9 are plan views showing an adhesive layer according to an embodiment of the present disclosure.

(20) With reference to FIG. 5, the liquid crystal display (LCD) according to an embodiment of the present disclosure may include an LCD panel LCP, an upper polarizer UPOL, and an optical film OPT.

(21) The LCD panel LCP may include an upper substrate and a lower substrate opposing each other with a liquid crystal layer interposed therebetween. The upper polarizer UPOL may be on a top surface of the LCD panel LCP. The lower polarizer LPOL may be on a bottom surface of the LCD panel LCP. The upper polarizer UPOL may have light transmission axes or light blocking axes aligned in a first direction. The lower polarizer LPOL may have light transmission axes or light blocking axes aligned in a second direction. If an LCD is normally black, the first light transmission axis and the second light transmission axis may be orthogonal to each other. In contrast, if an LCD is normally white, the first light transmission axis and the second light transmission axis may be disposed in parallel.

(22) The optical film OPT may include the lower polarizer LPOL, a first adhesive layer PSA1, a diffusion sheet DIF, and a prism sheet PS. The lower polarizer LPOL may include a core layer PVA, an upper protection layer UPL protecting the top surface of the core layer PVA, and a lower protection layer LPL protecting the bottom surface of the core layer PVA. The core layer PVA may polarize light and may be made of, e.g., polyvinyl alcohol (PVA). Depositing PVA formed by a depositing method or coating PVA formed by a coating method may be used as the core layer PVA, although embodiments are not limited thereto. The core layer PVA may be deformed by moisture included in the air. Accordingly, a protection layer may be positioned on at least one surface of the core layer PVA. In an embodiment of the present disclosure, the upper protection layer UPL may be over the core layer PVA, and the lower protection layer LPL may be under the core layer PVA. The upper protection layer UPL and the lower protection layer LPL may be made of, e.g., triacetatecellulose (TAC), acryl, polyethylene terephthalate (PET), polycarbonate (PC), or polyethylene naphthenate (PEN), although embodiments are not limited thereto. The upper protection layer UPL may adhere to the core layer PVA by a first ultraviolet (UV) adhesive layer UR1, and the lower protection layer LPL may adhere to the core layer PVA through a second UV adhesive layer UR2. Any appropriate transparent adhesives may be used as the first UV adhesive layer UR1 and the second UV adhesive layer UR2.

(23) In an embodiment of the present disclosure, the lower polarizer LPOL may have a structure including the core layer PVA, the upper protection layer UPL on the top surface of the core layer PVA, and the lower protection layer LPL on the bottom surface of the core layer PVA. Alternatively, embodiments may omit at least one of the upper protection layer UPL and the lower protection layer LPL.

(24) The diffusion sheet DIF may distribute light passing through the prism sheet PS so that the light has a uniform brightness distribution over the entire surface of the LCD panel LCP. For example, in the case of the edge-type backlight unit, a side face on which a light source is positioned may be brighter than a side face that is opposite the side face on which a light source is positioned. Furthermore, in the case of the direct-type backlight unit, a portion in which a light source is positioned may be brighter than the surrounding portion of the light source. The diffusion sheet DIF may uniformly diffuse a brightness distribution of light that is not uniform over the entire surface of the LCD panel LCP.

(25) The diffusion sheet DIF may include a support film PET and a diffusion unit DR on the support film PET, and may include a plurality of first beads BD1. The support film PET may transmit light incident from a light source, and may support the diffusion unit DR. To this end, the support film PET may be made of a material that is capable of transmitting light incident from a light source and that has a resistance force against moisture in the air, for example, polyethylene terephthalate (PET), polycarbonate (PC), polypropylene (PP), polyethylene (PE), polystyrene (PS), and/or polyepoxy (PE), but is not limited thereto. The support film PET may be thin in accordance with the thinness of a backlight unit, for example, a thickness of 10 m to 250 m. If the support film PET has a thickness of 10 m or more, the backlight unit can be made as thin as possible within the limits in which the mechanical physical and heat-resistant properties of the optical film are not deteriorated. Furthermore, if the support film PET has a thickness of 250 m or less, the thinness of the backlight unit can be achieved and the mechanical physical and heat-resistant properties of the optical film can also be maximized.

(26) The diffusion unit DR into which the plurality of first beads BD1 has been dispersed may be positioned on the support film PET. The diffusion unit DR may support the plurality of first beads BD1 while dispersing them. The diffusion unit DR may be made of the same kind of resin as the support film PET, or may be made of resin different from that of the support film PET.

(27) The plurality of first beads BD1 may be made of the same kind of resin as the support film PET, or may be made of resin different from that of the support film PET. The diffusion unit DR may include 10-50 weight % of the plurality of first beads BD1. The size of the first beads BD1 may be properly selected depending on a thickness of the diffusion unit DR, and may be, e.g., 1 m to 10 m. The first beads BD1 may have substantially the same size, and may have a uniform distribution within the diffusion unit DR. In some embodiments, the first beads BD1 may have different sizes, and may have an irregular distribution within the diffusion unit DR. The diffusion sheet DIF may improve the uniformity of light by diffusing the light. A total haze of the diffusion sheet DIF may be 20% to 100% to cover an underlying light source.

(28) The prism sheet PS may include a prism portion PP having prism patterns formed on a base sheet SS. The base sheet SS may transmit light incident from the light source, and may protect the prism portion PP of the prism sheet PS. To this end, the base sheet SS may be made of a material that is capable of transmitting light incident from the light source and that has a resistance force against moisture in the air, for example, polyethylene terephthalate (PET), polycarbonate (PC), polypropylene (PP), polyethylene (PE), polystyrene (PS), and/or polyepoxy (PE), but is not limited thereto. The base sheet SS may be formed to have a thickness in accordance with the thinness of the backlight unit, for example, a thin thickness of 10 m to 250 m. If the base sheet SS has a thickness of 10 m or more, the backlight unit can be made as thin as possible within the limits in which the mechanical physical and heat-resistant properties of the optical film are not deteriorated. Furthermore, if the base sheet SS has a thickness of 250 m or less, the thinness of the backlight unit can be achieved and the mechanical physical and heat-resistant properties of the optical film can also be maximized.

(29) The prism portion PP may be disposed on the base sheet SS, and may focus (or concentrate) light incident from the light source by the plurality of prism patterns. The prism portion PP may include a first prism pattern P1, having a first height, and a second prism pattern P2, having a second height. The first height and the second height may be different.

(30) The LCD according to an embodiment of the present disclosure may have a structure in which the prism sheet PS has been laminated on the diffusion sheet DIF by a third UV adhesive layer UR3. For example, a portion of the plurality of prism patterns P1 and P2 of the prism portion PP formed in the prism sheet PS may be inserted into the third UV adhesive layer UR3. The first prism patterns P1 having the first height and the second prism patterns P2 having the second height may be alternately disposed in the prism sheet PS. Accordingly, a portion of a peak having a higher one of the first height and the second height may be inserted into the third UV adhesive layer UR3. For example, if the first height is greater than the second height, part of the first prism patterns P1 having the first height may be inserted into the third UV adhesive layer UR3.

(31) As described above, although a portion of the at least one first prism pattern P1 may be inserted into the third UV adhesive layer UR3, the second prism patterns P2 may be spaced apart from the third UV adhesive layer UR3 at a specific interval. That is, an air layer may be interposed between the third UV adhesive layer UR3 and the second prism patterns P2. If the prism portion PP of the prism sheet PS does not include peaks having different heights, the size of the air layer may be significantly reduced and a light-focusing characteristic may be deteriorated because all the peaks of the prism portion PP would be inserted into the third UV adhesive layer UR3. As a result, brightness may be deteriorated because light may not be sufficiently refracted. Accordingly, in an embodiment of the present disclosure, the first prism patterns P1 and the second prism patterns P2 may have different heights. In an embodiment of the present disclosure, a sufficient air layer can be secured between the third UV adhesive layer UR3 and the second prism patterns P2 because the prism patterns P1 and P2 of the prism portion PP of the prism sheet PS may have different heights, thereby being capable of minimizing a brightness loss.

(32) The prism sheet PS may further include a hard coating layer HC having a plurality of third beads BD3 on the bottom surface of the base sheet SS. The hard coating layer HC may protect the prism sheet PS against an external impact or physical force. The plurality of third beads BD3 may be dispersed in resin in a small quantity. Although the hard coating layer HC has been illustrated as being included in the FIG. 5 example, the hard coating layer HC is optional and may be omitted.

(33) The adhered diffusion sheet DIF and prism sheet PS may adhere to the lower polarizer LPOL. For example, the first adhesive layer PSA1 may be disposed between the lower polarizer LPOL and the diffusion sheet DIF. The first adhesive layer PSA1 may attach the lower polarizer LPOL to the diffusion sheet DIF. Any appropriate adhesive having high elasticity and a good adhesive characteristic and is capable of preventing being peeled off by reducing the generation of a fine bubble may be used as the first adhesive layer PSA1. For example, pressure sensitive adhesives (PSA), UV adhesives, or water-based adhesives may be used as the first adhesive layer PSA1. Furthermore, the first adhesive layer PSA1 may function as an adhesive, and may also may protect the sheets against an external impact because it has specific elasticity.

(34) In an embodiment of the present disclosure, although the diffusion sheet DIF and the lower polarizer LPOL may adhere to each other by the first adhesive layer PSA1, light can be diffused from the diffusion sheet DIF. To this end, in an embodiment of the present disclosure, the first adhesive layer PSA1 formed between the diffusion sheet DIF and the lower polarizer LPOL may include a plurality of second beads BD2. A condition in which the diffusion of light is generated may include that the light has to be refracted due to a difference between the refractive indices of two media.

(35) In general, materials used in the optical film OPT may have a refractive index in the range of, e.g., 1.5 to 1.7. If the diffusion sheet DIF and the lower polarizer LPOL adhere to each other by the first adhesive layer PSA1, the diffusion of light may not be generated because there may be no difference between the refractive indices of the diffusion sheet DIF and the first adhesive layer PSA1. For this reason, in an embodiment of the present disclosure, an air layer Air may be between the diffusion sheet DIF and the first adhesive layer PSA1 by including the plurality of second beads BD2 in the first adhesive layer PSA1. The air layer Air may be disposed in the remaining space other than the first adhesive layer PSA1 between the diffusion sheet DIF and the lower polarizer LPOL.

(36) For example, with reference to FIG. 6, the optical film OPT according to an embodiment of the present disclosure may include the first adhesive layer PSA1 between the lower polarizer LPOL and the diffusion sheet DIF. The refractive indices of the first beads BD1 and diffusion unit DR of the diffusion sheet DIF may have a range of, e.g., 1.5 to 1.7. The refractive indices of the first adhesive layer PSA1 and the second beads BD2 dispersed in the first adhesive layer PSA1 may have a range of, e.g., 1.5 to 1.7. The air layer Air between the diffusion sheet DIF and the first adhesive layer PSA1 may have a refractive index of 1.0.

(37) Accordingly, light that is incident from the bottom of the diffusion sheet DIF to the lower polarizer LPOL may pass through the air layer Air. Because the diffusion sheet DIF and the air layer Air may have different refractive indices, the light may be refracted at the interface of the diffusion sheet DIF and the air layer Air. Thus the path of the light may be changed. When the path of the light is changed, the light may be focused upward or may be diffused laterally. The light passing through the air layer Air may be refracted again at the interface of the first adhesive layer PSA1 having a different refractive index, and may be focused or diffused. Accordingly, the optical film OPT according to an embodiment of the present disclosure may include the first adhesive layer PSA1 having the plurality of second beads BD2 between the diffusion sheet DIF and the lower polarizer LPOL. As a result, there are advantages in that the diffusion sheet DIF and the lower polarizer LPOL can adhere to each other and in that the air layer Air may also be formed between the diffusion sheet DIF and the first adhesive layer PSA1, thereby being capable of diffusing light.

(38) Furthermore, in an embodiment of the present disclosure, the diffusion sheet DIF and the first adhesive layer PSA1 may be spaced apart from each other at a specific area so that the air layer Air may be formed between the diffusion sheet DIF and the first adhesive layer PSA1. To this end, the first adhesive layer PSA1 according to an embodiment of the present disclosure may include the plurality of second beads BD2. The plurality of second beads BD2 dispersed in the first adhesive layer PSA1 may form an uneven surface of the first adhesive layer PSA1. The diffusion sheet DIF adhered to the first adhesive layer PSA1 may also have an uneven surface due to the first beads BD1. When the first adhesive layer PSA1 and the diffusion sheet DIF adhere to each other, the convex parts PSAC of the first adhesive layer PSA1 and the convex parts DIFC of the diffusion sheet DIF may come into contact with each other in some places. The convex part PSAC of the first adhesive layer PSA1 may form a step along with another contiguous area, and the convex part DIFC of the diffusion sheet DIF may also form a step along with another contiguous area. Accordingly, the air layer Air may be formed between locations where the convex part PSAC of the first adhesive layer PSA1 and the convex part DIFC of the diffusion sheet DIF are in contact with each other. That is, the air layer Air may be formed in the area where the first adhesive layer PSA1 and the diffusion sheet DIF are not in contact with each other.

(39) As described above, in an embodiment of the present disclosure, the convex part PSAC of the first adhesive layer PSA1 and the convex part DIFC of the diffusion sheet DIF may be in contact with other at a specific area, and the first adhesive layer PSA1 and the diffusion sheet DIF may not contact each other in the remaining areas. Accordingly, the air layer Air may be formed between the first adhesive layer PSA1 and the diffusion sheet DIF. To this end, the first adhesive layer PSA1 according to an embodiment of the present disclosure may be irregularly positioned on the surface of the lower polarizer LPOL.

(40) With reference to FIG. 7, the first adhesive layer PSA1 including the plurality of second beads BD2 may be irregularly positioned on the lower polarizer LPOL. The first adhesive layer PSA1 may isolate the lower polarizer LPOL and the diffusion sheet DIF while attaching them. If the first adhesive layer PSA1 including the plurality of second beads BD2 is uniformly coated on the lower polarizer LPOL as a single layer, the adhesion between the lower polarizer LPOL and the diffusion sheet DIF may be strengthened, but the isolation between the lower polarizer LPOL and the diffusion sheet DIF may be weak. For this reason, the first adhesive layer PSA1 according to an embodiment of the present disclosure may be irregularly positioned on the lower polarizer LPOL so that the diffusion sheet DIF may adhere to the lower polarizer LPOL in the area in which the second beads BD2 of the first adhesive layer PSA1 are positioned, and the diffusion sheet DIF may be isolated from the lower polarizer LPOL in the area in which the second beads BD2 of the first adhesive layer PSA1 are not positioned. As a result, the air layer Air may be formed because the diffusion sheet DIF and the first adhesive layer PSA1 may be spaced apart from each other in the area in which the second beads BD2 of the first adhesive layer PSA1 are not positioned.

(41) With reference to FIGS. 7 and 8, the first adhesive layer PSA1 according to an embodiment of the present disclosure may be disposed in a dot shape. In this case, the first adhesive layer PSA1 may be positioned in a form in which water drops are dispersed, including the plurality of second beads BD2, or may be positioned in a rectangular dot shape including the plurality of second beads BD2. Areas in which the first adhesive layer PSA1 is not formed may surround the areas having the first adhesive layer PSA1 on the lower polarizer LPOL. Embodiments are not limited to these shapes.

(42) In contrast, with reference to FIG. 9, the first adhesive layer PSA1 according to an embodiment of the present disclosure may be formed on the entire bottom surface of the lower polarizer LPOL in a layer form, but the plurality of second beads BD2 may be irregularly disposed. In this case, the plurality of second beads BD2 may be grouped to form a plurality of groups. Although not shown, the first adhesive layer PSA1 according to an embodiment of the present disclosure may have any arbitrary shape if the groups of a plurality of second beads BD2 are spaced apart from each other, and may also have a line-by-line form. Embodiments are not limited to these examples.

(43) The plurality of second beads BD2 included in the first adhesive layer PSA1 according to an embodiment of the present disclosure may be included in the first adhesive layer PSA1 in a specific area density range so that the second beads BD2 function to attach the lower polarizer LPOL to the diffusion sheet DIF, and also to isolate them. The plurality of second beads BD2 may have an area density of 50 to 200 per mm.sup.2 within the first adhesive layer PSA1. In this case, if the area density of the plurality of second beads BD2 is 50 or more per mm.sup.2, the adhesive force between the first adhesive layer PSA1 and the diffusion sheet DIF can be increased and the diffusion characteristic of light can be improved. If the area density of the plurality of second beads BD2 is 200 or less per mm.sup.2, brightness of light can be prevented from being deteriorated.

(44) The optical film OPT in which the lower polarizer LPOL, the first adhesive layer PSA1, the diffusion sheet DIF, and the prism sheet PS have been laminated into one film as described above may adhere to the bottom surface of the LCD panel LCP through a second adhesive layer PSA2.

(45) As described above, the optical film according to an embodiment of the present disclosure has an advantage in that it can diffuse light incident from the lower side by refracting the light at the interface of the diffusion sheet and the air layer and at the interface of the air layer and the first adhesive layer because the first adhesive layer including the plurality of second beads is formed between the lower polarizer and the diffusion sheet. Furthermore, the LCD according to an embodiment of the present disclosure has an advantage in that it can prevent a moir phenomenon from occurring by securing the haze of the diffusion sheet through the optical film.

(46) Furthermore, in an embodiment of the present disclosure, the lower polarizer, the first adhesive layer, the diffusion sheet, and the prism sheet are integrated and disposed under the LCD panel. Accordingly, there is an advantage in that the LCD can be made thin as possible because separate optical films are omitted and the thickness of the backlight unit is reduced.

(47) A method for manufacturing the optical film according to an embodiment of the present disclosure is described below.

(48) FIGS. 10 to 12 are cross-sectional views showing a process for manufacturing the optical film according to an embodiment of the present disclosure.

(49) With reference to FIG. 10, the lower polarizer LPOL may be prepared. The lower polarizer LPOL may be formed by coating the first UV adhesive layer UR1 on the upper protection layer UPL; coating the second UV adhesive layer UR2 on the lower protection layer LPL; and then laminating the core layer PVA, the upper protection layer UPL, and the lower protection layer LPL at the same time.

(50) The first adhesive layer PSA1 in which the second beads BD2 have been mixed may be formed on the lower protection layer LPL of the formed lower polarizer LPOL. The first adhesive layer PSA1 may be formed by inserting adhesive resin in which the second beads BD2 have been mixed into a spray device (SPD), for example, a spray device such as a sprayer, and then spraying the adhesive resin on the lower polarizer LPOL. In this case, the adhesive resin may be sprayed on the lower polarizer LPOL to widely disperse the adhesive resin. Furthermore, process conditions, such as a shape of a spray nozzle, the amount of spray, and a jet velocity, may be controlled so that the adhesive resin is not sprayed on the lower polarizer LPOL in a uniform layer form. Furthermore, the first adhesive layer PSA1 may be coated in a thickness of 1 to 20 m to secure an adhesive force.

(51) Next, with reference to FIG. 11, the diffusion sheet DIF including the diffusion unit DR may be formed by coating resin, including the plurality of first beads BD1, on the support film PET. Furthermore, the prism sheet PS may be formed by coating resin on the base sheet SS and by forming the prism portion PP using a mold, for example, a soft mold. Furthermore, the hard coating layer HC may be formed by coating resin, including the plurality of third beads BD3, on the bottom surface of the prism sheet PS. The third UV adhesive layer UR3 is coated on the bottom surface of the formed diffusion sheet DIF, and then may attach to the prism sheet PS by laminating the prism sheet PS. The prism portion PP of the prism sheet PS may be inserted into the third UV adhesive layer UR3, and then may adhere to the diffusion sheet DIF.

(52) With reference to FIG. 12, a surface on which the first adhesive layer PSA1 of the lower polarizer LPOL has been coated and an uneven surface may be disposed to face each other due to the first beads BD1 of the diffusion sheet DIF. Furthermore, the optical film OPT may be formed by laminating the lower polarizer LPOL, the integrated diffusion sheet DIF, and prism sheet PS. The optical film OPT may be formed to have the final haze of 20% to 100% by controlling the haze of the diffusion sheet DIF and the first adhesive layer PSA1. The formed optical film OPT may be cut to a desired size and shape, and may be attached to the bottom surface of an LCD panel.

(53) Experimental data regarding the optical characteristics of LCDs according to comparative examples and the embodiments of the present disclosure is described below. FIG. 13 is a table showing a light profile and brightness according to the density of the beads included in the first adhesive layer in the LCD of FIG. 5 according to an embodiment of the present disclosure. In this example, the particle diameter of a bead is 4 m, although embodiments are not limited thereto.

(54) FIG. 13 shows that as the area density of the beads included in the first adhesive layer increases to 80, 100, 120, and 140 per mm.sup.2, light profiles are uniformly distributed, and brightness also increases from 1912 to 2292 cd/m.sup.2. From the experiment results shown in FIG. 13, it may be seen that, as the density of the beads included in the first adhesive layer increases, the uniformity of light is improved and light brightness is also improved.

(55) FIG. 14 is a cross-sectional view showing an LCD according to a comparative example 1. FIG. 15 is a cross-sectional view showing an LCD according to a comparative example 2. FIG. 16 shows a light profile image of the LCD according to the comparative example 1. FIG. 17 shows a light profile image of the LCD according to the comparative example 2. FIG. 18 shows a light profile image of the LCD according to an embodiment of the present disclosure.

(56) With reference to FIG. 14, in the LCD according to the comparative example 1, an upper polarizer is positioned on the top surface of an LCD panel. A lower polarizer, to which an upper protection layer and a lower protection layer are adhered with a core layer interposed therebetween, is adhered to the bottom surface of the LCD panel by an adhesive layer. A diffusion sheet and two prism sheets are positioned under the LCD panel, thereby forming the LCD.

(57) With reference to FIG. 15, in the LCD according to the comparative example 2, an upper polarizer is positioned on the top surface of the LCD panel. A lower polarizer, to which an upper protection layer and a lower protection layer are adhered with a core layer interposed therebetween, is adhered to the bottom surface of the LCD panel by an adhesive layer. A diffusion sheet is adhered to the bottom surface of the lower polarizer by an adhesive layer not including a bead. A first prism sheet is adhered to the bottom surface of the diffusion sheet. A second prism sheet is spaced apart from the first sheet without adhering to the first sheet (in contrast to the FIG. 14 comparative example 1), thereby forming the LCD.

(58) The LCD according to an embodiment of the present disclosure that is referred to for the FIG. 18 light profile image corresponds to the LCD of the FIG. 5 example, according to an embodiment of the present disclosure.

(59) FIG. 16 shows a light profile in which light is uniformly distributed in the LCD of the comparative example. In this case, brightness of the comparative example 1 was 100% in the experiment. FIG. 17 shows a light profile in the LCD of the comparative example 2, wherein the uniformity of light is lower than that of the comparative example 1 and brightness was 88% in the experiment, compared to the 100% brightness of the comparative example 1. FIG. 18 shows a light profile in the LCD according to an embodiment of the present disclosure, wherein light uniformity is similar to that of the comparative example 1 and brightness was also 98% in the experiment, which is similar to the brightness 100% of the comparative example 1.

(60) The experiment results reveal that the LCD according to an embodiment of the present disclosure had light uniformity or brightness equal to that of the comparative example 1 in which the lower polarizer and the diffusion sheet were separated. Furthermore, the LCD according to an embodiment of the present disclosure had significantly improved light uniformity and an 10% increase of brightness compared to the comparative example 2 in which the lower polarizer and the diffusion sheet had adhered together by the adhesive layer that does not include beads.

(61) As described above, the optical film according to an embodiment of the present disclosure has an advantage in that it can diffuse light incident from the lower side by refracting the light at the interface of the diffusion sheet and the air layer and at the interface of the air layer and the adhesive layer because the adhesive layer including the plurality of beads is formed between the lower polarizer and the diffusion sheet. Furthermore, the LCD according to an embodiment of the present disclosure has an advantage in that it can prevent a moir phenomenon from occurring by securing the haze of the diffusion sheet because it includes the optical film. Furthermore, the LCD according to an embodiment of the present disclosure has advantages in that it can omit separate optical films because the lower polarizer, the adhesive layer, the diffusion sheet, and the prism sheet are integrated under the LCD panel and it can be made as thin as possible because the thickness of the backlight unit can be reduced.

(62) It will be apparent to those skilled in the art that various modifications and variations may be made in the present disclosure without departing from the spirit or scope of the invention. Thus, it is intended that embodiments of the present disclosure cover the modifications and variations of this invention provided they come within the scope of the appended claims and their equivalents.